| HS Code | 653830 |
| Productname | LyondellBasell Icorene 2550 UV+ GRY 7853 Polyethylene, Linear Low Density |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.925 g/cm³ |
| Meltflowrate | 5.0 g/10 min (190°C/2.16 kg) |
| Tensilestrengthatyield | 11.7 MPa |
| Tensilestrengthatbreak | 17.2 MPa |
| Elongationatbreak | 800% |
| Flexuralmodulus | 345 MPa |
| Notchedizodimpactstrength | 80 J/m |
| Shoredhardness | 50 |
| Vicatsofteningpoint | 95°C |
| Uvstabilization | Yes |
| Color | Grey |
| Processingmethod | Rotational Molding |
As an accredited LyondellBasell Icorene 2550 UV+ GRY 7853 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 2550 UV+ GRY 7853 LLDPE is supplied in 25 kg polyethylene bags, palletized and shrink-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded with LyondellBasell Icorene 2550 UV+ GRY 7853 Linear Low Density Polyethylene; palletized, secured, dry container, standard shipment. |
| Shipping | LyondellBasell Icorene 2550 UV+ GRY 7853 is a nonhazardous, gray, UV-stabilized linear low-density polyethylene. Ship in sealed bags, boxes, or octabins. Store in cool, dry, ventilated conditions, away from heat, sunlight, and contamination. Follow standard polymer handling and local transport regulations; no dangerous goods classification required. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid strong oxidizing agents. Use grounding/bonding to control static during handling. Maintain clean, dry conditions and follow local regulations for combustible dust and plastic resin storage. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored dry, cool, and ventilated in original packaging, away from sunlight. |
In rotational moulding, a linear low density polyethylene powder with a pre-compounded grey colour and UV-stabilised package is evaluated by how the powder bed densifies during the heating phase, not solely by melt flow. LyondellBasell Icorene 2550 UV+ GRY 7853 Polyethylene, Linear Low Density is supplied as a ready-to-use dry powder for single-shot and two-layer rotational moulding operations; the grey 7853 pigmentation removes dry-blend colour variation while the UV+ formulation addresses outdoor weathering. Incoming resin should be checked under ISO 1133-1:2022 at 190°C/2.16 kg for melt-flow-rate consistency and under a powder moisture method before production because batch-to-batch variance in dry flow, trapped moisture, and oven exhaust conditions are measurable production variables that influence surface porosity and low-temperature impact retention.
Potable water tanks and rainwater cisterns are rotationally moulded from this grade in enclosed shuttle machines with cast aluminium moulds. Incoming powder is stored at 20–25°C and the moisture content is verified below 0.05% by weight before charging; when relative humidity exceeds 60%, the powder is air-purged at 40°C until the moisture analyser reading returns below 0.05% because surface moisture creates steam pinholes in walls above 5 mm. The oven setpoint is 285–300°C and the peak internal air temperature is controlled at 200–220°C. A biaxial rotation ratio of 4:1 is maintained during the first 60% of the heating cycle, and the final demoulding temperature is held below 70°C to keep shrinkage deviation under 1.5%. Compliance for potable water contact rests on FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and NSF/ANSI 61 for North American municipal installations. The formulation addition ratio is 100 parts Icorene 2550 UV+ GRY 7853; a maximum of 10 parts of clean, in-house LLDPE regrind is introduced only in the non-food-contact outer layer or in non-food grey tank shells because higher regrind reduces dart impact and can compromise migration-test consistency. Downstream production involves single-shot powder loading, mould closure, oven dwell sufficient to reach peak internal air temperature, forced-air pre-cooling, water-mist cooling, and part extraction with 2–3° draft. Terminal products include 500–20,000 L vertical rainwater harvesting tanks, underground potable water storage cells, and rectangular drinking-water transport tanks. The impact performance of each production lot is typically verified on prototype cut-outs by ISO 6603-2 instrumented puncture impact at -20°C; published data for this specific configuration is limited, so lot-release thresholds are normally derived from the end-user’s design wall thickness rather than a universal resin specification.
