| HS Code | 326345 |
| Density | 0.935 g/cm³ |
| Melt Flow Rate | 3.5 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 17 MPa |
| Tensile Strength At Break | 20 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 600 MPa |
| Tensile Impact Strength | 200 kJ/m² |
| Shore D Hardness | 55 |
| Vicat Softening Temperature | 115°C |
| Brittleness Temperature | < -70°C |
| Environmental Stress Crack Resistance | >1000 h |
| Uv Stabilization | Yes |
| Color | Red 4733 |
As an accredited LyondellBasell Icorene 2550 UV+ RED 4733 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 2550 UV+ RED 4733 is packaged in 25 kg polyethylene bags, palletized and stretch-wrapped for protected transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell Icorene 2550 UV+ RED 4733 Linear Low Density Polyethylene, 25 kg bags, palletized and secured. |
| Shipping | LyondellBasell Icorene 2550 UV+ RED 4733 Polyethylene, Linear Low Density is shipped as non-hazardous plastic resin, typically in 25 kg bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers; protect from moisture, heat, sunlight, and contamination. Not regulated for DOT/IMDG/IATA. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Palletize securely, avoid excessive stacking and prolonged UV exposure. Use first-in, first-out inventory. Maintain ambient temperatures. Material is combustible; protect from ignition sources. Follow manufacturer guidelines. |
| Shelf Life | Shelf life is typically 12–24 months when stored in original, unopened packaging, cool, dry, and protected from direct sunlight. |
For a 5,000-litre vertical closed-head tank intended for ammonium sulphate dosing, the mould is charged with 32–36 kg of Icorene 2550 UV+ RED 4733 powder into a steel mould with a wetted surface area of 6.8–7.2 m²; the charge-to-surface-area ratio gives a nominal sidewall of 5.8–7.0 mm and knuckle regions of 8–10 mm during biaxial rotation at a 4.0:1 primary-to-secondary speed ratio. The grade is supplied as a red-compounded, UV-stabilised linear low-density polyethylene powder and is not diluted with uncoloured polymer or additional pigment masterbatch; if regrind is introduced, the ratio is held at 15 wt% maximum because higher regrind in rotomoulding powder lowers low-temperature impact performance under ASTM D256 and can shift moulded colour by more than 1.5 CIE units measured as ΔE under ISO 11664-4 D65/10°. Processing takes place on a multi-arm carousel rotational moulding machine with a 2.8 m swing, forced-air oven set at 285–300°C, and primary/secondary arm speeds of 4.0 rpm and 1.0 rpm; the peak internal air temperature at the vent is brought to 200–210°C before transfer to centrifugal forced-air cooling at 0.8–1.2 m/s until PIAT falls to 90°C, followed by water mist at 15–25°C to reduce warpage at the threaded insert bosses. Tensile yield stress is verified on a wall section under ASTM D638-14, density under ASTM D1505-18, environmental stress-crack resistance under ASTM D1693-21 Condition B in 10% Igepal CO-630 at 50°C, and the closed vessel is pressure-tested at 35 kPa air pressure under water for pinhole detection. The finished product is a closed-head agricultural chemical dosing tank for neutral to mildly acidic fertiliser solutions; contact with aromatic hydrocarbons, ketones, or strong oxidising acids is outside the service envelope of this LLDPE and should be excluded by the end-user specification.
Rotational moulding of a 10,000-litre horizontal non-potable water storage tank for drip irrigation uses a two-piece steel mould fitted with four knurled steel threaded bosses that are preheated to 140–160°C and inserted before charging; the shot weight is 65–75 kg, producing a nominal 6–7 mm sidewall and 8–10 mm rib sections. The steel inserts are specified with a wall-thickness-to-insert-diameter ratio of at least 2.0:1 to limit cracking at the boss roots during cooling, and the insert depth is held below 50% of the local wall thickness so that the inner surface remains sealed. The carousel oven is set at 295–300°C, with a 4.0:1 rotation ratio used for the horizontal cylinder; peak internal air temperature is controlled at 195–205°C. Cooling is forced-air only to 90°C before demoulding to avoid the additional thermal shock of water mist on the metal-to-polyethylene boss interfaces, which can generate micro-voids and reduce leak-tightness. Notched Charpy impact is tested under ISO 179-1/1eA at −20°C, with only ductile failure mode accepted at the gate area; the UV-stabilised red surface is evaluated for colour change after 4,000 h xenon-arc exposure under ASTM G155 Cycle 1, with ΔE limited to 4.0 against the unexposed control. The terminal product is a non-potable drip-irrigation buffer tank for outdoor farms; it is not intended for potable water unless the complete article is certified against a drinking-water contact standard such as NSF/ANSI/CAN 61, which is not automatically conferred by the resin alone.
