| HS Code | 503314 |
| Density | 0.924 g/cc |
| Melt Flow | 20 g/10 min |
| Tensile Strength At Yield | 9.00 MPa |
| Tensile Strength At Break | 14.0 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 260 MPa |
| Hardness Shore D | 48 |
| Vicat Softening Point | 84.0 °C |
| Melting Point | 122 °C |
| Brittleness Temperature | < -70.0 °C |
| Color | Red |
As an accredited LyondellBasell Icorene 2550 RED 4706 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg multi-wall bags, 40 bags per pallet, LyondellBasell Icorene 2550 RED 4706 Linear Low Density Polyethylene resin. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell Icorene 2550 RED 4706 Linear Low Density Polyethylene; palletized 25 kg bags, shrink-wrapped and secured. |
| Shipping | LyondellBasell Icorene 2550 RED 4706 is a non-hazardous LLDPE resin supplied as red pellets, typically in 25 kg bags or octabins on pallets. Ship in clean, dry trucks or containers, protected from moisture, heat, sunlight, and contamination. No special dangerous-goods handling required. Store in a cool, dry, well-ventilated area. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, and ignition sources. Keep material in original, unopened bags or containers on pallets, protected from moisture, dust, and physical damage. Avoid prolonged UV exposure. Maintain good housekeeping; prevent spills from creating slipping hazards. Use first-in, first-out stock rotation. Keep away from strong oxidizing agents. Do not stack excessively. |
| Shelf Life | The shelf life is typically 24 months when stored in original unopened packaging in a cool, dry area, away from direct sunlight. |
For agricultural chemical storage tanks, LyondellBasell Icorene 2550 RED 4706 is charged at 100 wt% as supplied, with no additional external pigment concentrate. Dry regrind of the same red compound may be added up to 25 wt% only after tensile strength and environmental stress-cracking resistance are revalidated according to ISO 527-1:2019 and ASTM D1693-15. The powder is screened through 35 mesh (500 µm); warehousing above 60% relative humidity requires drying at 60–70 °C for 2–4 h to prevent pinhole porosity during particle coalescence. Rotational moulding tools for this application are heated in forced-air ovens at 260–290 °C, while peak internal air temperature is maintained at 200–220 °C. A dark red tint containing infrared-absorbing pigmentation can shorten the time required to reach peak internal air temperature relative to unpigmented LLDPE; therefore cycle time must be re-established by internal thermocouple measurement rather than transferred from natural powder recipes. Deviation above +5 °C from the lot-specific optimum is not accepted without revalidation because overbaking increases carbonyl index and reduces ESCR, while underbaking produces incomplete coalescence at wall thicknesses of 6–12 mm. On carousel machines, demoulding above 55 °C has been observed to cause sidewall warpage and parting-line distortion in tanks above 1000 L. Chemical compatibility is confirmed by immersion testing in representative fertilizer and pesticide formulations under ASTM D543-21; rigid plastics IBC configurations may require additional performance assessment under UN Model Regulations, Chapter 6.5. End-product types include stationary fertigation tanks, secondary containment basins, and 1000 L rigid plastics IBC shells.
| Property | Designation |
|---|---|
| Melt flow rate | ASTM D1238-20 (190 °C/2.16 kg) |
| Density | ASTM D1505 |
| Tensile yield strength | ISO 527-1:2019 |
| Elongation at break | ISO 527-1:2019 |
| Flexural modulus | ASTM D790-17 |
| Low-temperature impact | ASTM D256-23 |
| Environmental stress-cracking resistance | ASTM D1693-15 |
| Colour measurement | ASTM D2244-23 |
Marine buoy hulls and fender shells use the same red compound at 100 wt%; dilution with natural LLDPE is not recommended above 10 wt% because signal visibility under IALA Recommendation R1001 depends on opaque pigment coverage. The moulding process is performed on biaxial-arm rotomoulding or shuttle machines with aluminium two-piece tools, oven temperature 250–280 °C, and peak internal air temperature 190–210 °C. Cooling is staged: forced air for 10–15 min, followed by water mist until the mould surface reaches 45–55 °C. On biaxial-arm machines, water quenching below 45 °C has produced outer-skin compression and internal voids near foam-fill cutouts; this failure mode is reduced by maintaining cooling rate below 10 °C/min. Material acceptance includes ISO 179-1:2010 Charpy notched impact at -20 °C, ASTM D1693-15 ESCR, and ASTM D638-14 tensile evaluation. End products include port lateral marker buoys of 0.5–3 m, mooring buoys, and floating fender shells. Mineral-filled polyethylene regrind is incompatible because raised density and filler exfoliation reduce saltwater ESCR retention.
