Lyondellbasell Icorene 2550 Grn 6218 Polyethylene Linear Low Density

LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density

    • Product Name: LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 542798
    Density 0.925 g/cm³
    Melt Mass Flow Rate Mfr 190 C 2 16 Kg 0.80 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 20.7 MPa
    Tensile Elongation At Break 800%
    Flexural Modulus 276 MPa
    Vicat Softening Temperature 96°C
    Melting Temperature 123°C
    Brittleness Temperature -70°C
    Hardness Shore D 50
    Color Green

    As an accredited LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 2550 GRN 6218 Linear Low Density Polyethylene comes in 25 kg polyethylene-lined paper bags, palletized.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Icorene 2550 GRN 6218 Linear Low Density Polyethylene, securely stacked for ocean transport.
    Shipping LyondellBasell Icorene 2550 GRN 6218 is a linear low-density polyethylene resin supplied in 25 kg polyethylene bags, octabins, or bulk. It is non-hazardous for transport, not DOT/IMDG regulated. Store in a cool, dry, ventilated area away from direct sunlight and ignition sources. Handle with normal industrial hygiene.
    Storage Store LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density, at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and ignition sources. Keep original containers closed to prevent moisture, dust, and contamination. Use clean handling equipment, avoid excessive stacking, and protect from UV exposure. Maintain good housekeeping to prevent slipping on spilled pellets.
    Shelf Life Shelf life is 24 months when stored in original unopened packaging in a dry, cool, well-ventilated area away from direct sunlight.
    Application of LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density

    LyondellBasell Icorene 2550 GRN 6218, a linear low density polyethylene powder for rotational moulding and specialty compounding, is assessed across five downstream application sectors. Each sector identifies industry compliance standards, formulation addition ratio, downstream production process, and terminal finished product types. Where published data for this specific green-pigmented configuration is limited, the ranges given are bounded by standard rotomoulding LLDPE industrial practice and should be checked against supplier lot certification.

    How Rotational Molding Process Parameters Dictate Wall Thickness Uniformity in IBC Liners

    Intermediate bulk container liners are rotomoulded from the powder where stress-cracking resistance and low-temperature ductility determine service reliability under chemical load. On carousel-type rotomoulding machines with three or four stations, the powder is dry-blended in a high-speed turbo mixer at 600–1,200 rpm for 3–5 min to disperse stabilizer and reduce electrostatic fines. The mould is charged at ambient temperature, clamped, and rotated biaxially at a minor-axis/major-axis ratio of 4:1 to 8:1, while the oven chamber is held at 280–320 °C. Peak internal air temperature measured by an infrared pyrometer is controlled between 190 °C and 210 °C; failure to reach this window leaves partially fused particle boundaries at the IBC sidewall-to-corner transition, creating pinholes and reduced environmental stress crack resistance. Extended peak internal air temperature above 220 °C oxidises the inner surface and produces discoloured weld lines. Wall thickness is maintained at 3–6 mm for a 1,000 L IBC liner by adjusting oven dwell time from 20 min to 40 min, with forced-air cooling followed by ambient stabilisation to minimise shrinkage. Pre-drying at 80 °C for 2 h is required when ambient relative humidity exceeds 60%, because surface moisture on the powder increases pinhole frequency at the fusion boundary.

    • ISO 17855-1:2020 governs the designation system for polyethylene moulding and extrusion materials; ASTM D1998-15 applies to polyethylene upright storage tanks; UN packaging certification for intermediate bulk containers under ADR/RID/IMDG requires hydrostatic pressure testing at 100 kPa for liquids of relative density up to 1.5. Environmental stress crack resistance is evaluated by ASTM D1693-15 condition B, with typical acceptance above 500 h for chemical storage service.
    • Formulation addition ratio: the grade is processed as 100 wt% base powder; pre-blended antioxidant/UV stabilizer is added at 0.1–0.5 wt%; clean in-house rotomoulding regrind may be incorporated at 0–5 wt% without loss of ESCR when the particle size distribution remains above 35 mesh.
    • Downstream production process: carousel or shuttle rotomoulding machine, high-speed dry blender, oven residence 20–40 min, biaxial rotation 4:1–8:1, forced-air cooling, hydraulic demoulding, then deflashing and fitting insertion.
    • Terminal finished product types: 220 L closed-head drums, 1,000 L IBC liners, 5,000–30,000 L vertical storage tanks, double-wall bunded containment pallets, and chemical dosing tanks.

