Lyondellbasell Icorene 2550 Nat 0000 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 500443
    Density 0.925 g/cm³
    Melt Index 2.5 g/10 min
    Melt Flow Ratio 16
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 34.5 MPa
    Elongation At Break 700%
    Flexural Modulus 262 MPa
    Hardness Shore D 50
    Haze 6%
    Gloss 80%
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g

    As an accredited LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density is supplied in 25 kg bags, 55 bags per pallet, stretch-wrapped.
    Container Loading (20′ FCL) LyondellBasell Icorene 2550 NAT 0000 LLDPE loaded in 20′ FCL: palletized 25 kg bags, stretch-wrapped, securely braced for ocean shipment.
    Shipping Shipped as solid pellets in 25 kg bags, 1,000 kg octabins, or bulk trucks/railcars. Not classified as dangerous goods for transport. Keep dry, cool, and away from direct sunlight, heat, and contamination. Handle with normal industrial hygiene; avoid moisture and static discharge. Use standard freight.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Maintain stable ambient temperatures; follow manufacturer’s recommendations and local regulations. Prevent slip hazards from spilled pellets.
    Shelf Life Shelf life is 24 months when stored in original unopened packaging in a cool, dry, well-ventilated area away from sunlight.
    Application of LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density

    Thin-wall injection moulding lines configured for polyolefin closures introduce the resin in an undiluted state at 100 wt%; when surface slip and demoulding become rate-limiting, a separately metered colour or slip masterbatch is added at 2–4 wt%, so that the active slip agent in the final part remains between 800–1500 mg/kg. Food-contact applications fall under FDA 21 CFR 177.1520(c) and under Commission Regulation (EU) No 10/2011, where overall migration must not exceed 10 mg/dm² under the specified time–temperature conditions for aqueous and fatty simulants. Converters supplying closures for aseptic or hot-filled beverages additionally verify organoleptic neutrality by a panel score not exceeding the manufacturer’s internal limit, commonly ≤ 1.5 on a 0–3 scale, using ASTM E1870-11 as a reference procedure.

    On a 250–450 t hybrid toggle press with a 22–25:1 L/D general-purpose screw, the melt temperature is maintained at 210–250 °C, with rear zones set at 180–200 °C and the nozzle at 230–250 °C. The grade’s nominal melt flow rate of 25 g/10 min under ISO 1133-1:2022, condition 190 °C/2.16 kg, permits flow length-to-thickness ratios up to 180:1 for wall sections of 0.45–1.2 mm. Clamp force requirements are calculated at 2.5–4.0 kN per projected square centimetre. Hot-runner systems fitted with valve gates are preferred; open-gate hot-runner tips operating with a mould surface below 23 °C exhibit increased gate drool and stringing, which is controlled by reducing hot-runner tip temperature by 5–10 °C relative to the centre-stream setpoint.

    Process monitoring uses a melt cushion of 3–6 mm; below 2 mm, shot-to-shot weight variation rises above 0.5 % because the cushion collapses and compressibility borrows from the check-ring return, while above 8 mm residence time contributes to low-molecular-weight volatiles and increases the probability of seal contamination. Machine-side performance is assessed at 24 h intervals by measuring density according to ASTM D792-20, tensile yield strength according to ASTM D638-22 Type IV specimens, and environmental stress-crack resistance on notched specimens under ASTM D1693-21 in 10 % Igepal CO-630 at 50 °C, with failure below 300 h triggering a review of blend ratio and mould residence time. Terminal parts are tamper-evident overcaps, lightweight hinged closures, and thin-wall dairy or condiment containers.

    What Limits Pigment and Filler Loading When Icorene 2550 NAT 0000 Serves as Masterbatch Carrier?

