| HS Code | 906271 |
| Manufacturer | LyondellBasell |
| Product Name | Icorene 2550 UV+ YEW 2240 |
| Material Type | Polyethylene, Linear Low Density (LLDPE) |
| Density | 0.925 g/cm³ |
| Melt Flow Rate | 0.8 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Vicat Softening Temperature | 100°C |
| Melting Temperature | 125°C |
| Hardness Shore D | 50 |
| Brittleness Temperature | < -70°C |
| Thermal Expansion Coefficient | 2.0E-4 1/°C |
| Water Absorption | < 0.01% |
| Uv Stabilization | Yes |
As an accredited LyondellBasell Icorene 2550 UV+ YEW 2240 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg); also available in 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL: LyondellBasell Icorene 2550 UV+ YEW 2240 Linear Low Density Polyethylene, palletized bagged resin, shrink-wrapped, stacked, secured in dry container. |
| Shipping | LyondellBasell Icorene 2550 UV+ YEW 2240 LLDPE ships as non-hazardous polyethylene pellets in 25 kg bags, big bags, or octabins on pallets. Transport in clean, dry trucks or containers. Store away from moisture, heat, and direct sunlight. No special dangerous goods documentation required. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed and pallets stable to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures that may cause softening, caking, or fusion. Use first-in, first-out stock rotation. Do not store near food, feed, or incompatible materials. Protect from physical damage. Refer to SDS for handling. |
| Shelf Life | No specific shelf life; stable under normal storage conditions if kept cool, dry, and away from sunlight/heat. |
In rotational moulding of agricultural chemical storage tanks, the selection of Icorene 2550 UV+ YEW 2240 is governed by nominal density of 0.935 g/cm³ under ISO 1183-1:2019 and melt flow rate of 2.5 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. Compliance reference: ASTM D1998-15 for polyethylene upright storage tanks, ISO 16101:2004 for compatibility testing of plastics packaging for dangerous goods, and UN 1H2 design-type qualification where the moulded article is used as an intermediate bulk container. The blend ratio is 100 parts by mass of the as-supplied UV-stabilised LLDPE powder; clean regrind from the same grade may be incorporated up to 20 wt%, while dry-blend colour masterbatch is limited to 0.3 wt% to avoid measurable loss in environmental stress crack resistance under ASTM D1693-15e1. Moulding proceeds at oven set temperatures of 280–300 °C; peak internal air temperature is held between 195 °C and 205 °C, with cooling rates of 10–15 °C/min through the crystalline solidification zone until demoulding at 70 °C or below. If powder is exposed to relative humidity above 60%, it is pre-dried at 60 °C for 2 h before charging to prevent steam porosity along the inner wall. Rotomoulded outputs include saddle sprayer tanks, dual-compartment agricultural IBCs, secondary containment sumps, and horizontal transport tanks of 500–10 000 L nominal capacity.
The design of rotationally moulded marine hulls and flotation chambers is governed by Directive 2013/53/EU for recreational craft and ISO 12215-1:2019 structural scantlings for monohull small craft, with flotation modules checked against applicable buoyancy stability criteria. The rotomoulding charge is 100 parts by mass of Icorene 2550 UV+ YEW 2240; where a foam co-fill is required to reduce part density, a chemical blowing agent masterbatch is dry-blended at 0.8–1.2 wt% to target apparent core density of 0.55–0.65 g/cm³. The moulding cycle differs from solid-walled tanks: cavity temperature overshoot is deliberately limited to 195–200 °C because higher internal air temperature destabilises foam cell structure and produces skin-layer thickness variation across a 4:1 biaxial arm ratio. On a three-arm rock-and-roll machine with 1.8 m swing diameter, demoulding is postponed until skin temperature falls below 60 °C; premature release at 80 °C causes warpage and weld-line cracking at the insert flange. End products comprise kayak hulls, rotomoulded pontoon floats, aquaculture cage floats, fender shells, and dock modules. Published multi-year weathering data for the specific YEW 2240 colour pack under ASTM D4329-21 cycle A is limited; the UV+ package is not a substitute for periodic inspection of load-bearing marine parts.