    For agricultural chemical and liquid fertilizer storage, the grade is converted into monolayer rotomoulded shells exposed to urea ammonium nitrate, glyphosate formulations, and organophosphate adjuvants. Unlike IBC chemical service, the failure mode is not solely environmental stress crack resistance but also oxidation initiated by residual fertiliser salts at scratched inner surfaces. On rock-and-roll rotomoulding lines used for horizontal saddle tanks, the powder is charged into a cylindrical mould and heated at 260–300 °C with a wall thickness of 4–8 mm. The pre-coloured green surface masks field staining, but it also imposes a higher surface-temperature limit under solar load; dark-green parts in continuous outdoor exposure can reach 70–80 °C, which accelerates oxidative induction time loss unless the stabilizer package is verified by ISO 4892-2:2021. The cooling stage is extended by 15–20% relative to white parts to avoid warpage caused by differential crystallisation through the wall. Because agricultural tanks are frequently pressure-washed with sodium hypochlorite solutions, avoid storage at concentrations above 5% active chlorine and at inlet temperatures above 40 °C; published permeation data for this specific green-pigmented rotomoulding grade in concentrated agrochemical adjuvants is limited, so field immersion testing under EN ISO 175:2010 is recommended before full commercial deployment.

    • ISO 4892-2:2021 covers laboratory weathering by xenon-arc exposure; EN ISO 175:2010 provides chemical resistance immersion test methods; ASTM D1693-15 condition C is used for ESCR ranking under detergent or fertiliser contact. If potable water contact is required, the moulder must verify compliance with FDA 21 CFR 177.1520(c) or equivalent national food-contact legislation on a lot-specific basis.
    • Formulation addition ratio: 100 wt% base powder; additional UV stabilizer at 0.1–0.3 wt%; clean regrind at 0–10 wt%; no dry pigment addition because the green colour is supplied in the grade.
    • Downstream production process: rock-and-roll rotomoulding line, internal air temperature 190–200 °C, wall thickness 4–8 mm, cooling 20–30 min, then post-mould drilling and brass insert installation.
    • Terminal finished product types: horizontal saddle tanks, crop sprayer tanks, fertiliser hoppers, livestock water troughs, and portable foamer tanks.

    Carrier Resin Requirements in Twin-Screw Colour Masterbatch Manufacture

    Colour masterbatch manufacture uses this grade as a low-melt-point carrier when the target film, injection moulding, or rotomoulding matrix is polyethylene. The resin is dosed through a loss-in-weight feeder into a co-rotating twin-screw extruder with an L/D ratio of 40:1 and a screw diameter of 50–75 mm. Because the powdered grade has a melt flow rate in the rotomoulding range, the extruder temperature profile is held between 160 °C and 220 °C, with the melt temperature at the die controlled at 200–230 °C to avoid thermal degradation of phthalocyanine green pigments. Dispersion quality is assessed by filter pressure rise on a 50 µm candle filter; pressure increase above 0.5 MPa during the trial indicates pigment agglomerates that will cause screen pack plugging in downstream film lines. The powder form requires a sealed conveying system and screw-side venting because fine particles below 100 µm can fluidise in the feed throat and create surge feeding at screw speeds above 600 rpm. Underwater pelletising is preferred over strand pelletising because the high melt flow index can produce strand sag and inconsistent pellet geometry.

    • EN 13900-5:2005 specifies assessment of pigment dispersion in polyolefin masterbatches; ISO 1133-1:2022 controls melt flow rate stability before and after extrusion; ISO 4892-2:2021 evaluates weathering performance of the final pigmented polyolefin article. Heavy-metal limits in the finished masterbatch are assessed under REACH 1907/2006/EC and, where applicable, RoHS 2011/65/EU.
    • Formulation addition ratio: carrier resin at 30–60 wt% for organic pigments and 40–60 wt% for inorganic pigments; pigment loading at 20–40 wt%; processing aids at 1–5 wt%; antioxidant at 0.1–0.3 wt%.
    • Downstream production process: co-rotating twin-screw extruder with L/D 40:1, melt temperature 200–230 °C, die-face water-ring or underwater pelletising, post-extrusion drying to 0.05% maximum moisture, and 50 µm melt filtration.
    • Terminal finished product types: colour masterbatch for polyethylene blown film, injection moulding, and rotational moulding; additive masterbatches with antiblock, slip, and UV stabilizer.