At −20°C, the failure mode of rotomoulded playground panels is evaluated by instrumented puncture under ISO 6603-2 at 4.4 m/s striker velocity and 2.0 kg striker mass; the acceptance criterion is ductile deformation without radial cracking because brittle behaviour at the panel edge can produce sharp fragments after service impact. Icorene 2550 UV+ RED 4733 is processed without additional UV stabiliser masterbatch or pigment; regrind of the same red lot is limited to 10 wt% to preserve the compounded UV stabiliser concentration, while regrind from uncoloured or off-spec polymers is excluded. Published data for this exact red pigmentation in playground tunnel tooling is limited, so the processing window is derived from general rotationally moulded UV-stabilised LLDPE practice. In a four-cavity cast aluminium mould producing tunnel roof segments and flat side panels with a target wall thickness of 4.5–5.5 mm, the carousel oven is set at 270–280°C; the tunnel cavity uses a 4.0:1 primary-to-secondary rotation ratio, and the flat panel uses 3.5:1 to prevent powder bridging at the shallow edge. Peak internal air temperature is held at 190–200°C for 8–10 min after PIAT is reached, then the part is cooled by forced air at 1.0–1.5 m/s until PIAT falls to 80°C; water mist cooling is avoided on this thin-wall aluminium tooling because rapid mould-surface cooling below 60°C increases differential shrinkage and warpage. The resin contribution is verified by melt flow rate under ISO 1133-1:2022, density under ASTM D1505-18, and low-temperature impact under ISO 6603-2; the assembled play structure is separately assessed under EN 1176-1:2017 and ASTM F1487-21 for entrapment, fall-height, and impact attenuation, which are system properties not established by resin tests. The terminal products are red tunnel roof segments, side panels, and crawl-through sections for modular playground equipment.
In suspended mussel longline aquaculture, the moulded polyethylene float shell is rotomoulded as a hollow body and then filled with rigid two-part polyurethane foam through the vent; for a 30-litre buoy, the shell shot weight is 1.8–2.4 kg, giving a wall thickness of 3.5–4.5 mm, while the foam fill density is set at 35–45 kg/m³ free-rise density and the mixed cream time is below 35 s. The shuttle machine uses aluminium mould shells and an oven setpoint of 260–280°C; the thin wall reaches a peak internal air temperature of 180–195°C, and exposure above 190°C is limited to 20 min to reduce surface oxidation and colour shift in the red UV-stabilised shell. After demoulding, the shell is pressure-tested at 15 kPa air under water to detect pinholes, and the interior is flame-treated to 40–45 dyn/cm wetting tension measured by ASTM D2578 before polyurethane foam is injected at a 1:1 volume ratio with a low-pressure metering machine, leaving 10% headspace for foam expansion. The filled float is hydrostatically tested at a water depth equivalent of 100 kPa for 24 h, with permanent volume loss limited to 2%. The terminal product is a foam-filled buoy for mussel socks and aquaculture perimeter lines; it is not designed for continuous immersion below 5 m or for repeated impact against concrete quay walls, because LLDPE creeps under sustained hydrostatic load and the foam core loses buoyancy if the shell is punctured.