Because sustained soil pressure, intermittent hydrostatic loading, and dissolved road salts control service life, underground stormwater chambers moulded from LLDPE require the highest practical environmental stress crack resistance. Compliance reference: ASTM F1759-97(2018) for subsurface polyethylene structures and EN 13598-1:2010 for plastics manholes and inspection chambers in non-pressure drainage. The controlling material property is ESCR under ISO 22088-3 and ASTM D1693-15e1 Condition A. Charge composition is maintained at 100 parts by mass Icorene 2550 UV+ YEW 2240 with regrind limited to 10 wt%; carbon black masterbatch at 0.5–0.8 wt% is permitted if a black shell is specified, but no calcium carbonate filler is added because elastic modulus rises and low-temperature ductility falls below the ASTM D5276-19 dart impact threshold. Processing uses multi-part CNC steel tools on carousel rotomoulding machines; wall thickness is held at 8–12 mm, with stiffening ribs moulded integrally rather than fastened. After oven dwell, the shell is cooled at ≤15 °C/min until core temperature reaches 65 °C; faster cooling induces surface tensile quench stresses and increases the risk of environmental stress cracking at rib roots. Manufactured articles include stormwater detention modules, inspection chambers, road drainage sumps, leachate collection troughs, and underground utility covers.
| Application sector | Primary standard | Secondary standard or test method |
|---|---|---|
| Agricultural chemical tanks | ASTM D1998-15 | ISO 16101:2004, UN 1H2 |
| Marine hulls and flotation | Directive 2013/53/EU | ISO 12215-1:2019 |
| Underground stormwater chambers | ASTM F1759-97(2018) | EN 13598-1:2010 |
| Distribution pallets and hoppers | ISO 8611-1:2021 | EC 1935/2004 if food contact claimed |
| Exterior play components | EN 71-3:2019+A1:2021 | ASTM F1487-21 |
| Cold-chain insulated bodies | EC 1935/2004 | 21 CFR 177.1520 |
For distribution pallets, collapsible bulk containers, and gravity hoppers in pharmaceutical, chemical, and dry-food logistics, the process route begins with dry powder charging into cast aluminium tools fitted with fork-tunnel inserts. Compliance is assessed under ISO 8611-1:2021 pallet test methods, with hygienic pallets additionally validated against EC 1935/2004 if food contact is claimed; 21 CFR 177.1520 applies only where the supplier’s regulatory dossier confirms the grade-specific formulation. The powder charge consists of 100 parts by mass of the LLDPE powder; regrind addition may be increased to 25 wt% because wall ductility remains adequate, but reprocessed material must be sourced from the same product to avoid altering the UV additive package. Moulding at 285 °C oven temperature and peak internal air temperature of 198 °C produces a 6–10 mm wall; after cooling to 70 °C, the shell is trimmed by five-axis CNC equipment to maintain flat deck tolerances of ±1 mm across 1.2 m deck spans. The resulting components include nestable distribution pallets, collapsible hopper boxes, drum cradles, dunnage trays, and stackable bin shells.
Outdoor play components and street furniture shells rotomoulded from Icorene 2550 UV+ YEW 2240 are specified where colour retention, tactile surfaces, and ductile impact response after weathering are required. Compliance standards include EN 71-3:2019+A1:2021 for migration of certain elements, ISO 8124-1:2018 for mechanical and physical properties of toys, and ASTM F1487-21 for public playground equipment. The dry-blend is 100 parts by mass of the as-supplied UV-stabilised powder; additional lightfast pigment masterbatch is limited to 0.5 wt% because higher pigment loadings may reduce ultraviolet screening of the underlying polymer matrix. Slides, panels, and ride-on shells are moulded in electro-polished aluminium cavities at 280–290 °C, with peak internal air temperature restricted to 195 °C; the mould is then air-cooled at 12 °C/min to 55 °C before release to avoid sink marks on visible surfaces. Inserts for handrails and mounting bosses are positioned as 304 stainless steel or brass components and are encapsulated during the moulding cycle rather than retrofitted. Outputs include slide hoods, playhouse panels, spring rider seats, outdoor bench shells, and modular planters. The operational boundary is that continuous service above 60 °C surface temperature is not recommended because LLDPE softens and creep under load becomes measurable.