Agricultural chemical storage tanks present a more demanding processing window because the grey UV-stabilised compound contains an antioxidant and weathering stabiliser package, but tank manufacturers still qualify each incoming lot by ASTM D543 immersion using representative agrochemical formulations—commonly a 10% ammonium sulfate solution, a 5% urea solution, and a commercial glyphosate formulation at 23°C and 60°C. The industry compliance standard for above-ground rotationally moulded polyethylene tanks is EN 13575:2012, which includes hydrostatic pressure testing, impact testing at -20°C, and chemical resistance verification; transport configurations may additionally require UN ADR/RID certification as an intermediate bulk container or as fixed tank equipment depending on final assembly. The formulation addition ratio is 100 parts Icorene 2550 UV+ GRY 7853 powder; if a dark grey UV absorber masterbatch is added to extend service life in subtropical storage yards, the separate masterbatch is restricted to 1–2 parts because excessive stabiliser masterbatch can create local viscosity variation and visible flow lines on the inner mould surface. Downstream production on a rotomoulding line uses rock-and-roll or shuttle machines for cylindrical tanks up to 5,000 L. The mould is loaded as a single charge; the oven setpoint is 280–310°C, with internal air temperature reaching 210–230°C before forced-air cooling is initiated. A slower cooling profile is used compared with potable water tanks: the cooling rate is held below 5°C/min in the 120–70°C interval to minimise frozen-in stress at the rib roots, since stress concentrations in thick-walled agricultural tanks accelerate environmental stress cracking when exposed to wetting agents. Typical wall thickness is 8–12 mm, with thicker sections at saddle supports and outlet boss areas. Terminal finished products include horizontal sprayer tanks, fertilizer nurse tanks, pesticide induction hoppers, and stationary chemical dosing reservoirs. Tank manufacturers inspect parting-line porosity using pressure decay testing at 0.3 bar and avoid flame treatment on the inner surface because oxidised polyethylene can show altered migration behaviour in aggressive formulations.
Under marine buoyancy and dock-float exposure, the grade is processed for hollow shell structures rather than for thick-walled chemical tanks. The governing outdoor exposure requirement is ISO 4892-2:2013 xenon-arc accelerated weathering; producers also test low-temperature impact retention by ISO 179-1 on moulded plaques at -30°C. The formulation addition ratio is 100 parts Icorene 2550 UV+ GRY 7853 powder for the outer shell; the shell wall is rotomoulded at 4–6 mm and subsequently filled with a two-component closed-cell polyurethane foam. The downstream production process is staged: the shell is rotomoulded, cooled below 45°C, then demoulded before foam filling, because the exotherm of the reacting polyurethane can push the inner wall above 80°C and soften the LLDPE if the shell is filled too early. Oven setpoint is held at 260–280°C and peak internal air temperature is clamped at 190–210°C to avoid overbaking the thinner shell; the biaxial rotation ratio is reduced to 3.5:1 during the first stage to improve wall uniformity around moulded-in rope eyes and inspection ports. Terminal products are dock floats, buoyancy collars, work-boat fender shells, and offshore marker buoys. The operational boundary is the combination of saltwater abrasion and dynamic flexure; published fatigue data for this specific rotomoulded shell configuration is limited, so design qualification requires a prototype programme with service-level wave-frequency cycling rather than extrapolation from a datasheet value.
