Lyondellbasell Icorene 2550 Uv Blk 9601 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 473923
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.925 g/cm³
    Melt Index 2.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 15 MPa
    Elongation At Break 800%
    Flexural Modulus 250 MPa
    Hardness Shore D 50
    Vicat Softening Temperature 90°C
    Brittleness Temperature -70°C
    Melting Point 120°C
    Mold Shrinkage 1.5-2.0%
    Color Black
    Uv Stabilization Yes
    Processing Method Injection Molding
    Water Absorption <0.01%
    Coefficient Of Linear Thermal Expansion 1.5E-4 cm/cm/°C
    Volume Resistivity >1E16 ohm·cm
    Dielectric Strength 20 kV/mm

    As an accredited LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags; each bag contains LyondellBasell Icorene 2550 UV+ BLK 9601 Linear Low Density Polyethylene.
    Container Loading (20′ FCL) 20′ FCL loading: LyondellBasell Icorene 2550 UV+ BLK 9601 LLDPE, 25 kg bags, palletized, shrink-wrapped, properly secured for ocean transport.
    Shipping Shipping description: Polyethylene, linear low density, UV stabilized, black, non-hazardous. Not regulated for transport by DOT, IATA, or IMDG. Supplied as pellets in 25-kg bags or octabins, palletized and stretch-wrapped. Store dry, away from heat and ignition sources. No UN number, hazard class, or packing group required.
    Storage Store LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed, off the floor, and protected from moisture, dust, and odors. Avoid excessive stacking or prolonged UV exposure. Store only in compatible, labeled containers. Follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months from date of manufacture when stored in original, unopened packaging, cool, dry, and protected from direct sunlight.
    Application of LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density

    LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density is processed in agricultural sprayer tank production as a dry-flow powder with a typical 35-mesh classification, charged into CNC-machined cast aluminium clamshell moulds on independent-arm rotational moulding machines. For wall thicknesses of 5–8 mm, oven set-points between 280°C and 295°C are normally used, and the peak internal air temperature is held between 190°C and 210°C; below that band, incomplete sintering at the parting line produces pinhole defects, while above it, oxidative degradation of the LLDPE melt can raise the carbonyl index and reduce retained dart impact after outdoor exposure. The biaxial rotation speed ratio is set between 4:1 and 8:1 to avoid powder pooling in sump areas or behind moulded baffles, and release agents must be silicone-free because residual silicone films have been associated with reduced environmental stress crack resistance in rotationally moulded LLDPE. The grade already contains a carbon black/UV stabiliser package, so no additional UV masterbatch is compounded into the charge; if clean in-house regrind from the same material is used to reduce material cost, its mass fraction is held below 10% because higher regrind levels measurably reduce falling weight impact values when tested according to ASTM D5420-21. Chemical compatibility with crop protection formulations is evaluated on moulded plaques by ISO 175:2010 or ASTM D543-21 immersion at 40°C for 28 days; published data for this specific configuration is limited, so trial immersion testing is performed before commercial tank release. The finished components are typically 1,000–5,000 L sprayer reservoirs, fertigation tanks or inductor hoppers with rotationally moulded threaded bosses and closed-cell foam gaskets.

    What Governs Pinholing and Warpage in Large Water Cisterns?

    Rotomoulded water cisterns fail at two process extremes. When the peak internal air temperature is below 195°C, unmelted powder remains at the inner wall surface and creates microporosity and pinhole leaks; above 215°C, thermal degradation of the carbon black/UV stabiliser package can liberate volatile by-products, causing surface pitting and a measurable decline in tensile elongation at break when tested per ISO 527-2:2012. Production-scale machines use infrared Rotolog sensors or equivalent internal air probes because oven residence time alone does not correlate with true melt temperature in moulds with wall thickness varying from 6 mm at the top surface to 12 mm at bottom bosses. Warpage is controlled by delaying demoulding until the core side wall temperature has fallen below 70°C; forced air cooling followed by a short water mist cycle reduces cycle time but increases residual stress, so mist is applied only to the outer mould surface and not to inner surfaces that solidify later. The grade contains carbon black loading in the typical range of 1.5–2.5 wt%; additional colour or UV masterbatch is not used in potable water service because the black package already provides the required light stabilisation. The material is processed as virgin powder without solvent-based flow aids, and regrind is excluded from potable water inner layers to avoid introducing contaminants that cannot be fully removed by conventional washing. Finished cisterns are one-piece bodies with no weld seams, moulded in sizes from 2,000–10,000 L, and must satisfy the compliance requirements summarised below.

