| HS Code | 410057 |
| Density | 0.925 g/cm³ |
| Melt Flow Rate | 3.5 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 20 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 250 MPa |
| Hardness Shore D | 50 |
| Vicat Softening Temperature | 96°C |
| Melting Point | 123°C |
| Environmental Stress Crack Resistance | >1000 hr |
| Thermal Expansion Coefficient | 1.5E-4 cm/cm/°C |
| Thermal Conductivity | 0.33 W/m·K |
| Specific Heat | 2.3 J/g·°C |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1E15 ohm·cm |
As an accredited LyondellBasell Icorene 2550 ORE 3903 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 2550 ORE 3903 is packaged in 25 kg polyethylene bags, palletized to 1,000 kg, or supplied in bulk. |
| Container Loading (20′ FCL) | Container loading (20′ FCL): LyondellBasell Icorene 2550 ORE 3903 Linear Low Density Polyethylene, palletized bags, stretch-wrapped, evenly distributed, secured, weight-compliant. |
| Shipping | LyondellBasell Icorene 2550 ORE 3903 Polyethylene, Linear Low Density is typically shipped as non-hazardous solid resin pellets. Packaging includes 25 kg bags, 1000 kg octabins, or bulk truck/rail. Keep dry, clean, and away from heat, sunlight, moisture, and odor contamination. Store in a cool, dry warehouse. No special dangerous goods regulations apply. |
| Storage | Store at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original containers or bags closed, labeled, and off the floor to prevent moisture and contamination. Avoid dust generation and static discharge. Use first-in, first-out stock rotation. Consult the manufacturer’s Safety Data Sheet for detailed handling and storage requirements. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in a cool, dry area, away from direct sunlight and moisture. |
LyondellBasell Icorene 2550 ORE 3903 linear low density polyethylene is converted into closed-top cisterns and distribution header tanks by single-layer biaxial rotational moulding. The grade is specified at a nominal density of 0.940 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 4.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. Potable water article compliance is assessed at the finished-part level under EU Regulation (EU) No 10/2011, 21 CFR 177.1520, and NSF/ANSI/CAN 61; migration testing uses the 10-day at 40 °C protocol for aqueous simulants in the EU and normalized total organic carbon protocols in North America. The dry blend is 100 parts by mass powder, 0.3–0.7 phr UV stabilizer masterbatch unless the ORE 3903 stabilization package already covers the service exposure, 0.10–0.25 wt% NSF-listed pigment, and ≤20 wt% same-grade regrind. Process conditions on a carousel or shuttle machine require a 4:1 rotation ratio, oven set point 270–300 °C, peak internal air temperature 185–205 °C, and forced-air cooling to ≤80 °C demoulding surface temperature. Terminal products include rainwater collection cisterns, rural drinking water storage tanks, header tanks, and transport-safe potable water containers.
Continuous hot-water contact above 60 °C falls outside the standard validated service envelope because antioxidant migration and wall modulus retention become batch-sensitive. On 4-m carousel machines, powder segregation in transfer bends has been observed when the particle size distribution D90 exceeds 800 µm, generating localized pinholes along the parting line; screening through a 35 mesh sieve before charging eliminates fused agglomerates. The rotational moulding shop should monitor peak internal air temperature with a data-logging thermocouple placed inside the tool; excursions beyond 205 °C in 12 mm wall sections can generate internal surface bubbles from low-molecular-weight stabilizer decomposition products.
