Lyondellbasell Icorene 2550 Uv Red 4759 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 190036
    Product Name LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density
    Manufacturer LyondellBasell
    Material Type Linear Low Density Polyethylene (LLDPE)
    Density 0.925 g/cm3
    Melt Index 3.5 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 20.0 MPa
    Elongation At Break 800%
    Flexural Modulus 350 MPa
    Hardness Shore D 50
    Vicat Softening Point 95°C
    Melting Point 123°C
    Impact Strength 100 ft-lb (ARM, -40°C)
    Color Red
    Uv Stabilization Yes
    Form Powder
    Processing Method Rotational Molding
    Thermal Conductivity 0.33 W/m·K
    Specific Heat Capacity 2.3 J/g·°C
    Coefficient Of Linear Thermal Expansion 1.5E-4 cm/cm/°C

    As an accredited LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, stacked on pallets; each pallet contains 55 bags, totaling 1,375 kg.
    Container Loading (20′ FCL) 20′ FCL container loading of LyondellBasell Icorene 2550 UV+ RED 4759 LLDPE in palletized bags, securely stowed for ocean transport.
    Shipping LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density is non-hazardous and not DOT/IMDG/IATA regulated. Ship in original sealed bags, boxes, or octabins on pallets. Protect from moisture, heat, sunlight, and contamination. No placards required; follow local transport rules. Avoid dust and static discharge.
    Storage Store LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original containers tightly closed to prevent moisture, dust, and contamination. Avoid excessive stacking or physical damage. Store at ambient temperature. Use appropriate PPE and good housekeeping. Follow local regulations and the manufacturer’s SDS recommendations.
    Shelf Life Cool, dry, ventilated storage away from direct sunlight; typical shelf life is 24 months in unopened original packaging when stored properly.
    Application of LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density

    For agricultural crop-protection liquid handling, seamless rotationally molded LLDPE containers are produced from Icorene 2550 UV+ RED 4759 at a neat addition ratio of 100 parts by weight; post-industrial regrind is limited to 15 parts by weight where UN 1H1 packaging certification under 49 CFR 178.509 and ADR 6.1.3 must be maintained, because reclaimed powder lowers environmental stress-crack resistance measured under ASTM D1693 and can produce non-linear failure at molded-in pinch-off seams. For non-UN static storage tanks, up to 25 parts regrind may be used after batch validation, provided the wall thickness at the tank shoulder, measured by ultrasonic gauge, does not fall below 4.5 mm. The downstream production process uses cast aluminium or fabricated steel molds on a multi-arm shuttle machine; the powder is charged, the mold is closed, and biaxial rotation at an arm ratio of 4:1 occurs inside an oven with an air temperature of 280 °C to 300 °C. Peak internal air temperature is controlled to 190 °C to 210 °C; excursions above 230 °C deplete the hindered amine light stabilizer and accelerate red pigment fade, while temperatures below 180 °C leave unmelted LLDPE particles at the inner surface. Forced-air cooling followed by water mist reduces warpage; total cycle time for a 1,000 L tank typically ranges from 28 min to 35 min. Finished article types in this segment include 150 L to 1,000 L sprayer tanks, induction hoppers, chemical storage drums and UN-rated outer packagings. Continuous contact with aromatic hydrocarbons, concentrated nitric acid or oxidizing agents above 40 °C is an operational boundary; field data from agricultural tank lines indicate that wall-thickness coefficient of variation on a four-arm shuttle can exceed 10% when oven temperature distribution varies by more than ±10 °C, causing thin-gauge shoulder sections and leakage at dropped tool conditions.

    How Do Marine Buoy Shells Maintain Impact Resistance After Prolonged UV Ageing?