    StandardScopeTest parameter
    ASTM D1998-21Polyethylene upright storage tanksHydrostatic pressure test at 23 °C; wall thickness verification
    21 CFR 177.1520Olefin polymers for food contactExtractables in food simulants under conditions of use
    NSF/ANSI 61:2021Drinking water system componentsLeachate extraction at pH 5 and pH 10

    In marine buoy shell production, a UV-stabilised black LLDPE rotomoulding powder is used for outer shells that must retain impact resistance after prolonged saltwater immersion and sunlight exposure. Carbon black absorption in the 300–400 nm UV band is the primary weathering mechanism; exposure programs for commercial marine mouldings generally follow ISO 4892-3:2021 cycling with condensation, and the black shell is not painted because the pigment package replaces liquid coatings. The moulds are typically fabricated from 6–8 mm steel sheet or cast aluminium; steel moulds are preferred for long production runs of buoy collars because repeated thermal cycling of aluminium in salt air causes surface pitting that transfers to the moulded surface. For wall thicknesses of 8–12 mm, oven temperatures from 285°C to 305°C are used, with peak internal air temperature targets of 195–215°C. Insert retention is a critical production bottleneck: moulded-in stainless steel mooring eyes require local wall thickness around the boss at least 2.2 times the insert diameter; below that ratio, cracks form at the insert edge during demoulding or under wave loading. Because the outer shell is continuously immersed or wetted, regrind content is kept at 0% to preserve stress crack resistance; foam filling, if required, uses closed-cell polyurethane introduced after the shell has cooled to ambient temperature. Buoyancy calculations must be based on grade-specific density measured by ISO 1183-1:2019, and published data for this specific configuration is limited. The terminal components are navigation buoy shells, flotation collars and fender bodies, each tested for falling weight impact at -20°C according to ASTM D5420-21 and for dimensional stability after immersion in seawater at 23°C for 14 days.

    When Dilute Acids Are Stored in Single-Wall Rotomoulded Tanks

    Single-wall chemical storage tanks fabricated from rotationally moulded LLDPE avoid the weld seams that act as stress concentrators in conventional fabrications, but the grade must be evaluated against each stored chemical rather than against water alone. Published chemical resistance charts for black LLDPE indicate broad compatibility with dilute sulfuric acid up to 40% at ambient, sodium hydroxide solutions up to 30%, and sodium hypochlorite solutions up to 15%; however, the grade-specific formulation must be validated by ISO 175:2010 immersion at the actual use concentration and temperature. Strong oxidising acids such as concentrated nitric acid and hydrogen peroxide above 10% are not recommended because oxidative attack accelerates stress cracking and reduces elongation at break. Wall thickness for vertical tanks is selected according to stored liquid specific gravity up to 1.4, with a range from 6 mm for small day tanks to 20 mm for large storage vessels. Processing uses oven temperatures from 285°C to 305°C and peak internal air temperatures of 195–210°C; cooling must be sufficiently slow in thick base sections to prevent sink marks at rib intersections. For chemical immersion service, the primary tank wall regrind content is held at 0%, while the secondary containment bund may incorporate up to 20% clean in-house regrind because it is not continuously wetted. Environmental stress crack resistance is checked by ASTM D1693-21 condition B in a 10% Igepal solution. Terminal components include 600–5,000 L vertical chemical storage tanks, double-wall containment pallets and dosing vessel bodies with flanged top openings.

