Lyondellbasell Icorene 2550 Uv Yew 2422 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 874052
    Manufacturer LyondellBasell
    Trade Name Icorene
    Grade 2550 UV+ YEW 2422
    Material Type Polyethylene, Linear Low Density (LLDPE)
    Density 0.924 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 18.0 MPa
    Elongation At Break 700%
    Flexural Modulus 180 MPa
    Vicat Softening Temperature 90°C
    Melting Point 120°C
    Uv Stabilization Yes
    Processing Method Rotational Molding
    Form Powder

    As an accredited LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg bags, 40 bags per pallet (1,000 kg), or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 2550 UV+ YEW 2422 Linear Low Density Polyethylene in palletized 25 kg bags, strapped.
    Shipping LyondellBasell Icorene 2550 UV+ YEW 2422 is a non-hazardous linear low density polyethylene resin. It is typically shipped as pellets in 25 kg bags, palletized and stretch-wrapped, or in bulk bags, trucks, or railcars. Store dry, cool, and out of direct sunlight. No dangerous goods placards required.
    Storage Store LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed and palletized to prevent moisture, contamination, and dust. Avoid excessive stacking pressure and prolonged high temperatures. Use first-in, first-out rotation, and store separately from food, feed, and drinking water.
    Shelf Life Shelf life: 24 months from manufacture if stored in original packaging in a cool, dry area, away from direct sunlight.
    Application of LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density

    Application scope for LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density. The grade is supplied as a rotomolding powder and the downstream sectors included below are rotational molding conversion lines only; film, injection molding, and blow molding are excluded because the powder consolidation mechanism differs and the dry-blend particle size distribution is not optimized for those processes. Grade-specific density, melt flow rate, and powder mesh distribution are controlled by the manufacturer and supplied on the certificate of analysis. When mechanical data are used for product design, relevant test methods include ISO 1133-1, ISO 1183-1, ISO 527-2, and DIN EN ISO 527-2. Two operational boundaries apply before processing: powder exposed to relative humidity above 60% is pre-dried at 60–70 °C for 2–4 h, and amine-based additives are not introduced into the dry-blend without prior weathering validation under ISO 4892-2 because amine-bearing stabilizers can interact with the pre-compounded UV+ system.

    What Limits Peak Internal Air Temperature in the Rotomolding of Water Storage Tanks?

    In the rotomolding of potable water storage tanks, underground cisterns, and municipal distribution node liners, the primary processing conflict is the relationship between peak internal air temperature and residual environmental stress crack resistance. The formulation addition ratio is 100 wt% LyondellBasell Icorene 2550 UV+ YEW 2422 for natural wall sections; when a tinted or upgraded stabilizer shell is specified, an LLDPE-based masterbatch is added at 2–4 wt% in a paddle-type dry-blend mixer, with the letdown kept below 5 wt% to prevent dry-blend segregation and loss of wall adhesion. Compliance verification for potable water contact typically references AS/NZS 4020, NSF/ANSI 61, and EU 10/2011 for migration testing, while the olefin polymer base is evaluated under FDA 21 CFR 177.1520 when the article falls within the food-contact category. Wall sections for water tanks are typically 6–25 mm, and finished product types include cylindrical potable water tanks, underground cistern bodies, loft tanks, and manway shells.

    The downstream rotational molding line is configured around the peak internal air temperature limitation rather than oven setpoint alone. Shuttle and carousel machines are fitted with cast aluminum or machined steel molds that rotate at a biaxial ratio of 4:1 to 5:1. In production, forced-air or infrared oven temperatures are usually set at 280–300 °C, but the oven residence time is trimmed so that the peak internal air temperature reaches 200–220 °C. Operation below 190 °C is rejected because the inner wall exhibits under-consolidated powder residues and pinhole porosity under light-box inspection; operation above 225–230 °C accelerates thermo-oxidative degradation and shortens environmental stress crack resistance life measured by ISO 22088-3. Cooling is sequenced from forced air at 15–25 °C to fine water mist only after the outer mold skin falls below 150 °C, preventing differential shrinkage that can cause dome and lid assemblies to mismatch gasket seats. The finished tank is demolded at ≤80 °C and inspected for wall thickness distribution using ultrasonic thickness gauges or sectioned first-off parts.