    When marine buoy shells are rotationally molded from Icorene 2550 UV+ RED 4759, the addition ratio is 100 parts by weight neat; dilution with unpigmented LLDPE is kept at or below 5 parts by weight because the red chromophore system and hindered amine stabilizer are compounded as a coupled package, and further dilution reduces the surface protection required for accelerated weathering under ISO 4892-2:2013. Compliance for this segment is application-dependent rather than resin-inherent; incoming powder lot quality is typically verified against ISO 1133-1:2022 for melt flow rate, while molded plaques are tested for notched Izod impact under ASTM D256 and low-temperature brittleness under ASTM D746. Classification societies may require traceability to ISO 9001:2015 when the floats form part of buoyage systems, though no single mandatory marine equipment standard applies to private mooring floats. The downstream production process uses biaxial rotational molding with fabricated steel or cast aluminium molds; target wall thickness is 8 mm to 12 mm, oven set point is 280 °C to 300 °C, and peak internal air temperature is controlled at 195 °C to 210 °C. Cooling is deliberately staged for 45 min to 60 min because rapid water quenching produces visible shrink marks and warpage at mounting inserts; linear mold shrinkage for LLDPE rotomolding powders typically ranges from 2.0% to 3.5%, and published data for this specific red-pigmented grade should be obtained from LyondellBasell for precise mold scaling. Terminal finished products include navigation buoys, mooring floats, modular pontoon segments and fender shells. Polyurethane foam filling is performed only after the shell has cooled below 45 °C, as residual exotherm can create sink marks above foam injection points; continuous immersion in aromatic or chlorinated solvents is outside the operational boundary.

    Outdoor recreational equipment shell thickness and UV stabilization limits

    Because outdoor recreational equipment is installed without post-painting in most public parks, the UV-stabilized red-pigmented powder is used neat at 100 parts by weight; post-industrial regrind is limited to 10 parts by weight to keep heavy metal migration within the analytical detection limits of EN 71-3:2019+A1:2021 and to avoid shifting the red shade beyond a customer-approved delta E tolerance of 1.5 CIELAB units. Compliance standards for this segment include ASTM F1487-21 for public playground equipment, EN 71-3:2019+A1:2021 for migration of certain elements, and REACH Regulation (EC) No 1907/2006 Annex XVII restrictions; no food-contact claim under FDA 21 CFR 177.1520 is made for this red-pigmented grade in playground applications unless the fabricator performs migration testing on the finished article. The downstream process uses biaxial rotational molding in cast aluminium molds with a target wall thickness of 5 mm to 6 mm; oven set point is 260 °C to 280 °C, peak internal air temperature is 185 °C to 200 °C, and forced-air cooling at 20 °C to 25 °C is applied for 20 min before demolding. Mold surface texture is a process variable that affects gloss retention under ISO 4892-2:2013; high-gloss mouth-contact areas may require post-mold abrasion testing. Terminal finished product types include slide hoods, tunnel sections, climbing panels, activity panels and canopy roof modules. Operational boundaries include avoiding secondary adhesive bonding without corona treatment, because the mold release surface energy below 38 mN/m prevents reliable adhesive wetting and creates bond-line failure under field loading.

    Industrial material handling bins and refuse container bodies molded from the same LLDPE powder present a different process conflict: the dominant failure is demolding warpage and corner-thinning under rapid cycle conditions, not colour retention. The addition ratio is 100 parts by weight virgin powder with up to 25 parts post-industrial regrind for non-certified waste containers; when molded articles must meet EN 840-1:2020 for two-wheeled refuse containers, regrind is capped at 15 parts because cold-impact performance at -20 °C under ISO 179-1 may fall below the minimum specified by the standard if reclaimed powder introduces low-molecular-weight fractions. Compliance references EN 840-1:2020 for dimensions and structural integrity, ASTM D638 for tensile yield of molded plaques, and ASTM D790 for flexural modulus. The downstream production process uses single-layer rotational molding; a 240 L bin is produced with wall thickness of 4 mm to 6 mm, while 1,100 L containers require 8 mm minimum corner thickness. Oven temperature is 270 °C to 290 °C, peak internal air temperature is 190 °C to 205 °C, and total cycle time is 22 min to 30 min. Demolding is delayed until the internal surface temperature falls below 60 °C; extraction above this threshold produces warpage at the rim and dimensional nonconformance on the comb-lift interface. Terminal finished products include 240 L and 1,100 L refuse bins, pallet boxes, hoppers, and industrial collection containers. Contact with concentrated oxidizing acids above 40 °C is outside the operational boundary.