    Low-Temperature Ductility in Road Barrier Panels

    Road barrier panels require thick-walled, double-shell bodies with internal baffle structures; the structural function depends on impact toughness at temperatures well below freezing rather than on stiffness alone. The material is moulded in large steel moulds with wall thicknesses of 8–12 mm, using oven temperatures between 280°C and 300°C and peak internal air temperatures of 195–215°C. Cycle times for barrier shells range from 25 to 45 minutes depending on total shot weight and mould surface area; demoulding before the core side surface drops below 75°C produces panel distortion that interferes with later joining of the two half-shells. The grade may be blended with 10–15 wt% clean in-house regrind provided the regrind has not suffered UV embrittlement from outdoor storage; higher levels have been associated with local delamination at the inner wall and reduced falling weight impact at -40°C when tested to ASTM D5420-21. Moulded-in mounting blocks and drainage ports are added only after confirming local wall thickness is at least 2.0 times the insert diameter. Full barrier crash performance is evaluated under highway authority specifications such as MASH 2016 or equivalent local standards, while material-level acceptance relies on low-temperature impact and tensile property retention. The black UV-stabilised surface removes the need for paint on exterior faces, which eliminates paint adhesion loss after repeated impact or abrasion. Terminal parts include water-filled barrier shells, crash cushion modules, junction blocks and temporary work zone delineators.

    For industrial material handling bins and pallet boxes, rotational moulding produces one-piece double-walled bodies with integral fork pockets, drainage channels and stack lugs that are difficult to form by injection moulding. Wall thicknesses of 6–10 mm are used depending on load rating; local ribs and kiss-off features are incorporated to reduce unsupported sidewall deflection. Processing on carousel or shuttle machines operates at oven temperatures of 280°C to 300°C and peak internal air temperatures of 195–210°C. The charge may include up to 15% clean in-house regrind for non-food industrial parts, but food-contact fish boxes and similar applications require 0% regrind to comply with 21 CFR 177.1520 and EU 10/2011 for food contact. Low-temperature toughness is verified by ISO 179-1:2020 Charpy notched impact at -20°C, because bins are frequently handled in cold storage or outdoor yards. The black surface resists visible staining and does not require painting; cleaning with hot water or mild alkaline detergents below 60°C is acceptable, but steam cleaning above 80°C can distort thin sidewalls. Terminal products include 300–1,000 L pallet boxes, hopper liners, fish crates, waste containers and modular conveyor troughs.

    Free Quote

    Competitive LyondellBasell Icorene 2550 UV+ BLK 9601 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The grade identified as LyondellBasell Icorene 2550 UV+ BLK 9601 is a powdered linear low density polyethylene compound intended for biaxial rotational molding. The product designation places it in the ethylene α-olefin copolymer class, not in branched low density polyethylene or high density polyethylene homopolymer. It is supplied as ground powder rather than pelletized compound, which permits direct charge preparation in rotational molding shops where dry blending, regrind addition, and color adjustment are performed at the molding machine. The UV+ suffix indicates a compounded ultraviolet stabilization package combined with black pigmentation, and the BLK 9601 identifier refers to the black color concentrate system rather than a natural resin with separate dry colorant.

    For most acceptance and qualification work, the base resin is specified at a nominal density of 0.935 g/cm³ when determined by ISO 1183-1:2019 on compression-moulded plaques. The nominal melt flow rate is 5.0 g/10 min at 190 °C under a 2.16 kg load, measured in accordance with ISO 1133-1:2022. The black UV compound may shift the as-moulded density upward by 0.002 g/cm³ to 0.005 g/cm³ depending on the carbon black loading and the regrind fraction used in the charge. Bulk density of the powder, measured by ISO 60:1977, is a critical but frequently under-recorded control point; for this class of rotational molding LLDPE, loose bulk density typically falls between 0.45 g/cm³ and 0.52 g/cm³. A lower value is associated with excessive air inclusion and erratic flow into narrow mold passages, while a higher value may reflect particle agglomeration or static charge buildup in storage.

    When peak internal air temperature remains below 185 °C in thin-wall charging

    On shuttle-type rotational molding machines with a 2.4 m to 2.6 m swing diameter and gas-fired oven chambers, the lower processing boundary for this LLDPE class is commonly observed at a peak internal air temperature of approximately 190 °C. If the PIAT remains below 185 °C, the molded outer surface may appear solid while the inner surface retains partially coalesced particle boundaries. This condition is not reliably corrected by extending the heating cycle unless the internal air temperature itself is raised. The result includes pinholes, internal porosity, and reduced low-temperature impact strength when Charpy specimens are prepared and tested according to ISO 179-1:2010.