The operating windows for the six downstream tracks are consolidated below for incoming quality planning; the values are production guidelines rather than universal specifications.
| Downstream track | Key compliance standard | Formulation addition ratio | Peak internal air temperature | Nominal wall thickness |
|---|---|---|---|---|
| Potable water tanks and rainwater cisterns | FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, NSF/ANSI 61 | 100 parts; maximum 10 parts regrind | 200–220°C | 6–8 mm |
| Agricultural chemical storage tanks | EN 13575:2012, ASTM D543 | 100 parts; optional 1–2 parts UV masterbatch | 210–230°C | 8–12 mm |
| Marine buoyancy shells and dock floats | ISO 4892-2:2013, ISO 179-1 | 100 parts outer shell; PU foam fill post-mould | 190–210°C | 4–6 mm |
| Outdoor playground components | EN 1176-1:2017, ASTM F1487-21 | 100 parts; 2–3 parts dry-blend pigmented layer | 190–210°C | 3–5 mm |
| Underground wastewater tanks | EN 12566-1:2016 | 100 parts; maximum 10 parts clean regrind | 210–230°C | 8–12 mm |
| Mobile waste and recycling containers | EN 840-1:2012, EN 840-2:2012 | Outer skin 100 parts; recycled core up to 30 parts per 100 parts total | 200–220°C | 5–8 mm |
For outdoor playground enclosures, slide shells, and tunnel modules, the grey UV-stabilised LLDPE powder is processed on independent-arm rotomoulding machines with textured aluminium moulds. Compliance is assessed under EN 1176-1:2017 for general playground safety and ASTM F1487-21 for North American public playground equipment; the finished part is also screened against REACH Annex XVII restrictions for phthalates and PAHs before export. The formulation addition ratio is 100 parts Icorene 2550 UV+ GRY 7853; when multicolour parts are required, the grey structural base is isolated from bright dry-blend pigments by sequential charging, with the ground colour layer added at 2–3 parts per 100 parts total charge and the grey structural skin retained at 97–98 parts. Downstream production involves two-stage charging or a drop-box introduction: the main grey powder is loaded first, followed by the pigmented outer powder after the grey layer has begun to densify. The oven setpoint is 260–280°C, lower than tank moulding, to protect thin 3–5 mm walls and textured features from overbaking. Peak internal air temperature is clamped at 190–210°C. Demoulding cannot rely on high linear shrinkage because playground parts contain deep undercuts and rotationally moulded-in handgrips; mould release agents are applied to the aluminium cavity before every shot and the part is ejected below 60°C to reduce scuffing. Terminal products are slide bedways, tunnel sections, climbing panels, and rotationally moulded spring-rider bodies. The operational boundary is strict: the grade is not qualified for translucent or high-gloss rotomoulded playground components because the grey 7853 pigment produces a matte surface and hiding power, not an appearance-surface finish.
Buried wastewater tanks and pump chambers are rotomoulded with this grade because the UV-stabilised grey shell remains serviceable during extended above-ground yard storage before installation, while the polymer backbone provides the stress-crack resistance required in shifting soil. The industry compliance standard is EN 12566-1:2016 for prefabricated septic tanks. The formulation addition ratio is 100 parts Icorene 2550 UV+ GRY 7853 powder; a maximum of 10 parts of clean, dry in-house LLDPE regrind is allowed only in access covers and external non-load-bearing ribs, not in the main liquid-containing shell, because regrind variability lowers stress-crack resistance at the boss roots. Downstream production uses shuttle rotomoulding machines with fabricated steel or aluminium moulds reinforced to handle the 8–12 mm wall thickness. The oven setpoint is 280–300°C and the internal air temperature reaches 210–230°C; the cooling stage is extended to below 5°C/min from 120°C to 60°C to reduce frozen-in shrinkage forces at moulded-in ribs and access openings. Moulded ribs must maintain a root radius of at least 5 mm and a draft angle of at least 2° to avoid crack initiation during demoulding and soil loading. Terminal products are 2,000–5,000 L septic tanks, sewage holding tanks, and pump chambers. Hydrostatic testing after demoulding follows the manufacturer’s EN 12566-1 test programme; published data for this specific formulation in saturated clay soils is limited, so installers are instructed to follow the tank supplier’s bedding requirements for backfill material rather than relying solely on rotomoulded shell stiffness.
