Lyondellbasell Icorene 2550 Uv Grn 6426 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ GRN 6426 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ GRN 6426 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 716904
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Additive UV Stabilizer
    Color Green
    Density 0.935 g/cm³
    Melt Mass Flow Rate Mfr 3.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 17 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 800%
    Flexural Modulus 700 MPa
    Notched Izod Impact 500 J/m
    Vicat Softening Temperature 115 °C
    Melting Temperature 125 °C
    Environmental Stress Crack Resistance Escr >1000 hr
    Hardness Shore D 55

    As an accredited LyondellBasell Icorene 2550 UV+ GRN 6426 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 UV+ GRN 6426 Linear Low Density Polyethylene supplied in 25 kg moisture-proof bags, palletized for bulk handling.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell Icorene 2550 UV+ GRN 6426 LLDPE, 25 kg bags, palletized, stretch-wrapped, secured; approx. 18–20 MT net.
    Shipping Shipping description: LyondellBasell Icorene 2550 UV+ GRN 6426 LLDPE is a non-hazardous polymer resin, supplied as pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep dry, avoid excessive heat and ignition sources. No UN number, hazard class, or marine pollutant designation required. Follow local transport regulations.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged storage near strong oxidizers, solvents, or odorous materials. Maintain ambient temperatures, protect from UV degradation, and use original packaging on pallets. Ensure good housekeeping and follow local regulations. Use normal warehouse handling.
    Shelf Life Shelf life is typically 12 months when stored in original, unopened packaging in a cool, dry, well-ventilated area.
    Application of LyondellBasell Icorene 2550 UV+ GRN 6426 Polyethylene, Linear Low Density

    Icorene 2550 UV+ GRN 6426 is a UV-stabilised linear low density polyethylene powder supplied by LyondellBasell for rotational moulding. Producer-published nominal values include density 0.935 g/cm³ under ASTM D1505 and melt flow rate 5.0 g/10 min under ASTM D1238 at 190°C/2.16 kg. The green 6426 colour package is pre-compounded into the powder. Applications are specified where a component requires outdoor weathering, chemical stress-crack resistance, low-temperature ductility and moulded-in colour.

    Agricultural Sprayer Tanks and UV-Stabilised Chemical Containment

    Rotational moulding lines producing agricultural sprayer tanks use shuttle machines or carousel machines with mould charges calculated for a nominal wall thickness of 6 mm to 10 mm. The powder is charged into cast aluminium or fabricated steel moulds. Heating occurs in a forced-air oven at 280°C to 320°C. Internal air temperature is held at 190°C to 205°C for full consolidation. The rotation ratio is set at 4:1 to 5:1 on major and minor axes. Cooling begins with forced ambient air, then water mist, until demould temperature falls below 60°C. This sequence minimises warpage in flat sidewalls and threaded inserts. Tanks produced in this grade carry non-potable agricultural chemicals. Stress-crack resistance is validated under ASTM D1693-15 condition C. The density of 0.935 g/cm³ supports F50 values typically above 1,000 h in this test. UV retention is assessed by ISO 4892-2 method A. The integrated UV package retards surface oxidation and chalking. Moulded-in green 6426 eliminates post-mould wet painting. Colour consistency is controlled by spectrophotometric ΔE targets at receiving inspection. Chemical resistance is specific. The grade is compatible with many dilute agrochemical formulations but not with concentrated oxidisers, strong acids at elevated temperature, or aromatic solvents. Converters must run immersion tests under ASTM D543 using the actual tank formulation before serial production.

    ApplicationTest methodTypical acceptance criterion
    Agricultural sprayer tanksASTM D1693-15 condition CF50 above 1,000 h
    Outdoor UV weatheringISO 4892-2 method AΔE ≤ 10 after 2,000 h
    Low-temperature impactASTM D746Ductile failure at -20°C
    Chemical compatibilityASTM D543No surface cracking or weight change above 2%

    Marine buoyancy shells moulded from this grade are produced on carousel-type machines with steel or cast aluminium moulds. Wall thickness is typically 8 mm to 12 mm for impact resistance against docks and vessel hulls. The mould is charged with powder and a polyurethane foam system is injected after demoulding. Low-temperature ductility is tested under ASTM D746 or ISO 812. The material is selected because rotomoulded LLDPE in this density range retains ductile failure below -20°C. Seawater resistance is evaluated by long-term immersion under ASTM D543 and by UV exposure under ISO 4892-2. A critical process boundary is the rate of cooling from 200°C to 70°C. Forced air cooling is preferred over water quench for thick marine shells to reduce residual stress. Stress relaxation around moulded-in stainless steel lifting eyes is checked by sectioning after pull-out testing to 1.5 times the service load. The green pigmentation is present through the wall. Abrasion from beach handling does not expose unpigmented resin. Published data for the filled foam composite configuration is limited. Converter-specific drop tests and foam adhesion checks are required before serial production.

