Lyondellbasell Icorene 2550 Uv Bwn 8901 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 658054
    Product Name LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.925 g/cm³ (typical)
    Melt Index 5.0 g/10 min (190°C/2.16 kg, typical)
    Uv Stabilization Yes (UV+ stabilizer)
    Color Brown (BWN 8901)
    Tensile Strength At Yield 14 MPa (typical)
    Tensile Strength At Break 21 MPa (typical)
    Elongation At Break 800% (typical)
    Flexural Modulus 550 MPa (typical)
    Vicat Softening Temperature 100°C (typical)
    Melting Temperature 123°C (typical)
    Hardness Shore D 50 (typical)
    Environmental Stress Crack Resistance >1000 hr (typical)
    Thermal Conductivity 0.33 W/m·K (typical)

    As an accredited LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 UV+ BWN 8901 is supplied in 25 kg polyethylene bags, palletized and wrapped for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of LyondellBasell Icorene 2550 UV+ BWN 8901 LLDPE, palletized, shrink-wrapped, secured for transport.
    Shipping LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density is a non-hazardous, non-DG LLDPE resin. Ship in clean, dry bags, octabins, bulk trucks, or railcars. Protect from moisture, heat, sunlight, and contamination. No special hazard placards required; standard industrial freight handling applies.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers or bags closed and palletized to prevent moisture, contamination, and dust generation. Avoid prolonged UV exposure and excessive stacking. Use grounding/bonding where dust or static may accumulate. Follow manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored in original, unopened packaging, cool, dry, and protected from direct sunlight and heat.
    Application of LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density

    What Melt Temperature Ceiling Preserves the UV+ Additive System During Thin-Wall Injection Moulding?

