| HS Code | 611792 |
| Product | LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.925 g/cm³ |
| Melt Flow Rate | 5.0 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 15.0 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Tensile Modulus | 276 MPa |
| Hardness Shore D | 50 |
| Vicat Softening Point | 90°C |
| Melting Point | 122°C |
| Brittleness Temperature | -70°C |
| Color | Green |
| Uv Stabilization | Yes |
| Processing Method | Rotational Molding |
As an accredited LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Icorene 2550 UV+ GRN 6006 is supplied in 25 kg moisture-resistant polyethylene bags, palletized with 40 bags per pallet (1,000 kg total). |
| Container Loading (20′ FCL) | LyondellBasell Icorene 2550 UV+ GRN 6006 Linear Low Density Polyethylene, loaded in 20′ FCL container, securely palletized for ocean shipment. |
| Shipping | LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density, is non-hazardous and not regulated for transport. Ship in 25 kg bags, boxes, or bulk containers. Store cool, dry, and out of direct sunlight; avoid dust generation and use standard PPE. No special ventilation required; normal freight handling is suitable. |
| Storage | Store LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density, in a cool, dry, well-ventilated area in closed original packaging. Keep away from direct sunlight, heat, ignition sources, moisture, and strong oxidizers. Maintain clean, dust-free conditions; use first-in, first-out rotation. Avoid excessive stacking, and protect bags from tearing, punctures, or contamination. Do not store outdoors unprotected. |
| Shelf Life | Shelf life is typically 12 months from manufacture when stored unopened, dry, cool, and away from direct sunlight and heat. |
In agricultural fertigation and low-pressure liquid storage, LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density is processed as a precompounded green rotomoulding powder rather than as a pellet compound. Powder charging is calculated from the projected outer surface area and the specified minimum wall thickness; for a 5000 L upright tank with a nominal wall of 8 mm, shot weight is generally in the range of 85–95 kg. The powder is typically supplied with a particle-size distribution passing a 35 mesh screen (500 µm), and bulk density variations across silo batches should be controlled within ±0.03 g/cm³ to maintain consistent charge weights. A dual-axis carousel machine with a primary/secondary rotation ratio of 4:1 and speeds of 5/1.5 rpm is a common starting configuration for 7–9 mm sections. Oven set points are maintained between 285 °C and 300 °C, and the part is removed only after the peak internal air temperature measured by a Rotolog probe or equivalent internal thermocouple remains at 195–205 °C for a minimum plateau of 2–4 min. The cooling profile is staged: 5–8 min of forced ambient air, water mist until the mould surface reaches 60–70 °C, and then fixture cooling to prevent base distortion. The precompounded GRN 6006 colour removes the need for in-plant masterbatch let-down at the moulding cell; however, clean in-house regrind from the same grade is typically limited to 15–20 wt% because higher additions are associated with a measurable reduction in Charpy notched impact energy under ISO 179-1:2010 and a loss in stress-cracking resistance under ASTM D1693-15. Fitting bosses, outlet threads, and baffle mounts are spin-welded or hot-plate welded from matching LLDPE stock, and welded assemblies are destructively tested under ISO 527-2:2012 conditions. Regulatory qualification for the finished tank commonly references ASTM D1998-21 for upright polyethylene storage tanks and ISO 17855-1:2014 for polyethylene moulding and extrusion materials. Contact with potable water should not be assumed from the base polymer alone; the base LLDPE may fall under 21 CFR 177.1520(c), but the pigment and stabiliser package must be separately cleared under the applicable drinking-water or food-contact regulation, such as EU Regulation (EU) No 10/2011 when relevant. Strong oxidizing acids, ketone solvents, and aromatic hydrocarbon streams are not acceptable service media for this material at continuous temperatures above 40–60 °C, because environmental stress cracking accelerates with increasing chemical activity and wall stress.