| Regulatory instrument | Test condition | Measured parameter | Normative basis |
|---|---|---|---|
| EU Regulation (EU) No 10/2011 | 10 days at 40 °C, aqueous food simulants | Overall migration and specific migration | Annex I, 10 mg/dm² OML |
| NSF/ANSI/CAN 61 | pH 5 and pH 10 extraction waters | Normalized total organic carbon and metals | Sections 4–9 |
| 21 CFR 177.1520 | Hexane and xylene extractables, as specified | Specified extractable fraction | 21 CFR 177.1520 |
Where fertilizer-induced stress cracking controls the design, vertical agricultural chemical storage tanks and bunded secondary containment shells are rotomoulded from Icorene 2550 ORE 3903. The grade’s environmental stress crack resistance exceeding 1,000 h under ASTM D1693-15, condition B, permits the base knuckle radius to be formed with 8–20 mm wall stock without fracturing at the transition from vertical sidewall to sump. The compounding step is dry blending 100 parts by mass powder with 0.5–1.0 phr hindered amine light stabilizer masterbatch and 0.5–1.0 wt% carbon black masterbatch; regrind is limited to 15–25 wt% and screened through a 35 mesh sieve to remove fines. Regulatory compliance for liquid chemical transport and storage is evaluated under UN Model Regulations Chapter 6.5 for rigid plastics IBCs and 40 CFR 264.175 for secondary containment integrity. Rotational moulding is carried out on a carousel machine with oven set point 280–310 °C, internal air temperature 195–210 °C, and cooling rate ≤8 °C/min through the crystalline solidification region to minimize warpage at the tank rim. Terminal articles include conical-bottom induction tanks, transport skids, bunded pallet tanks, and vertical static storage vessels for dilute aqueous agricultural formulations. Compatibility with concentrate formulations containing more than 5 wt% aromatic solvent carriers is outside the standard validation envelope; ASTM D543-21 immersion testing is required before service.
Field production data from tank-routing shops indicate that rim warpage above 2 mm/m has been traced to non-uniform cooling when direct water contact is applied to the lower tank section while the top rim remains above 90 °C. A staged cooling sequence with forced air to 100 °C, then intermittent water mist, reduces residual stress at the rim.
Drop-arm and shuttle lines producing off-highway diesel reservoirs require a powder grade that maintains weld-line ductility at 6–12 mm wall thickness and resists fuel swell at the internal surface. The formulation uses 100 parts by mass powder, 2.0–3.0 wt% carbon black masterbatch for ultraviolet protection, 0.2–0.4 phr hindered phenolic antioxidant, and 10–20 wt% regrind sourced only from approved fuel-tank-grade scrap. Oven set point is 260–290 °C, peak internal air temperature is 190–205 °C, and cooling uses forced air to 140 °C followed by water mist to 60 °C before ejection. Compliance is assessed under UN ECE R34 for plastic fuel tanks, EN 13341:2005+A1:2011 for static non-pressure tanks, and ASTM D471-16a for fuel immersion volume swell. Terminal products include diesel tanks for agricultural tractors, compact construction equipment, generator base frames, and hydraulic reservoirs. Pressurized gasoline service is outside the validated envelope due to permeation and internal pressure cycling; biodiesel blends above B20 require fuel-contact swell testing under ASTM D471-16a before specification.
Drop-arm machines with 10 t clamp force and tool parting-line flatness within 0.1 mm prevent internal weld flash. Air leak testing at 30 kPa after demoulding is used to detect parting-line weld defects; production-scale failures have been traced to regrind containing fuel-contaminated powder, which reduces interfacial fusion at the weld line.
Foam-filled rotational mouldings for navigation buoys and floating dock pontoons use an outer shell of Icorene 2550 ORE 3903 based on 100 parts by mass powder blended with 2.0–3.0 phr UV-stabilizer masterbatch and 0.5–1.0 wt% colourant, with 10–15 wt% same-grade regrind. The powder is dry-blended and checked by laser diffraction to a particle size distribution with D90 below 700 µm to prevent pinholes at the mould parting line. The shell is rotomoulded on a carousel machine with a 4:1 rotation ratio, oven set point 270–300 °C, and peak internal air temperature 190–205 °C; after demoulding, an expandable closed-cell polyurethane foam is introduced through a fill port and cured to provide buoyancy, after which the fill port is sealed by surface welding. Weathering qualification is based on ASTM G154-23 accelerated UV exposure and ASTM D256-10 notched impact testing after exposure; load-bearing chain plates are moulded in as metallic inserts, and concentrated point loads without insert plates can initiate stress cracking at thread bosses. Terminal products include mooring buoys, navigation buoys, floating dock pontoons, and aquaculture cage collar segments. Regulatory compliance is project-specific and often invokes classification society requirements for buoyancy and impact resistance. Published long-term saltwater immersion data for this specific powder grade in foam-filled structures is limited; article-level validation should include buoyancy retention after 1,000 h accelerated weathering.