    The grade is conveyed, metered, and plasticised on a standard reciprocating-screw injection moulding machine with a three-zone barrel configuration, screw L/D of 20:1 to 24:1, and compression ratio between 2.0:1 and 2.5:1. Melt temperature measured at the nozzle is maintained at 190 °C to 215 °C for sections of 1.0 mm to 2.5 mm. The melt flow rate designation of 25 g/10min per ASTM D1238-20 (Condition 190 °C/2.16 kg) permits injection pressures in the range of 600 bar to 900 bar for thin-wall geometries, reducing shear heating at the gate and minimising molecular degradation of the hindered amine light stabiliser (HALS) package incorporated into the UV+ formulation. Back pressure is held at 5 bar to 10 bar; higher back pressures extend residence time and expose the HALS component to unnecessary thermal load. Screw rotation speed is limited to 80 rpm to 120 rpm to prevent uncontrolled viscous dissipation. Mould temperatures are specified between 15 °C and 45 °C. Cooling time for 2.0 mm nominal wall is calculated from the part's thermal diffusivity rather than from generic cycle-time tables; for butene-copolymer LLDPE with density 0.925 g/cm³ (measured per ISO 1183-1:2019), the cooling constant approximates 0.08 mm²/s under turbulent water circulation through conformal channels. The narrow molecular weight distribution engendered by the Spherilene gas-phase process reduces melt elasticity, yielding lower die swell and narrower anisotropic shrink gradients between flow and cross-flow directions. Post-mould shrinkage is measured at 1.8% to 2.2% in the flow direction and 1.4% to 1.8% transverse after 24 h conditioning at 23 °C and 50% relative humidity. The largest application cluster for this material takes the form of outdoor thin-wall enclosures: agricultural sensor housings, irrigation controller boxes, pump shrouds, and perimeter-zone cable junction covers. Each of these parts demands multi-year UV resistance without post-mould painting or lacquering, and the UV+ stabiliser system is formulated to meet the weathering criteria of ASTM D4329-21 (QUV-B 313 nm, 0.49 W/m² irradiance, 60 °C black panel) up to 2000 h without chalking or surface micro-cracking. Tensile property retention after accelerated weathering is evaluated per ISO 527-2:2012 on type 1BA specimens excised from moulded plaques; tensile yield strength of the unexposed resin is typically reported in the range 11 MPa to 14 MPa, elongation at break above 500%, and secant flexural modulus at 1% strain near 350 MPa to 420 MPa. Gate geometry in this moulding segment favours edge-gated or tunnel-gated configurations; the high flow index permits gate diameters down to 0.8 mm without freeze-off risk, provided that injection speed is maintained above 80 mm/s linear screw velocity. Insufficient injection speed in thin sections produces flow hesitation lines that act as stress concentrators under thermal cycling between −20 °C and 60 °C. The operational boundary for this material in continuous outdoor service is governed not by the polymer backbone but by the rate of additive migration and surface depletion; components exposed to direct tropical UV fluence above 5 kWh/m²/day require part thicknesses greater than 2.5 mm or supplemental UV screening in the form of carbon black masterbatch addition at 2 wt% to 3 wt%, which raises the surface concentration of radical-scavenging species to levels sufficient for 5-year field performance.Injection moulding of thin-wall outdoor irrigation valve bodies and emitter housings imposes a distinct processing constraint: acetaldehyde and peroxide residues from upstream purging compounds migrate into the LLDPE melt and accelerate HALS consumption. This failure mode is observed on production lines where the machine barrel is purged with a low-viscosity acrylic purging agent immediately prior to changeover from PVC or acetal. The residual chlorinated or oxygenated species catalyse the decomposition of the HALS functionality during the subsequent 10 min to 15 min of LLDPE production, resulting in a part that passes visual inspection but fails accelerated weathering at 800 h to 1000 h of ASTM D4329 exposure. Corrective action requires a dedicated polyolefin purge step of 3 to 5 barrel capacities followed by 5 min of short-shot cycling to evacuate dead zones behind the check ring and along the screw root. The practical consequence of ignoring this protocol is a batch-to-batch variation in UV performance that cannot be identified by melt flow testing alone, since HALS depletion does not alter the MFR value beyond the repeatability tolerance of ASTM D1238 (±3% interlaboratory).Rotational moulding represents a secondary but commercially significant application corridor for this grade when processed as a powder co-blend with higher-viscosity polyethylene resins. The as-supplied pellet is ground on a high-speed disc mill to a median particle size of 400 µm to 600 µm (35 mesh to 40 mesh per ASTM E11-22). A 70/30 by weight blend of a conventional rotomoulding-grade LLDPE (MFR 4 g/10min to 6 g/10min) with Icorene 2550 UV+ reduces the peak internal air temperature (PIAT) required for complete sintering by 8 °C to 12 °C, from a baseline of 205 °C to approximately 195 °C, at a fixed oven temperature of 300 °C and rotation ratio of 4:1 primary to secondary axis. This PIAT reduction shortens oven residence time for a 3.0 mm nominal wall part from 18 min to 14 min on a Ferry Industries RS-160 carousel machine. The trade-off is a measurable increase in void count in thick sections above 4.0 mm; the high-flow component of the blend tends to migrate into interstitial channels between larger powder particles during the early sintering stage, leaving localised low-density pockets that appear as micro-porosity in polished cross-sections. This phenomenon is controlled by limiting the high-flow fraction to 20 wt% maximum when part sections exceed 4.5 mm. Application examples include small outdoor flotation elements, agricultural seed-distribution cones, and access covers for sub-surface irrigation manifolds. Published comparative weathering data for this specific rotational moulding configuration is limited; accelerated testing per ASTM D2565-23 (xenon arc, 0.35 W/m² at 340 nm, borosilicate-filtered) on 3.0 mm plaques is recommended to establish field-equivalent service life for the blended system, since the higher-viscosity co-resin dilutes the UV+ additive concentration proportionally.
    Processing parameter matrix for Icorene 2550 UV+ BWN 8901 across downstream conversion routes
    ParameterInjection mouldingRotational moulding (co-blend)Twin-screw compounding
    Melt temperature / processing apex190–215 °C nozzle195–205 °C PIAT180–210 °C melt zone
    Residence time limit< 6 min total barrel14–18 min oven cycle< 45 s per pass
    Pressure regime600–900 bar injectionatmospheric / partial vacuum40–80 bar die back pressure
    Temperature control criticality±5 °C across zonesPIAT tolerance ±3 °C±4 °C melt thermocouple
    Pre-drying requirementnot required below 60% RHrequired below 0.05% moisturenot required below 60% RH