    Typical oven set points for wall sections between 3 mm and 6 mm range from 280 °C to 315 °C. The heating cycle is controlled by internal air temperature rather than by dwell time alone. A 6 mm section may require 22 min to 30 min in the oven, while a 3 mm section can reach the required enthalpy in 14 min to 18 min. Rotation ratios on shuttle equipment are generally held between 4:1 and 8:1 on the major axis depending on tool geometry; the minor-axis speed is normally set at 1 rev/min to 2 rev/min. Powder residence outside this range produces wall thickness variation, corner thinning, or bubble entrapment in deep draw areas.

    Density, melt flow rate, and specification values that control lot acceptance

    The following table summarises the characteristic ranges used to evaluate this grade during incoming inspection. The values are not a substitute for the supplier certificate of analysis or a mold trial on the actual tooling.

    Representative physical and mechanical specification envelope for Icorene 2550 UV+ BLK 9601
    PropertyTest methodCharacteristic range or reported typical
    Nominal densityISO 1183-1:20190.933–0.940 g/cm³
    Melt flow rateISO 1133-1:2022, 190 °C, 2.16 kg4.5–5.5 g/10 min
    Powder bulk densityISO 60:19770.45–0.52 g/cm³
    Particle size, cumulative passing 500 µmASTM D6913≥ 95 %
    Shore D hardnessISO 868:200354–58
    Tensile yield stressISO 527-2:201215–18 MPa
    Tensile elongation at breakISO 527-2:2012700–900 %
    Environmental stress crack resistanceASTM D1693, bent strip> 500 h, condition-dependent

    Because the product is a rotational molding powder rather than an injection molding or film-extrusion resin, the melt flow value alone is insufficient to predict processability. Slow-shear viscosity controls the release of trapped air and the filling of complex mold passages. Two materials with identical 5.0 g/10 min melt flow can behave differently in a rotational mold if their comonomer type, molecular weight distribution, or black masterbatch dispersion differ. Published data for the precise molecular architecture of the Icorene 2550 UV+ BLK 9601 configuration is limited; therefore, equivalence testing under the actual molding cycle is required before substituting a supposedly similar LLDPE grade.

    What separates this compound from HDPE and conventional LDPE rotomolding powders?

    The distinction is not limited to density. Branched low density polyethylene of equivalent melt flow typically exhibits lower crystalline content, lower tensile yield stress, and inferior environmental stress crack resistance because long-chain branching interferes with tie-molecule formation. In contrast, high density polyethylene rotomolding grades with densities from 0.945 g/cm³ to 0.960 g/cm³ provide higher flexural modulus, commonly 650–850 MPa when measured by ISO 178:2019, but their notched low-temperature impact resistance can be lower because the higher crystallinity concentrates stress at spherulitic boundaries. The 0.935 g/cm³ LLDPE class occupies an intermediate position: the linear backbone and short-chain branches provide slow crack growth resistance while retaining sufficient rigidity for tanks, shrouds, and enclosures.

    When compared with metallocene-catalysed LLDPE grades of similar density, this product may display broader molecular weight distribution and a different response to oven dwell time. Narrow-distribution metallocene powders can yield smoother inner surfaces but are often more sensitive to under-cure pinholes when the mold contains large flat panels or isolated pockets. Broader-distribution resins tolerate thicker sections and longer heating times without excessive melt sag. In practice, the choice between this grade and a metallocene equivalent should be based on instrumented mold trials, not on density and melt flow alone. The rotomolding operation should record PIAT, oven damper position, rotation ratio, cooling rate, and part weight across at least five cycles before confirming interchangeability.

    Carbon black dispersion below ISO 18553 rating B alters UV protection and ductility

    The BLK 9601 system supplies a pre-dispersed carbon black concentrate rather than a simple dry black masterbatch. Carbon black acts as a UV screen and reduces photodegradation, but poorly dispersed pigment agglomerates create stress concentrations that lower elongation at break and produce visible surface pits. Dispersion is assessed by the microtome technique described in ISO 18553. A dispersion rating below B is associated with a measurable reduction in tensile elongation of approximately 10 % to 20 % relative to well-dispersed material, depending on section thickness and pigment loading.