    In post-consumer recycled polyolefin compounding, the grade is dry-blended at 10–25 wt% with washed polypropylene or high-density polyethylene flake to restore impact toughness lost after oxidative chain scission. The powder form allows direct feeding into a twin-screw extruder without pre-melt side-feeding and avoids the uneven viscosity distribution caused by pelletised elastomers. On a 75 mm co-rotating twin-screw extruder operated at 400–600 rpm, the blend is processed at 200–230 °C and pelletised under water-ring cutting. The key processing conflict is viscosity mismatch: if the grade is added above 25 wt%, the tensile yield strength of a recycled injection moulding compound falls below the threshold required for structural crates, and the flexural modulus drops by 20–30% depending on the recycled polypropylene content. Conversely, addition below 10 wt% does not provide sufficient notched impact improvement to justify the formulation cost. The powder must be introduced into the melt phase after the recycled flake has passed the plastication zone; feeding both components in the same main hopper can produce low-bulk-density segregation and shot-to-shot viscosity variation.

    • ISO 179-1:2023 defines Charpy notched impact testing; ISO 180:2023 defines Izod impact testing; ISO 178:2019 defines flexural modulus determination; ISO 527-2:2012 governs tensile testing of moulding compounds.
    • Formulation addition ratio: 10–25 wt% Icorene 2550 GRN 6218 in recycled polyolefin matrix, plus 0.2–0.5 wt% antioxidant and 1–3 wt% compatibilizer when mixed post-consumer PP/HDPE streams are used.
    • Downstream production process: twin-screw compounding with main feed and side feed, screw speed 400–600 rpm, melt temperature 200–230 °C, water-ring pelletising, then injection moulding at clamp force 120–250 t depending on part size.
    • Terminal finished product types: post-consumer crates, pallets, garden furniture, storage bins, and non-visible automotive liner components.

    When Pre-Coloured Green LLDPE Powder Replaces Dry Pigment Addition in Outdoor Rotomouldings

    Outdoor playground components and street furniture are rotomoulded with the pre-coloured powder to eliminate dry pigment addition, which reduces dust exposure and batch-to-batch colour drift. The powder is dry-blended with 0.2–0.4 wt% hindered amine light stabilizer and 0.1–0.2 wt% antioxidant if the supplied grade does not already contain a full outdoor package. Thick-walled playground rotomoulding uses a biaxial ratio of 8:1 and an oven temperature of 270–310 °C; the mould surface is coated with a semi-permanent release agent, and internal air is purged with nitrogen at 0.1–0.3 bar to reduce oxidative discolouration of the green pigment. The cooling cycle is staged: 20 min forced air to 80 °C, followed by 10–15 min ambient cooling before demoulding to prevent warpage in elongated slide shells. Because playground parts are assembled with mechanical fasteners, post-mould drilling must be performed after full crystallisation; immediate drilling within 30 min of demoulding can produce stress whitening around the hole perimeter.