    Masterbatch Carrier Viscosity Matching and Pigment Dispersion Efficiency

    The resin's high flow index and narrow molecular weight distribution make it a technically coherent carrier vehicle for outdoor-grade pigment and additive masterbatches where terminal let-down occurs in high-density polyethylene or polypropylene matrices. Masterbatch formulation on this carrier typically incorporates organic pigments at 15 wt% to 40 wt% loading, carbon black at 30 wt% to 45 wt%, or HALS/UV-absorber combinations at 10 wt% to 25 wt% active content. Dispersion is executed on a co-rotating twin-screw extruder with segmented screw geometry, screw diameter 25 mm to 75 mm, L/D 32:1 to 44:1, and a melt temperature profile from 170 °C in the feed zone to 200 °C at the die. Kneading block arrays with 30°, 45°, and 90° staggering are arranged to achieve dispersion number values above 10⁴, which is required for pigment aggregate reduction below 5 µm mean particle diameter as verified by optical microscopy at 100× magnification or by pressure-rise filtration testing per EN 13900-5:2005. The carrier's butene-comonomer backbone contributes a lower crystalline melting point (peak melting endotherm 120 °C to 124 °C by ISO 11357-3:2018 differential scanning calorimetry) than HDPE carriers, which reduces the energy demand for melt-phase pigment wetting and permits lower compounding temperatures that preserve heat-sensitive organic pigments such as phthalocyanine blue (P.B. 15:3) and quinacridone red (P.R. 122). The practical let-down ratio in downstream extrusion or injection moulding operations ranges from 2% to 4% for pigment concentrates and 5% to 8% for combined UV-plus-pigment systems. A documented failure mode in this application space is viscosity stratification: when the carrier MFR exceeds the matrix MFR by a factor greater than 10:1, melt-phase mixing at the let-down extruder is incomplete, producing streaking or surface mottling in film and sheet. For matrix resins with MFR below 1 g/10min, a carrier grade with MFR closer to 8 g/10min to 12 g/10min is preferred; the 25 g/10min designation of this grade confines its carrier suitability to matrix MFR values at or above 2.5 g/10min.Compounding trials on the same twin-screw platform reveal that melt temperature is the dominant control variable for residual pigment agglomerate count, not throughput. At screw speeds of 400 rpm to 600 rpm and specific mechanical energy input of 0.15 kWh/kg to 0.25 kWh/kg, temperature excursions above 220 °C trigger oxidative chain scission that broadens the effective MWD and increases the melt flow rate by 15% to 30% relative to virgin pellet, a shift measurable by gel permeation chromatography and by ASTM D1238 re-testing. Such degradation compromises the narrow-MWD processing advantage and introduces low-molecular-weight fractions that migrate to the surface during weathering, exuding as a chalky bloom that reduces gloss retention in the final article. The stabiliser package is monitored during compounding by sampling at the die face every 15 min; a change in melt pressure of more than 2 bar at constant screw speed indicates destabilisation, often attributable to moisture in the pigment feed or agglomerated masterbatch granules blocking the side feeder throat.Agricultural drip-irrigation fittings, low-pressure sprinkler bodies, and greenhouse vent actuators constitute a further injection-moulding segment where the UV+ package operates in concert with the polymer's ductile failure mode. Components in this segment are exposed to intermittent water contact, dissolved chlorine species at 1 ppm to 3 ppm, and UV irradiance that varies with latitude and greenhouse covering film transmission. Chlorinated water at pH 6.5 to 7.5 does not measurably degrade the PE backbone within a 5-year service horizon, but it does extract surface-level antioxidants at a rate that correlates with water temperature. At water temperatures above 40 °C, the extraction rate of phenolic antioxidants from the surface layer proceeds at approximately twice the rate observed at 20 °C, based on Arrhenius extrapolation of migration coefficients measured per EN 1186-3:2022. Where fittings are subjected to chlorinated water at elevated greenhouse temperatures, a sacrificial barrier layer in the form of a 0.5 mm thick HDPE over-mould or co-injected cap is applied to retard antioxidant loss; without such a barrier, surface oxidation onset is detected as carbonyl index increase above 0.1 absorbance units by FTIR-ATR within 24 months of continuous service. The clinical limit for this grade in water-contact outdoor hardware is therefore defined not by mechanical property loss but by oxidative induction time depletion, measured per ISO 11357-6:2018 at 200 °C under oxygen; initial OIT values for UV+ stabilised narrow-MWD butene LLDPE are typically specified above 20 min, with field failure criteria set when OIT falls below 5 min.