Within cold-chain logistics, fish boxes, insulated transport crates, and double-wall lidding constitute a downstream segment in which Icorene 2550 UV+ YEW 2240 is used as the outer shell surrounding an insulating core. Food-contact status must be verified for each finished article; the relevant references are EC 1935/2004 for framework compliance and 21 CFR 177.1520(c) for olefin polymers as articles or components of food-contact materials. Outer skin composition is 100 parts by mass of the LLDPE powder; regrind is restricted to 10 wt% for the inner wall and is not used on the product-contact surface unless the plant’s hygiene validation covers post-consumer reprocessing. The downstream process is dual-step: a rotational moulding cycle at 270–285 °C forms the double-wall shell and lidding, after which polyurethane foam of 2.0–5.0 wt% of total part mass is injected into the cavity through sealed ports; overfilling beyond 5.0 wt% causes shell distortion. Finished articles include tubs for fresh fish transport, insulated pallet boxes for pharmaceutical intermediates, double-wall lids for dairy distribution, and temperature-controlled dunnage trays. The operational limitation is that hot-fill media above 65 °C is not recommended because shell stiffness drops and vacuum deformation may occur during subsequent cooling.
Competitive LyondellBasell Icorene 2550 UV+ YEW 2240 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 UV+ YEW 2240 is a linear low density polyethylene (LLDPE) resin engineered for rotational molding processes in which low-shear melt consolidation and controlled wall thickness distribution are primary requirements. The product designation encodes multiple technical layers: the Icorene trade name identifies LyondellBasell’s dedicated ethylene copolymer platform, the numeric suffix “2550” denotes a specific density–melt flow configuration within that platform, the “UV+” qualifier signifies an integrated ultraviolet stabilization package formulated for prolonged outdoor exposure, and “YEW 2240” designates the pigment dispersion and additive carrier system. Rotational molding grades of LLDPE typically occupy a density envelope of 0.915 g/cm³ to 0.940 g/cm³, measured in accordance with ISO 1183-1:2019, and exhibit melt mass-flow rate values between 2 g/10 min and 8 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022. The copolymer architecture—incorporating a butene or hexene comonomer along the polyethylene backbone—produces short-chain branching that depresses crystallinity relative to high-density polyethylene (HDPE) homopolymer while retaining sufficient modulus for load-bearing hollow parts. Published technical data sheets for this specific Icorene configuration should be consulted for batch-level property verification, because rotational molding resin performance is materially influenced by part wall thickness, oven temperature profiling, and cooling rate on production-scale equipment.
The UV+ designation indicates that the resin incorporates a synergistic stabilizer package rather than a single hindered amine light stabilizer (HALS) species. In outdoor rotational molded parts—storage tanks, agricultural reservoirs, playground components, and marine buoys—ultraviolet radiation in the 290 nm to 400 nm range initiates photo-oxidative chain scission in polyethylene. This degradation mechanism proceeds through free-radical intermediates, leading to carbonyl formation, embrittlement, surface crazing, and eventual loss of tensile elongation. The UV+ system in Icorene 2550 UV+ YEW 2240 combines a primary HALS component, which scavenges free radicals through the cyclic Denisov mechanism, with a UV absorber that dissipates incident photon energy as thermal radiation. The HALS component operates at a concentration range of 0.05 wt% to 0.30 wt% within the compounded resin, and its efficiency in LLDPE matrices is retained across multiple thermal histories because the stabilizer does not undergo irreversible consumption during processing at typical rotational molding peak internal air temperatures of 180 °C to 220 °C. Xenon-arc accelerated weathering per ISO 4892-2 is the conventional test used to quantify retention of elongation at break and the development of surface oxidation index. For rotationally molded LLDPE parts intended for 5- to 10-year exterior service in temperate climates, UV-stabilized grades demonstrate significantly lower carbonyl index growth rates than unmodified control samples, though published data for the specific YEW 2240 formulation at defined wall thicknesses is limited and should be established through project-specific weathering trials.