    What Limits Low-Temperature Impact Retention in Roto-Moulded Playground Platforms?

    The limiting variable is not initial impact strength but retained instrumented puncture energy after outdoor weathering. Exterior playground platforms, roof caps, slides and climbing panels are rotationally moulded with nominal wall thickness from 5 mm to 8 mm. Moulds are run on independent-arm carousel machines. Impact resistance is measured by ISO 6603-2 instrumented puncture or ASTM D3763. Converters specify ductile failure at -10°C after 2,000 h of ISO 4892-2 exposure. UV+ stabilisation delays embrittlement but does not eliminate progressive oxidation at surface gloss boundaries. Designers therefore specify minimum outside radii of 10 mm and avoid sharp ribs that create stress concentration. Moulded-in colour is evaluated for ΔE under ISO 7724. The 6426 green batch is checked against master standards on each lot. The powder must be dry-flowable. Moisture content above 0.03% by weight can cause pinholing in thin-wall panels. Pre-drying is required when storage humidity exceeds 60% RH. Gate marks are removed by trimming and the trimmed edge is flame-treated only when a secondary bond is required.

    When Internal Air Temperature Exceeds 205°C, Post-Mould Warpage and Colour Shift Require Quantification

    Process audits on shuttle-type rotational moulding lines show that raising internal air temperature beyond 205°C does not improve impact strength. The polymer reaches full consolidation at 190°C to 205°C. Above 205°C, cycle time increases and the melt can degrade at the inner surface. Degradation is detected as a yellowish shift in the green 6426 value and a reduction in ASTM D638 tensile elongation at break. Thermo-oxidative stability is measured by ASTM D3895 differential scanning calorimetry. A shift in oxidative induction time of more than 20% from the virgin powder lot indicates over-cure. Oven set point should be 280°C to 320°C. The mould surface temperature must not exceed 260°C for this grade. Rotational speeds are held at 4:1 primary-to-secondary axis. Warpage after cooling is quantified by placing the part on a granite surface plate and taking dial indicator readings across a 300 mm span. Deviation above 3 mm is rejected for flat tank sidewalls. Cooling below 60°C before demoulding is mandatory for parts with moulded-in inserts.

    Processing parameterTypical setting or requirementMeasurement device
    Oven air temperature280°C to 320°CForced-air oven thermocouple
    Internal air temperature190°C to 205°CInternal air probe
    Mould surface temperatureBelow 260°CContact pyrometer
    Major/minor rotation ratio4:1 to 5:1Axis speed check
    Demould temperatureBelow 60°CInfrared pyrometer
    Powder moistureBelow 0.03% by weightKarl Fischer titration

    In cold-store and food-processing material handling, solid-wall pallets and dunnage trays are rotationally moulded from Icorene 2550 UV+ GRN 6426. The dimensions are commonly 1,200 mm × 1,000 mm × 150 mm. Wall thickness ranges from 5 mm to 8 mm. Interchangeable inserts create anti-slip top surfaces. The grade provides low-temperature impact resistance under ASTM D5420 or ASTM D3763. Failure in cold-room service must remain ductile at -30°C. Cleanability is evaluated by repeated washdown with 60°C alkaline detergent. Stress-crack resistance under ASTM D1693 condition C is reviewed after 100 washdown cycles. The green 6426 colour allows colour-coding of operational zones. The resin is not recommended for continuous immersion in concentrated hypochlorite solutions. Cracks may initiate at gate marks or sharp internal corners. Corner radii should not fall below 8 mm for pallet feet.

    Outdoor Electrical Enclosures and Telemetry Cabinets

    Outdoor electrical enclosures roto-moulded in this grade are specified where the cabinet must withstand direct sunlight, rain, dust and occasional impact. Moulds are fitted with brass or stainless steel threaded inserts to receive door hinges and mounting rails. Wall thickness ranges from 5 mm to 7 mm. Ingress protection is verified to IEC 60529 with IP65 or IP66 after insert moulding. UV resistance is assessed under ISO 4892-2. The moulded-in green colour retains ΔE below 10 after 2,000 h in xenon arc testing. Dimensional stability after thermal cycling from -30°C to 60°C is checked with ISO 75-2 deflection temperature and with thermal cycling on sealed enclosures. The LLDPE matrix has lower stiffness than glass-reinforced polyester. Large flat doors require ribbing or steel backing frames to limit deflection below 10 mm under a 500 N point load. Earthing bosses and cable glands are welded or spin-welded. Spin welding speed is set at 1,500 rpm to 2,000 rpm for 2 s to 4 s to avoid melt fracture. The material should not be used in continuous exposure to concentrated mineral acids or in direct contact with ketones.