    When Traffic Barrier Ballast Shells Require Red Pigment Retention Under Chronic UV Exposure

    In temporary traffic control zones, molders of barrier ballast shells use Icorene 2550 UV+ RED 4759 neat at 100 parts by weight; regrind addition is not recommended above 10 parts by weight because the red chromophore system in UV+ RED 4759 is compounded for a specific let-down ratio, and over-dilution leads to visible shade drift under ISO 4892-2:2013 exposure beyond 1,000 h. Compliance standards for this track include ASTM D638 for tensile properties of molded plaques, ASTM D256 for notched Izod impact at -30 °C, and ISO 4892-2:2013 cycle A for artificial weathering; where temporary work-zone devices are supplied to North American public agencies, retroreflectivity requirements for attached sheeting are governed by ASTM D4956, not by the molded shell itself. The downstream production process is rotational molding on carousel or shuttle machines with fabricated steel molds; wall thickness is held at 6 mm to 10 mm, oven set point is 280 °C to 310 °C, peak internal air temperature is 195 °C to 215 °C, and post-mold cooling is staged to avoid panel curvature greater than 3 mm/m. Terminal finished products include water-filled barrier shells, ballast bases, delineator drums, crash cushion modules and temporary fencing feet. Operational boundaries exclude high-speed impact systems that demand energy absorption validated under EN 1317, because LLDPE rotomolded shells are generally used as ballast or low-speed delineation modules rather than crash-rated restraint elements; published data for this specific red-pigmented grade in EN 1317-compliant barrier systems is limited.

    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 UV+ RED 4759 Polyethylene, Linear Low Density is a precompounded, UV-stabilised, red-pigmented rotational moulding powder in the Icorene range. The grade designation identifies three elements: the 2550 melt-flow position within the Icorene product family, the UV+ light-stabiliser package, and the red pigment formulation referenced as RED 4759. The base polymer is a linear low density polyethylene with controlled short-chain branching, supplied as a dry powder for monolayer rotational moulding. It is not intended for injection moulding, blown film, or sheet extrusion.

    The material is suited to rotationally moulded parts requiring uniform red coloration and outdoor weathering stability without dry-blending a separate pigment masterbatch. Because the pigment and stabiliser are already dispersed, the moulding operation avoids high-shear melt compounding and reduces colour drift, pigment agglomerates, and airborne pigment dust. The UV+ designation indicates a formulated light-stabiliser package; the exact additive ratio is proprietary and is not disclosed on the public datasheet. Specific numerical values for melt mass-flow rate, density, tensile properties, and weathering retention are reported on the lot certificate of analysis. Relevant release methods include ISO 1133-1:2022 for melt mass-flow rate, ISO 1183-1:2019 for density, and ISO 527-2:2012 for tensile yield stress and elongation. Published data for this specific UV+ RED 4759 configuration is limited; the natural base-grade datasheet should not be substituted for lot-specific values.

    What separates a precompounded red LLDPE from natural-powder external pigmenting?

    The principal difference from natural LLDPE rotational moulding powder is the integration of colorant and light stabiliser into the powder feedstock. In a natural-powder operation, pigment masterbatch is dry-blended at the moulder, which introduces mixer efficiency, colour uniformity, and dust exposure variables. The precompounded grade reduces those variables and provides more consistent colour across production lots. However, the red pigment modifies infrared absorption relative to unpigmented powder. On a rotational moulding machine, this can shift the effective heat transfer into the mould and require a different oven setpoint or peak internal air temperature to achieve full densification. Colour difference is conventionally evaluated under D65 illumination with a 10° observer using ASTM D2244-22 or ISO 7724-2:2019.

    The pigment may also act as a low-level nucleating agent during cooling, influencing crystallisation onset and shrinkage. Quantitative nucleation data for this specific grade is limited, so mould trials should include dimensional checks at the parting line and on flat surfaces before production approval.