Process conditions for Icorene 2550 UV+ YEW 2240 on multi-axis rotational molding machines are governed by the low-shear rheology of the resin. Unlike injection molding, where shear rates in the gate region exceed 10³ s⁻¹, rotational molding imposes uniformly low shear on the melt pool, typically below 10 s⁻¹. The low-shear viscosity of LLDPE at processing temperatures is therefore a more meaningful process indicator than melt flow rate alone. On biaxial carousel machines with mold swing diameters of 1.5 m to 3.0 m, the oven dwell time required to achieve a fully coalesced part is a function of mold wall thermal conductivity, part wall thickness, and the sintering temperature of the resin. For Icorene 2550 UV+ YEW 2240, the recommended processing window begins with peak internal air temperature of approximately 185 °C to 200 °C, sustained for a period determined by wall thickness, followed by controlled cooling through forced air and water mist. The resin’s sintering behavior follows the standard LLDPE coalescence model first described by Frenkel and more recently validated through rheological and surface-tension measurements on rotational molding grades. Insufficient peak temperature results in incomplete densification and residual internal voids at the wall core; excessive peak temperature accelerates oxidative degradation and reduces impact strength. Pre-drying is generally not required when the resin is stored in sealed, unopened containers at ambient relative humidity below 60%. If storage conditions exceed that threshold, moisture absorption on pellet surfaces is possible and 2 h of forced-air drying at 60 °C is recommended prior to grinding.
The selection of Icorene 2550 UV+ YEW 2240 over a conventional butene-copolymer LLDPE or an HDPE rotational molding grade involves trade-offs among low-temperature impact resistance, stiffness, environmental stress crack resistance (ESCR), and UV durability. LLDPE grades produced with butene comonomer typically exhibit density values of 0.918 g/cm³ to 0.926 g/cm³ and provide superior low-temperature impact performance relative to HDPE homopolymer, which exhibits density values of 0.940 g/cm³ to 0.950 g/cm³ and correspondingly higher flexural modulus. Icorene 2550 UV+ YEW 2240 occupies the intermediate density region where impact strength at -20 °C, measured as notched Izod per ISO 180:2023, can exceed 40 kJ/m² for properly molded specimens while flexural modulus falls between 250 MPa and 450 MPa per ISO 178:2019. These ranges are family-typical rather than grade-specific and should be verified against the supplier technical data sheet. In ESCR testing using a 10% Igepal CO-630 solution at 50 °C per ASTM D1693, LLDPE copolymer grades substantially outperform HDPE homopolymer because short-chain branching interrupts crystalline continuity and impedes slow crack growth. This property is critical in rotational molded chemical storage tanks and agricultural sprayer tanks, where hoop stress and internal pressure fluctuations create sustained load conditions. Compared to metallocene-catalyzed LLDPE grades, Icorene 2550 UV+ YEW 2240 is engineered to balance processability on conventional rotational molding equipment with acceptable mechanical property retention, though published comparative data for the specific YEW 2240 variant at multi-year weathering intervals is limited.
Compliance for Icorene 2550 UV+ YEW 2240 spans multiple regulatory and industry standards relevant to end-use markets. Under European chemical regulation, the base polyethylene resin complies with REACH registration requirements as a polymer, with the UV stabilizers and pigment components subject to substance-level registration where applicable. For potable water contact applications, the resin must be evaluated against national implementation standards derived from EU Regulation 10/2011 and its amendments, which specify overall migration limits of 10 mg/dm² for plastic materials intended for repeated food-contact use. In agricultural tank applications, compliance with ISO 23320 series standards for chemical suitability of plastics is often required. The UV stabilizer system must also satisfy the active substance requirements under EU Regulation 528/2012 only if the product is intended for biocidal claim-based applications, which is typically not the case for passive UV-protected polyethylene parts. For parts destined for use in the United States, the resin’s food-contact status should be confirmed against 21 CFR 177.1520, which governs olefin polymers for repeated-use food-contact articles. The YEW 2240 pigment package must be verified against ISO 787 series methods for pigment dispersion quality when color consistency is a part acceptance criterion.
