Lyondellbasell Icorene 2550 Uv Whi 1111 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 409617
    Material Type Polyethylene, Linear Low Density
    Density 0.925 g/cm³
    Melt Flow Rate 2.0 g/10 min
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 18 MPa
    Tensile Elongation At Break 700%
    Flexural Modulus 300 MPa
    Hardness Shore D 50
    Vicat Softening Temperature 100 °C
    Melting Temperature 123 °C
    Uv Stabilization Yes
    Color White

    As an accredited LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene is supplied in 25 kg bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with 25 kg bags of LyondellBasell Icorene 2550 UV+ WHI 1111 Linear Low Density Polyethylene, palletized and secured.
    Shipping Shipping description: LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density is a non-hazardous LLDPE resin. Not DOT, IMDG, or IATA regulated; no UN number, hazard class, or packing group. Ship in sealed bags, octabins, or bulk; keep dry, avoid heat/ignition sources, and follow local transport rules.
    Storage Store in a cool, dry, well-ventilated warehouse, preferably at ambient temperature. Keep original bags/containers sealed, palletized, and off the floor. Protect from direct sunlight, moisture, heat, sparks, flames, and strong oxidizers. Avoid prolonged high temperatures and UV exposure. Maintain good housekeeping, prevent dust generation and contamination, and follow first-in, first-out inventory practices.
    Shelf Life Typically 24 months from date of manufacture when stored in original unopened packaging, cool, dry, and away from direct sunlight.
    Application of LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density

    When Icorene 2550 UV+ WHI 1111 is charged at 100 wt% of the polymer fraction in single-wall and double-wall chemical storage tank rotational molding, the process window is controlled by the relationship between internal air temperature and the oxidative induction time of the pre-compounded UV stabilizer package; peak internal air temperature is ordinarily held at 190–205 °C while the oven set point is maintained between 260 °C and 290 °C on multi-axis carousel equipment. A wall thickness of 6 mm typically requires a plateau of 20–28 min inside the oven, followed by forced-air cooling to 80 °C before water mist is introduced, and demolding is not initiated until the mold surface has fallen below 70 °C to avoid warpage at the tank rim and fitting bosses. Powder stored in open gaylord boxes at ambient relative humidity above 60% should be pre-dried at 60–70 °C for 1 h before charging if surface condensation is observed, although the LLDPE backbone itself is not hygroscopic. The addition ratio for regrind is restricted to 0–20 wt% of the total charge for aggressive oxidizer, strong acid, or surfactant-containing service; for non-aggressive water-like fluids, clean plant regrind from the same grade may be used up to 35 wt% without automatic rejection under the relevant tank specification, but each lot should be re-tested for environmental stress-crack resistance because regrind accelerates crystalline morphology changes. No external UV masterbatch is required in the skin layer because the grade is supplied as UV+ WHI 1111; if custom pigmentation is specified, a PE-matrix color masterbatch is limited to 0.5–1.5 wt% to avoid shifting the melt flow rate beyond the supplier’s published range and to prevent settling of high-density pigments in vertical walls during sintering. Compliance for this end-use is assessed under ASTM D1998-21 for polyethylene upright storage tanks, EN 13575:2012 for rotational molded thermoplastics tanks in chemical service where applicable, and FDA 21 CFR 177.1520(c) when stored substances fall under food-contact jurisdiction; mechanical acceptance is typically based on ISO 527-2:2012 tensile yield stress, ISO 178:2019 flexural modulus, and ASTM D1693-21 Condition B environmental stress-crack resistance. Terminal parts produced under this scenario include vertical cylindrical chemical tanks, secondary containment basins, bunded dosing skids, and double-wall dyke tanks for sodium hypochlorite, ferric chloride, and agricultural surfactant storage, all of which require post-molding dimensional inspection of wall thickness distribution across the lower knuckle radius and fitting plate because thickness variance greater than ±15% of nominal wall at insertion points is a common cause of long-term stress cracking.

    What Regrind Level and Cooling Rate Prevent Warpage in Angled Agricultural Sprayer Tank Ribs?