A 1,000-litre bulk bin for transfer of dry mineral fillers and masterbatch granules is rotomoulded from the same red UV-stabilised LLDPE powder using a single-cavity steel mould with a 14.0 kg shot weight, producing a nominal 6 mm sidewall and a 7 mm top rim; the carousel oven is set at 285°C and the peak internal air temperature is controlled at 195–205°C, with forced-air cooling to 85°C before demoulding to preserve flat sidewall geometry. Because red pigments can contain regulated heavy metals if sourced from non-EU feedstocks, the moulded bin is tested under RoHS 2011/65/EU Annex II; lead, mercury, and chromium VI are each at or below 1,000 mg/kg, and cadmium is at or below 100 mg/kg. For combustible dust service, the surface resistivity of the rotomoulded wall is measured under ASTM D257; if the value exceeds 1.0×1012 Ω/square, external earthing and area classification measures are required because the LLDPE shell is not inherently dissipative. Regrind is limited to 25 wt% for industrial use, and only clean, unpigmented or same-lot red regrind is reintroduced to avoid changing the UV and colour balance. If the same bin geometry is proposed for dry food ingredients, the complete article must separately satisfy FDA 21 CFR 177.1520(c) and EU 10/2011 with an overall migration limit of 10 mg/dm²; the resin alone does not automatically confer food-contact status because the pigment and stabiliser package must also be assessed. The terminal product is an industrial bulk bin for non-fatty dry powders and granules, not intended for hot liquid filling or solvent-based cleaning agents.
| Application area | Standard / test method | Property / acceptance criterion |
|---|---|---|
| Closed-head agricultural chemical tank | ASTM D1998-21 | Vessel design and pressure-test criteria for upright polyethylene tanks; 35 kPa air under water |
| Rotomoulded tank wall | ASTM D638-14 | Tensile yield stress and elongation at yield on cut wall section |
| Resin density conformity | ASTM D1505-18 | Density gradient column at 23°C; typical LLDPE rotomoulding range 0.935–0.940 g/cm³ |
| Low-temperature impact | ASTM D256 / ISO 179-1/1eA | Notched impact at −20°C; ductile failure required |
| Environmental stress-crack resistance | ASTM D1693-21 Condition B | 10% Igepal CO-630 at 50°C; no premature cracking |
| Playground assembly conformity | EN 1176-1:2017 / ASTM F1487-21 | System-level impact attenuation, entrapment, and structural integrity; resin data alone is not sufficient |
| Combustible dust service | ASTM D257 | Surface resistivity ≤1.0×1012 Ω/square for dissipative classification; otherwise earthing measures required |
| Food contact if proposed | FDA 21 CFR 177.1520(c) / EU 10/2011 | Complete article migration ≤10 mg/dm²; resin alone does not confer approval |
| Pigmented article heavy metals | RoHS 2011/65/EU Annex II | Pb ≤1,000 mg/kg, Cd ≤100 mg/kg, Hg ≤1,000 mg/kg, Cr(VI) ≤1,000 mg/kg |
| Colour retention / weathering | ISO 4582:2017 / ASTM G155 Cycle 1 | Xenon-arc 3,000–4,000 h; ΔE ≤4.0 against unexposed control |
When a temporary road-barrier base is specified for water ballast, the shell is rotomoulded as a one-piece body and filled on site with 40–60 L of water; the empty shell weight is 18–22 kg, sidewall thickness is 5–6 mm, and bottom rib sections are 8–10 mm thick to resist abrasion during sliding on asphalt. The carousel oven is set at 295–300°C with a 4.0:1 biaxial rotation ratio; peak internal air temperature is held at 200–210°C to ensure full fusion at the rib roots, and cooling is forced air only to 90°C to prevent warpage of the long, flat base. The red UV-stabilised LLDPE shell is used without post-mould painting; colour retention is measured after 3,000 h xenon-arc exposure under ISO 4582:2017 or ASTM G155 Cycle 1, with ΔE limited to 4.0. Impact performance of the material is verified under ASTM D256 at −20°C, and tensile properties under ASTM D638-14; the finished product is a water-ballasted temporary traffic-control barrier base for highway work-zone delineation. It is not by itself an energy-absorbing crash cushion, and any claim of impact attenuation must be established for the complete system under EN 12767:2019 or the governing road-authority specification, not inferred from the polyethylene shell alone.
Competitive LyondellBasell Icorene 2550 UV+ RED 4733 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The resin identified as LyondellBasell Icorene 2550 UV+ RED 4733 is a pre-pigmented, ultraviolet-stabilised linear low-density polyethylene powder supplied for rotational moulding of hollow parts. The base grade Icorene 2550 is supplied as a free-flowing powder with a melt flow rate measured under ISO 1133-1:2022 at 190 °C and 2.16 kg; the published typical value for the UV+ series is 5.0 g/10 min. Density determined by ISO 1183-1:2019 is 0.935 g/cm³. The UV+ designation indicates a hindered amine light stabiliser and UV absorber package; RED 4733 identifies a specific red colorant formulation compounded into the powder. The grade is intended for hollow parts manufactured on biaxial rotational moulding machines, including outdoor tanks, agricultural containers, automotive fluid reservoirs, leisure products, and general industrial enclosures.