    Single-pigment and additive masterbatches using Icorene 2550 NAT 0000 as the carrier resin are let down into film, injection moulding, and extrusion coating grades at 1–5 wt% depending on pigment strength and opacity requirement. The carrier fraction in the masterbatch itself is not fixed; in titanium dioxide concentrates with 50–70 wt% TiO2, the carrier is held at 30–50 wt%, whereas carbon black concentrates at 40–50 wt% filler commonly require 50–60 wt% carrier to maintain strand pellet hardness and prevent pellet breakage during pneumatic conveying. Final let-down ratios in film extrusion are commonly 1–3 wt% masterbatch, corresponding to 0.04–0.12 wt% active pigment; in injection moulding, let-down ratios of 2–4 wt% are more typical.

    Compounding safety and end-use status are conditioned by Regulation (EC) 1907/2006 Annex XVII, the Waste Electrical and Electronic Equipment Directive 2011/65/EU Annex II limits for lead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg, and hexavalent chromium 1000 mg/kg, and, for food-packaging masterbatches, FDA 21 CFR 177.1520 and EU No 10/2011 with their specific migration conditions. In a co-rotating twin-screw extruder with 40:1 L/D, the carrier entering at the main port is melted at 170–200 °C; pigment is introduced through a side feeder at L/D 24–28 at screw speeds between 300–650 rpm. Holding the rear zone below 170 °C is prevented because carrier pellets then enter the kneading block only partially plasticized, producing screw torque excursions above 85 % of motor load and melt-temperature spikes above 220 °C at the die.

    Vacuum devolatilisation is applied at -0.08 MPa to remove low-volatile oligomers and residual moisture; if the vent port is placed after the first mixing zone and before the final distribution mixing section, melt-index retention remains within 5 % of the neat value as measured by ISO 1133-1:2022. Pelletising uses a four-hole strand die with water-bath temperature fixed at 40–60 °C, followed by air knives; pellet moisture is kept below 0.15 % by Karl Fischer titration, because higher moisture creates steam voids during let-down injection moulding and contributes to splay. Terminal product forms include colour masterbatch, slip/antiblock masterbatch, black UV-stabilized agricultural film masterbatch, and additive carriers for PE rotomoulding powders, with final let-down ratios adjusted to maintain the targeted final additive concentration within the converter’s statistical process control window.

    Cast Film Extrusion of Pallet Stretch Hoods and the Chilled Roll Blocking Boundary

    Cast film conversion of Icorene 2550 NAT 0000 typically uses the material as the machine-direction outer layers in 5-layer A/B/C/B/A dies, where the A layers may be 100 wt% Icorene 2550 NAT 0000 or a blend with metallocene LLDPE at 0–30 wt% to suppress chill-roll blocking. The core layer, which may consist of polypropylene or a higher-melting polyolefin, is coextruded at a skin-to-core ratio of 20–35 % per skin. Cast film lines process the grade at die temperatures of 240–270 °C, with air gap set at 15–45 mm; shorter gaps reduce neck-in but increase chill-roll sticking, while larger gaps above 60 mm produce edge-curl and gauge variation beyond ±5 % at 18 µm total thickness.

    Formulation addition ratio in a stretch-hood film is governed by the required holding force and puncture resistance: the resin fraction is maintained at 92–98 wt% of the plastic film, with polyisobutylene or similar tackifier in the outer layers at 0.5–1.5 wt%, and a silica or erucamide slip/antiblock masterbatch at 0.5–2.0 wt%. Film physical properties are tested according to ISO 527-3:2018 for tensile, ASTM D5748-19 for cling and stretch performance, and ASTM D6458-18 for puncture resistance; film thickness profile is measured by ASTM D5947-18. Terminal product types are pallet stretch hoods, furniture and appliance protective over-wrap, and agricultural bale-wrap films, where line speeds at 450–900 m/min are common.

    Paperboard liquid packaging lines running slot-die extrusion coating at 250–400 m/min incorporate Icorene 2550 NAT 0000 into the heat-seal layer at 20–40 wt% blended with tubular or autoclave LDPE; the remaining 60–80 wt% is a low-neck-in LDPE selected for melt strength, because undiluted high-flow LLDPE can produce edge-trim waste above 15 % and promote draw resonance at coating weights below 15 g/m². The blend is processed on a 30:1 L/D barrier screw at a melt temperature of 280–320 °C, with a slot die gap of 0.5–1.0 mm and an air gap of 150–250 mm; the substrate is preheated by infrared to 40–60 °C to promote adhesion, and the melt curtain is nipped onto the board at 120–180 kN/m.