The YEW 2240 additive carrier is not an inert component; it functions as both a pigment dispersion vehicle and a low-molecular-weight diluent that modifies the melt viscosity of the compound. In rotational molding, the pigment and carrier system is pre-compounded into the resin rather than dry-mixed at the feed hopper, ensuring consistent color development and preventing localized pigment agglomeration during the grinding step. However, the presence of a carrier resin with a melt flow rate higher than the base LLDPE can create local viscosity gradients during the sintering phase. In molds with complex internal baffles or sharp corner radii below 12 mm, these gradients manifest as weld line weakness where opposing melt fronts converge. Weld line strength in LLDPE rotational molded parts is typically evaluated through instrumented dart impact on specimens taken from the convergence zone, per ISO 6603-2, with acceptance criteria set at a minimum energy absorption value relative to the nominal wall area. Mold design parameters—including vent size, parting line geometry, and internal corner radii—interact with the YEW 2240 carrier viscosity to determine whether weld line regions meet specified impact performance. A poorly matched carrier system can reduce impact energy absorption at the weld line by up to 30% relative to the base resin, while a well-matched carrier maintains weld line performance within 10% of nominal. The mold maker’s recommended corner radius standards for LLDPE, which typically call for minimum 9 mm to 12 mm internal radii to avoid stress concentration, should be maintained across all features to avoid compounding the weld line effect.
| Property | LLDPE (Icorene 2550 family) | HDPE Rotomolding Grade | LDPE Rotomolding Grade |
|---|---|---|---|
| Density (ISO 1183-1:2019) | 0.918–0.930 g/cm³ | 0.940–0.950 g/cm³ | 0.915–0.925 g/cm³ |
| Melt mass-flow rate (ISO 1133-1:2022) | 3–7 g/10 min | 2–6 g/10 min | 5–10 g/10 min |
| Notched Izod at 23 °C (ISO 180:2023) | 35–60 kJ/m² | 10–25 kJ/m² | 20–35 kJ/m² |
| Flexural modulus (ISO 178:2019) | 250–450 MPa | 700–1100 MPa | 150–250 MPa |
| ESCR, 10% Igepal CO-630 (ASTM D1693) | >500 h, F50 | 10–100 h, F50 | 50–200 h, F50 |
The comparative property ranges presented in Table 1 are family-typical values drawn from rotational molding industry reference data and are intended for grade-selection purposes only; supplier technical data sheets for specific Icorene grades should take precedence. In rotational molding production environments, measurement of these properties on actual molded panels rather than compression-molded specimens is the accepted practice, because wall thickness control variability in production ovens can exceed ±10% of nominal and directly influences all mechanical property outcomes.
| Compliance Area | Standard or Regulation | Relevant Parameter |
|---|---|---|
| Density measurement | ISO 1183-1:2019 | Method A immersion |
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg |
| Tensile properties | ISO 527-2:2012 | Type 1B specimen |
| Flexural properties | ISO 178:2019 | 3-point bending |
| Notched Izod impact | ISO 180:2023 | Method A, notch radius 0.25 mm |
| Xenon-arc weathering | ISO 4892-2 | Cycle 1, borosilicate inner filter |
| Food contact (EU) | EU Regulation 10/2011 | Overall migration <10 mg/dm² |
| Food contact (US) | 21 CFR 177.1520 | Olefin polymer, repeated use |
Operational boundaries for Icorene 2550 UV+ YEW 2240 include avoidance of combination with pro-oxidant masterbatches, which would negate the UV+ stabilization system by initiating premature chain scission during processing and service. The resin must not be processed at melt temperatures exceeding 260 °C for extended dwell periods, because the HALS component undergoes thermal decomposition at elevated temperatures and the polyethylene backbone begins to form conjugated unsaturation that accelerates photo-oxidative degradation. Storage of finished parts in direct contact with copper or brass fittings should be evaluated for metal-catalyzed oxidative degradation, which occurs through a electron-transfer mechanism at the metal–polymer interface. For pigmented grades such as YEW 2240, color consistency requires controlled grinding temperature during powder production; grinding temperatures above 50 °C on the mill may cause pigment streaking and uneven surface gloss in the final molded part. Production-scale observations on twin-screw compounding lines with an L/D ratio of 40:1 indicate that stabilizer dispersion uniformity is dependent on screw profile elements that provide sufficient distributive mixing without excessive specific energy input that would exceed 0.25 kWh/kg and risk stabilizer degradation.