    Because chemical attack in storage occurs predominantly at weld lines of linear PE fabricated tanks, agricultural sprayer and fertigation vessels are rotomolded as seamless shroud-formed shells. The formulation addition ratio for the structural shell is 100 wt% Icorene 2550 UV+ YEW 2422; a carbon black or colored LLDPE masterbatch is introduced at 2–3 wt%, and an additional hindered amine light stabilizer masterbatch is added at 1–2 wt% only where extended equatorial UV exposure exceeds the baseline UV+ package. Compliance for agricultural chemical containment is demonstrated by chemical resistance testing under ISO 175:2010 using representative pesticide, fertilizer, and adjuvant formulations, with stress crack resistance evaluated by ISO 22088-3 on specimens cut from the tank wall. The downstream production process is rotational molding: the powder is dry-blended in a paddle mixer, charged into cast aluminum or machined steel molds, heated in an oven at 270–310 °C, and rotated at 4:1 to 5:1 biaxial ratio until the peak internal air temperature reaches 195–220 °C. Wall sections are generally 5–12 mm, and forced-air cooling is applied until demolding at ≤80 °C. Finished product types include sprayer tanks, fertigation vessels, water treatment chemical dosing tanks, and foam marker tanks.

    Without Post-Mould Painting, Outdoor Street Furniture Demands a High-UV LLDPE Shell

    Outdoor furniture shells—public seating, modular benches, litter bin bodies, and park table tops—are rotomolded dry-blend from 100 wt% Icorene 2550 UV+ YEW 2422 with a pigment masterbatch addition ratio of 2–3 wt%; additional hindered amine light stabilizer masterbatch is restricted to 0.5–1.5 wt% because surface bloom from excess stabilizer can reduce adhesion of after-applied graphics. Compliance for public seating and table surfaces is referenced to EN 581-1:2017 and EN 581-3:2017 for safety, while accessible components intended for children are tested under EN 1176-1:2017. UV weathering is verified by ISO 4892-2 exposure cycles with color change and impact retention measured at the exposure level specified in the purchaser’s outdoor specification. The downstream production process uses rotational molding machines with mold surface textures to produce grained or matte finishes; oven setpoints are 280–300 °C, peak internal air temperature is controlled to 195–215 °C, wall thicknesses range 6–10 mm, and demolding occurs at ≤70 °C to avoid warping of wide seating surfaces. Finished product types include street benches, picnic table tops, litter bin shells, and modular planter bodies.

    Rotational molding sectorWall thicknessOven setpointPeak internal air temperatureBiaxial rotation ratioDemolding temperature
    Potable water storage6–25 mm280–300 °C200–220 °C4:1–5:1≤80 °C
    Agricultural chemical vessels5–12 mm270–310 °C195–220 °C4:1–5:1≤80 °C
    Outdoor street furniture6–10 mm280–300 °C195–215 °C4:1≤70 °C
    Marine buoy and floating dock shells5–8 mm280–300 °C195–215 °C4:1≤70 °C
    Insulated cold chain boxes6–12 mm280–310 °C195–220 °C4:1≤80 °C
    Playground structural shells6–10 mm280–300 °C195–215 °C4:1≤70 °C

    In marine buoy and floating dock production, closed-cell buoy hull shells are rotomolded from linear low density polyethylene because the wall must absorb berthing impact at low temperature without notch propagation. The formulation addition ratio is 100 wt% Icorene 2550 UV+ YEW 2422; a UV masterbatch is added at 1–2 wt% when the buoy color must survive extended saltwater UV exposure. The shell wall is typically 5–8 mm; below 4 mm, puncture impact energy during docking can exceed the material’s low-temperature ductile failure threshold, and above 10 mm, cooling gradients in the buoy hull create internal voids at the molded-in lift eyes. Material evaluation for low-temperature impact is carried out by ISO 6603-2 at -30 °C; UV resistance is assessed by ISO 4892-2; water absorption is measured under ISO 62. Downstream production uses shuttle or carousel rotational molding machines, cast aluminum molds with internal air channels for lift eye core pins, oven setpoints of 280–300 °C, rotation ratio 4:1, and peak internal air temperature of 195–215 °C. Cooling is forced air initially, followed by water mist only after the shell reaches 150 °C. Finished product types include navigational buoy bodies, floating dock segments, raft fender shells, and aquaculture float collars.