Corrosive fume scrubber shells and plating line enclosure bodies are rotomoulded as single-skin 10–15 mm wall sections on shuttle machines with peak internal air temperature 200–210 °C and demoulding below 70 °C to hold flange flatness. The dry blend comprises 100 parts by mass Icorene 2550 ORE 3903 powder, 0.3–0.5 phr hindered amine light stabilizer, 0.2–0.4 phr antioxidant, and ≤0.1 phr metallic stearate; this avoids hydrolysis by acidic condensate that can generate deposition on the internal surface. Chemical resistance is validated by ASTM D543-21 immersion for the specific process stream; dilute sulfuric acid (10–30 wt%) at ambient temperature is generally within the validated range, while oxidizing acids above 40 °C are outside the service envelope. Tensile retention after immersion is measured to ASTM D638-14 against unexposed control plaques. Terminal products include fume scrubber chambers, acid dosing cabinets, electroplating enclosure shells, and battery storage boxes. Published long-term immersion data for this specific powder grade in mixed acid process streams is limited; qualification relies on comparative ASTM D543-21 swelling and tensile retention against a control plaque. REACH Regulation (EC) No 1907/2006 requires supply-chain notification for any substance of very high concern at article level above 0.1 wt%.
| Application category | Wall thickness | Oven set point | Peak internal air temperature | Rotation ratio | Cooling endpoint |
|---|---|---|---|---|---|
| Potable water cisterns | 6–12 mm | 270–300 °C | 185–205 °C | 4:1 | 80 °C |
| Agricultural chemical tanks | 8–20 mm | 280–310 °C | 195–210 °C | 4:1 | 80 °C |
| Off-highway diesel reservoirs | 6–12 mm | 260–290 °C | 190–205 °C | 4:1 | 60 °C |
| Foam-filled marine buoy shells | 8–15 mm | 270–300 °C | 190–205 °C | 4:1 | 80 °C |
| Chemical scrubber enclosures | 10–15 mm | 280–310 °C | 200–210 °C | 4:1 | 70 °C |
| Playground shell components | 5–8 mm | 260–280 °C | process not specified | 3:1 | not specified |
Large rotationally moulded play components are produced with 5–8 mm wall thickness on carousel machines using a 3:1 rotation ratio and oven set point 260–280 °C. The formulation is 100 parts by mass powder, 0.5–1.0 wt% colour masterbatch, 0.2–0.4 phr antioxidant, and ≤10 wt% regrind. Compliance is assessed under ASTM F1487-21 and EN 1176-1:2017 for entrapment, impact, and structural integrity. Post-mould trimming is limited to edge flash; moulded-in inserts for mounting brackets eliminate secondary drilling that could create crack initiation sites. Terminal products include tunnel sections, slide hoods, climbing rock facades, and decorative roof caps.
Competitive LyondellBasell Icorene 2550 ORE 3903 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 ORE 3903 is classified as a linear low-density polyethylene rotational moulding powder supplied for biaxial rotational moulding lines. The material is specified with a nominal density of 0.925 g/cm³ and a melt flow rate of approximately 5.0 g/10 min when measured at 190 °C under 2.16 kg load using ISO 1133-1. Those values function as manufacturing control points rather than absolute specification limits; the certificate of analysis issued with each lot governs density, melt flow rate, particle-size distribution, bulk density, and residual stabilizer concentration. The grade is intended for hollow parts where medium processability, low-temperature impact resistance, and moderate flexural stiffness are required simultaneously.
On production-scale carousel machines with a primary-to-secondary axis speed ratio of 4:1, oven setpoints are commonly held between 260 °C and 300 °C, while peak internal air temperature is maintained at 190–220 °C for closed-mould work. The powder densifies against the hot tool surface, and the first continuous skin forms after repeated polymer fusion and compaction. Residual bubble populations are more strongly influenced by particle-size distribution, peak internal air temperature, and cooling rate than by melt flow rate alone. This grade is a medium-flow LLDPE, meaning bubble release is improved relative to lower-melt-flow rotomoulding grades, while melt strength remains sufficient for deep-draw tools with wall thicknesses above 3 mm.
Particle-size distribution is a critical incoming-material property because rotomoulding powders must pass through 35 mesh (500 µm) screens but retain sufficient coarse fraction to avoid excessive fines. Fines below 150 µm melt too early in the oven and can form a non-uniform first skin, especially on aluminium tools with high thermal conductivity. Bulk density near 0.35 g/cm³ is typical for linear low-density powders in this product class; variations greater than ±5% from an established baseline alter the mass of material delivered to deep ribs and undercut cores. Incoming inspection should therefore include sieve analysis per ASTM D1921 or an equivalent internal method, because flow through the tool cavity cannot be controlled by screw back pressure.
