| HS Code | 903905 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.925 g/cm3 |
| Melt Index 190 C 2 16 Kg | 2.5 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength | 200 g |
| Haze | 6% |
| Gloss | 85% |
| Vicat Softening Point | 95°C |
| Melting Point | 122°C |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 2550 BUE 5148 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 2550 BUE 5148 Linear Low Density Polyethylene is supplied in 25 kg bags, typically palletized for transport. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with LyondellBasell Icorene 2550 BUE 5148 LLDPE; palletized 25 kg bags, shrink-wrapped, secured for ocean freight. |
| Shipping | LyondellBasell Icorene 2550 BUE 5148 Polyethylene, Linear Low Density, is shipped as non-hazardous resin pellets, typically in 25 kg bags or 1,000 kg jumbo bags, palletized and wrapped. It is not DOT/IMDG regulated. Transport by truck, rail, or container at ambient temperature; keep dry and avoid direct sunlight/heat. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep in tightly closed original bags or containers, palletized off the floor to prevent moisture uptake and contamination. Avoid excessive stacking or pressure that may deform pellets or packaging. Maintain clean handling areas; no special temperature control is required under normal conditions. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored unopened in original packaging, cool, dry, and away from direct sunlight. |
On multi-layer blown-film lines converting 40–150 µm agricultural silage cover structures, Icorene 2550 BUE 5148 is typically specified for the outer skins or for the backing ply where dart impact, tear propagation, and low-temperature flexibility control field performance. The anaerobic ensiling environment demands a film that survives repeated mechanical tensioning on clamp pits and feed-out machinery, not a high oxygen-barrier structure, because the cover’s primary function is physical exclusion of water ingress and oxygen contact at the exposed face. A standard three-layer layout in commercial practice uses a 20/60/20 thickness split: the skin layers carry 2.0–4.0 wt% of a polyethylene-based UV/carbon black masterbatch and 0.3–0.8 wt% of a silicate antiblock, while the core may contain up to 20 wt% of clean edge-trim reclaim provided that melt flow stability is maintained. EN 13206:2017 sets dimensional, weathering, and impact requirements for thermoplastic films used in agriculture and horticulture; EU REACH and RoHS documentation is carried through the masterbatch and raw material supplier chain rather than through film fabrication alone.
On a single-screw line with a 25:1 L/D barrier screw and an internal bubble cooling system, the die gap is set between 1.8 mm and 2.5 mm, blow-up ratio is kept at 2.0:1 to 2.8:1, and the frost line is held at 6 to 9 die diameters above the die face; melt temperature is typically 190–220°C. Gauge variation above ±5% across the web remains a documented production bottleneck because uneven film thickness generates localized tension when the cover is mechanically drawn over the silage clamp; this is best controlled by internal bubble cooling and a segmented die lip rather than by raising melt temperature alone. Processing aids are sometimes introduced at 0.1–0.3 wt% to suppress melt fracture and die-lip buildup, but the exact concentration must be confirmed against the additive package stated in the supplier’s certificate of analysis. The finished silage cover is cut to 8–12 m widths and is deployed as a 100–150 µm monolayer or three-layer sheet, with tensile properties commonly reported under ISO 527-3:2018 and dart impact under ASTM D1709. One limitation: as a butene-copolymer LLDPE, the grade does not provide the oxygen barrier of EVOH or of a vermiculite-coated barrier film, so silage losses can occur if the cover is perforated or if the film is stored under heavy UV exposure without a stabilizer package; published data for this specific configuration is limited when the core layer contains reclaimed post-industrial film above 20 wt%.
Periodic thickness oscillation, termed draw resonance, becomes the controlling process defect when a five-layer cast line runs below 18 µm final gauge at high pre-stretch. In machine stretch film, Icorene 2550 BUE 5148 is used as the outer cling layer or as a balancing skin layer because its butene comonomer distribution gives a controlled balance between elongation and puncture resistance. A typical five-layer A/B/C/B/A architecture uses a layer ratio of 10/20/40/20/10; the outer layers contain 0.5–2.0 wt% polyisobutene-based cling masterbatch and the internal skins contain 0.2–0.5 wt% antiblock. The core may carry 20–30 wt% metallocene-catalyzed LLDPE to raise dart puncture and elongation, while the butene LLDPE outer layers reduce adhesive transfer to the wrapped product. Compliance is documented under ASTM D5748 for stretch wrap puncture resistance, ASTM D5458 for peel cling, and ISO 7765-1 for free-falling dart impact.