    Compliance for the coated board follows FDA 21 CFR 176.170(c) for direct food contact with aqueous and fatty foods, and European Regulation (EU) No 10/2011 with overall migration not exceeding 10 mg/dm²; the coating layer must also meet ISO 527-3 film tensile requirements after corona treatment to 40–44 mN/m. Terminal products are gable-top milk and juice cartons, hot- and cold-drink paper cups, and frozen food folding cartons, where the Icorene 2550 NAT 0000 fraction increases hot-tack performance and seal-through-contamination resistance compared with 100 % LDPE seal layers. Adhesive lamination alternatives may be used, but extrusion coating is selected when converters require monolayer polyethylene seal surfaces without solvent-borne polyurethane adhesives.

    When Blown Film Converters Blend Icorene 2550 NAT 0000 into LDPE-Rich Food Contact Structures

    On blown film towers, the addition of Icorene 2550 NAT 0000 is usually constrained to 10–25 wt% because the grade’s high melt flow rate lowers bubble stability when the blow-up ratio exceeds 3.0:1; at 25 wt% and above, dart-drop impact measured by ASTM D1709-22 Method A can decline and bubble breathing becomes visible at frost line heights beyond 800 mm. The base resin is typically a tubular LDPE of 0.2–0.4 g/10 min MFR; the LLDPE addition raises seal initiation temperature and permits downgauging because the blend retains tensile strength at 40–60 µm film thickness.

    On a 3-layer IBC tower with die diameter 350–500 mm, die gap 1.8–2.5 mm, and output per die circumference of 0.8–1.6 kg/h/mm, the outer layers contain 15–20 wt% Icorene 2550 NAT 0000 while the core remains LDPE to preserve bubble geometry. Melt temperatures are kept at 185–210 °C, with frost line height controlled at 500–700 mm; internal bubble cooling air is supplied at 5–15 °C when line speed exceeds 120 m/min.

    Food-contact compliance is verified under FDA 21 CFR 177.1520(c) and EU No 10/2011, including overall migration below 10 mg/dm²; seal strength is tested by ASTM F88/F88M-21, and oxygen transmission rate by ASTM D3985-17 at 23 °C, 0 % RH. Terminal products are frozen vegetable pouches, bakery bread bags, and overwrap for fresh produce, where the LLDPE blend contributes to seal integrity through traces of fat and starch dust. Published data for this specific configuration is limited; converters adjust the blend ratio downward to 15 wt% when extruder backpressure exceeds 25 MPa or when haze values measured by ASTM D1003-21 rise above 8 %.

    Free Quote

    Competitive LyondellBasell Icorene 2550 NAT 0000 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 NAT 0000 is supplied as a natural linear low-density polyethylene powder intended primarily for rotational molding and, where required, additive compounding. Manufacturer literature lists a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and a density of 0.925 g/cm³ under ISO 1183-1. The NAT 0000 suffix denotes the absence of carbon black and titanium dioxide, not the absence of thermal stabilisers. Because the powder is unpigmented, converters can introduce colour concentrates or functional masterbatches during dry blending before mold charging, provided the masterbatch carrier is compatible with a butene-based LLDPE matrix.

    What Distinguishes a Butene-Based LLDPE from Homopolymer, LDPE, and Metallocene Alternatives?

    In contrast to high-pressure low-density polyethylene, the reactor architecture of this linear low-density material introduces short-chain branches along an essentially linear backbone without the long-chain branching that governs LDPE extensional viscosity. The primary α-olefin comonomer in the Icorene 2550 NAT 0000 reactor recipe is butene-1, which lowers crystallinity relative to HDPE and shifts the ductile-to-brittle transition to lower temperature. In comparison with octene-1-based metallocene LLDPE, a butene-based grade typically displays a less uniform comonomer distribution and a different shear-thinning signature. The practical consequences are lower dart impact and lower environmental stress crack resistance at the same density, but often easier powder densification during rotomolding because of a broader melting range. The absence of long-chain branching distinguishes the material from LDPE in extrusion bubble stability, but in rotary molding that distinction is secondary to powder flow and melt densification behaviour. Where ESCR is critical for tanks holding surfactant-containing liquids, qualification should use ASTM D1693 condition C or ISO 22088-3, not merely a density comparison.