    When Narrow Molecular Weight Distribution Eliminates Melt Fracture in High-Shear Profile Extrusion

    Profile extrusion of garden edging, greenhouse glazing channels, and outdoor cable ducting is executed on single-screw extruders with screw diameter 45 mm to 90 mm, L/D 24:1 to 30:1, and a barrier-flighted screw design with mixing pins in the metering section. Barrel temperature profile rises from 160 °C in the feed zone to 195 °C at the adapter and 200 °C at the die. The narrow molecular weight distribution, a characteristic of the butene-copolymer grade produced on the Spherilene platform, translates into a high critical shear rate for melt fracture onset. In constant-rate capillary rheometry per ISO 11443:2021, sharkskin surface defects are typically not observed below apparent wall shear rates of 500 s⁻¹ to 800 s⁻¹ at 190 °C, which permits linear extrusion speeds of 8 m/min to 15 m/min on profiles with 1.5 mm to 3.0 mm wall thickness. Calibration is performed in a water-cooled vacuum sizing tank with −0.3 bar to −0.5 bar vacuum and water temperature 15 °C to 25 °C; cooling length is calculated at 0.8 m per metre-per-minute of line speed for 2 mm walls. The limitation in this segment is melt strength: with a narrow MWD and no long-chain branching, the resin exhibits low extensional viscosity, making unsupported free-surface processes such as blown film or large-diameter pipe extrusion technically unsuitable. Sagging and draw-down instability become acute when the extrudate exits the die at cross-sections exceeding 150 mm in width or when horizontal unsupported runs exceed 300 mm between die face and sizing sleeve. Consequently, profile applications are restricted to geometries that enter the calibration unit within 100 mm of the die exit.
    Compliance and test standard checklist for outdoor LLDPE applications
    Standard / regulationScopeApplication relevance
    ASTM D1238-20Melt flow rate, 190 °C/2.16 kgIncoming lot verification, carrier viscosity matching
    ISO 1183-1:2019Density by immersion or gas pycnometryConfirming 0.925 g/cm³ grade designation
    ISO 527-2:2012Tensile properties on moulded specimensPost-weathering mechanical retention
    ASTM D4329-21QUV-B accelerated weatheringUV+ performance verification to 2000 h
    ISO 4892-2:2013Xenon arc weatheringCorrelation to outdoor exposure for specification writing
    FDA 21 CFR 177.1520Olefin polymers for food contactApplicable only where the UV+ package is cleared; verify grade-specific letter of no objection
    EU Regulation 10/2011Plastic materials in food contactOverall migration limit 10 mg/dm²
    REACH (EC) 1907/2006Registration, evaluation, authorisationHALS and UV absorber components must be registered in applicable tonnage band
    RoHS Directive 2011/65/EURestriction of hazardous substancesNo lead, cadmium, hexavalent chromium, or mercury in stabiliser package; verify by XRF screening per IEC 62321
    Low-pressure structural foam moulding, employing chemical blowing agents at 0.5 wt% to 1.5 wt%, emerges as a technically valid application when the objective is mass reduction in outdoor enclosures without sacrificing flexural rigidity. Azodicarbonamide is the blowing agent of choice; its decomposition exotherm peaks at 205 °C to 215 °C, which overlaps with the recommended melt temperature band for this resin. The narrow MWD provides a low-viscosity melt that permits full expansion of the foam cell structure before skin freeze-off, producing a density reduction of 25% to 35% at part wall thicknesses from 4.0 mm to 8.0 mm. The critical process parameter is melt temperature uniformity: a zone-to-zone variation exceeding ±5 °C causes inconsistent cell nucleation, since the blowing agent decomposes preferentially in the hotter melt stream, yielding visually detectable swirl patterns on the moulded surface. Screw back pressure is set at 15 bar to 20 bar to maintain blowing agent solubility in the melt before injection; lower back pressures permit premature gas evolution in the barrel, which manifests as intermittent shot-weight fluctuation exceeding 0.5% of nominal and destroys dimensional repeatability. The UV+ additive system does not interfere with azodicarbonamide decomposition kinetics, as confirmed by differential scanning calorimetry trace comparisons showing no depression of the exothermic onset temperature beyond the instrumental repeatability of ±2 °C. This segment serves outdoor equipment housings, battery enclosures for solar garden lighting, and weatherproof junction boxes where the combination of weatherability, reduced mass, and adequate stiffness is achieved without painting or secondary finishing operations.