    Agricultural sprayer tank molding with LLDPE powder differs from cylindrical chemical storage because the mold contains angular baffles, return ribs, and threaded insert bosses that generate differential cooling rates; a multi-axis rotational molding machine is programmed with a primary-to-secondary axis speed ratio that shifts from 2:1 to 5:1 depending on arm position, and the peak internal air temperature is held at 195–205 °C for 22–30 min to ensure powder coalescence in narrow rib cross-sections while avoiding oxidation in the thinnest wall sections. In this scenario the base resin charge is 100 wt% Icorene 2550 UV+ WHI 1111 in the outer skin; same-lot grinder dust and trimmed regrind may be incorporated at 15–25 wt%, but regrind above 25 wt% is not recommended where compliance with ISO 179-1:2010/1eA notched Charpy impact at -20 °C is required because repeated thermal history increases the crystalline fraction and reduces low-temperature ductility at the tank base corner. Chemical resistance of the molded wall against typical agrochemical formulations is evaluated under ISO 175:2010 immersion testing in 2% aqueous simulant solutions of the as-used dopant and carrier solvent; when the tank is used for pesticide or liquid fertilizer transport, the complete part is additionally assessed against EN 13575:2012 static tank requirements and, for European circulation, the relevant UN packaging codes for liquid agricultural products. Process cooling is staged: after oven removal, forced-air cooling is applied until the internal air temperature falls below 100 °C, then intermittent water spray is allowed only when the mold surface is below 90 °C to reduce warpage at baffle intersections; demolding below 70 °C is used because the coefficient of linear thermal expansion of LLDPE produces visible rib sidewall dimples at higher release temperatures. Terminal finished products are tractor-mounted sprayer tanks in the 200–2,000 L range, skid-mounted foam marker tanks, induction hopper bodies, and row-crop spot-sprayer reservoirs, each with molded-in fitting boss dimensions verified by optical comparator against the CAD model before hydrostatic testing.

    In marine and outdoor leisure product molding, the UV-stabilised white LLDPE powder is charged as the outer skin at 100 wt% into cast aluminium or CNC-machined composite moulds used for sit-on-top kayaks, insulated cooler shells, and deck hatch covers; where a foam core is specified, the second charge contains the same base powder with 0.5–1.0 wt% azodicarbonamide-based chemical blowing agent, and the skin layer remains unblown at 100 wt% Icorene 2550 UV+ WHI 1111 to maintain the required surface hardness and UV resistance. The mould is rotated at a primary-to-secondary axis ratio of 4:1, while the oven set point is maintained at 260–285 °C and the internal air temperature is raised to 190–200 °C for a plateau of 18–25 min depending on the largest wall thickness; cooldown is performed with forced air to an internal air temperature of 80 °C, followed by a water-mist step only if the outer skin has reached 90 °C to avoid gas-cell collapse in the core and cosmetic whitening at the skin-core interface. Compliance for food-contact cooler interiors is assessed under FDA 21 CFR 177.1520(c) and, for European Union use, under EU Regulation No. 10/2011 overall migration limits when the food-contact surface is tested in a 10-day exposure at 40 °C with the specified food simulant; outdoor weatherability is screened under ISO 4892-2:2013 xenon-arc exposure, and articles marketed with play value are evaluated under EN 71-3:2019+A1:2021 for migration of specific elements. Terminal products in this segment are rotationally molded kayak hulls, insulated cooler boxes, marine seating shells, baitwell liners, and outdoor furniture shell assemblies; wall-thickness uniformity in the kayak scupper holes and cooler latch bosses is controlled by limiting the demold temperature to below 70 °C and by measuring the finished wall with an ultrasonic gauge at not fewer than 12 defined grid points per part.

    Sequential Charge Timing Governs Air-Gap and Fusion Integrity in Double-Wall Potable Water Tanks