Rotomoulded mobile waste and recycling containers built with this grade are produced as large two-wheel and four-wheel bodies rather than thin-wall indoor bins. Compliance is governed by EN 840-1:2012 for two-wheeled containers and EN 840-2:2012 for four-wheeled containers, including drop tests, lid-abuse tests, and environmental stress-crack resistance after contact with waste leachate simulants. The formulation addition ratio for the outer UV-exposed skin is 100 parts Icorene 2550 UV+ GRY 7853 powder; in two-layer moulding, a recycled LLDPE core can be added up to 30 parts per 100 parts total charge, provided the finished container still passes the EN 840 low-temperature drop test specified in the relevant part. The downstream production process uses carousel or independent-arm rotomoulding machines with a two-shot charging sequence; the outer skin is loaded first, heated to partial densification, then the recycled core is introduced through the drop box, and the cycle continues until the full wall reaches peak internal air temperature of 200–220°C. Moulds are fabricated from aluminium with wear-resistant parting-line inserts because the large flat side panels cause differential cooling and require parting-line flash control. Nominal wall thickness is 5–8 mm, with thicker rims and wheel pockets. Terminal finished products include 120–1,100 L two-wheeled and four-wheeled waste and recycling containers used in kerbside collection. The grade is not selected for closed-body containers that need hot-wash compatibility above 80°C or conductive antistatic liners; those are outside the qualified envelope.
Competitive LyondellBasell Icorene 2550 UV+ GRY 7853 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 UV+ GRY 7853 is a linear low density polyethylene rotational moulding powder supplied with a pre-compounded grey color and a UV+ light-stabilization package. The model code identifies three components: the Icorene 2550 base resin series, the UV+ additive stabilization system, and GRY 7853 as the grey colorant formulation. This grade is intended for conversion by rotational moulding of hollow parts that require outdoor weathering resistance, low-temperature ductility, and consistent pigment dispersion. Lot-specific certificates of analysis provide the melt mass-flow rate measured at 190 °C with a 2.16 kg load according to ISO 1133-1:2022, density according to ISO 1183-1:2019, bulk density according to ASTM D1895-17, and particle size distribution by sieve analysis according to ASTM D1921-18. Because the pigment and UV stabilizer package alter melt rheology and density relative to natural powder, the grade-specific nominal values should not be inferred from general LLDPE ranges without consulting the manufacturer’s technical data sheet.
As a material class, linear low density polyethylene spans a density range of 0.915 g/cm³ to 0.940 g/cm³ when measured by ISO 1183-1:2019. Rotational moulding LLDPE powders typically require a melt mass-flow rate below 10 g/10 min at 190 °C/2.16 kg to maintain bubble-release control; the exact Icorene 2550 UV+ value is stated on the lot certificate. These class ranges are not product specifications, but they define the design space into which the grade is positioned.
In practice, this material is used for outdoor fluid storage tanks, agricultural hoppers, marine floats, and other hollow parts where a grey surface reduces the visual impact of soiling and provides a uniform factory-compounded color. The grey pigment contributes to ultraviolet opacity, but the primary weatherability is derived from the UV+ package. Processors handling this powder should not regard it as a natural LLDPE to which a dry colorant is added on the shop floor; the pre-dispersion step eliminates pigment agglomerates that otherwise appear as surface specks or reductions in tensile elongation. For colour consistency, measurements may be performed with a spectrophotometer using CIELAB coordinates under ISO 11664-4:2008; lot-to-lot agreement is normally specified as a ΔE tolerance in the supplier quality plan.
Production of a pre-compounded grey UV+ LLDPE powder typically involves melt compounding in a twin-screw extruder with a length-to-diameter ratio between 40:1 and 52:1, followed by pelletizing and cryogenic grinding to a controlled particle size distribution. This route is preferred over dry-blending because the UV stabilizer and grey pigment are distributed within each powder particle, reducing segregation during shipping and hopper discharge. Batch-to-batch color consistency is controlled through feeder calibration and spectrophotometric verification on moulded plaques. If a converter switches from dry-blended pigment to a pre-compounded grade, the elimination of free pigment can reduce dust in the plant and improve color uniformity, but the oven cycle may require adjustment because the melt absorbs infrared radiation differently from a natural powder with external pigment.