| Layer | Thickness split | Resin assignment | Critical test |
|---|---|---|---|
| Outer cling | 10% | Icorene 2550 BUE 5148 + cling masterbatch | ASTM D5458 |
| Internal skin | 20% | Butene LLDPE + antiblock | ASTM D1894 |
| Core | 40% | mLLDPE / butene LLDPE blend | ASTM D5748 |
| Internal skin | 20% | Butene LLDPE + antiblock | ASTM D1894 |
| Outer cling | 10% | Icorene 2550 BUE 5148 + cling masterbatch | ASTM D5458 |
On a cast-film line with die gap 0.5–0.8 mm, air gap 120–180 mm, and chill roll temperature 15–22°C, line speed is commonly pushed to 300–600 m/min for 12–23 µm films. The draw ratio between die gap and final gauge then reaches 25:1 to 35:1; beyond a critical value, periodic bands of ±2–3 µm appear in the web and cause pre-stretch failures on turntable wrappers. This failure mode is suppressed by widening the die gap, raising the melt temperature within the supplier-approved range, or adding a processing aid at 0.1–0.3 wt%, not by reducing chill roll temperature alone. Edge trim in cast stretch is usually 5–8%; if reclaimed trim exceeds 10% of the core layer, gels and clinging variability become batch-to-batch defects. The finished 17–23 µm machine film is operated at pre-stretch ratios up to 250% on powered wrappers; low-temperature unwind and cling retention are the final acceptance criteria, not tensile strength alone.
Flat-bottom form-fill-seal sacks running 80–120 µm film on three-layer blown lines present a different failure chain: drop impact and longitudinal tear at the weld region, not draw resonance. The compliance target for such sacks is usually ISO 21898:2004 for thermoplastic sacks, with cube-drop data reported under ISO 7965-2 and dart impact under ASTM D1709; food-contact grades must comply with FDA 21 CFR 177.1520 and EU 10/2011 when used for dry foods or resin pellets. In practical formulation, 10–20 wt% high-pressure LDPE is added to the butene LLDPE base to suppress bubble oscillation at a low blow-up ratio of 1.8:1 to 2.2:1, because low BUR increases machine-direction tear resistance but reduces bubble stability; this is compensated by setting the die gap to 2.0–2.5 mm and holding the frost line at 7–8 die diameters.
Internal bubble cooling with a stabilisation cage is mandatory when line throughput exceeds 250 kg/h, otherwise the bubble will wander and the weld seam will shift from the centre of the sack. Slip and antiblock masterbatch additions of 0.3–0.8 wt% are selected to keep the coefficient of friction below 0.2–0.3 under ASTM D1894; this allows sack opening on the filling spout without blocking. The finished product is a 20–50 kg sack for resins, fertiliser granules or polymer pellets; fitness-for-use is judged by a 1.0 kg dart impact using Method A staircase per ASTM D1709 and by a minimum Elmendorf tear value determined by the end-user specification rather than by a universal minimum. In high-humidity warehouses, surface condensation on cold pellets can raise the effective humidity above 70% and produce blocking at the inner surface if the antiblock concentration is below 0.3 wt%; this is a known batch-to-batch variance issue, not a resin failure.
In frozen food flexible packaging, the sealant layer is exposed to sub-zero storage and rapid heat-seal dwell times on vertical form-fill-seal equipment. Icorene 2550 BUE 5148 is placed into the sealant layer only when the converter accepts the higher seal initiation temperature of butene LLDPE relative to metallocene-catalyzed grades; otherwise it is moved into the core or outer layers to supply stiffness and dart impact without retarding seal cycle time. The food-contact structure is a three-layer blown film with a thickness split of 20/60/20; the sealant layer commonly contains 60–80 wt% of the LLDPE grade plus 20–40 wt% of high-pressure LDPE, while the core carries 10–15 wt% of a white masterbatch for opacity and 0.2–0.4 wt% of a oleamide or erucamide slip additive. Compliance is established under FDA 21 CFR 177.1520 and EU 10/2011, with overall migration measured under the food-contact conditions specified in EU 10/2011 Annex V; hot-tack and seal strength are tested in accordance with ASTM F1921/F1921M and ASTM F88/F88M.