    Double-wall potable water tank manufacturing with this LLDPE grade uses a sequential charge method in which the outer wall charge at 100 wt% Icorene 2550 UV+ WHI 1111 is first sintered to a partial melt plateau at an internal air temperature of 195–200 °C, then the mould is removed from the oven, air-cooled until the internal air temperature falls to 135–145 °C, and a second charge of the same material is introduced before the mould is returned to the oven for a second fusion stage of 15–20 min; this staged thermal history preserves the air gap between the inner and outer skins without causing delamination at the interface because the first skin retains enough residual heat to permit interfacial mixing without slumping under its own weight. The addition ratio for regrind is set at 0–15 wt% and is permitted only from the same potable-water-approved production line; post-consumer regrind is rejected, and any colorant or stabilizer adjustment in the inner potable-water contact layer must be documented under the supplier’s food-contact formulation lock. Oven temperature is maintained at 270–290 °C on shuttle or carousel rotational molding equipment, the rotational ratio is held near 3:1 for finished wall thicknesses between 5 mm and 10 mm, and demold is performed below 70 °C to limit rim distortion. Compliance is established under NSF/ANSI/CAN 61 for drinking water system components, FDA 21 CFR 177.1520(c) for food-contact olefin polymers, and EN 12573-1 or EN 13575:2012 where static thermoplastics tank construction applies; mechanical acceptance often includes ISO 527-2:2012 tensile tests on specimens cut from the tank wall and ISO 1133-1:2022 melt flow rate verification of the charged powder. Terminal products are vertical and slimline rainwater tanks, underground potable water storage cisterns, horizontal emergency water tanks, and mobile water tank shells for remote worksites, all produced without external post-mold welding at the shell and with molded-in inserts for fittings and sanitary pipe connections.

    Aquaculture Float Moulding and UV Stabiliser Retention Limits

    Aquaculture float production uses large aluminium or cast-iron shells with internal diameters exceeding 1 m in many configurations; the LLDPE powder is charged at 100 wt% as the sole polymer, and closed-loop regrind from rejected floats is limited to 10–20 wt% because the UV stabiliser package undergoes incremental depletion during each molding cycle. The process requires oven temperatures of 260–280 °C and peak internal air temperatures of 190–195 °C for wall thicknesses between 4 mm and 8 mm; rotation is maintained at a primary-to-secondary axis ratio of 3:1 to 4:1 on double-arm carousel machines, and final cooling is performed with forced air rather than water because premature water application to a sealed hollow mould can produce internal vacuum and shell deflection at the demold line. Oxidative induction time before and after each molding cycle is measured under ISO 11357-6:2018, and the regrind fraction is only accepted if the post-molding OIT remains above the supplier’s minimum value for the grade; weathering resistance is screened under ISO 4892-2:2013 xenon-arc exposure to verify that the UV+ white stabilizer package has not been diluted below specification. There is no harmonized European product standard for aquaculture floats, so mechanical acceptance is commonly based on ISO 527-2:2012 tensile yield stress and ISO 178:2019 flexural modulus on specimens cut from flat gate sections of the float walls. Published data for the specific seawater immersion life of this formulation is limited, so formulation lock is maintained by OIT and xenon-arc acceptance thresholds rather than an extrapolated years-of-life claim. Terminal finished articles include cylindrical bait cage floats, modular pontoon cubes, shellfish longline buoys, and collar floats for finfish cages; all closures and lifting eyes are molded in as inserts, and each hollow part is pressure-tested after demolding at a differential pressure of 20–40 kPa to detect pinholes before dispatch.

    When Post-Consumer Regrind Is Rejected in Insulated Fish Tub Production

    Insulated fish tub and food-contact material handling container molding starts with a direct food-contact inner skin charged at 100 wt% virgin Icorene 2550 UV+ WHI 1111; post-consumer regrind is rejected from this layer, and only same-process regrind with documented food-contact approval may appear in the foam core at 15–20 wt%. The triple-layer rotational molding sequence is executed on a carousel machine with dropbox or manifold charging: the inner skin is sintered first at an internal air temperature of 195–200 °C, the foam core is then added at 0.5–1.0 wt% azodicarbonamide-based chemical blowing agent in the same base powder, and the outer skin is charged last to encapsulate the foamed core; oven set points are held between 270 °C and 290 °C, and the cooldown curve is controlled so that the internal air temperature falls below 80 °C before demold. Compliance for food-contact service is evaluated under FDA 21 CFR 177.1520(c) and EU Regulation No. 10/2011, with overall migration testing on the final container performed using the food simulants and time-temperature conditions assigned to the intended food category; cleaning-agent compatibility is demonstrated by surface resistance testing under ISO 175:2010 against 1–3% alkaline detergent solutions at 40 °C. The terminal article types are insulated fish storage tubs, meat lugs, dairy transport containers, and seafood transfer bins; wall-thickness mapping by ultrasonic gauge is specified for the bottom corner radius and stacking rib because thickness below 4 mm at those features creates a bending-fatigue crack initiation site when loaded containers are stacked at 2–4 unit heights.