    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ GRN 6426 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 UV+ GRN 6426 is a linear low density polyethylene rotational moulding powder supplied as a pre-compounded green compound. The grade designation separates three functional elements: the base 2550 powder, the UV+ stabilization system, and the GRN 6426 green colour match. The material is delivered as a free-flowing powder for closed-mould biaxial rotational moulding, not as pellets for injection moulding, film extrusion, or blow moulding. Published industrial documentation for the natural 2550 base resin identifies a density near 0.935 g/cm³ and a melt flow rate near 5.0 g/10 min at 190 °C and 2.16 kg load. Pre-compounded colour and stabilizer carriers may shift these values on a lot-specific basis; certification release should therefore be made from the certificate of analysis rather than generic literature.

    Why does the UV+ designation alter outdoor service life validation for rotomoulded parts?

    The UV+ package is not a topical coating or a post-moulding treatment. It is a compounded stabilization system intended to delay photo-oxidative chain scission, surface microcracking, and impact loss in outdoor rigid parts. The exact stabilizer chemistry is proprietary to the manufacturer. Systems of this class in polyolefin rotational moulding commonly combine a hindered amine light stabilizer with a UV absorber, but the specific ratio, carrier resin, and synergistic co-additives for GRN 6426 are not disclosed in public technical literature. Accelerated weathering comparisons are typically performed under ISO 4892-2 using xenon-arc exposure with controlled irradiance and black-standard temperature. Field service life cannot be derived from a single accelerated weathering interval because ultraviolet dose, part thickness, surface orientation, temperature cycling, and pigment loading all modify the observed degradation rate. Photo-oxidation in polyethylene is commonly tracked by an increase in carbonyl index measured by transmission Fourier transform infrared spectroscopy, but published carbonyl index data for this exact grade are limited. For a production part, validation should include retained tensile elongation, low-temperature impact, and surface colour change on moulded plaques of the intended wall thickness after xenon-arc or outdoor exposure at the intended service location.

    For processing, the powder is charged into a cold or preheated closed mould mounted on a biaxial carousel or shuttle rotational moulding machine. Oven air setpoints for this melt-flow class are commonly maintained between 260 °C and 315 °C, while the peak internal air temperature is controlled to approximately 200 °C. Demoulding is normally initiated after the internal mould surface temperature has fallen below 70 °C. A wall thickness of 3 mm to 6 mm is typical for tanks, containers, and covers; thicker sections require longer oven residence and may develop internal voids if the powder has not fully sintered before melt densification. During mould rotation, primary and secondary speed ratios are commonly set between 4:1 and 6:1 for cylindrical parts, but the correct ratio is geometry-dependent. Incorrect rotation ratios can produce thinning at the poles or the equatorial plane. Cooling with forced air followed by controlled water mist reduces warpage in large flat panels, while excessively rapid water quenching can increase shrinkage and surface marking. The powder is not hygroscopic, but stored material should be protected from standing water or condensation because surface moisture can create steam defects and impair surface finish. Contamination by polypropylene, polyvinyl chloride, paper dust, or sand interferes with particle coalescence and leads to pinholes, delamination, or brittle zones.

    Rheology and particle size requirements for biaxial sintering in closed moulds

    Rheologically, the material is intended to provide sufficient low-shear viscosity to limit melt drainage from vertical mould walls during heating while retaining enough melt flow for particle coalescence at conventional rotomoulding temperatures. The nominal melt flow rate of 5.0 g/10 min places the grade in the upper melt-flow range for thick-wall rotomoulding. Higher melt flow grades fill thin features more readily but may sag on deep vertical sections; lower melt flow grades improve wall uniformity but require longer sintering and may trap air. The powder particle size distribution is equally critical. Industrial rotomoulding powders are commonly classified through a 35-mesh sieve with an opening of 500 µm, with most of the distribution falling between 150 µm and 425 µm. Coarse particles sinter slowly and can leave pit marks, while excessive fines increase dry-flow variability and uneven charging. Dry-flow behaviour is measured by funnel methods such as ISO 6186. A free-flowing powder reduces bridging in feed hoppers and permits uniform wall thickness distribution during multi-axis rotation.