Representative starting process windows for a dual-axis carousel machine are set out below. These are not substitutes for part-specific mould optimisation.
| Nominal wall thickness class | Oven set point (°C) | Peak internal air temperature (°C) | Oven residence time (min) | Primary/secondary rotation speed (rpm) | Rotation ratio |
|---|---|---|---|---|---|
| 4–6 mm | 280–290 | 190–195 | 20–30 | 6/1.8 | 4:1 |
| 7–9 mm | 285–300 | 195–200 | 30–40 | 5/1.5 | 4:1 |
| 10–15 mm | 290–310 | 200–210 | 45–65 | 4/1.2 | 3.5:1 |
Accelerated weathering of green rotomoulded exterior components is carried out under ISO 4892-2:2013 cycle 1 using xenon-arc irradiation with controlled irradiance at 340 nm and black-standard temperature of 65 °C, or under ASTM G154-16 cycle 1 using UVA-340 fluorescent lamps. Colour shift is measured under CIE D65/10° geometry and reported as ΔE*; gloss retention is assessed under ISO 2813:2014 at 60° incident angle. For UV-stabilised LLDPE grades, oxidative degradation commonly appears first as surface microcracking and localised gloss loss on high-stress regions, such as the outer radius of a moulded-in handle or a threaded boss. Because the green pigment is precompounded at the resin supplier, the processing plant cannot adjust pigment tone by dry-blending; colour consistency therefore depends on maintaining uniform powder bulk density during silo storage and avoiding segregation during pneumatic transfer. Hygroscopic uptake is not a primary concern for polyethylene, but condensation on cold powder can introduce pinholes; if sacks are stored below dew point, pre-drying at 60–70 °C for 2–4 h in a dry-air hopper is recommended before charging. Published data for this exact GRN 6006 precompounded colour under a specific xenon dose are limited, so multi-year colour retention sign-off for a particular part should be based on a part-specific weathering protocol rather than a generic resin datasheet. The UV package does not eliminate the need for mould release control; residual silicone release agents can increase dirt pickup and create differential surface degradation under UV exposure.
For freshwater ponds, aquaculture raceways, and small-harbour float systems, the same grade is rotationally moulded as a hollow closed-cell shell. Shell wall thickness is commonly 5–9 mm, and the primary-axis/secondary-axis rotation ratio is set to 3.5:1 to 4:1 to improve powder distribution around the rotational centre. Peak internal air temperature is held between 195 °C and 205 °C; lower temperatures produce pinholes at the mould parting line, while higher temperatures darken the green surface and generate gas porosity from mould release degradation. After demoulding, closed-cell polyurethane foam is injected when positive buoyancy is required, and the pour hole is closed by heated-tool welding a moulded cap according to DVS 2207-1. The exotherm of the foam fill can briefly raise the inner shell wall above 90–100 °C; therefore foam expansion pressure and rise time must be controlled to avoid post-mould distortion. Buoyancy bodies intended for navigation are outside the scope of generic plastic material approval; green is recognised as a starboard lateral mark colour under IALA recommendations, but local competent-authority certification of luminance and chromaticity coordinates must be obtained. Low-temperature impact of the hollow shell is assessed under ISO 179-1:2010 on notched specimens machined from the tank wall, and puncture resistance under ISO 6603-2:2000. The operational boundary is continuous immersion: the UV-stabilised grade is designed for above-waterline outdoor exposure; below-sediment or chemically contaminated water service requires long-term ESCR testing under ASTM D1693-15 because wetting agents accelerate crack growth in stressed sections around inserts. Published data for this exact green 6006 compound under marine biofouling and cyclic salt-spray conditions are limited, so immersed-service validation should be conducted on the complete moulded article.
Thin-wall landscape components such as planter liners, litter bin bodies, and playground shell elements are moulded at 3–5 mm wall thickness in polished aluminium or electroless-nickel tooling. The powder is charged to produce a controlled wall tolerance of ±0.3 mm on flat surfaces when the mould is fitted with thermocouple arrays; internal air temperature is the primary control variable, not oven timer alone. Oven residence time is shortened to 18–26 min at 280–290 °C, followed by forced-air cooling for 10–12 min and then water mist to lower the demoulding temperature. Rapid cooling reduces cycle time but increases residual stress and warpage in large flat panels; production trials show that warpage on a 600 mm wide planter wall can exceed 2 mm when the part is demoulded at 100 °C instead of 65–75 °C. Surface defects such as orange peel and porosity are controlled by mould release selection; silicone release agents can migrate into the outer polymer layer and alter subsequent adhesion of printed or bonded trim. Mechanical acceptance for landscape components is usually based on ISO 527-2:2012 tensile property retention and ISO 179-1:2010 impact after weathering, not on the raw-powder melt flow rate. The precompounded green colour provides a visual match to park furniture specifications, but gloss and colour should be compared on a full-thickness moulded plaque, not on a compression-moulded test plate. When used in playground equipment, the complete assembly must meet EN 1176-1:2017 or ASTM F1487-21; the resin supplier does not certify the finished structure.