Diesel transfer tanks and generator day tanks moulded from red-tinted LLDPE must maintain hydrostatic burst resistance and low-temperature ductility after diesel swelling. The pigmented outer layer is charged at 100 wt% as supplied; where a permeation barrier is specified, an inner surface treatment such as post-mould fluorination or sulfonation is applied, with the pigmented red layer representing 80–90 wt% of total shot weight. Rotational moulding is carried out in steel or aluminium biaxial tools at oven setpoints of 250–270 °C, with peak internal air temperature controlled at 200–215 °C and demoulding below 50 °C. Threaded brass inserts require mechanical anchoring because LLDPE does not form a structural adhesive bond without functionalisation; insert bosses should maintain local wall thickness at least 1.5× nominal wall to resist post-mould cracking. Steel inserts act as heat sinks and cause local undercure unless preheated to 60–80 °C before charging. Compliance for static thermoplastic diesel tanks references EN 13341:2005+A1:2011; testing includes hydrostatic pressure, impact at -20 °C, and fuel swelling under ASTM D543-21. Transportable tank configurations may require additional assessment under UN Model Regulations, Chapter 6.5. End products include 20–2000 L diesel transfer tanks, generator day tanks, and auxiliary fuel cells. Dry blending with HDPE regrind above 15 wt% is not recommended because differential shrinkage creates warpage at baffles and weakens weld lines.
Where food-processing plants use red-pigmented monolithic bins and dollies for colour-coded allergen or sanitation zones, the material is charged at 100 wt% as received, and rework is limited to 25 wt% from identical food-compliant lots. Rotomoulding uses cast aluminium tools with oven temperatures of 260–285 °C, peak internal air temperature of 195–210 °C, and forced-air cooling to 45–55 °C before demould. Release agents, if required, are restricted to food-contact-compliant synthetic siloxanes validated for overall migration under EN 1186-1:2002. Olefin polymer compliance is checked against FDA 21 CFR §177.1520(c) and EU Regulation (EU) No 10/2011, Annex I; heavy-metal pigment restrictions are verified under RoHS Directive 2011/65/EU, Annex II. End products include 50–1000 L mobile ingredient totes, washdown catch basins, and colour-coded drum dollies. Post-consumer regrind is incompatible unless it meets the same food-contact compliance; otherwise overall migration and sensory taint become uncontrolled.
Outdoor playground slides, tunnel tubes, and climbing shapes require the red compound to retain impact strength after accelerated weathering and to resist surface chalking. The powder is charged at 100 wt% as supplied; where a lighter red shade is required, dry blending with a UV-stabilised natural LLDPE of matched melt flow rate is permitted at 10–30 wt%, but only after colour and weatherability revalidation under ASTM D2565-16 or SAE J2527. Carousel rotomoulding tools are heated to 260–290 °C, with peak internal air temperature held at 195–215 °C; forced-air cooling proceeds until mould surface temperature is 55 °C or lower. Premature demoulding of long slide bedways has produced concave warpage and tensile hinge-line stress in production runs; this is controlled by reducing cooling rate below 15 °C/min and comparing post-mould dimensions after 24 h at 23 °C/50 % RH against the tool cavity. Playground material acceptance involves ASTM F1487-17 and EN 1176:2017; mechanical acceptance is assessed by ASTM D638-14, ISO 180, and ASTM D790-17. End products include slide bed sections, tunnel tubes, roof caps, and climbing grips. Zinc stearate external lubricants are incompatible because they can interfere with post-mould adhesive bonding and UV coating adhesion on high-gloss red surfaces.
Rotomoulded red LLDPE enclosures for underground irrigation valves and electrical warning covers must resist soil load without long-term creep buckling. The material is used at 100 wt% as supplied; regrind is limited to 15 wt% because multiple melt histories reduce creep resistance and increase oxidation index. Ribbed steel moulds are heated to 250–280 °C, peak internal air temperature is maintained at 190–210 °C, and cooling rate is controlled below 15 °C/min to minimise post-mould shrinkage. Demoulding is performed below 60 °C. Clearance between rib and shell must accommodate shrinkage of 1.5–2.5 % typical for this LLDPE rotomoulding class; published data for this specific configuration is limited, so first-article shrinkage is measured over 48 h after demoulding. Load-bearing verification is conducted under ASTM D2990 tensile creep and ASTM D790-17 flexural modulus; buried outdoor service also uses ASTM D638-14 and ASTM D1693-15. End products include 6–24 in round valve boxes, meter pit shells, and electrical warning covers. Blending with high-melt-index LLDPE above 10 wt% is incompatible because powder segregation during transit causes wall-thickness variation and localised thin spots under rib roots.