On the blown-film line, a die gap of 1.8–2.2 mm and blow-up ratio of 2.2:1 to 2.8:1 are used to balance machine-direction and transverse-direction seal-strength anisotropy; the frost line is maintained at 6–8 die diameters. Melt temperatures above 220°C can oxidise the slip additive and raise seal initiation temperature, so the converter typically operates at 190–210°C and uses a 25:1 L/D screw with a Maddock mixing section to homogenise the slip phase. The terminal product is a pillow bag or flat pouch used for frozen vegetables, french fries, or ice cream at film thicknesses from 25 µm to 60 µm; the acceptance protocol includes a -20°C storage test and a sealing-pressure window of 0.3–0.6 MPa on the sealer jaws. If the sealant layer is downgauged below 20 µm, hot-tack strength becomes the bounding constraint rather than tensile strength.
Solvent-based adhesive lamination is replaced in polyolefin-based pouches when the converter imposes a single-pass coating weight of 12–20 g/m² and needs a heat-sealable outer ply without post-curing. In this application, Icorene 2550 BUE 5148 is blended at 20–40 wt% into a high-pressure LDPE coating resin to reduce neck-in and to raise film tear resistance after the laminate is creased. The extrudate is applied onto paperboard, aluminium foil, or corona-treated polyester at a melt temperature of 285–315°C; the exact upper limit is governed by the supplier’s thermal stabilisation documentation, because butene LLDPE can generate off-taste by-products if it is overheated for long residence times. Adhesion is developed through a primer and ozone treatment on the web, not through the resin alone; the converter must control air gap to 200–300 mm and chill roll temperature to 15–20°C to prevent thermal degradation at the interface.
Compliance for food-contact laminates is covered by FDA 21 CFR 177.1520 and EU 10/2011; migration testing is performed on the finished laminate under the intended food type and sterilisation condition, and the standards are assigned by the end-use packaging specification rather than by the resin grade alone. The production-scale equipment is a single-screw extruder with 30:1 L/D and a barrier screw; die gap is set at 0.4–0.6 mm, and the line is equipped with edge-trim slitting and closed-loop gauge control. A documented limitation is that the addition of LLDPE above 40 wt% can increase backpressure and reduce draw-down capacity at coat weights below 8 g/m²; published data for this specific configuration is limited, so line trials are required to set the maximum line speed. The terminal product includes retort pouches, lidding films, and aseptic brick laminates where seal integrity after creasing is the decisive acceptance variable.
On cast coextrusion lines producing 25–60 µm masking films for acrylic, polycarbonate, or coated metal sheets, Icorene 2550 BUE 5148 is used in the backing layer rather than in the pressure-sensitive adhesive layer when low gel count and consistent unwind are required. The film is a two-layer or three-layer structure: a backing layer of 70–80 wt% butene LLDPE and 20–30 wt% LDPE, plus an adhesive layer based on EVA or styrenic block copolymer that contains 10–25 wt% of the LLDPE to control surface smoothness. Peel adhesion is measured against stainless steel under ASTM D3330/D3330M and against the actual sheet surface under FINAT FTM 1; the required peel force is product-specific and falls in the range of 0.5–5.0 N/25 mm, depending on whether the mask is intended for long-term exterior exposure or for short handling protection.
Cast coextrusion uses a die gap of 0.6–0.8 mm, a chill roll temperature of 15–20°C, and a corona treatment dose of 20–40 W·min/m² to anchor the adhesive layer; if the corona dose is below 10 W·min/m², delamination occurs during slitting. The terminal product is slit to 1.2–2.5 m widths and supplied in 500–2000 m rolls; the acceptance specification includes a residual-adhesion test on the protected sheet after 7 days at 60°C, usually reported as the percentage change in peel force under ASTM D3330/D3330M. The operational boundary is that butene LLDPE does not provide the low-modulus conformability of a tailored mLLDPE masking layer, so it is not recommended for deep-draw or rough-textured surfaces unless the backing layer is downgauged and the adhesive layer is thickened.