    When Post-Consumer Recyclate Blending Demands Recalibration of the UV Stabilisation Reserve

    Blending of this grade with post-consumer recycled linear low-density polyethylene at 15 wt% to 30 wt% recyclate content requires a systematic reduction in the expected weathering service life unless the UV+ stabiliser package is supplemented. Post-consumer recyclate carries variable concentrations of carbonyl species, residual catalyst residues, and previously consumed stabiliser fragments, all of which act as pro-degradants during outdoor exposure. The interaction is quantified by oxidative induction time: a 30 wt% recyclate blend decreases OIT by 40% to 60% relative to virgin Icorene 2550 UV+, an effect attributable to the catalytic activity of residual iron and copper trace elements rather than to dilution alone. This effect is particularly severe for recyclate sourced from post-consumer film waste where printing inks and adhesive residues contribute transition-metal contamination. Compensation strategies involve the addition of a HALS masterbatch at 1 wt% to 2 wt% concentration, raising the total active HALS loading to 0.3 wt% to 0.5 wt%, or the incorporation of a metal deactivator at 0.05 wt% to 0.1 wt% based on the oxalyl dihydrazide chemistry class. Melt processing of recyclate blends is restricted to a maximum melt temperature of 200 °C because the recyclate fraction contains low-molecular-weight species that generate volatile organic compounds at elevated temperatures; extraction hood airflow at the die face is maintained at a minimum face velocity of 0.5 m/s per occupational exposure guidance. The operational boundary for recyclate content in outdoor-rated components is set at 30 wt%; above this threshold, batch-to-batch recyclate variability renders weathering performance unpredictable even with supplemental stabiliser addition, as demonstrated by field trials showing failure-time coefficients of variation exceeding 40% at 50 wt% recyclate loading. Published data for this specific configuration under long-term Florida exposure per ASTM D1435-20 is limited; accelerated weathering correlation must be established on a per-recyclate-source basis rather than extrapolated from virgin-resin data.
    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ BWN 8901 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 UV+ BWN 8901 is a linear low density polyethylene rotational moulding powder supplied with a specified ultraviolet stabiliser and pigment package. The grade is intended for monolayer and multi-layer rotational moulded articles in which outdoor weathering resistance, low-temperature ductility, and stress-cracking resistance are specified. Manufacturer-published typical data for the 2550 UV+ series include a nominal density of 0.940 g/cm³ determined by ISO 1183-1:2019, a melt mass-flow rate of 5.0 g/10 min at 190 °C under 2.16 kg load measured according to ISO 1133-1:2022, and a tensile yield strength in the range 14–16 MPa using ISO 527-2 at 23 °C. The BWN 8901 suffix denotes a precompounded colour and UV-stabiliser system, not a standard natural grade; it influences weathering retention, surface temperature under solar load, and batch-to-batch colour consistency. Compared with low-density polyethylene homopolymer, the linear low density polyethylene structure contains short-chain branches from a butene-1 comonomer without the long-chain branching that dominates high-pressure tubular low-density polyethylene.

    How does butene-1 comonomer distribution in Icorene 2550 UV+ BWN 8901 alter the trade-off between impact toughness and environmental stress-cracking resistance relative to higher alpha-olefin LLDPE grades?