    When insulated fish boxes and cold chain totes are exposed to repeated hot-water sanitation cycles, the rotomolded wall must resist stress cracking at internal corners while providing a seamless hygienic surface. The formulation addition ratio for the shell is 100 wt% Icorene 2550 UV+ YEW 2422; color masterbatch is added at 2–3 wt%, and an internal mold release additive is dosed at 0.1–0.5 wt% only when demolding undercuts are present. Compliance for food-contact use references FDA 21 CFR 177.1520 and EU 10/2011, with cleaning validation performed under the purchaser’s specified sanitation protocol. The downstream production process is rotational molding: the powder is dry-blended in a paddle mixer, charged into molds with biaxial rotation ratio 4:1, heated at 280–310 °C, and held to a peak internal air temperature of 195–220 °C. Wall sections of 6–12 mm are cooled in forced air at 15–25 °C; demolding occurs at ≤80 °C. Finished product types include insulated fish boxes, cold chain tote shells, industrial transport bins, and pallet body moldings.

    SectorCompliance referencesCritical test methodVerification boundary
    Potable water storageAS/NZS 4020, NSF/ANSI 61, EU 10/2011, FDA 21 CFR 177.1520ISO 22088-3Peak internal air temperature 200–220 °C; ESCR on tank wall specimens
    Agricultural chemical vesselsISO 175:2010, ISO 22088-3ISO 175:2010Mass change after immersion per purchaser chemical matrix
    Outdoor street furnitureEN 581-1:2017, EN 581-3:2017, EN 1176-1:2017ISO 4892-2UV exposure level per purchaser specification
    Marine buoy and floating dock shellsISO 6603-2, ISO 4892-2, ISO 62ISO 6603-2Impact at -30 °C; wall ≥5 mm
    Insulated cold chain boxesFDA 21 CFR 177.1520, EU 10/2011FDA 21 CFR 177.1520Food-contact migration according to final wall thickness
    Playground structural shellsEN 1176-1:2017, ASTM F1487-21, EN 71-3EN 71-3Heavy-metal migration limits for accessible surfaces

    Under EN 1176, Rotomolded Playground Shells Cannot Use Post-Consumer Fillers in Structural Layers

    Playground structural shells—slides, climbing elements, tunnel sections, and spring rider bodies—are rotomolded from 100 wt% Icorene 2550 UV+ YEW 2422; pigment masterbatch addition ratio is 2–3 wt%, and post-consumer or commingled filler is not introduced into the structural layer unless the finished article is revalidated under the relevant parts of EN 1176 or ASTM F1487-21. Compliance for accessible surfaces includes heavy-metal migration testing under EN 71-3, REACH SVHC disclosure, and flammability assessment where the playground equipment falls within EN 1176-1:2017. The downstream production process uses shuttle-type rotational molding machines with biaxial rotation ratio 4:1, oven setpoints of 280–300 °C, peak internal air temperature 195–215 °C, and wall thicknesses of 6–10 mm to balance impact toughness and cycle time. Molds with molded-in grip surfaces or textured shells require parting-line venting to avoid trapped gas; demolding is conducted at ≤70 °C to prevent distortion of thin curved slide shells. Finished product types include slide shells, tunnel sections, play panel bodies, and spring rider bases.

    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ YEW 2422 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 UV+ YEW 2422 is a linear low density polyethylene (LLDPE) powder supplied for biaxial rotational moulding. The manufacturer-reported typical melt flow rate is 5.5 g/10 min when determined at 190°C under a 2.16 kg load in accordance with ISO 1133-1:2022, and the nominal density is 0.925 g/cm³ when measured to ISO 1183-1. The YEW 2422 identifier denotes a light stabiliser and ultraviolet absorber package incorporated into the powder, not a post-mould coating. The material is therefore positioned for hollow parts that require outdoor weathering resistance, low-temperature impact, and resistance to environmental stress cracking rather than for high-stiffness structural sections.

