| HS Code | 643418 |
| Density | 0.925 g/cm³ |
| Melt Index | 50 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 9.65 MPa |
| Tensile Strength At Break | 8.27 MPa |
| Tensile Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Hardness Shore D | 50 |
| Vicat Softening Point | 93.3 °C |
| Deflection Temperature At 0 46 Mpa | 60 °C |
| Brittleness Temperature | -76.1 °C |
As an accredited LyondellBasell Icorene 2550 BLK 9001 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg net) for LyondellBasell Icorene 2550 BLK 9001 LLDPE. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 2550 BLK 9001 LLDPE; palletized 25 kg bags, securely stowed and restrained for ocean transport. |
| Shipping | Shipping description: LyondellBasell Icorene 2550 BLK 9001 Polyethylene, Linear Low Density, black pellet resin. Typically non-hazardous; not DOT, IMDG, or IATA regulated. No UN number, class, or packing group assigned. Transport in moisture-resistant bags, boxes, or bulk containers. Keep dry, cool, ventilated, and away from ignition sources. |
| Storage | Store LyondellBasell Icorene 2550 BLK 9001 Polyethylene, Linear Low Density indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original containers/packages closed, palletized, and protected from moisture, dust, contamination, and physical damage. Avoid strong oxidizers. Minimize dust accumulation, ensure ventilation, prevent prolonged UV exposure, and follow local regulations plus manufacturer recommendations. |
| Shelf Life | Shelf life is typically 12 months from date of manufacture when stored in original unopened packaging in a cool, dry area. |
In a 2,000 L vertical cylindrical tank rotomoulded for agricultural water treatment additive dosing, Icorene 2550 BLK 9001 is introduced as a pre-compounded black LLDPE powder with a nominal particle distribution below 500 µm. The mould charge is calculated from the projected surface area of the cavity at 3.2 kg/m², corresponding to a nominal wall thickness of 6 mm after sinter consolidation. Oven air temperature is held at 285°C during the heating cycle, and peak internal air temperature is maintained at 190°C for 8 minutes to complete powder coalescence. The biaxial rotation ratio is set at 4:1 with a primary axis speed of 8 min⁻¹ and a secondary axis speed of 2 min⁻¹. A heating cycle of 22 minutes is followed by forced-air cooling until the internal air temperature falls to 80°C before demoulding. On production-scale shuttle machines, the most frequent defect is porosity at the upper pole where the powder bed remains static during rotation reversal. That defect is controlled by specifying a powder dry flow value below 30 s/100 g and by maintaining ambient relative humidity below 60% before charging. If surfaced condensation occurs during storage, the powder is dried at 70°C for 2 hours in a desiccant bed. The finished tank shell is evaluated to ASTM D1998-21 for design stress and leakage under hydrostatic load. Chemical compatibility is confirmed by immersion testing according to ISO 175:2010; published data for this specific grade in ferric chloride solution at 10% concentration is limited, so end-use qualification is required. The terminal article is a 2,000 L vertical dosing tank with a 6 mm nominal wall and ultraviolet-stabilised black exterior for outdoor installation.
In 5,000 L rainwater retention vaults and below-ground storage chambers, Icorene 2550 BLK 9001 is dry-blended with clean, unpigmented post-industrial rotomoulding regrind at mass fractions up to 20%. The upper limit is not determined by density but by environmental stress crack resistance measured on notched constant-strain tensile specimens immersed in 10% Igepal CO-630 at 50°C according to ASTM D1693-15. A dry blend containing 20% regrind can shift melt flow index by less than 0.5 g/10 min when tested at 190°C/2.16 kg under ISO 1133-1:2022, yet the ESCR F50 value often falls by a relative 15–30% depending on the regrind thermal history and residual antioxidant content. The mould is a 5,000 L vault with a 5 mm wall and internal ribs spaced at 1.5 m to resist soil loading. Cooling rate at the base boss must not exceed 10°C/min because faster quenching widens the skin-core density differential and reduces slow crack growth resistance at the connection stub. This vault is tested to AS/NZS 4766 for rotational moulded polyethylene storage tanks intended for rainwater and non-potable water. If potable water contact is specified, additional testing under AS 4020 is required because the black pigment and additive package of the 9001 formulation cannot be assumed compliant without migration and taste analysis. The terminal component is a 5,000 L underground rainwater retention vault with a 5 mm minimum wall, ribbed side panels, and a domed access opening capable of receiving a 450 mm polyethylene riser.