    Rotational molding with this density band is generally performed in carousel, shuttle, or rock-and-roll equipment. The powder is charged into a metal mold, and biaxial rotation distributes the melt across the cavity under oven heating. For medium-fluidity LLDPE, oven air temperatures are commonly set between 260 °C and 320 °C, with a peak internal air temperature between 190 °C and 230 °C. Published machine-specific tolerance data should be consulted; excessive peak internal air temperature above 230 °C accelerates oxidative degradation in unpigmented natural grades, while insufficient peak temperature below 190 °C leaves unmeted porosity lines and weld-line weakness. Cooling must be controlled after demolding because rapid water-mist cooling can increase warpage in large flat panels, whereas slow cooling in ambient air improves dimensional stability but extends cycle time. In thin-shell parts, converters report that the practical peak internal air temperature window for uniform wall thickness may be as narrow as ±5 °C; instrumented mold probes are required to hold that window consistently.

    Density and comonomer content set the low-temperature ductility envelope.

    Low-temperature impact performance in rotational molded parts is not governed solely by density; it is modulated by α-olefin type, molecular weight distribution, and thermal history. The density of 0.925 g/cm³ positions the product in the lower crystallinity band of linear polyethylene, promoting elongation at break above 800 % when tested under ISO 527-2 or ASTM D638. Brittleness temperature by ASTM D746 is reported below -76 °C, which supports service in cold-climate outdoor containment. For applications involving impact at freezer temperatures, dart impact testing under ISO 7765-2 or ASTM D5628 is required; published data for this specific configuration is limited, so end-use qualification on rotomolded plaques is mandatory. Welded seams produced at peak internal air temperatures below 190 °C frequently show a reduction in tensile strength relative to the isotropic wall; tensile property retention should be confirmed on sections cut from the actual part rather than from compression-molded plaques.

    Typical property profile for Icorene 2550 NAT 0000
    PropertyTypical valueTest method
    Melt flow rate5.0 g/10 min at 190 °C/2.16 kgISO 1133-1:2022, ASTM D1238
    Density0.925 g/cm³ISO 1183-1, ASTM D1505
    Tensile strength at yield12 MPaISO 527-2, ASTM D638
    Tensile elongation at break800 %ISO 527-2, ASTM D638
    Vicat softening temperature94 °CISO 306, ASTM D1525
    Brittleness temperature< -76 °CASTM D746
    Environmental stress crack resistance1000 h condition BASTM D1693

    Unlike high-flow LDPE, the melt of this LLDPE does not exhibit the same degree of long-chain branching-induced melt strength, which can alter the onset of pinhole formation in complex mold depressions. The powder bulk density, usually between 0.35 g/cm³ and 0.40 g/cm³, affects the fill ratio and must be consistent across silo lots to avoid shot-weight variation in automated charging systems. In twin-screw compounding trials on corotating machines with L/D between 30:1 and 40:1, melt temperature should be kept below 220 °C to limit gel formation; published data for this exact resin under high-shear compounding is limited. Dry-flow consistency can be tracked by establishing an internal control limit using the funnel method of ASTM D1895; lots showing a deviation greater than 5 s from the converter’s baseline should be quarantined before use in automated shot-weighing systems.