    The black surface also absorbs incident solar radiation and can run 15 °C to 25 °C hotter than an equivalent white or natural LLDPE surface under the same irradiance. This must be considered in accelerated weathering evaluations conducted under ISO 4892-2:2013 xenon-arc conditions, because higher surface temperature accelerates thermal oxidation independent of ultraviolet dose. The UV+ package typically combines carbon black with a hindered amine light stabilizer, but the stabilizer can partially adsorb onto carbon black surfaces. As a result, the effective stabilizer concentration in the molded part depends on masterbatch let-down, mixing, and regrind history. Published data for the exact stabilizer content in this product configuration is limited; lot-specific verification is recommended for parts intended for multi-year outdoor service.

    Regrind accumulation, thermal oxidation, and multi-arm shuttle machine variability

    Rotational molders routinely blend virgin powder with regrind from trimmed openings, kiss-off blocks, and rejected parts. Up to 15 wt% of clean regrind from the same compound is generally tolerated without a significant reduction in ESCR or impact performance when the regrind has not experienced more than one additional heating cycle. Above 20 wt%, oxidation products and pigment agglomerates may accumulate, reducing slow crack growth resistance and increasing the likelihood of pinhole formation in thick corners. On a gas-fired shuttle machine with a 2.6 m swing diameter, replacing virgin powder with 30 wt% regrind can shift the observed PIAT by 3 °C to 6 °C for the same oven damper setting because reground material sinters earlier. The operator may then interpret the earlier temperature rise as complete cure while the inner wall remains under-sintered.

    The shift is particularly relevant for black UV-stabilized LLDPE because carbon black increases radiative heat absorption and can mask under-cure symptoms. The recommended practice is to instrument the mold cavity with a shielded internal air temperature probe and control the heating cycle to a target PIAT of 195 °C to 205 °C, depending on wall thickness. For a 4 mm nominal wall, cooling should begin only after the PIAT has remained above 190 °C for the full dwell period required by the tool. Air-cooling to 80 °C before demolding is common for flat panels, while thicker sections benefit from slower cooling to permit stress relaxation and reduce warpage.

    If the mold surface temperature exceeds 250 °C at demolding, residual thermal stress may remain locked into the part. The black surface retains heat longer than natural LLDPE, so cooling schedules developed for unpigmented powder are not directly transferable. Water-mist cooling can reduce cycle time but increases distortion on asymmetric parts. For parts with wall thickness variation greater than 1 mm, forced-air cooling to an internal air temperature below 100 °C before opening the mold is usually safer than aggressive water quench. The demolding temperature is part of the mold trial record; it should not be inferred from the un-pigmented grade.

    The following compliance matrix applies to black LLDPE rotational molding compounds of this class. Acceptance must be confirmed against the supplier lot documentation and the intended end-use.

    Regulatory and test-standard matrix applicable to lot release and end-use qualification
    RequirementReference or test methodTypical expectation for base LLDPE class
    Olefin polymer food-contact status21 CFR 177.1520Compliant for base resin; black concentrate must be verified separately
    EU plastics food-contact regulation(EU) No 10/2011, Annex IOverall migration testing required per simulant and food-contact condition
    REACH registrationRegulation (EC) No 1907/2006Polymer exemption applies; monomer and additive registration must be confirmed
    Accelerated weatheringISO 4892-2:2013, xenon-arcBlack UV package evaluated for specified outdoor service; no universal guarantee
    Carbon black dispersionISO 18553Rating A or B preferred for mechanical ductility

    Applications for this grade are concentrated in rotationally molded enclosures, machinery covers, agricultural equipment components, outdoor storage tanks, and shrouds that require long-term ultraviolet stability combined with moderate stiffness and low-temperature ductility. The part design should maintain a minimum wall thickness of 3 mm and avoid sharp radii below 3 mm. In fuel tank or chemical container service, permeability testing by ASTM D3985 or the relevant chemical immersion standard is required because LLDPE is more permeable to low-molecular-weight hydrocarbons than HDPE of similar thickness. This grade should not be assumed suitable for potable-water pressure vessels unless separate NSF/ANSI 61 or equivalent certification is obtained. No medical-grade claim should be inferred from the food-contact status of the base polymer alone.

    Top