Competitive LyondellBasell Icorene 2550 RED 4706 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 RED 4706 is supplied as an integral red-pigmented linear low density polyethylene powder for rotational moulding. The base polymer is an ethylene/α-olefin copolymer produced with a metallocene single-site catalyst. The 2550 grade designation corresponds to a nominal melt mass-flow rate of 5.0 g/10 min measured at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022, and a nominal density of 0.925 g/cm³ determined by ISO 1183-1:2019 Method D. The suffix RED 4706 identifies the commercially compounded red colour package. The material is normally delivered as a ground powder with a top size suitable for dry-flow charging; it is not a pelletised injection moulding feedstock and is not intended for film extrusion.
The principal difference is not the nominal comonomer content but its placement. In a conventional multi-site Ziegler-Natta butene LLDPE, the comonomer is preferentially incorporated into the high molecular mass fraction, leaving the low molecular mass fraction nearly linear. This heterogeneity creates a high-temperature melting shoulder and a high-molecular-weight tail. High-temperature gel permeation chromatography performed according to ISO 16014-1:2019 typically shows a polydispersity index of 3.5–5.0 for Ziegler-Natta grades, while the metallocene architecture of Icorene 2550 narrows the distribution to a value generally below 3.0. The short-chain branching is distributed more uniformly across all chain lengths. In practice, this shifts the sintering behaviour observed on heating in a rotomoulding oven. The metallocene material enters the terminal melting region closer to a single peak and has a lower high-temperature shoulder; differential scanning calorimetry according to ISO 11357-3:2018 places the peak melting temperature near 122 °C for the 0.925 g/cm³ resin class. For the rotomoulder, that means the particle coalescence and bubble dissolution stages occur earlier than for a comparable multi-site resin, but the operating window between complete densification and thermal oxidation also becomes narrower.
For dry-flow charging, the powder is ground to a nominal 35 mesh (500 µm) top size. The dry-flow time measured on a 50 g sample per ASTM D1895-96 Method A is typically below 30 s, while bulk density falls between 0.32 g/cm³ and 0.38 g/cm³. A powder with dry-flow time below 20 s does not guarantee uniform fill in deep rib bosses; the critical variable on an independent-arm machine is the interaction between bulk density and the charging funnel flow pattern. Material stored at relative humidity above 80% or brought from a cold warehouse into a warm moulding hall may develop surface moisture that bridges at hopper throats. Pre-drying for 2 h at 70 °C in a circulated-air drier is the standard correction. Passing the powder through a magnetic drawer before the charging hopper is advised because grinding operations can introduce metallic fines; this practice is common on production lines equipped with a 10,000 gauss magnetic separator.
| Property | Test method | Unit | Nominal value or range |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | g/10 min | 5.0 |
| Density | ISO 1183-1:2019 Method D | g/cm³ | 0.925 |
| Powder top size | ASTM D1921 | µm | 500 nominal |
| Bulk density | ASTM D1895-96 Method A | g/cm³ | 0.32–0.38 |
| Peak melting temperature | ISO 11357-3:2018 | °C | 120–125 |
| Tensile yield stress | ASTM D638-14 Type IV, 50 mm/min | MPa | 13–15 |
| Tensile elongation at break | ASTM D638-14 | % | >800 |
| Flexural modulus | ISO 178:2019 | MPa | 350–450 |
On a multi-arm rotomoulding machine with a 3 mm nominal wall thickness, the practical peak internal air temperature for the 2550 grade is between 195 °C and 230 °C. The lower boundary is set by residual microvoids at the inner mould surface and along weld lines; below 190 °C, particles may fuse but the viscosity remains too high for complete bubble removal, leaving pinholes. The upper boundary is controlled by red pigment heat stability and the onset of oxidative chain scission. In field evaluations on an off-axis carousel machine with forced-air cooling, oven residence times were reduced by approximately 8–12% when the internal air temperature was increased from 200 °C to 220 °C, but the red surface darkened measurably if the part remained above 230 °C for more than 2 min. The acceptable heating rate through the melt transition is tooling-dependent; thin flat panels develop uneven wall thickness when the heating rate exceeds 15 °C/min before the powder has completely consolidated.