    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 UV+ WHI 1111 Polyethylene, Linear Low Density is supplied as a rotational moulding powder in which the WHI 1111 suffix identifies a white-pigmented variant of the UV-stabilised Icorene 2550 UV+ matrix. The designation does not indicate a separate polymer chemistry; the base polymer remains a linear low density polyethylene. The UV+ stabiliser package is intended to slow oxidative and photo-oxidative degradation during outdoor service, while the white pigment contributes opacity and changes radiative heat transfer during powder heating.

    The intended conversion route is rotational moulding. Hollow articles produced from this grade include outdoor fluid storage tanks, agricultural spray tanks, chemical containment vessels, playground components, and material-handling bins. The powder is suitable for carousel, shuttle, and rock-and-roll machines; injection moulding, blow moulding, and film extrusion are outside the designed conversion window.

    Typical published values for the natural Icorene 2550 UV+ matrix include a melt mass-flow rate of 5.0 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022 and a density of 0.940 g/cm³ according to ISO 1183-1:2019. The white-pigmented WHI 1111 configuration may show a density shift on the order of 0.005–0.010 g/cm³ because titanium dioxide increases mass fraction, but published data for the WHI 1111-specific configuration is limited; incoming inspection should therefore rely on the batch certificate of analysis rather than on natural-grade data.

    Reported typical values for the natural Icorene 2550 UV+ matrix
    PropertyTest methodTypical value
    DensityISO 1183-1:20190.940 g/cm³
    Melt mass-flow rate at 190 °C/2.16 kgISO 1133-1:20225.0 g/10 min
    Tensile stress at yieldISO 527-2:201218 MPa
    Tensile strain at breakISO 527-2:2012600%
    Flexural modulusISO 178:2019550 MPa

    Mechanical property assessment for acceptance testing should use compression-moulded specimens prepared under the annealing conditions listed in the grade datasheet. Tensile values are not direct indicators of rotomoulded part performance because pigment-induced nucleation and cooling-rate gradients produce different crystallinity and tie-molecule populations. Part qualification should include instrumented puncture testing according to ISO 6603-2:2023 or ASTM D3763-21 at the minimum service temperature.

    What Limits Peak Internal Air Temperature in White-Pigmented Rotomoulding Powders?

    In rotational moulding, peak internal air temperature must exceed the crystalline melting range to sinter the powder layer, but it must remain below the temperature where thermo-oxidative chain scission consumes the stabiliser rapidly. For a linear low density polyethylene with a density of 0.940 g/cm³, the melt is typically processed with a peak internal air temperature between 200 °C and 230 °C, depending on wall thickness and oven residence time. The white pigment in WHI 1111 alters the relationship between oven set-point and internal air temperature because titanium dioxide increases near-infrared reflectance at the powder surface while the mould metal absorbs long-wavelength radiation. The practical consequence is that the white powder may heat more slowly in the early stage and then retain heat through the cooling cycle; published measured absorbed energy data for this specific white formulation is limited.

    Thermal stabiliser consumption can be monitored indirectly by melt flow rate drift after repeated rotational moulding cycles. A rise or fall beyond the reproducibility limit of ISO 1133-1:2022 indicates either chain scission or crosslinking. Severe yellowing of un-pigmented or lightly stabilised material is not useful for white grades; instead, whiteness index and yellowness index measured according to ASTM E313-20 and ASTM E1331-09 can quantify early degradation on the inner surface.

    Thermal and Rheological Differences From Non-UV Natural Grades

    The primary difference between Icorene 2550 UV+ WHI 1111 and a non-UV natural rotomoulding grade of the same density is not melt temperature but stabiliser content and surface optics. The UV+ package may include hindered amine light stabilisers and phenolic antioxidants; the white pigment may be coated titanium dioxide. These additives can influence oxidation induction time measured by differential scanning calorimetry under ISO 11357-6:2018, although exact values are product-batch specific. In processing, the additives do not require a major screw change because rotational moulding is a low-shear process; however, dry-air conveying velocities above 25 m/s can generate fines and triboelectric charge.

    Compared with a butene-based rotomoulding LLDPE of similar density, Icorene 2550 UV+ exhibits a different short-chain branching distribution, which is reflected in slow crack growth resistance measured according to ISO 16770:2019 and in low-temperature impact. The exact ranking depends on specimen preparation; projected field data from rotomoulded water tanks suggest improved stress-crack resistance in the equatorial weld area, but published data specific to WHI 1111 is limited.