Where the stored liquid is classified as water-polluting, a single-piece rotomoulded bund or spill pallet is specified because the absence of weld seams removes the primary leak path. The grade is moulded at a floor thickness of 8–12 mm, with corner radii kept above 25 mm to reduce internal stress concentration. The outer containment volume is sized for 110% of the largest inner storage container as a minimum under common secondary-containment regulations; the SPCC rule under 40 CFR 112 specifies adequate containment capacity but does not specify a polymer grade. Chemical compatibility is assessed under ASTM D543-21 using representative test liquids; the LLDPE matrix resists many aqueous salts, weak acids, and alkalis, but should not be used with strong oxidizing acids, ketones, or aromatic hydrocarbon streams at elevated temperature. Because the green 6006 compound contains a UV stabiliser rather than a conductive carbon black package, it is not rated for storing flammable liquids where static discharge is a risk. Moulding experience shows that the sump floor is the critical zone for impact; full-container drop impact is often tested from 900 mm onto a concrete floor at −20 °C. Such tests should be run under ISO 6603-2:2000 conditions, and the specimen should be cut from the moulded sump corner, not from a flat plaque.
| Requirement | Standard or method | Use in containment article qualification |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Incoming powder lot verification at 190 °C/2.16 kg |
| Density | ISO 1183-1:2019 | Base material identity and charge-weight calculation |
| Notched impact strength | ISO 179-1:2010 | Low-temperature performance of sump corner specimens |
| Environmental stress cracking | ASTM D1693-15 / ISO 22088-3:2006 | Service fluid selection and insert area validation |
| Chemical resistance | ASTM D543-21 | Compatibility screening with stored liquids |
| Accelerated weathering | ISO 4892-2:2013 / ASTM G154-16 | Outdoor UV performance of exposed outer walls |
| Upright storage tank standard | ASTM D1998-21 | Finished tank material and fabrication requirements |
Refuse collection bodies and curbside rollout bins are produced on large carousel rotomoulding lines where the dominant throughput constraints are powder densification and mould release. For a 240 L curbside bin body with 5–6 mm wall, the mould is charged with approximately 11–14 kg of powder; oven temperature is set at 285–300 °C, and the peak internal air temperature is driven to 195–205 °C. The green 6006 precompounded grade eliminates pigment metering at the machine, but transfer lines must be cleaned between product changes because coloured powder carry-over creates visible contamination. Impact resistance is measured after conditioning for 72 h at −20 °C under ISO 179-1:2010, and UV exposure is validated under ISO 4892-2:2013 cycle 1 for no significant change in tensile yield stress after 2000 h. Dimensional stability is checked by measuring the body opening diagonal to ±2 mm after 48 h post-mould conditioning; this is a production-line control, not a resin property. The operational boundary is in hot, high-UV climates where the bin surface temperature may exceed 70 °C; at that surface temperature, warpage risk is dominated by mould design and wall thickness, not by the neat-polymer heat deflection temperature. Assembly with wheels and axles requires mechanical fasteners designed to avoid stress-cracking at holes; bolt torque must be limited so that hoop stress around an insert does not exceed the material’s environmental stress-cracking threshold under ASTM D1693-15.
Competitive LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 UV+ GRN 6006 Polyethylene, Linear Low Density is supplied as a pre-compounded rotational moulding powder. The product designation separates the 2550 series LLDPE rheology class, the UV+ stabilisation package, and the GRN 6006 green colour code. The base polymer is an ethylene-α-olefin linear low-density polyethylene intended for low-shear consolidation against heated mould surfaces in biaxial carousel, shuttle, rock-and-roll, and open-flame rotational moulding equipment. Unlike injection moulding or extrusion grades, process characterisation does not begin with screw recovery or injection pressure; the relevant inputs are powder dry flow, particle-size distribution, bulk density, mould surface temperature, oven air temperature, and internal air temperature. The material is commonly specified for hollow outdoor articles such as water tanks, agricultural chemical reservoirs, light-duty marine components, and landscape parts with wall sections in the range of 2.5 mm to 12 mm. Outside this envelope, production-scale processing reports commonly show increased pinhole risk in thin sections and void formation in thick sections.