Integral red colour eliminates a coating line and avoids the film thickness variability associated with spray-applied finishes. The RED 4706 package is dispersed into the polymer matrix before grinding. Published spectral data for this specific pigment concentration are limited, so a xenon-arc weathered ΔE value is not cited here. For outdoor articles, ultraviolet resistance should be verified by ISO 4892-2:2013 xenon-arc exposure or ISO 4892-3:2016 QUV exposure using lot-specific plaques. Red pigmentation also changes the solar absorption of the moulded surface. A red part exposed to full sun can develop surface temperatures significantly above the ambient air temperature; the designer should use a solar absorptance value above 0.7 for thermal load calculations unless a specific value is supplied by the pigment manufacturer. In tank wall stress calculations, this surface heating must be superimposed on the chemical load. For non-appearance structural components, natural or black grades are often specified instead because the carbon black package can provide a lower unit-cost UV stabilisation route.
The low shear viscosity and its temperature dependence determine how quickly bubbles can diffuse out of the melt. A 5.0 g/10 min metallocene LLDPE has a lower zero-shear viscosity than a 3.0 g/10 min product of the same density, which allows the same wall thickness to be formed at a lower peak internal air temperature or with a shorter curing hold. However, the same narrow distribution reduces the rubbery modulus during the cooling phase. When the mould is opened too early or cooling is non-uniform, the part may exhibit warpage because residual stress is frozen before the semicrystalline network has fully developed. Forced-air cooling at 10–15 °C/min through the 90 °C to 60 °C interval is used on commercial lines to balance cycle time against distortion. The red pigment can act as a nucleating agent and may shift crystallisation to slightly higher temperature during cooling; published data for the 4706 package in this matrix is limited, but lot-to-lot pigment dispersion should be monitored because poor dispersion can create local crystallinity gradients and visible colour streaks.
In rotationally moulded storage tanks, chemical dosing cabinets, tool boxes, decorative outdoor equipment, and industrial packaging where a red surface is required without painting, Icorene 2550 is selected over a conventional Ziegler-Natta LLDPE when the part has fine ribs and tight corner radii. The narrower melting range improves powder fill-out around intricate tool features. A conventional multi-site butene grade with the same nominal melt flow rate generally has a broader processing window and greater tolerance to over-cure, but it may require a higher peak internal air temperature to eliminate surface holes and may show lower low-temperature impact at equivalent density. The comparison is therefore not one-directional. If the moulder runs long oven cycles because of oven loading, a Ziegler-Natta grade may be more forgiving; if the cycle can be temperature-controlled within a ±10 °C PIAT band, the metallocene grade can provide shorter cycles and better low-temperature fracture resistance.
| Process attribute | Icorene 2550 RED 4706 | Conventional Ziegler-Natta butene LLDPE |
|---|---|---|
| Catalyst architecture | metallocene single-site | multi-site Ziegler-Natta |
| Molecular weight distribution | narrow, polydispersity index generally below 3.0 | broad, polydispersity index 3.5–5.0 |
| Short-chain branching distribution | homogeneous | heterogeneous |
| Melt mass-flow rate | 5.0 g/10 min | 2.0–6.0 g/10 min depending on grade |
| Density | 0.925 g/cm³ | 0.924–0.928 g/cm³ typical |
| Peak melting endotherm | narrow, near 122 °C | broad, with high-temperature shoulder |
| Peak internal air temperature window | 195–230 °C | 200–240 °C |
| Over-cure tolerance | lower | higher |
| Weld-line fill-out in fine ribs | improved at equivalent wall thickness | may require longer hold or higher PIAT |
| Low-temperature impact at equal part weight | improved | lower |
Because the base resin and the red pigment are regulated separately, no food-contact status can be inferred from the base resin alone. The natural mLLDPE may meet the olefin polymer requirements of 21 CFR 177.1520, but the red pigment must independently comply with the colorant provisions of 21 CFR 178.3297 for food-contact use. For industrial parts, the user should obtain a product-specific REACH compliance statement and verify heavy-metal limits under RoHS Directive 2011/65/EU, particularly for cadmium, lead, and hexavalent chromium in red colorants. Storage should avoid temperatures above 60 °C, direct sunlight, and contact with strong oxidising agents or aromatic solvents; prolonged contact with chlorinated hydrocarbons can plasticise the surface and reduce stress crack resistance. The product is not recommended for injection moulding or profile extrusion because the powder feed characteristics and the absence of pelletised stabiliser distribution are unsuitable for screw-fed processes.