    • EN 71-3:2019+A1:2021 specifies migration limits for certain elements in toy materials; ASTM F1487-21 covers public playground equipment design and material durability; ISO 4892-2:2021 evaluates xenon-arc weathering; REACH 1907/2006/EC applies to substances of very high concern in the finished article.
    • Formulation addition ratio: 100 wt% base powder; optional medium-density polyethylene blend at 10–30 wt% to raise flexural modulus for long flat panels; added UV stabilizer at 0.2–0.4 wt% and antioxidant at 0.1–0.2 wt%.
    • Downstream production process: carousel rotomoulding with 8:1 biaxial ratio, nitrogen purge at 0.1–0.3 bar, oven temperature 270–310 °C, staged cooling, post-mould drilling and assembly.
    • Terminal finished product types: playground slides, climbing panels, sandpit shells, outdoor seating, planter shells, and street furniture components.
    Table 1. Formulation addition ratios and processing control parameters by downstream application
    Downstream sectorTypical addition ratioCore processing parametersPrincipal reference standards
    IBC liners and chemical storage tanks100 wt% base; 0.1–0.5 wt% AO/UV; 0–5 wt% regrindOven 280–320 °C; PIAT 190–210 °C; biaxial ratio 4:1–8:1ISO 17855-1:2020; ASTM D1693-15; ASTM D1998-15
    Agricultural chemical and fertiliser tanks100 wt% base; 0.1–0.3 wt% UV; 0–10 wt% regrindOven 260–300 °C; wall 4–8 mm; internal air 190–200 °CISO 4892-2:2021; EN ISO 175:2010; ASTM D1693-15
    Colour masterbatch carrierCarrier 30–60 wt%; pigment 20–40 wt%; additives 1–5 wt%Extruder L/D 40:1; melt 200–230 °C; filtration 50 µmEN 13900-5:2005; ISO 1133-1:2022; ISO 4892-2:2021
    Recycled polyolefin impact modification10–25 wt% in recycled PO matrixTwin-screw 400–600 rpm; melt 200–230 °C; injection clamp 120–250 tISO 179-1:2023; ISO 180:2023; ISO 178:2019
    Outdoor playground and street furniture100 wt% base; 10–30 wt% MDPE optional; stabilizers 0.1–0.4 wt%Oven 270–310 °C; biaxial ratio 8:1; nitrogen purge 0.1–0.3 barEN 71-3:2019+A1:2021; ASTM F1487-21; ISO 4892-2:2021
    Table 2. Compliance checklist matrix by downstream sector
    SectorStandard or regulationClause or test method focusCompliance verification point
    IBC liner rotomouldingADR/RID/IMDG; ASTM D1693-15; ISO 1133-1:2022Hydrostatic pressure; ESCR condition B; melt flow rateLot-level melt flow rate within declared tolerance; ESCR above 500 h; drop and stack test certification
    Agricultural tank rotomouldingEN ISO 175:2010; ISO 4892-2:2021; FDA 21 CFR 177.1520(c) if potableChemical resistance; xenon weathering; olefin polymer food-contact statusImmersion trials in field-use chemicals; colour change and stabilizer retention after weathering; food-contact lot certification
    Masterbatch manufacturingEN 13900-5:2005; ISO 1133-1:2022; REACH 1907/2006/ECPigment dispersion; carrier melt flow stability; SVHC contentFilter pressure rise below 0.5 MPa; melt flow rate shift below 10%; SDS and SVHC declaration
    Recycled compoundingISO 179-1:2023; ISO 180:2023; ISO 527-2:2012Impact strength; tensile yield strength; flexural modulusNotched impact improvement versus unreinforced recycled control; tensile yield loss below 20% at 25 wt% addition
    Outdoor playgroundEN 71-3:2019+A1:2021; ASTM F1487-21; ISO 4892-2:2021Element migration; structural durability; UV degradationMigration limits for arsenic, cadmium, lead, mercury; impact and entrapment tests; weathering colour stability
    Free Quote

    Competitive LyondellBasell Icorene 2550 GRN 6218 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 2550 GRN 6218 is a linear low density polyethylene (LLDPE) rotational moulding grade supplied as a green pigmented powder. The ethylene/α-olefin copolymer backbone is designed for low-shear melt coalescence, low-temperature ductility, and resistance to slow crack growth in hollow parts. The GRN 6218 designation identifies a green colour package dispersed through the powder rather than applied as a surface coating. The material is intended for use in biaxially rotating tools in which a measured charge is heated, fused, and cooled to form a seamless hollow shell. Published values for the unpigmented base resin indicate a density of 0.925 g/cm³ when determined according to ISO 1183-1:2019 and a melt flow rate of 5.0 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022. The green concentrate can alter infrared absorption, colour-dependent heat build-up, and certain mechanical properties; the certificate of analysis for the specific lot remains the controlling specification.

    The polymerization architecture of the base resin is relevant to its behaviour in rotational moulding. The molecular weight distribution is broader than that of a typical film-grade LLDPE, providing a longer sintering window between the onset of melting and final void-free coalescence. In a differential scanning calorimetry ramp at 10 °C/min, the base resin generally exhibits a broad melting endotherm with a peak between 120 °C and 125 °C and a crystallization onset near 108 °C on cooling. The broad melting endotherm is not a processing defect; it permits a gradual transition from the solid powder bed to the molten film and reduces the risk of sudden bubble entrapment when the internal air temperature rises. The green pigment does not normally shift the melting point by more than 2 °C, but it can change the surface emissivity and the rate of heat absorption. Processing controls should therefore be based on internal air temperature rather than visual melt pool disappearance.

    What Limits Oven Residence Time in a Rotational Moulding Charge?