Outdoor failure in rotomoulded LLDPE is commonly driven by photo-oxidative chain scission that reduces tensile elongation at break, followed by surface chalking and eventual stress crack initiation. The UV+ system is designed to interrupt this sequence through radical scavenging and excited-state quenching. Typical light-stabilizer packages for moulding-grade LLDPE combine hindered amine light stabilizers with a UV absorber and, in grey grades, an opacifying pigment that reduces subsurface photoinitiation. Accelerated weathering of such compositions may be evaluated by xenon-arc exposure according to ISO 4892-2:2013, with comparative testing against a natural or black control after intervals of 500 h, 1000 h, and 2000 h. Because accelerated weatherability does not translate linearly to field service life, validation under actual use orientation and wet-dry cycling is required. Published data for this specific configuration is limited; lot-specific weathering data should be requested when the intended service exceeds continuous outdoor exposure of 2 years.
The grey colorant may also reduce solar heat absorption relative to black grades, which has implications for warpage in flat-wall tanks exposed to direct sunlight. Differential surface temperatures between sun-exposed and shaded walls can exceed 20 °C in black parts; grey grades moderate this gradient but do not eliminate it. The moulder should also measure retained tensile elongation at break per ISO 527-2:2012 after weathering rather than relying on visual color shift, because a modest ΔE may mask substantial embrittlement. Outdoor agricultural and marine applications subject the material to ultraviolet radiation, cyclic temperature changes, impact from stones or ice, and contact with chemicals. The choice of a UV-stabilized LLDPE is justified where specifications require minimum retained tensile elongation after accelerated weathering, often set at ≥50% of original value after 2000 h xenon-arc exposure per ISO 4892-2:2013. However, because not all formulations meet the same retained elongation, the exact acceptance level must be fixed by the end-user or OEM, not assumed from the grade name. The grey color does not convey chemical resistance; compatibility testing with actual service fluids at 40 °C or the maximum use temperature should follow ISO 175:2010 or ASTM D543-21.
On rotational moulding lines, the powder is processed in shuttle, carousel, or rock-and-roll machines with cast aluminium moulds or fabricated stainless steel moulds. Oven circulating air temperatures for LLDPE powders are commonly set between 280 °C and 320 °C, while the peak internal air temperature inside the mould is held between 190 °C and 210 °C. Residence time depends on wall thickness and mould mass; thin-wall parts may require only 12–18 min in the oven, while thick sections above 10 mm can require more than 30 min. These are processing starting points, not grade-specific specifications. The grey pigment alters heat absorption, so the thermal profile must be established with thermocouples inside the mould and validated by physical property retention rather than by visual melting alone.
A critical process conflict exists between bubble dissolution and thermo-oxidative degradation. Raising peak internal air temperature improves removal of trapped gas and increases impact strength up to a plateau, but exceeding 220 °C for extended periods consumes the antioxidant stabilizer and can shift the grey color toward yellow. Conversely, under-curing below 180 °C leaves incomplete particle fusion and lowers tensile impact performance. The acceptable peak internal air temperature range is therefore narrow, and production records should log both the oven set point and the internal air temperature curve for each cycle. On carousel machines with multiple arms, thermal reproducibility across arms can vary by ±5 °C; arm-to-arm validation is necessary before releasing production molds.