Competitive LyondellBasell Icorene 2550 BUE 5148 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 BUE 5148 Polyethylene, Linear Low Density, is a powder-grade linear low-density polyethylene supplied for rotational moulding. The numerical identifier 2550 designates the base resin grade, while the alphanumeric suffix BUE 5148 is a product configuration identifier that may specify a colourant and stabiliser package; exact composition is recorded on the safety data sheet and the grade technical datasheet. Linear low-density polyethylene of this type is produced by copolymerization of ethylene with an alpha-olefin, producing short-chain branches that reduce crystallinity relative to high-density polyethylene while retaining higher tensile yield stress and improved environmental stress crack resistance compared with high-pressure low-density polyethylene. Grade identity is verified through melt mass-flow rate measurement according to ISO 1133-1:2022 or ASTM D1238-20 at 190 °C under 2.16 kg, and through density measurement according to ISO 1183-1:2019 or ASTM D792-20 at 23 °C. Published values for this exact suffix are limited; lot-release properties should therefore be obtained from the certificate of analysis rather than transferred from an unmodified LLDPE datasheet.
Compared with an unmodified LLDPE rotational moulding powder, the BUE 5148 configuration is differentiated primarily by the additive and colourant package rather than by a change in polymer backbone. The base resin remains a linear low-density polyethylene; however, pigment particle size, thermal absorptivity, and stabiliser volatility can alter mould heat-up response. Dark or saturated pigments may increase radiative heat absorption and shorten the time required to reach peak internal air temperature on a given tool, whereas light or reflective pigments can extend the heating cycle. This shift is measured with a mould-mounted infrared pyrometer or through-the-part thermocouple; it is not predicted reliably from melt temperature alone. Relative to high-pressure LDPE powder, the LLDPE base exhibits lower long-chain branching, changing the sintering rate under low-shear rotational moulding. Moulded parts generally show higher tensile yield stress and improved environmental stress crack resistance when assessed according to ASTM D1693-15. Compared with HDPE rotomoulding grades, the lower crystallinity of LLDPE reduces flexural modulus; converter practice is to increase nominal wall thickness by 1–2 mm where bending stiffness is the limiting design criterion.
On production-scale carousel and shuttle rotomoulding machines, the mould is charged at ambient temperature with a predetermined weight of powder, rotated biaxially inside an oven at a speed ratio commonly between 4:1 and 8:1, and heated until the part reaches a consistent peak internal air temperature. Polyethylene rotational moulding powders generally require peak internal air temperature values in the 180–220 °C range; values below this range produce incomplete sintering and a powdery inner surface, while excessive values can promote oxidative degradation, colour shift, and reduced impact resistance. Oven set points are often set between 260–320 °C, but these are not a substitute for peak internal air temperature control because tool mass, wall thickness, and oven air velocity change the heating response. The powder should be free of surface moisture; although polyethylene is not hygroscopic, condensation during storage can generate pinholes. If storage relative humidity exceeds 60%, pre-drying with dry air at 60–80 °C is typical. Drying above 100 °C is avoided because powder particles may agglomerate or additive components may degrade. Particle-size distribution is verified by sieve analysis according to ASTM D1921; coarse fractions retained above 710 µm can create surface roughness, while excessive fines can reduce dry flow and increase dust generation. Dry flow and bulk density are measured by ASTM D1895.
Sintering behaviour in rotational moulding is governed by melt viscosity and particle coalescence rather than by high-shear melt pumping. The early stage of particle fusion is viscosity-controlled; trapped air must diffuse out through interparticle voids without forming blowholes. For this reason, moulders monitor peak internal air temperature, oven residence time, and cooling rate together rather than adjusting one variable alone. Oven residence time is not a fixed grade property. For nominal wall thicknesses between 3–6 mm, cycle time may vary significantly with tool material, part geometry, and venting. Forced-air cooling from peak internal air temperature to demould temperature at roughly 10–20 °C/min is typical for medium-wall parts; water mist can reduce cycle time but increases residual stress and dimensional variation. Vents must remain clean because blocked vents cause gas entrapment and pinholes, especially in deep-draw locations.