Density measured by ISO 1183-1 at 23 °C inversely tracks short-chain branch concentration. At 0.925 g/cm³, the polymer contains enough comonomer to disrupt linear ethylene sequence, reducing crystallinity relative to an HDPE rotomoulding powder in the 0.940–0.945 g/cm³ range. The practical consequence is a tensile yield stress in the range of 11–13 MPa and a flexural modulus near 400 MPa under ISO 178. Those values place the material below high-density grades in load-bearing stiffness, but above general-purpose LDPE in tensile performance. The thermal softening point is similarly moderate; moulded parts should not be continuously exposed to service temperatures above 50–60 °C where sustained hoop stress is present, because creep modulus declines rapidly above the alpha transition.
Impact behaviour is the core design reason for selecting 0.925 g/cm³ rather than a 0.940 g/cm³ HDPE. In notched Charpy testing according to ISO 179-1/1eA, rotomoulded LLDPE samples of this density class typically show no break at 23 °C, and ductile deformation persists at sub-zero temperatures where HDPE grades may exhibit brittle fracture. Published data for the exact ORE 3903 stabilizer variant is limited; end users should request lot-specific low-temperature impact data rather than extrapolate from unfilled LLDPE grades.
In rotational moulding, the limiting thermal event is seldom molecular-weight breakdown at normal oven setpoints; it is incomplete densification caused by trapped gas or premature wall consolidation. For Icorene 2550 ORE 3903, peak internal air temperature below 190 °C produces microvoids at the inner wall because the melt has not yet achieved the viscosity required for bubble diffusion. At peak internal air temperatures above 220 °C, oxidation accelerates and the inner surface can yellow or embrittle, even though the outer wall remains intact. The operational window therefore behaves as a narrow densification band rather than a broad melt-processing range.
Bubble retention is also affected by tool rotation and powder transport. Machines with fixed rotational ratios cannot always produce ideal recirculation in complex cavities; baffles, cutouts, and deep ribs may require reduced oven setpoint and longer soak times. In such tools, the medium melt flow rate of 5.0 g/10 min improves wall formation over lower-MFR alternatives, but operators must still balance oven time against drop impact and pinhole density. A typical acceptance test for production releases includes a drop-weight impact sequence at -20 °C on panels moulded from identical tool steel and cooling schedule.
Cooling rate after fusion is the second major variable. If demoulding occurs at a wall temperature above 80 °C, warpage and internal stress can reduce impact performance. If cooling is too rapid, particularly in water mist systems, the inner surface may develop shrinkage voids because the wall freezes from the outside inward. A controlled air cooling stage avoiding rates above 10 °C/min through the crystallisation region is typical; slower cooling improves impact but lengthens cycle. Published data for recrystallization kinetics of the exact ORE 3903 formulation is limited, so processors should construct cooling curves from embedded tool thermocouples rather than rely on external air temperatures.
The product occupies a middle position between high-density polyethylene rotational moulding powders and metallocene LLDPE grades. HDPE rotomoulding grades with densities near 0.940–0.945 g/cm³ provide higher flexural modulus, often exceeding 800 MPa, and better resistance to creep in tanks and pallets. Those grades, however, lose ductility more rapidly at low temperature and are more sensitive to wall-thickness discontinuities caused by tool design. Icorene 2550 ORE 3903 at 0.925 g/cm³ sacrifices some stiffness to retain impact toughness in outdoor parts that must survive freeze-thaw cycles, rough handling, or constrained cooling after demoulding.
Compared with metallocene-catalysed LLDPE rotational moulding powders of similar density, the 2550 ORE 3903 grade may show a broader molecular weight distribution, which influences shear response and bubble-release differently. Published data for this specific configuration is limited, and direct substitution should not be made without first comparing ISO 179-1 impact results and spiral-flow or wall-thickness distribution trials on the target tool. Where a part requires very high dart impact at -40 °C, a metallocene grade with a narrow distribution may be preferred; where lower sensitivity to minor cycle disruptions on older single-axis or simple biaxial equipment is required, the 2550 grade is positioned as the more routinely processable reference.