    The oven residence time is governed by the rate at which the powder bed reaches the crystalline melt state, the collapse of interstitial voids, and the oxidative stability of the polymer film at the tool surface. For Icorene 2550 GRN 6218, the peak internal air temperature should reach 190–205 °C before the tool is moved to the cooling station. The upper limit is not simply a flow threshold; prolonged exposure above 315 °C at the inner surface can deplete the hindered amine light stabilizer system, oxidize the green organic pigment, and produce near-surface microvoids. In thick sections greater than 6 mm, the temperature gradient between the outer tool-side skin and the inner air-side skin becomes the controlling variable. When the tool wall is brought to 260–280 °C, the outer skin may exceed 240 °C while the inner skin remains below 180 °C, depending on part mass and tool thermal conductivity. Under these conditions, the operator must extend the hold period rather than increase the oven set point; raising the set point above 300 °C in a thick steel tool can accelerate pigment degradation before the inner surface has fully coalesced.

    In production-scale shuttle and carousel machines, the main processing failure for this grade is not incomplete melting but uneven wall thickness caused by premature particle stick-work in the mould corners. The powder has a bulk density in the range of 0.38–0.42 g/cm³ and a particle size distribution that allows a compact charge to settle quickly in a closed mould. When the charge size is calculated correctly for a 3–6 mm nominal wall, the biaxial rotation speed should be set so that the powder avalanches continuously across the cavity surface. If the minor-axis speed is too low, material accumulates in the inner corners and produces a thickness variation exceeding 0.7 mm across a 600 mm panel. If the major-axis speed is too high, the powder is held against the tool by centrifugal force and the inner surface remains sandy or pockmarked. A ratio of roughly 4:1 between the major and minor axes is a practical starting point for symmetric parts; asymmetric parts require tool-specific speed profiling.

    The material should be conditioned to 20–25 °C before charging. Powder stored in a cold warehouse and fed directly into a warm mould can pick up condensation, which then becomes steam during fusion and forms pinholes. Drying is not normally required at ambient relative humidity below 60%; above 60% RH, a dehumidified hopper or container storage at 30 °C for 24 h reduces the risk of moisture-induced porosity. Vent-hole design interacts with the grade’s pigment package. Because the green powder absorbs more infrared energy than natural resin, internal air pressure can rise faster. The vent tube must remain unobstructed during the entire heating cycle; a vent diameter of at least 6 mm for a 200 L mould cavity is a common starting point, but the exact size should be determined from the internal gas pressure and the tool seal design. A blocked vent can lead to ballooning of the green part, and the resulting wall thickness may fall below the design minimum without being detected visually.

    When Film-Grade Butene-LLDPE Is Substituted in Rotational Moulding Tooling

    Substitution of a general-purpose film-grade butene-LLDPE into a rotational moulding tool is a common cost-reduction test that exposes the difference between the narrow molecular weight distribution needed for blown film bubble stability and the broader melt behaviour needed for low-shear coalescence. Icorene 2550 GRN 6218 is differentiated from film-grade LLDPE by its powder geometry, its melt flow rate, and its additive stabilization. Film-grade pellets must be cryogenically ground for rotomoulding, which raises the fines content and produces an inconsistent bulk density; heat transfer to the powder bed then becomes dependent on particle shape and size distribution. The molecular weight distribution of the 2550 base resin permits a lower viscosity at rotomoulding shear rates, allowing bubbles to escape before the inner surface freezes. A film resin with a nominal 1.0 g/10 min melt flow rate requires either a higher oven temperature or a longer residence time, which can push the green pigment and the stabilizer past their thermal endurance limit.

    Comparative profile of Icorene 2550 GRN 6218 base resin against typical rotomoulding alternatives
    PropertyIcorene 2550 GRN 6218 base resinFilm-grade butene-LLDPEConventional rotomoulding HDPE
    Density, ISO 1183-1:20190.925 g/cm³0.918–0.922 g/cm³0.940–0.945 g/cm³
    Melt flow rate, ISO 1133-1:20225.0 g/10 min1.0–2.5 g/10 min4.0–7.0 g/10 min
    Tensile stress at yield, ISO 527-2:201213.5 MPa10–12 MPa20–23 MPa
    Flexural modulus, ISO 178:2019350 MPa240–300 MPa750–900 MPa
    Environmental stress crack resistance, ASTM D1693-15 F50, 10% Igepal>1000 h300–600 h50–200 h