Third-party qualification programmes for rotationally moulded LLDPE parts typically apply the following characterisation matrix. The matrix is provided as a test-method checklist, not as a release-value table for this suffix; grade-specific values must be taken from the LyondellBasell certificate of analysis.
| Measured attribute | Test method | Condition | Relevance to rotational moulding |
|---|---|---|---|
| Density | ISO 1183-1:2019 / ASTM D792-20 | 23 °C | Confirms base resin crystallinity and stiffness target |
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-20 | 190 °C, 2.16 kg | Indicates melt flow and sintering behaviour under low shear |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638-14 | 50 mm/min for rigid specimen | Controls load-bearing performance in tanks and structural parts |
| Flexural modulus | ISO 178:2019 / ASTM D790-17 | Method-defined strain rate | Guides wall-thickness adjustment relative to HDPE |
| Charpy notched impact | ISO 179-1:2020 / ASTM D6110-18 | 23 °C and -30 °C | Assesses low-temperature toughness of moulded articles |
| Environmental stress crack resistance | ASTM D1693-15 | 50 °C, 10% or 100% Igepal CO-630 | Critical for chemical tanks and containers with residual stress |
| Oxidative induction time | ISO 11357-6:2018 | 200 °C, oxygen atmosphere | Screens stabilisation adequacy and long-term thermal ageing risk |
| Vicat softening temperature | ISO 306:2013 | A50 / B50 | Relates to safe service temperature under low mechanical load |
| Heat deflection temperature | ISO 75-2:2013 | 1.8 MPa, flatwise | Used for stiffness-related thermal limits, though rotomoulded parts are often stress-limited |
Test specimens are cut from flat moulded plaques or from the actual part. Part-specific cooling history, pigment dispersion, and inner-surface oxidation can shift mechanical data relative to compression-moulded reference plaques. Comparative qualification therefore requires identical specimen geometry, moulding history, and conditioning according to ISO 291:2008 or equivalent laboratory atmosphere control.
Typical rotationally moulded components produced from linear low-density polyethylene powder include chemical storage tanks, intermediate bulk containers, agricultural hoppers, marine buoys, kayaks, automotive fenders, recreational structures, and material-handling bins. Wall thickness in these applications commonly ranges from 3–6 mm, but deep-draw geometry and tool-temperature variation can produce wider thickness distribution. On production lines, pinholes and blowholes are induced by moisture, blocked vents, or insufficient peak internal air temperature; warpage and sink marks are observed when cooling is too rapid or when the part is forced from the mould before it is sufficiently rigid. Aluminium tooling is frequently used for prototype and short-run projects because its thermal conductivity of 150–200 W/(m·K) shortens cycle time; carbon steel moulds with conductivity near 40–50 W/(m·K) are more common for large tanks where slower, more uniform heating is beneficial. Surface treatments and mould release agents must be selected for the service temperature range; silicone-based release products can interfere with post-mould welding, painting, or adhesive bonding.
In multi-layer rotational moulding, a pigmented outer skin is moulded first, followed by a foam or natural LLDPE core. The interface must reach sufficient temperature for interlayer adhesion; if the peak internal air temperature is too low, delamination occurs at the skin-core boundary. Because pigments can alter heat absorption, cycle records should be re-established when a tool is converted from natural powder to the BUE 5148-configured powder. Foamed core layers require a chemical blowing agent with a decomposition onset that overlaps the resin sintering range; local overtemperature from exothermic decomposition can create internal voids and surface gas marks. Amine-containing antistatic additives are screened for compatibility with the phenolic and phosphite stabilization used in many polyolefin formulations; incompatibility can cause colour shift, plate-out, or reduced long-term thermal stability. Unlike polar ethylene-vinyl acetate copolymers, LLDPE does not rely on vinyl acetate content for flexibility; therefore chemical resistance to aggressive liquids is generally improved, but adhesion to polar substrates may be lower unless the surface is oxidized or primed. Weld lines, insert bosses, and post-mould routed openings should be located away from the highest residual stress zones because the lower modulus of LLDPE permits greater strain recovery than rigid HDPE structures.
Prior to substitution on an existing tool, the moulder should compare dry flow, sieve distribution, melt mass-flow rate, and density against the incumbent grade. Direct food-contact status for the BUE 5148 pigmented configuration should be confirmed under FDA 21 CFR 177.1520 or EU Regulation 10/2011; compliance of the base polymer does not automatically extend to the pigmented compound. Electrical and electronic applications should be checked against RoHS substance restrictions, and the EU importer should verify REACH registration obligations. The powder should not be blended with polypropylene, PVC, or acetal residues; these contaminants can create unmetled domains and delamination in the moulded wall. If a lot has been stored under high humidity or temperature cycling, surface moisture and particle agglomeration should be evaluated before charging the mould. Published data for this specific configuration is limited; therefore, grade-release values, processing limits, and regulatory end-use compliance should be obtained from the LyondellBasell technical datasheet, certificate of analysis, and current safety data sheet.