Particle size distribution of the powder directly influences dry-flow, cavity packing, and surface replication. Coarse fractions above 500 µm may cause pinholes and incomplete particle fusion at short oven cycles; excessive fines below 150 µm can increase dust generation and reduce bulk density. Rotomoulders can assess particle size distribution by ASTM D1921-18 using stacked sieves. For grey grades, fines may also carry a higher colorant concentration than coarse particles because of particle segregation during handling. Bulk density measured by ASTM D1895-17 should be monitored on incoming lots; changes greater than ±5% relative to the qualified baseline may indicate lot segregation or moisture uptake. Dry-flow behavior on production hoppers is often more sensitive to particle shape and static charge than the small density differences between natural and pigmented powder.
| Property evaluated | Standard method | Relevance to grey LLDPE rotomoulding |
|---|---|---|
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | Consistency of mould filling and bubble release |
| Density | ISO 1183-1:2019 | Stiffness, chemical permeability, and part mass |
| Bulk density | ASTM D1895-17 | Hopper flow and powder packing in mould cavities |
| Particle size distribution | ASTM D1921-18 | Surface replication and dry-flow behavior |
| Tensile yield strength and elongation at break | ISO 527-2:2012 | Mechanical durability and detection of processing degradation |
| Charpy notched impact strength at -20 °C | ISO 179-1:2023 | Low-temperature ductility in outdoor service |
| Environmental stress crack resistance | ASTM D1693-21 | Resistance to cracking in detergent or chemical exposure |
| Accelerated weathering | ISO 4892-2:2013 | UV+ stabilizer effectiveness and pigment fastness |
Rotomoulding powders do not generally require the same predrying as hygroscopic engineering resins, but surface moisture from condensation can create bubbles and surface defects in thick-walled parts. If the powder has been stored in unsealed containers at relative humidity above 60%, a drying cycle at 60–70 °C for 2–4 h is advisable before processing. Silo and hopper temperatures should remain below 50 °C to prevent additive blooming and pigment segregation. Contamination with iron or copper fines must be avoided because transition-metal residues accelerate thermo-oxidative degradation of polyethylene; hoppers, grinders, and mould release systems should be inspected for wear metals. External color concentrates and processing aids should not be assumed compatible: acidic or metal-stearate-based additives can antagonize hindered amine light stabilizers and reduce the outdoor performance of the UV+ package. Compatibility trials should compare accelerated weathering retention after 1000 h xenon-arc exposure per ISO 4892-2:2013 on both the control and modified compounds.
Direct exposure of the powder to ultraviolet radiation during storage should be minimized; prolonged UV exposure of the powder can consume stabilizer before processing. Storage in closed silos and opaque bags is therefore part of protecting the UV+ system. If the powder is stored at temperatures above 40 °C for extended periods, additive blooming and static charge accumulation may occur. Static charge can be reduced by maintaining relative humidity between 40% and 60%, but RH above 60% may increase surface moisture. These are operational boundaries established by general powder handling practice rather than grade-specific chemical limits.
In service, parts moulded from this grade are typically used in agricultural pesticide tanks, outdoor water storage tanks, marine buoys, and housings where a grey factory color is preferred. The selection of LLDPE rather than HDPE is often driven by environmental stress crack resistance in contact with detergent or mild chemical solutions, evaluated per ASTM D1693-21, and by low-temperature impact performance measured as notched Charpy impact per ISO 179-1:2023. The grey pigment provides opacity that may protect light-sensitive contents from visible-spectrum transmission, but the material should not be considered a barrier to oxygen or carbon dioxide; transmission rates are governed by wall thickness and test conditions such as 23 °C and 0% RH per ISO 15105-2:2014. Published data for this specific configuration is limited, and permeation behavior for aggressive solvents must be tested on the finished article.
For regulatory compliance, converters must verify whether the grey UV-stabilized grade meets the relevant food-contact, toy, and potable water requirements for their jurisdiction. Polyethylene homopolymers and copolymers may be covered by FDA 21 CFR 177.1520; however, the specific pigment and stabilizer formulation in GRY 7853 and the UV+ package may not be automatically cleared for direct food-contact or potable water use. European compliance must be assessed under EU 10/2011 for plastic food-contact materials and articles, with migration testing according to the relevant simulant and time/temperature conditions. RoHS compliance for electrical and electronic equipment housings should also be verified lot-by-lot, because grey pigments may contain limited regulated metals depending on the colorant system.