    Selected typical physical property values reported for LyondellBasell Icorene 2550 UV+ YEW 2422
    PropertyTest methodTypical value
    DensityISO 1183-10.925 g/cm³
    Melt flow rateISO 1133-1:20225.5 g/10 min
    Tensile yield strengthISO 527-212 MPa
    Tensile elongation at breakISO 527-2>800%
    Flexural modulusISO 178220 MPa
    Environmental stress-crack resistance, F50ASTM D1693>1000 h

    The values listed above are typical lot averages, not minimum or maximum specification limits. Lot-specific certificates of analysis should be used for release testing because additive loading and slight molecular variation can affect final part performance.

    What distinguishes the 2550 UV+ YEW 2422 package from standard rotomoulding LLDPE powders?

    The principal difference is the stabiliser system rather than the base polymer architecture. A standard LLDPE powder with the same melt flow rate and density can undergo photo-oxidative chain scission at exposed surfaces, generating carbonyl species and reducing tensile elongation after outdoor exposure. The UV+ YEW 2422 package combines light stabilisation and ultraviolet absorption mechanisms, but the exact composition and loading are not disclosed on the public datasheet. Outdoor validation should therefore be performed according to ISO 4892-2 or ASTM D2565 using the final wall thickness and pigment package. For agricultural tanks and outdoor furniture, the relevant acceptance criterion is typically retained elongation at break under ISO 527-2, not visual colour shift alone.

    Photo-oxidation of unstabilised LLDPE proceeds through free-radical chain reactions initiated by UV absorption at carbonyl and catalyst residues. The hindered amine stabiliser in the YEW 2422 package functions by scavenging peroxy radicals, while the UV absorber converts incident UV into heat. The net effect is a slower rate of tensile elongation loss under xenon-arc exposure. For black or white pigmented parts, weathering resistance can be further extended because the pigment screens UV before it reaches the polymer; for unpigmented parts, the stabiliser package carries the full load. Accelerated weathering according to ISO 4892-2 cycle 1 typically uses a xenon-arc source with 0.35 W/m² irradiance at 340 nm, a black-standard temperature of 65°C, and a 102:18 min dry/spray cycle. Published data for this specific configuration is limited, and part-specific exposure testing is required.

    Compared with high-density rotomoulding grades in the 0.940 g/cm³ to 0.945 g/cm³ range, the lower density of this LLDPE grade reduces flexural modulus and softening temperature but increases low-temperature impact and environmental stress-crack resistance. Compared with a low-flow LLDPE rotomoulding powder with melt flow rate below 3 g/10 min, the 5.5 g/10 min flow allows shorter oven residence and better reproduction of ribs, inserts, and textured surfaces in complex tooling. The trade-off is a lower melt viscosity that can contribute to localised thinning at sharp external radii if the heating leg is run too long; mould tooling with generous radii and controlled internal air temperature is recommended.

    The difference between the UV+ YEW 2422 package and a precompounded UV masterbatch approach is also operationally significant. In rotational moulding, dry blending a generic LLDPE powder with a separate UV masterbatch can generate segregation during powder handling, especially in hopper-fed automatic loaders, producing stabiliser concentration gradients across the part. The factory-incorporated YEW 2422 package avoids this segregation risk by fixing the stabiliser distribution before packaging. This is a process reliability distinction that appears as reduced lot-to-lot colour shift and more uniform tensile elongation retention in exposed panels.

    The powder is charged at ambient temperature into a cast or fabricated aluminium mould mounted on a biaxial rotational moulding machine. The primary control variable is the internal air temperature measured by a through-tool thermocouple in the thickest wall section. For this density class, oven set points between 280°C and 320°C are common, while the internal air temperature needed to complete sintering is normally above 200°C. A transferable processing window cannot be established from oven set point alone because mould mass, wall thickness, burner efficiency, and offset-arm speed all affect the temperature lag. On a shuttle-type line with a 3.0 m offset arm, the lag can reach 15–30°C during the first 10 min of heating. Published data for this specific configuration is limited; production-scale optimisation should use internal air temperature traces rather than fixed oven residence time alone.