Specification control for the powder includes sieve analysis according to ASTM D1921-18, apparent density and pourability by ASTM D1895-17, and dry flow behaviour. Published data for the specific RED 4733 pigment loading is limited; the manufacturer’s certificate of analysis governs batch acceptance. Finished-part mechanical properties are dependent on peak internal air temperature, cooling rate, and wall thickness, not solely on resin melt flow rate.
Pre-compounded colour integration distinguishes RED 4733 from natural Icorene 2550 UV+ powder that requires dry blending with a masterbatch at the machine. On production-scale biaxial moulding lines, dry-blended colour systems can segregate during hopper charging or pneumatic transfer when particle size distributions differ between base powder and masterbatch. The pre-pigmented grade reduces streak formation and gives tighter batch-to-batch colour variance, although specific ΔE tolerances must be obtained from the manufacturer’s colour data.
The red pigment package can shift the heating profile of the powder bed. Darker or saturated colours increase absorption of radiant heat in open-flame or gas-fired ovens, which can reduce the time required to reach the 180 °C to 195 °C peak internal air temperature window. If oven residence time is not correspondingly adjusted, local oxidation at the mould surface may appear as yellowing or gloss loss. In contrast, natural or pale-coloured powders usually require longer oven dwell to reach the same internal air temperature under identical burner settings.
Mechanical property tests on LLDPE rotational moulding powders frequently show a reduction in tensile elongation at break for heavily pigmented grades relative to natural grades because pigment particulates can act as stress-concentration sites. The effect is evaluated by ISO 527-2:2012 at 23 °C; typical LLDPE tensile strain at break exceeds 500 % for unaged specimens, but the red-pigmented grade may show lower nominal values depending on dispersion quality.
Comparative stiffness data place this LLDPE grade below high-density and medium-density rotational moulding materials. HDPE rotomoulding powders commonly range from 0.940 g/cm³ to 0.950 g/cm³ density and can exceed 1000 MPa flexural modulus, whereas the published flexural modulus for this LLDPE series is approximately 550 MPa. The lower modulus gives improved ductility and low-temperature impact resistance, while HDPE may be selected where higher wall stiffness and greater deformation resistance under hydrostatic load are required. Melt flow rate also separates the grade from lower-fluidity LLDPE rotomoulding alternatives: a 5.0 g/10 min powder densifies more readily in complex mould details than an 3.0 g/10 min grade but may exhibit marginally lower environmental stress crack resistance.
In gas-fired biaxial rotational moulding machines with forced-air oven circulation, a typical setpoint for this grade is between 250 °C and 300 °C. The mould surface and the internal air temperature inside the mould should be measured continuously with an infrared pyrometer or thermocouple; peak internal air temperature is normally held between 180 °C and 195 °C for 3.0 mm to 8.0 mm walls. Powder tumbling, sintering, densification, and cooling follow the standard four-stage rotational moulding sequence. Residence time at peak temperature influences bubble removal, densification, and impact performance. Slow cooling is preferred for large flat panels to minimise warpage; water-fog or forced-air cooling reduces cycle time but can increase residual stress in parts with varying wall thickness.
Mould release selection should account for the red pigment and UV package; silicone-based semi-permanent release agents are used widely on aluminium moulds with grit-blasted or chemically etched surfaces. Powder conditioning is generally unnecessary for polyethylene at relative humidity below 60 %; if the powder is stored in humid conditions, surface moisture can produce pinholes and should be removed by drying at 60 °C for 2 h before charging. Particle size distribution and bulk density affect mould-surface reproduction; the powder should be handled with closed pneumatic conveying where possible to limit fines generation.
Arm impact testing of rotomoulded parts is carried out by ASTM D5628-18; tensile properties are typically measured on compression-moulded plaques or cut specimens from rotomoulded walls according to ISO 527-2:2012. Reported low-temperature brittleness for the LLDPE family is below -75 °C by ASTM D746-20, but the pre-pigmented grade requires part-specific verification because colorant dispersion can affect crack propagation.