Compared with a natural LLDPE rotomoulding powder, the GRY 7853 variant eliminates separate dosing of carbon black or organic pigment masterbatch and reduces the risk of inconsistent color between cycles. The UV+ package provides a standardized base level of light stabilization; a natural powder may require the moulder to compound or dry-blend a UV masterbatch, which introduces weighing accuracy and dispersion variables. In terms of mechanical behavior, the grey pigment and stabilizers do not alter the fundamental linear low density polyethylene structure but can change the melt rheology enough that the optimum oven cycle may differ by several minutes. Moulders should not assume identical peak internal air temperature curves when switching from natural to grey.
Compared with a rotomoulding HDPE, the LLDPE grade generally has a lower flexural modulus and higher ductility in notched impact tests. Flexural modulus is evaluated by ISO 178:2019; a typical rotomoulding HDPE may show higher room-temperature stiffness, while an LLDPE grade may show higher Charpy impact at low temperature measured by ISO 179-1:2023. For load-bearing structural parts, creep modulus and long-term deflection under load must be re-evaluated according to ISO 899-2:2003, because LLDPE can creep to a greater extent than HDPE at the same wall thickness and applied stress. Chemical resistance is generally strong for both material classes, but environmental stress crack resistance for LLDPE in detergent solutions may be higher than for many HDPE rotomoulding grades when compared by ASTM D1693-21.
Compared with a conventional branched LDPE rotomoulding powder, the linear structure of LLDPE increases tensile strength and puncture resistance, as measured by tensile properties per ISO 527-2:2012 and falling weight or slow-rate puncture impact per ISO 6603-2:2000. The lower melt strength of linear grades can, however, produce different bubble-release behavior in thick sections. This is a practical difference in rotomoulding: LDPE can tolerate a wider oven window without severe sagging or pinholing, while LLDPE gives better mechanical toughness once the process is optimized.
| Evaluation dimension | LLDPE grey UV+ relative to natural LLDPE | LLDPE grey UV+ relative to rotomoulding HDPE | Reference method |
|---|---|---|---|
| Colour consistency | Higher due to pre-dispersed pigment package | Higher; HDPE natural requires external colourant | Spectrophotometric CIELAB |
| Weatherability | Higher due to UV+ package and grey pigmentation | Typically higher; HDPE grade may require UV package | ISO 4892-2:2013 |
| Flexural modulus | Similar to natural LLDPE; minor pigment effect | Lower; HDPE density/stiffness higher | ISO 178:2019 |
| Low-temperature impact | Similar to natural LLDPE | Higher than typical HDPE for ductile failure | ISO 179-1:2023 |
| Environmental stress crack resistance | Similar to natural LLDPE; pigment may affect surface initiation | Higher than typical HDPE; LLDPE more resistant | ASTM D1693-21 |
Within the Icorene family, the UV+ designation distinguishes the grade from non-UV versions that would require post-mould painting or external UV masterbatch. The GRY 7853 suffix further separates it from natural and black versions in the same base resin series. This suffix system is common in rotational moulding powder portfolios; changing only the color suffix can alter the optimum oven residence time because the pigment affects the absorption of infrared energy. Users moving from GRY 7853 to a black grade or to the natural version should not carry over the same cycle without re-mapping internal air temperature.
Grey parts can reveal surface defects differently from black or natural parts. Weld lines, internal air track marks, and parting line flash are often more visible in grey than in black. For appearance-critical applications, the mould should be verified for venting, and the demoulding temperature should be controlled. Demoulding while the part is too hot can produce post-mould warpage, particularly in flat-walled grey tanks where irregular wall thickness creates differential thermal contraction. A controlled cooling step in forced air at 20–30 °C is generally used before demoulding; water mist cooling must be applied uniformly because non-uniform cooling across a grey surface can induce local shrinkage differences. Dimensional inspection should include a check of flatness across large panels and a wall-thickness map using ultrasonic thickness testing, because rotomoulding wall thickness variation is affected by powder flow, mould rotation ratio, and oven airflow distribution.