    The lower density of the 2550 base resin relative to conventional rotomoulding HDPE reduces flexural modulus and increases low-temperature ductility. This difference is operationally significant in agricultural tanks that must survive impact at -20 °C without brittle fracture. When the same tool is moulded in HDPE, wall stiffness rises by roughly 2–2.5 times, but the part may fail by stress crack at moulded-in inserts or sharp drain bosses if the tank is subjected to cyclic hydrostatic loading. The LLDPE grade is therefore selected for parts where deformation tolerance and slow crack growth resistance are more important than hoop stiffness. Compared with other LLDPE rotomoulding grades, the 2550 base resin is positioned in the medium melt flow rate class; higher-viscosity LLDPE grades may provide slightly better ESCR but require longer cycles. Lower-viscosity grades fill thin ribs more readily but can sacrifice impact toughness. The green colorant package further distinguishes Icorene 2550 GRN 6218 from natural rotomoulding LLDPE because it removes the need for dry colour blending at the machine, which reduces colour inconsistency and lowers the risk of pigment agglomeration on the inner surface.

    Mechanical property differences between this grade and a general-purpose HDPE rotary-moulded shell appear most clearly in the flexural modulus and the low-temperature impact region. The lower crystalline fraction of the LLDPE base resin produces a flexural modulus near 350 MPa when measured according to ISO 178:2019 on a compression-moulded plaque prepared from the base powder. In contrast, a conventional rotomoulding HDPE with a density of 0.942 g/cm³ typically exhibits a flexural modulus in the range of 750–900 MPa. The lower modulus is advantageous when the part must absorb impact without cracking, as in a thin-wall tank or fender; however, it reduces hoop stiffness in pressurised service. The tensile stress at yield of the base resin is approximately 13.5 MPa according to ISO 527-2:2012, and the elongation at break typically exceeds 600%. The green pigment can reduce elongation at break by a small amount because rigid pigment particles concentrate stress at large deformations. The reduction is normally less than 10% when the pigment is well dispersed, but it should be verified on the moulded part because wall thickness and internal air temperature affect final crystallinity and skin-core morphology. Published data for this specific green configuration is limited; mechanical design should therefore use a safety factor appropriate for a pigmented rotomoulding LLDPE rather than the natural base resin datasheet alone.

    Environmental Stress Crack Resistance, UV Stabilizer Retention, and Pigment Dispersion

    The environmental stress crack resistance of the base resin is measured by the failure time of notched specimens in a stress cracking agent. For the base grade, the F50 value exceeds 1000 h under 10% Igepal at 50 °C when evaluated according to ASTM D1693-15. This property is not solely a function of density; it depends on the comonomer distribution, the molecular weight distribution, and the crystalline tie-molecule population. The green pigment is a colourant system whose dispersion quality influences local stress concentration at the pigment-polymer interface. If the pigment is poorly dispersed, a notched part in a detergent or agricultural chemical environment may fail at a shorter time than the same part moulded from the unpigmented base resin. The reduction is not always captured by published base-resin values; for this reason, end-use chemical compatibility testing should be conducted on the finished pigmented article.

    The ultraviolet stabilizer package in Icorene 2550 GRN 6218 is intended for general outdoor exposure, but the grade is not a universal weathering solution. In applications such as water tanks exposed to high ultraviolet flux at elevations above 2500 m, surface oxidation may occur before mechanical loss is detected. The thermal history of the moulding cycle also affects stabilizer retention. If the peak internal air temperature is allowed to exceed 210 °C or if the tool is left in the oven after the inner surface has fully coalesced, the chromophore and the hindered amine stabilizer can co-deplete. Processors should periodically measure the yellowing index or carbonyl index of the inner surface when a long outdoor warranty is required.

    Regulatory and safety documentation for the final article must be established for the specific application and region. Standard polyethylene closure documents may support food-contact or potable-water use in the unpigmented base resin, but the green colour package in GRN 6218 requires separate evaluation under the applicable national or regional scheme. The material safety data sheet and food-contact statement should be obtained from LyondellBasell for the exact grade and colour combination. The product is not recommended for continuous immersion in strong oxidizers, aromatic solvents, or certain surfactant formulations that plasticize polyethylene. Welding and repair of the moulded part should be performed with the same grade or a compatible LLDPE rod; the use of HDPE welding rod can create a brittle fusion line because the two materials have different melt indices and shrinkage rates. Storage of the powder should avoid direct sunlight, open water spray, and temperatures above 50 °C to prevent caking and additive migration. Because published data for this specific green configuration is limited, the design engineer should request a lot-specific certificate of analysis and, for critical parts, a full mechanical evaluation at the minimum service temperature and maximum chemical exposure.