    DescriptorTest methodRepresentative valueUnit
    DensityISO 1183-1 / ASTM D15050.935g/cm³
    Melt flow rate, 190 °C, 2.16 kgISO 1133-1 / ASTM D12385.0g/10 min
    Tensile yield stressISO 527-217MPa
    Elongation at breakISO 527-2700%
    Flexural modulusISO 178650MPa
    Vicat softening temperature, A50ISO 306115°C
    Environmental stress crack resistance, condition BASTM D16931000h

    The values above are representative for the natural 2550 base resin, not specification minima for the pigmented GRN 6426 compound. A pre-compounded green concentrate can alter density, melt flow, modulus, and impact by a few percent depending on pigment dispersion, carrier melt index, and dilution ratio.

    When Green 6426 pigment shifts crystallization, shrinkage, and low-temperature impact retention

    The green pigment is not an inert tracer. Pigment particles can act as nucleating agents, increasing crystallization temperature and reducing spherulite size in linear low density polyethylene. This can reduce warpage in large flat panels but may increase isotropic shrinkage relative to an unpigmented powder. The magnitude depends on pigment particle size, dispersion quality, and processing temperature. For critical outdoor tanks, low-temperature drop impact testing should follow ISO 6603-2 or an equivalent instrumented impact method. The pre-compounded product eliminates separate weighing of pigment masterbatch at the moulding machine, reducing dry-blend error and colour variation across multiple production lots. It is typically considered for outdoor tanks, agricultural chemical containers, dock floats, industrial covers, and other thick-wall parts where ultraviolet resistance and green colour are required together. However, the pigment package alone does not protect the part from mechanical damage, abrasion, or aggressive chemical attack.

    Operational boundaries include avoiding prolonged melt temperatures above 300 °C. Oxidation at the inner mould surface can generate carbonyl species and reduce impact toughness; the peak internal air temperature should therefore be limited to approximately 200 °C to 220 °C unless process trials confirm acceptable retained properties. Oven residence should be controlled by the internal air temperature plateau and not by fixed time alone, because mould mass, wall thickness, and oven loading all alter the heating rate. Mould surfaces should be prepared with non-siloxane release systems; excessive release agent can inhibit particle fusion and create surface porosity. The material should not be blended with crosslinkable high density polyethylene or incompatible recycled feedstocks unless the complete melt stream is evaluated for rheology, pigment distribution, and impact retention. Published data for combinations of this grade with post-consumer rotomoulding recyclate are limited.

    Comparative engineering properties against HDPE and unmodified LLDPE powders

    Relative to a rotomoulding high density polyethylene of density near 0.945 g/cm³, the 0.935 g/cm³ linear low density polyethylene grade has lower flexural modulus and lower tensile yield stress but typically demonstrates higher environmental stress crack resistance and better low-temperature impact. For tank walls, the lower stiffness may require an increase in wall thickness or the addition of ribs to maintain deflection limits, while the improved environmental stress crack resistance supports use with more aggressive liquids and sustained outdoor exposure. Relative to an unmodified LLDPE rotomoulding powder, the UV+ GRN 6426 grade eliminates the need to meter separate pigment and stabilizer masterbatch at the machine, but the pigment package may slightly increase melt viscosity and therefore require a higher oven setpoint or longer sintering time. Compared with film-grade LLDPE, this product is intentionally produced in powder form with a higher melt flow rate and a stabilization system matched to thick rotomoulded sections rather than thin films. Film-grade resins should not be substituted in biaxial rotational moulding because pellet-based particle size and film additive systems are not optimized for powder sintering and wall formation.

    Compliance evaluation for a moulded article should include the following matrix where applicable:

    EvaluationStandard or regulationCondition
    Melt flow rateISO 1133-1 / ASTM D1238190 °C, 2.16 kg
    DensityISO 1183-1 / ASTM D150523 °C
    Vicat softening temperatureISO 306 / ASTM D1525A50 method
    Environmental stress crack resistanceASTM D1693Condition B, 100% Igepal
    Xenon-arc weatheringISO 4892-2Method A, daylight filter
    Restriction of hazardous substancesEU RoHS 2011/65/EUSupplier declaration for pigment and stabilizer package
    Chemical resistanceISO 175Moulded plaques, chemical-specific immersion

    Chemical compatibility follows the general behaviour of linear low density polyethylene: aqueous acids, alkalis, and salt solutions are normally tolerated at ambient temperature, whereas aromatic hydrocarbons, chlorinated solvents, and strong oxidizing acids can cause swelling, softening, or stress cracking. For a specific chemical at elevated temperature, testing on moulded plaques according to ISO 175 is required. The UV+ package should not be interpreted as allowing indefinite outdoor exposure; surface cleaning with abrasive pads or high-pressure hot water can accelerate removal of stabilized surface layers. Lot-to-lot variation in pigment dispersion can affect retained impact, so incoming inspection should include melt flow rate, particle size distribution, dry flow, and colour measurement against a retained standard.