    When cooling rate is treated as a first-order variable in mould stress development

    Residual stress in rotomoulded LLDPE arises after sintering, during the cooling leg. A slow cooling profile in still air reduces warpage in flat tank sidewalls but extends cycle time and can produce a coarser crystalline population with lower yield stress when measured under ISO 527-2. Forced-air cooling from the outer mould surface lowers demould time but can generate a through-thickness temperature gradient large enough to bow unsupported panels. Many production lines for water tanks and outdoor enclosures use a staged cooling sequence: air cooling to an internal air temperature near 90°C, followed by water mist or forced air until demould. The exact profile should be established by a design-of-experiments approach because the shrinkage anisotropy of LLDPE differs from that of HDPE rotomoulding powders. Warpage should be measured on a flat surface plate against a specified flatness tolerance, using dimensional data after 48 h of ambient conditioning to ISO 291 standard atmospheres.

    In production-scale rotomoulding, two recurring failure modes are observed: corner pinholes in parts with wall thickness below 3 mm when the peak internal air temperature is reached too late, and warpage in large flat panels when the cooling leg is forced-air dominant from one side. Both modes are usually traceable to the temperature and cooling gradient rather than to the powder itself. For an oven with infrared pyrometer control, the mould surface temperature can exceed the internal air temperature by 30–50°C early in the cycle, making single-point infrared measurement insufficient for the sintering endpoint.

    Chemical resistance and environmental stress-cracking benchmarks

    The grade’s environmental stress-crack resistance is reported above 1000 h F50 under ASTM D1693 in 100% Igepal. This property is relevant for rotationally moulded agricultural sprayer tanks, chemical storage bunds, and intermediate bulk containers where slow crack growth is the limiting failure mode. The behaviour in aliphatic hydrocarbons, dilute acids, and dilute alkalis at room temperature follows general LLDPE immersion trends; for oxidising acids, halogens, and aromatic solvents, component-specific immersion testing under ASTM D543 or ISO 22088-3 at the actual service temperature is required. Continuous exposure to strong oxidising media above 40°C is outside the normal service boundary unless validated by part-specific testing.

    The grade is not recommended for dry blending with copper-based antimicrobial powders unless oxidative induction time testing under ISO 11357-6 shows sufficient retained stabiliser performance, because copper ions can catalyse thermo-oxidative degradation of polyethylene. For potable water contact, end-use suitability must be confirmed under FDA 21 CFR 177.1520 or the applicable national regulation; lot-specific migration compliance is not implied by the standard datasheet.

    Processing window indicators for biaxial rotational moulding equipment

    Sintering is controlled by powder particle size distribution, bulk density, and melt flow rate. The fine-particle fraction affects mould fill consistency in narrow channels; an excessive fines fraction can increase static adhesion and reduce dry-flow through automatic powder loaders. The grade is supplied with a dry-flow additive system intended for consistent dispensing. Moisture absorption of LLDPE powder is low, but condensation on cold powder in high-humidity environments can produce surface porosity. Storage below 40°C in a dry area away from direct sunlight is required to avoid premature thermal and photo-oxidative consumption of the stabiliser package.

    For parts with nominal wall thickness between 4 mm and 12 mm, oven residence times commonly range from 18 min to 35 min depending on mould mass and burner efficiency. The oven residence time is not directly transferable between machines; the internal air temperature at the end of heating is the transferable parameter. A peak internal air temperature above 220°C can cause oxidation, discolouration, and loss of impact properties in thin sections. A minimum internal air temperature below 190°C can produce incomplete sintering and pinholes at sharp corners. These boundaries should be confirmed by instrumented trials on the actual tooling.

    Agricultural sprayer tanks and outdoor enclosure parts moulded from this grade rely on the combination of UV stabilisation and environmental stress-crack resistance. The grade is also used for outdoor playground components, buoys, and water tank lids where surface cracking after prolonged sunlight exposure is a known failure mode. In applications requiring higher modulus than the 0.925 g/cm³ density class, a high-density rotomoulding grade is specified instead. In applications requiring stiffness at continuous temperature above 50°C, a crosslinkable rotomoulding polyethylene or a polypropylene-based rotomoulding material may be required.