    Rotational Moulding Process Limits and Thermal Profile Control

    On carousel, shuttle, and rock-and-roll machines with mould swings up to 3.0 m, the internal air temperature inside the mould is the primary control variable, not the oven setpoint. For LLDPE powders, the oven environment is typically maintained between 250°C and 280°C, while the internal air temperature is ramped to 180°C–210°C to complete sintering and densification. A peak internal air temperature below 180°C may leave pinholes or incomplete sintering in thick sections. Sustained internal air temperatures above 230°C can degrade the UV stabiliser package and shift the red pigment. The part should be cooled slowly; cooling rates above 15 K/min can increase warpage and residual stress in flat LLDPE surfaces. The pigmented grade may require a slightly different oven setpoint than natural material because the red pigment changes radiative energy absorption, especially in thin-wall zones.

    Vent-opening pyrometry is required during process development. Sintering of LLDPE rotomoulding powder proceeds through surface melting, coalescence, densification, and air removal. Insufficient peak temperature leaves pinholing at the inner surface; excessive temperature creates oxidative degradation or colour shift. The UV+ package can mask early yellowing in the red pigment, so thermal damage may not be visible until mechanical properties decline. Test plaques and pyrometry are therefore more reliable than colour observation alone for detecting overbake.

    Process variableTypical LLDPE operating windowControl consequence for precoloured grade
    Oven setpoint250–280°CAdjust for pigment IR absorption
    Peak internal air temperature180–210°CDo not exceed 230°C to protect stabiliser
    Mould release temperature70–80°CMonitor for part distortion
    Cooling rate< 15 K/minHigher rates may increase warpage

    Typical LLDPE rotomoulding powders in this product class have density in the range 0.925–0.940 g/cm³. Exact density and melt mass-flow rate are lot-specific. The powder distribution is controlled to promote uniform wall build; a 500 µm top cut is common for rotational moulding powders, with controlled fines content. Tensile yield stress for rotomoulded LLDPE sheet is generally between 10 MPa and 14 MPa; elongation at break is typically above 600% before weathering. The UV+ package is intended to retain a portion of that elongation after outdoor exposure, but actual performance must be verified through accelerated weathering under ISO 4892-2:2013 or a real-time outdoor exposure program. Melt mass-flow rate values for LLDPE rotomoulding grades are measured with a 2.16 kg weight at 190°C. This is a low-shear index and does not fully predict rotational moulding behaviour; dry-flow and particle-size distribution are equally important. The 2550 code should be interpreted as a melt-flow position within the Icorene range, not as an exact melt index unless stated on the certificate of analysis.

    Comparison with High-Density Polyethylene and Lower-Flow Icorene Grades

    Compared with HDPE rotomoulding grades, the LLDPE base of Icorene 2550 UV+ RED 4759 generally provides lower flexural modulus, lower density, and higher resistance to environmental stress cracking. HDPE is selected where higher stiffness and a higher heat deflection temperature are needed. LLDPE is selected where the part must survive impact at temperatures below -20°C or where local stress concentration is present. The difference is structural: short-chain branching in LLDPE reduces crystalline density and changes craze propagation. Flexural modulus of LLDPE rotomoulded specimens is often below 400 MPa, while HDPE rotomoulding grades may exceed 700 MPa depending on density and test temperature. These ranges are generic; comparative values for the RED 4759 formulation should be generated under ISO 178:2019.

    Within the Icorene range, the 2550 designation positions the material at a higher melt-flow level than lower-flow rotomoulding grades. This supports filling of complex geometry, narrow ribs, and fine surface detail, but may reduce melt strength. Rotational moulding does not apply high shear, so melt flow is not the only determinant; powder particle shape, bulk density, and dry-flow behaviour also influence wall build. Users switching from a lower-flow LLDPE should expect a different peak internal air temperature and possibly a shorter densification window. Compared with flexible PVC or plasticised vinyl outdoor trim, the LLDPE product does not require plasticiser migration management. Compared with polypropylene, it offers better sub-zero impact but lower upper service temperature. None of these comparisons replaces a part-level validation program under the specified load and exposure conditions.