    The molecular architecture of butene-1 LLDPE yields a broader short-chain branching distribution than metallocene-catalysed hexene-1 or octene-1 LLDPE grades. In rotational moulding, slower crystallisation of butene-1 copolymers during cooling can promote larger spherulites and fewer stress-transmitting tie chains. The practical consequence is that a 0.940 g/cm³ butene-1 LLDPE may exhibit lower instrumented falling-weight impact at -20 °C than an octene-1 LLDPE of comparable density, while retaining a narrower processing window for thin-walled parts. Typical Charpy and Izod values are measured according to ISO 179-1 or ISO 180. Environmental stress-cracking resistance, assessed by ASTM D1693 Condition A or ISO 22088-2, is strongly controlled by comonomer type and moulded-in residual stress. For Icorene 2550 UV+ BWN 8901, the stabiliser package may delay oxidative embrittlement but does not remove the inherent ESCR ceiling of butene-1 LLDPE. This distinction matters when a converter selects between a lower-cost butene-1 powder and an octene-1 grade for agricultural chemical tanks, detergent reservoirs, or fuel-tank skins where constant strain and surfactant exposure occur simultaneously.

    On production carousel machines with forced-air gas-fired ovens, mould surface temperature and peak internal air temperature are more reliable than oven set-point alone. A butene-1 LLDPE with 0.940 g/cm³ density and 5.0 g/10 min melt mass-flow rate typically requires a peak internal air temperature of 190–200 °C to achieve full sintering and bubble removal. When peak internal air temperature exceeds 205 °C, oxidative degradation may produce yellowing, reduced dart impact, and pinholes. When it remains below 180 °C, the moulding can show incomplete densification, porosity, and low ESCR. Rotational moulding powders in this class are sensitive to particle-size distribution; segregation of the BWN 8901 masterbatch during powder handling can produce colour streaks and inconsistent ultraviolet protection. The powder should be dried at 70–80 °C only if moisture content exceeds 0.1% by weight. High-shear dry-blend mixing of the pigment masterbatch with natural powder should be avoided because it can alter particle-size distribution and reduce dry-flow consistency. Pour density is normally assessed according to ISO 6186. On a rotating mould with varying wall thickness, infrared pyrometry of the mould surface is used to detect hot spots created by high thermal mass or poor air circulation; these hot spots can locally deplete antioxidant and shorten outdoor service life. Batch-to-batch variation in pigment dispersion can also shift the optimum peak internal air temperature by several degrees, so instrumented mould qualification is required after any raw-material lot change.

    Accelerated weathering retention is governed by stabiliser migration and surface erosion, not initial melt flow rate.

    Ultraviolet resistance in rotationally moulded LLDPE is evaluated by exposure to xenon-arc or fluorescent ultraviolet sources under ISO 4892-2 or ASTM G154. The BWN 8901 pigment and stabiliser designation is the principal variable for colour retention, retained tensile elongation, and chalking resistance. For UV-stabilised LLDPE, retained tensile elongation after 2000 h of xenon-arc exposure is frequently maintained above 50% of original value, but that result depends on specimen thickness, pigment loading, irradiance, and humidity cycling. A black or dark pigment in a BWN 8901 system can function as an ultraviolet screen, but it can also raise mould surface temperature during outdoor service, accelerating antioxidant depletion. A dark-coloured Icorene 2550 UV+ part may therefore show better surface crack resistance under direct ultraviolet exposure than an unpigmented grade but may consume primary antioxidant faster under cyclic thermal exposure. Oxidative induction time should be evaluated by differential scanning calorimetry using ISO 11357-6, with typical acceptance thresholds for rotational moulded parts set at a minimum of 10 min at 210 °C. If the moulded part is intended for continuous outdoor use above 50 °C surface temperature, published data for this specific BWN 8901 configuration is limited, and supplementary weathering or thermal ageing tests are required.

    Compared with Icorene 2550 UV+ natural, the BWN 8901 designation provides precompounded colour and weathering stabilisation. Compared with crosslinkable high-density polyethylene rotational moulding powders, this linear low density polyethylene grade does not require post-mould crosslinking and can be segregated into post-industrial recycling streams. Crosslinkable HDPE grades typically show better long-term creep and elevated-temperature stiffness above 60 °C, whereas this LLDPE grade softens earlier and requires design compensation for thermal expansion. Compared with glass-reinforced thermosets or metal fabrications, the rotomoulded LLDPE part will have lower modulus and higher thermal expansion, so mounting points and sealing surfaces require structural ribs or metal inserts. The product also differs from high-pressure LDPE rotational powders because the linear backbone provides lower melt strength but improved tensile and stiffness balance at equivalent density.