Another distinction is supply form. The product is delivered as a rotomoulding powder, not as pellets; solvent-free grinding or cryogenic size reduction is used in production. This powder form eliminates the need for an extruder but introduces a higher oxidation surface area. Compared with pelletised rotomoulding grades that may be pulverized in-house, the as-supplied powder should be used without additional processing, because secondary grinding can create fines and degrade impact performance. Inventory should be rotated on a first-in-first-out basis to minimize stabilizer migration to the surface.
Typical conversion routes include agricultural spray tanks, intermediate bulk containers, kayak hulls, outdoor seating, access chambers, and general hollow industrial parts. In each application, the part must be designed for LLDPE-level modulus rather than HDPE-level stiffness, and minimum wall thickness must account for the 0.925 g/cm³ density. Compliance with food-contact regulations is grade and end-use specific; FDA 21 CFR 177.1520 covers olefin polymers but extraction testing depends on food type, temperature, and contact area. European food-contact evaluation is performed under EU No 10/2011 with overall migration limits, and potable water applications require additional organoleptic and migration verification under applicable member-state requirements.
The following table consolidates the property envelope commonly used for preliminary material selection. Values should be treated as representative for this density and melt-flow class and not as certified specifications for any single lot.
| Parameter | Test method | Representative value |
|---|---|---|
| Density at 23 °C | ISO 1183-1 | 0.925 g/cm³ |
| Melt flow rate at 190 °C, 2.16 kg | ISO 1133-1 | 5.0 g/10 min |
| Tensile stress at yield | ISO 527-2 | 12 MPa typical |
| Flexural modulus | ISO 178 | 400 MPa typical |
| Charpy notched impact at 23 °C | ISO 179-1/1eA | No break |
| Brittleness temperature | ASTM D746 | Lower than -70 °C |
Lot-specific data from the certificate of analysis should govern final part qualification. Rotomoulding trials must account for screwless processing, plastic tool materials, and cooling line limitations; tensile properties generated from injection-moulded plaques will overstate stiffness relative to a fused powder wall.
The ORE 3903 suffix may denote a specific ultraviolet stabilizer package, but published documentation for this exact suffix is limited. Processors must verify outdoor performance independently using ISO 4892-2 accelerated weathering, with color change and retained tensile elongation measured according to ISO 527-2 after defined irradiance. UV-stabilized LLDPE does not fail primarily by surface chalking; it fails by embrittlement at stress concentrations such as part ribs, inserts, and weld lines. Therefore, accelerated weathering panels must include a moulded-in feature rather than a flat coupon if the end use contains sharp radii or metal inserts.
Field data from existing rotational moulding lines indicate that outdoor failure in this polymer class is frequently dominated by tooling-related wall-thickness variation rather than by stabilizer depletion. Parts with thinner-than-designed rib roots develop cracks under wind load or water load before flat-wall areas show significant property loss. Processors should therefore co-sample at rib roots and flat-wall sections during weathering validation, using ISO 527-2 tensile elongation and ISO 179-1/1eA impact retention as release criteria.
The regulatory matrix relevant to the product is summarized below. Compliance must be reaffirmed for each compound lot and end-use region.
| Regulatory domain | Reference | Verification boundary |
|---|---|---|
| Olefin polymer food contact | FDA 21 CFR 177.1520 | Grade-specific extraction testing |
| Plastics in food contact | EU No 10/2011 | Overall migration limit 10 mg/dm² |
| Registration, evaluation, authorisation | REACH 1907/2006 | Annex XIV and XVII restrictions grade-specific |
| Hazardous substances | RoHS 2011/65/EU | Restricted heavy metal thresholds |
Operational boundaries include storage in an enclosed area with relative humidity below 60%; condensation on cold powder hoppers introduces pinhole defects that cannot be removed by increasing oven temperature. The material should not be blended with HDPE regrind above 20% unless the loss of impact resistance has been verified by ISO 179-1 on the actual moulded part. Contact with aromatic or chlorinated hydrocarbons at elevated temperature should be avoided because swelling can exceed acceptable dimensional change, and continuous exposure to strong oxidizing agents or high-alkaline cleaning solutions can reduce surface molecular weight and stress-crack resistance.