    When the part must pass outdoor weathering and chemical-exposure validation

    Reported application areas for UV-stabilised LLDPE rotomoulding powders include agricultural hoppers, outdoor equipment covers, small chemical storage tanks, and playground components. In these uses, the material is selected for low-temperature ductility and resistance to environmental stress cracking. Environmental stress crack resistance is commonly ranked under ASTM D1693-15b, Condition A, using 100% Igepal CO-630; LLDPE rotomoulding grades of this class often exceed 1000 h F50. The material is not recommended for strong oxidising acids, aromatic hydrocarbons, or continuous exposure to aggressive solvents at elevated temperature. Chemical compatibility must be validated on the pigmented compound because both the LLDPE base and the pigment package affect permeation and stress-crack resistance.

    Accelerated weathering under ISO 4892-2:2013 uses xenon arc exposure with daylight filters, typically at 0.35 W/m² at 340 nm, black-standard temperature 65°C. For a red pigmented LLDPE, the usual endpoint is a ΔE of 3.0 to 4.0 CIELAB units, but the specification depends on the application. Published data for this specific RED 4759 configuration is limited; outdoor Florida or Arizona data should be obtained for long-term performance validation.

    Regulatory status for the pigmented compound must be confirmed for the application region. LyondellBasell’s product stewardship documentation typically addresses REACH Regulation EC 1907/2006, RoHS Directive 2011/65/EU, and, where applicable, the food-contact framework EU 10/2011. Because the pigment package can alter migration behaviour, food-contact status is not automatically inherited from the natural base grade. If the application involves potable water or food contact, written confirmation from LyondellBasell is required for the exact RED 4759 formulation.

    Heavy-metal restrictions for pigmented polyethylene components are typically assessed according to EN 71-3:2019 for toy applications or RoHS Annex II limits for electrical and electronic equipment housings. The red pigment package RED 4759 may contain organic colorants or inorganic iron oxide; exact pigment composition should be obtained from the supplier when EU 10/2011 migration limits or FDA 21 CFR 177.1520 status is required. No inference of global food-contact approval should be made from the base resin alone. Under REACH, the grade may be subject to Article 33 communication duties if substances of very high concern exceed 0.1% w/w in the article. Users must verify the Safety Data Sheet and supplier declaration for the specific colorant package.

    Apply batch release methods to incoming lots before production

    ParameterStandard methodReported unitScope
    Melt mass-flow rate (190°C, 2.16 kg)ISO 1133-1:2022g/10 minBatch melt-flow position
    Density (23°C)ISO 1183-1:2019g/cm³Base resin density
    Tensile yield stress / elongationISO 527-2:2012MPa / %Moulded specimen mechanical strength
    Particle size distributionASTM D1921-18 / ISO 4610µm / % retainedRotomoulding powder dry-flow and wall build
    Vicat softening temperatureISO 306:2022, Method A50°CShort-term thermal resistance
    Environmental stress crack resistanceASTM D1693-15b, Condition A, 100% IgepalhChemical exposure ranking
    Accelerated weathering colour retentionISO 4892-2:2013 / ASTM G155-21ΔE, grey scaleUV-stabiliser efficiency

    On production-scale carousel machines, a recurring bottleneck with precoloured powders is shift in mould release temperature caused by pigmentation. The set-up should include trial runs that map internal air temperature against wall thickness at the parting line and at the farthest mould extremity. Wall thickness sampling should follow ISO 2818:2018 or an equivalent cut-sheet method. Incoming lots can be compared for dry-flow behaviour by funnel tests under ASTM D1895-96(2019) Method A. If the powder is stored at relative humidity above 60% or moved from cold storage to a warm shop floor, surface condensation may cause clumping; pre-drying at 60°C for 2 h in a dehumidified hopper is sufficient to restore uniform flow. Contact with copper or copper alloys in moulds, inserts, or tooling should be avoided because metal-catalysed thermo-oxidative degradation can occur at elevated processing or service temperatures.

    Top