The powder is not interchangeable with natural LLDPE of the same nominal melt flow rate. The green pigmentation modifies radiant heat absorption in the oven; on forced-air carousel machines, operators may need to lower oven temperature by 10–15 °C or reduce residence time by 2–4 min when wall thickness exceeds 6 mm, although published data for this specific GRN 6006 configuration is limited. Instrumented internal air-temperature measurement is mandatory. Peak internal air temperature should be maintained within 190–205 °C for the LLDPE matrix, while the mould surface remains in the melt-sintering range. If the cycle developed for a natural rotomoulding LLDPE is retained, wall-thickness gradients of 15–25% between thick and thin sections can appear on multicavity cast-aluminium or steel tools.
First, certificate of analysis values for melt flow rate and density must be compared against the incumbent grade. In rotational moulding, a melt flow rate shift of 1 g/10 min can alter bubble removal, knit-line integrity, and wall-thickness distribution. Second, particle-size distribution should be measured by dry sieving per ASTM D1921 or equivalent. Rotational moulding powders in this class are generally controlled to a maximum particle diameter of 500–600 µm, with fines below 150 µm limited to reduce static, dusting, and non-uniform mould filling. Third, dry flow should be confirmed by ASTM D1895-96 Method A. A dry-flow value below 20 s/50 g is often applied as a screening limit for uniform powder laydown, but supplier release limits take precedence for the GRN 6006 lot.
| Property | Test method | Typical range for the 2550-series LLDPE class |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 4.0–6.0 g/10 min at 190 °C/2.16 kg |
| Density | ISO 1183-1:2019 Method A | 0.930–0.940 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 Type 1B, 50 mm/min | 14–18 MPa |
| Elongation at break | ISO 527-2:2012 | >500% |
| Flexural modulus | ISO 178:2019 | 500–700 MPa |
| Vicat softening temperature | ISO 306:2022 A50 | 110–120 °C |
| Melting peak temperature | ISO 11357-3:2011 at 10 °C/min | 120–128 °C |
The terminal column in Table 1 is a class-level envelope, not a single-lot guarantee. Lot-specific values are controlled by the supplier certificate of analysis, and any substitution into an existing tool should be validated against the actual viscosity and density data of the GRN 6006 powder. No single table replaces instrumented trials on the target tool because wall thickness, oven air distribution, mould parting-line design, and rotational speed ratio all influence the consolidation outcome.
Powder dry-flow measurements require conditioning in closed containers between 18 °C and 25 °C. Exposure to relative humidity above 60% can permit surface moisture adsorption on the high-surface-area powder. The resulting steam evolution can generate pinholes and weld-line porosity during the sintering phase. When such exposure occurs, pre-drying in a dehumidified hopper at 60 °C for 1–2 h is commonly applied; published data for this specific GRN 6006 configuration is limited, so the dryer profile should be confirmed by moisture measurement rather than time alone.
The UV+ package in this grade is a proprietary stabiliser system. In rotomoulding compounds of this type, the stabilisation mechanism generally relies on hindered amine light stabilisers and a UV absorber, but the exact composition is not disclosed. The green pigment is pre-dispersed, eliminating the need for dry blending of masterbatch at the moulding facility. Dispersion quality can be assessed on compression-moulded films or plaques by optical microscopy, using the procedures of ISO 18553 for pigment agglomerate counting. Poor dispersion in a pigmented rotomoulding powder can produce local orientation, surface roughness, and reduced elongation at break; therefore incoming material should be checked for agglomerates larger than 50 µm if visual inspection of moulded parts shows colour streaking or dull patches.
Accelerated weathering for the green formulation should follow ISO 4892-2:2013 for xenon-arc exposure, with service life estimated only after comparison with outdoor exposures such as ISO 877-1 or Florida/Arizona reference ageing. No public endurance threshold is available for this GRN 6006 formulation, and accelerated hours do not translate linearly to field life. The UV+ package retards carbonyl formation and surface craze initiation, but the actual weathering response depends on pigment dispersion quality, part thickness, mould release residue, antioxidant consumption, and exposure orientation. Quality plans should therefore require retention of tensile elongation and visual appearance after a defined weathering interval that is tied to the geographic service environment, rather than relying on a single universal xenon-arc time.
In handling, the powder accumulates static charge at low humidity, particularly below 30% RH. Grounding of mixers, transfer lines, and collection hoppers is required to avoid uneven flow and dust explosion risk. Equipment cleaning is also a production-scale constraint: when switching from GRN 6006 to natural rotomoulding powder, residual green fines can contaminate unpigmented weld lines and cause visible colour streaks. Purge protocols should include mechanical brushing of the mould, vacuum cleaning of powder boxes, and characterisation of the first-shot surface after colour change.