    Rheology and oxidation-induction boundaries across the rotomolding cycle

    The material’s rheological response in the absence of long-chain branching is governed by molecular weight and short-chain branch distribution. At low shear rates relevant to mold coating, viscosity remains high enough to prevent excessive drainage from vertical walls, but at the low-shear time scales of the rotomolding cycle the powder must sinter and coalesce before oxidative induction is consumed. The oxidation-induction time under ISO 11357-6 at 200 °C on natural rotomolding LLDPE may be expected in the range of 10 min to 30 min depending on the additive package; published data for this specific configuration is limited. Converters should compile baseline oxidation-induction time data on incoming lots and reject material that falls below an agreed internal control limit because oven residence times in thick-wall molding can approach the same order of magnitude.

    At the critical threshold, peak internal air temperature must not exceed the point where the stabiliser package is consumed. For molds with wall thickness above 6 mm, oven residence times of 30 min to 60 min are common, placing oxidative stability under greater stress than thin-wall articles. The temperature difference between the oven set point and the melt-pool surface drives densification; if the oven set point is raised to shorten cycle time, the outer polymer layer may exceed 220 °C while the core remains below 190 °C. That thermal gradient leads to cross-sectional heterogeneity, internal voids, and a reduction in ESCR. The practical speed limit is therefore set by heat transfer into the mold and by the induction time of the stabiliser system, not by a single property value. Mold shrinkage for rotomolded polyethylene in this density range is commonly 2 % to 3 %; tooling dimensions must compensate for both shrinkage and post-mold cooling asymmetry.

    If a converter replaces LDPE with 2550 NAT 0000 in a shuttle rotomolder, what thermal profile shifts occur?

    Substitution of high-pressure LDPE with butene-based LLDPE of 0.925 g/cm³ changes the peak internal air temperature requirement and the cooling stage. Because the LLDPE grade has a lower melt strength and a broader melting range than branched LDPE, mold coating may be achieved at a slightly lower internal air temperature, but the sintering window is narrower. In shuttle machines with open-flame or forced-air ovens, operators should first reduce the oven set point by 10 °C to 20 °C relative to an LDPE formulation of equal melt index, then adjust by observing bubble collapse and pore elimination rather than by relying on cycle time alone. Published data for this exact conversion on a shuttle machine is limited; instrumented mold trials with internal temperature probes and tensile testing of weld lines under ASTM D638 are necessary to establish the new window. The cooling phase must also be revalidated because the broader melting range can increase post-mold shrinkage anisotropy when the part is extracted too early.

    Structural and processing distinctions among polyethylene reactor families
    Resin familyShort-chain branchingLong-chain branchingTypical density rangeRotomolding implication
    Butene LLDPE, Icorene 2550 NAT 0000Butene-1 branchesAbsent0.915–0.940 g/cm³Moderate ESCR, good low-temperature ductility, lower melt strength
    High-pressure LDPELow short-chain branchingExtensive0.915–0.932 g/cm³Higher melt strength, easier bubble stability in extrusion, lower ESCR than LLDPE at similar density
    HDPE homopolymerMinimalAbsent0.940–0.965 g/cm³Higher stiffness, lower low-temperature impact, lower ESCR
    Metallocene LLDPE, octene-basedControlled octene-1 distributionAbsent0.902–0.940 g/cm³Higher dart impact and ESCR, often narrower sintering window and higher cost

    Because the product is supplied as natural powder, outdoor weathering requires let-down of an adequate light stabiliser package. Typical UV formulation for polyethylene rotomolding uses a hindered amine light stabiliser at 0.2 wt% to 0.5 wt% and a UV absorber at 0.1 wt% to 0.3 wt% in a compatible polyolefin carrier; compatibility should be verified in a low-shear dry blend before production. The resin is not inherently antimicrobial, and wet storage of the powder can lead to condensation-induced feed bridging in auger and vacuum conveying lines. Pre-drying at 70 °C to 80 °C for 2 h is recommended when bulk storage has been exposed to relative humidity above 60 %. Chemical resistance data for linear polyethylene cannot be transferred automatically from one chemical formulation to another; immersion testing under ASTM D543 on the actual chemical mixture and service temperature is required before specifying tanks or liners. Food-contact compliance must be confirmed on the final article under 21 CFR 177.1520 and Regulation (EU) No 10/2011, and REACH obligations remain with the converter for the supplied formulation.

    Top