When the peak internal air temperature remains below approximately 170 °C, full coalescence of the LLDPE powder particles is incomplete. Porosity along the inner surface and microvoids in the wall become visible after cutting. Tensile elongation at break measured by ISO 527-2:2012 can fall below 200 % on poorly sintered walls, whereas well-densified LLDPE rotomoulded specimens normally exceed 500 %. Dart impact energy measured by ISO 6603-2:2016 also declines steeply when the peak temperature is insufficient; production-scale failures are observed as brittle fractures initiating from the inner pinhole layer.
Overheating above 210 °C internal air temperature causes oxidative degradation and can shift the red colour toward yellow, lower gloss, and reduce stabiliser concentration. Oxidative induction time measured by differential scanning calorimetry under ISO 11357-6:2021 is used to assess residual stabiliser in failed parts. The processing window is therefore narrow; operators should log peak internal air temperature for each mould rather than relying solely on oven timer settings.
For applications requiring food-contact status, the base polyethylene may be evaluated under FDA 21 CFR 177.1520 and (EU) No 10/2011, but the red colorant and UV stabiliser package must be separately authorised or covered by migration testing. Finished-article compliance under REACH requires SVHC content below 0.1 wt% per article. The matrix below summarises the applicable verification routes.
| Standard or regulation | Technical criterion | Method or clause |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Use conditions and food-type restrictions in Table 2 |
| (EU) No 10/2011 | Plastic materials and articles in food contact | Overall migration limit 10 mg/dm²; specific migration limits for additives |
| REACH | SVHC content in articles | Notification if > 0.1 wt% per article |
| RoHS 2011/65/EU | Restricted substances in electrical and electronic equipment | Pb, Hg, Cd, CrVI, PBB, PBDE limits |
The table does not constitute a declaration of conformity for the coloured grade; end users must obtain supplier documentation and conduct finished-article migration or content testing as applicable.
Exterior parts moulded from red-pigmented LLDPE are exposed to ultraviolet radiation, moisture, and thermal cycling. Xenon-arc weathering according to ISO 4892-2:2013 or fluorescent UV exposure according to ASTM G154-23 can be used to estimate colour shift and gloss retention. Colour difference is expressed as ΔE*ab under CIE L*a*b* coordinates per ISO/CIE 11664-4; gloss retention is measured at 60° by ISO 2813:2014.
UV stabilisers retard the free-radical oxidation sequence in the polyethylene matrix, but they do not prevent all pigment fading for saturated red colours. Surface chalking—a white, powdery degradation layer—occurs after the near-surface stabiliser is consumed; the onset depends on UV dose, pigment concentration, and wall thickness. Published data for this specific red formulation is limited; outdoor exposure in high-UV climates should be validated with 12-month Florida or Arizona weathering panels before specification.
The stabiliser package improves retention of tensile properties after weathering; tensile strength retention after 2000 h xenon-arc testing is typically above 80 % for UV-stabilised LLDPE rotomoulding grades, but the red shade may shift beyond a ΔE*ab of 3 before physical failure occurs.
Agricultural chemical tanks, water-storage vessels, and outdoor enclosures produced from LyondellBasell Icorene 2550 UV+ RED 4733 are typically evaluated for hydrostatic load, impact, and weathering. Welding of rotomoulded LLDPE parts requires clean, oxidation-free weld surfaces; hot-gas and extrusion welding are commonly used, with weld strength assessed by ISO 527-2:2012 or bend testing. Chemical resistance of the final article should be assessed in the intended fluid at the highest service temperature; environmental stress crack resistance of the base LLDPE grade is tested by ASTM D1693-21 and is generally greater than 1000 h in 100 % Igepal at 50 °C for uncompromised rotomoulded walls.
In rotational moulding shops using aluminium moulds of 6 mm to 12 mm thickness, cycle time for this grade is controlled by wall thickness and oven temperature rather than by melt flow rate alone. Unmoulded parts should be cooled uniformly to below 60 °C before demoulding to avoid distortion. Post-moulding trimming and assembly operations are conventional for LLDPE; no special surface treatment is required for bonding with polyurethane sealants where mechanical abrasion is used to raise surface energy.