Replacing this LLDPE grade with an HDPE rotational moulding resin typically raises flexural modulus from 500–700 MPa to 800–1200 MPa, but reduces low-temperature impact and may reduce environmental stress crack resistance. HDPE rotomoulding resins contain less short-chain branching, produce higher crystallinity, and exhibit a sharper melting peak, which narrows the thermal process window. Selection between Icorene 2550 UV+ GRN 6006 and an HDPE rotomoulding grade should therefore be made by comparing low-temperature Charpy impact per ISO 179-1/1eA, environmental stress crack resistance per ASTM D1693 Condition B, and flexural modulus per ISO 178:2019, not by density or melt flow rate alone. The LLDPE grade is typically favoured where shell impact resistance, low-temperature ductility, and environmental stress crack resistance outweigh the need for high stiffness.
| Chemistry class | Density by ISO 1183-1 | Flexural modulus by ISO 178:2019 | ESCR response by ASTM D1693 Condition B | Low-temperature impact tendency |
|---|---|---|---|---|
| LLDPE rotomoulding, UV-stabilised | 0.930–0.940 g/cm³ | 500–700 MPa | Typically >1000 h F50 | Higher ductility |
| HDPE rotomoulding | 0.945–0.965 g/cm³ | 800–1200 MPa | Often 100–500 h F50 | Reduced low-temperature toughness |
| Crosslinked PE rotomoulding | 0.920–0.940 g/cm³ | 400–800 MPa | Typically >1000 h F50 | Improves after cure; creep resistance higher |
The comparison in Table 2 is class-level and not a direct product-grade equivalence. Crosslinked PE is not a drop-in replacement for LLDPE because the process requires a peroxide cure step, a higher internal air-temperature profile, and different mould-release and venting practices. When comparing Icorene 2550 UV+ GRN 6006 with crosslinked rotomoulding powders, the relevant differences include lower continuous-use temperature capability for the thermoplastic LLDPE part and the absence of a post-cure network structure. The LLDPE grade is easier to reprocess, but its load-bearing performance at elevated temperature is lower than that of properly cured crosslinked polyethylene.
Compared with an unmodified Icorene 2550 powder, the UV+ GRN 6006 variant is expected to show similar short-term tensile yield and flexural modulus, but the added pigment and light stabiliser can alter thermal response. Colour change is not a reliable over-bake indicator for green parts, because pigment can mask early yellowing. Over-bake indicators include a measurable reduction in notched Charpy impact, an increase in melt flow rate per ISO 1133-1, and a broadened melting endotherm per ISO 11357-3. In production-scale tooling, exceeding 220 °C mould surface temperature in thick sections has been associated with void formation, additive decomposition, and loss of inter-particle boundary integrity.
At oven air temperatures above 300 °C, surface oxidation accelerates, and the green pigmentation may delay visual detection of degradation until after the part is sectioned. The recommended internal air-temperature limit of 205 °C is therefore used to limit oxidation and bubble growth. For parts with variable wall thickness, thermocouple placement at the thinnest and thickest cross-sections is necessary because internal air temperature alone does not capture local mould-surface overheating. Thin sections can become tacky and overbaked while thick sections remain insufficiently sintered if the rotational speed ratio is not adjusted for the pigment’s heat-absorption behaviour.
Regulatory status requires written confirmation from the supplier’s product regulation bulletin. For European use, REACH Article 33 declarations and the Candidate List of substances of very high concern should be reviewed. For potable-water or food-contact tanks, no blanket approval under EU Regulation 10/2011 or FDA 21 CFR 177.1520 should be assumed without supplier confirmation of the specific grade, colour package, and end-use conditions. The green pigment and UV stabiliser system may be subject to separate compliance review. Processors should retain lot-traceability records linking the GRN 6006 powder to the certificate of analysis, particularly for outdoor articles where weathering performance and migration limits are part of the purchase specification.
Material substitution into an existing tool requires instrumented trials rather than a single melt-flow comparison. The recommended sequence is to measure incoming bulk density and dry flow, adjust oven residence time and internal air temperature, produce wall-thickness survey parts, section the parts for void inspection, and test tensile yield, flexural modulus, and low-temperature impact on specimens cut from the same moulding. Only after this sequence can the replacement be considered validated for production. Published data for this exact GREEN 6006 configuration is limited in open literature, so the supplier certificate of analysis and application-specific trial data are the controlling technical references.