    UV+ stabilisation is relevant for parts installed at high solar irradiance. Accelerated weathering according to ISO 4892-2:2013 cycle 1 or ASTM G154-23 cycle 1 can detect relative retention of tensile elongation and surface chalking. For white-pigmented polyolefins, titanium dioxide can be protective if dispersed well, but poor dispersion creates pigment agglomerates that act as stress concentrations and reduce crack resistance. Gloss retention and colour shift can be evaluated according to ISO 2813:2014 and CIE L*a*b* under ASTM E308-22.

    When the Same Tool Runs a Black Masterbatch Dry-Blend Instead of WHI 1111

    Changing from a dry-blended black masterbatch to a precompounded white grade changes cooling behaviour. Black parts heat faster and may require a shorter oven residence time to reach the same peak internal air temperature; white parts may require more time in an infrared-dominated oven but less time in a convective oven. The difference can be 5–15% in cycle time depending on heater type, mould mass, and wall thickness. The operator should establish a time-resolved internal air temperature profile using a slip-ring thermocouple and adjust the peak temperature, not merely the cook time. Published data for this specific configuration is limited.

    Powder Feed, Fines Migration, and Hopper Bridging in Rotational Moulding Lines

    Rotational moulding powders are dry-blended with pigment only when the grade is not precompounded; however, in WHI 1111 the colour is part of the supplied powder. Sieve analysis of rotomoulding powders using ASTM D1921-24 is used to confirm that the fraction retained on 500 µm is below the level that would cause pinholing at sharp mould radii. Accumulation of fines below 150 µm increases dust formation and can reduce dry flow; bulk density measured according to ASTM D1895-12 is typically in the range of 0.35–0.40 g/cm³. Moisture pickup above 0.1 wt% at high relative humidity can lead to surface defects in parts, particularly in closed moulds with small vent openings.

    On production-scale carousel machines with 3000 mm swing and 1500 mm cube moulds, flow instabilities are more likely caused by uneven powder feed than by melt flow rate. Batch-to-batch variation in the fraction below 150 µm can change bulk density and hopper discharge. Polyethylene does not require predrying for normal processing because saturated moisture absorption is low; however, surface moisture from condensation in outdoor silos can create steam-induced voids. Drying in a desiccant hopper at 60 °C for 2 h is sufficient when surface moisture is suspected; the resin should not be exposed to temperatures above 80 °C during drying because partial melting of low-crystallinity fractions may fuse powder particles.

    Rotational moulding requires adequate vent tubes to avoid pressure differences. A plugged vent can cause blowouts, particularly in large tanks. Vent diameter should be proportional to mould volume; typical practice uses a vent diameter of at least 6 mm for smaller moulds, with larger diameters for parts exceeding 1 m³. Internal air pressure monitoring can detect pressure spikes.

    Chemical resistance follows LLDPE behaviour: the grade is generally resistant to aqueous salt solutions, dilute acids, and alkalis at ambient temperature; strong oxidising acids, aromatic solvents, and chlorinated hydrocarbons can soften or stress-crack the polymer, particularly at temperatures above 40 °C. Immersion testing per ISO 175:2023 can be used to determine mass change, dimensional change, and appearance change for a specific chemical.

    Food-contact suitability is not established by the product designation alone. If a final article is intended for food contact, the converter must request a product compliance statement for the specific lot and target market because white pigment and stabiliser systems are formulation-dependent. The base polyethylene may be evaluated under FDA 21 CFR 177.1520 or EU 10/2011, but the complete formulated grade requires disclosure of all additives. European Union REACH and RoHS compliance statements for the formulated powder should be obtained from the supplier for the specific production site.

    On shuttle machines with independently controlled arms, the white-pigmented powder can produce different wall thickness distribution than a natural powder when the same firing curve is used. The temperature gradient across the mould wall determines local solidification rate and shrinkage; white parts may show different sink marks near metal ribs. Adjusting the heating phase based on internal air temperature, rather than fixed time, is recommended. The final cooling stage should be maintained until the part surface temperature falls below 60 °C before demoulding to avoid warpage of large unsupported panels.

    Top