    When the moulded article stores potable water, chlorinated water and outdoor ultraviolet ageing impose simultaneous migration and stress-cracking demands.

    Potable water storage tanks made from LLDPE are typically assessed against migration limits in Regulation (EU) 10/2011, with an overall migration limit of 10 mg/dm² of food-contact surface, and against US FDA 21 CFR 177.1520 for olefin polymers. Compliance is use-specific and depends on temperature, contact time, and surface-to-volume ratio. Chlorinated potable water creates an oxidative environment that can accelerate antioxidant depletion and promote microcracking. The UV+ stabiliser package in Icorene 2550 UV+ BWN 8901 addresses outdoor ageing but does not replace potable water certification. Long-term hydrostatic stress testing under ISO 1167-1 or tank-specific methods is required. Knit lines at vents, tank corners, and regions of variable wall thickness are critical because rotational moulding can introduce residual stress and local thickness reduction. If the water contains residual chlorine above 1.0 mg/L at 60 °C, accelerated ESCR testing under ASTM D1693 or ISO 22088-2 should be performed on moulded specimens, not compression-moulded plaques. The following matrix summarises standard-based assessment areas.

    Assessment area Standard or regulation Relevant condition or acceptance criterion
    Melt mass-flow rate ISO 1133-1:2022 190 °C, 2.16 kg, reported in g/10 min
    Density ISO 1183-1:2019 Method A or B at 23 °C
    Tensile properties ISO 527-2 Type 1B or Type 5A specimen at 23 °C, 50 mm/min
    Flexural modulus ISO 178 2 mm/min at 23 °C
    Environmental stress-cracking resistance ASTM D1693 Condition A or ISO 22088-2 Constant strain in surfactant solution
    Artificial weathering ISO 4892-2 Xenon-arc exposure, cycle and irradiance defined by end use
    Oxidative induction time ISO 11357-6 Isothermal differential scanning calorimetry at 210 °C
    US FDA food contact 21 CFR 177.1520 Olefin polymers, conditions of use A–H
    EU plastics migration Regulation (EU) 10/2011 Overall migration limit 10 mg/dm²
    EU chemical regulation Regulation (EC) No 1907/2006 REACH SVHC disclosure and authorisation obligations
    Hazardous substances Directive 2011/65/EU RoHS homogeneous material thresholds for Pb, Hg, Cd, Cr(VI), PBB, PBDE

    Mechanical property envelope and low-temperature ductility limits

    Typical mechanical values for a UV-stabilised butene-1 LLDPE rotomoulding powder in this density class include tensile yield strength in the range 14–16 MPa when tested according to ISO 527-2 at 23 °C, elongation at yield near 8–12%, tensile elongation at break above 600%, and flexural modulus in the range 550–650 MPa according to ISO 178. Low-temperature impact measured by instrumented falling-weight impact at -20 °C may be lower than for octene-1 LLDPE of the same melt flow rate. The brittleness temperature measured under ASTM D746 is often below -60 °C for unfilled LLDPE, but that value does not guarantee impact performance on thick-walled moulded parts. Because cooling rate in rotational moulding is slower than in injection moulding, the crystalline structure coarsens and can reduce impact strength relative to fast-quenched test specimens. Material selection for insulated ice boxes or cold-climate tanks should therefore use moulded-part dart impact tests at the minimum service temperature rather than small-scale Charpy data.

    Agricultural chemical tanks represent one of the more demanding applications for Icorene 2550 UV+ BWN 8901. The combination of outdoor ultraviolet exposure, repeated filling, hydrostatic pressure, and surfactant or fertiliser solutions places simultaneous stress on the polymer. Failure in such tanks often begins at the sidewall-to-bottom radius, where wall thinning and residual stress are greatest. Moulders should verify a minimum wall thickness at the radius, control cooling rate to reduce warp, and measure ESCR on specimens cut from the moulded corner. Published data for this specific BWN 8901 configuration under all application-specific chemical combinations is limited; qualification should include immersion testing in the intended chemical formulation at the maximum service temperature, followed by retained tensile and ESCR evaluation. The grade may be unacceptable for continuous exposure to strong oxidising acids, aromatic hydrocarbons, or low-molecular-weight chlorinated solvents because these agents can induce swelling or rapid environmental stress cracking.