In saltwater marine fender bodies and subsea buoyancy collars, the pre-compounded black 9001 stabiliser package supplies the required ultraviolet absorption without a separate color masterbatch. A single-walled fender shell with a 1.5 m diameter is rotomoulded at a wall thickness of 4 mm using a charge weight of 2.1 kg/m². The mould is run on an independent-arm machine with a 5:1 rotation ratio; the primary axis runs at 6 min⁻¹ and the secondary axis at 1.2 min⁻¹. After demoulding, the shell is filled with a two-part polyurethane foam having a core density of 60 kg/m³. The foam fill is performed only after the shell surface temperature drops below 35°C; exothermic rise above 80°C at the inner wall can soften the LLDPE and create local depressions. The most serious failure mode on manufacturing lines is flange warpage at the bolting face when the part is removed before reaching dimensional stability. The shell is therefore held in a water-cooled jig for 15 minutes after demoulding until the flange flatness deviation is below 0.5 mm. Weathering performance is screened under ASTM G154-23 Cycle 1 for 2,000 h; black parts are inspected for colour shift with a target delta b below 3. Impact after cold exposure is evaluated according to ISO 6603-2:2023 at -20°C. The terminal product is a black fender shell of 4 mm wall thickness with closed-cell polyurethane core filling and stainless steel end plates overmoulded or bolted after shell production. Published data for this exact marine fender configuration using Icorene 2550 BLK 9001 is limited, so saltwater immersion qualification is recommended under ISO 175:2010 for a minimum of 1,000 h at 23°C and 50°C.
Stationary 150 L diesel day tanks require a minimum wall thickness of 6 mm at the fitting boss. Icorene 2550 BLK 9001 is rotomoulded as a single-piece tank with moulded-in brass inserts. The cooling cycle controls the inner-wall density gradient: forced-air quench at 0.8°C/s internal air temperature drop produces a denser inner skin, while slow cooling at 0.3°C/s yields more uniform crystallinity across the wall. In practice, a dual-stage cooling profile is applied: natural convective cooling from 190°C to 120°C, followed by forced air to 70°C before insert extraction. The failure mode is boss-area pinholing caused by powder bridging at the narrow annulus around the insert; a minimum boss radius of 6 mm and a local wall thickness of 7 mm reduce the incidence below 2% on multi-station carousel lines. The grade is processed without additional colour concentrate because the 9001 formulation already contains the black pigment and weathering stabiliser package. Do not dry-blend more than 10% natural regrind into fuel tanks, as ultraviolet opacity and surface quality around the filler neck can become inconsistent. Continuous exposure to aromatic hydrocarbons above 10% volume should be qualified separately; this grade is not marketed as a dedicated hydrocarbon barrier resin. For stationary aboveground diesel day tanks, UL 1314 or equivalent certification is referenced, but published data for this specific formulation in UL 1314-rated tanks is limited, so fuel contact mass change, thickness swell, and permeation must be confirmed by the fabricator using ASTM D543 or equivalent immersion practice. The terminal component is a 150 L generator day tank with a 6 mm nominal wall, 7 mm boss walls, moulded-in brass inserts, and a black ultraviolet-stable exterior.
| Application sector | Standard or regulation | Practical test condition |
|---|---|---|
| Agricultural vertical storage | ASTM D1998-21 | Hydrostatic design stress at 23°C; no leakage after 24 h |
| Rainwater retention vault | AS/NZS 4766 | Impact at -10°C; soil load deflection below 2% |
| Marine buoyancy shell | ASTM G154-23 | 2,000 h QUV; delta b below 3 |
| Diesel day tank | UL 1314 or equivalent | Fuel immersion; no continuous aromatic contact above 10% |
| Telecom enclosure | IEC 60529, UL 94 HB | IP65 dust and water ingress; horizontal burn rate |
| Refuse container | EN 840-2:2020, ISO 6603-2:2023 | Drop impact at -20°C; comb-lift dimensional set |
A 300 L agricultural feed hopper is rotomoulded with a nominal wall of 4 mm and external ribs whose root thickness is 3 times the nominal wall. Rib spacing is set at 300 mm to prevent oil-canning on flat side panels. The mould is filled with Icorene 2550 BLK 9001 at 2.4 kg/m². Heating occurs in a rock-and-roll machine with a 1:4 secondary-to-primary speed ratio; peak internal air temperature is 185°C. The part is cooled in a water mist cabinet until 75°C and then constrained in a steel cooling fixture for 20 minutes to lock the ribbed geometry. Warpage is measured diagonally across the top opening; a deviation above 4 mm on a 1.2 m span is rejected because it prevents proper seating of the discharge slide gate. The terminal component is a 300 L hopper with a 150 mm discharge nozzle and an integrally moulded rim for a flexible boot connection. Indirect food contact compliance can be evaluated under Regulation (EC) No 1935/2004, but complete compliance with Commission Regulation (EU) 10/2011 cannot be assumed for the black formulation because the specific carbon black and stabiliser package must be confirmed by migration testing. If abrasive feed materials are used, the wall at the lower cone is increased to 5 mm, and the part is inspected for breach holes after 1,000 cycles of slide-gate actuation. Published data for this specific dry feed handling configuration is limited; therefore a production trial with batch-to-batch powder lot evaluation is required before release.
Outdoor telecommunication enclosure bases and signal controller pedestals are rotomoulded as single-piece shells with a 4.5 mm nominal wall. Icorene 2550 BLK 9001 provides opacity and weatherability for enclosures exposed to roof-mounted or street-level solar loading. The base is charged at 2.8 kg/m² and processed on a biaxial carousel. Molded-in brass inserts are placed into pockets with a minimum pocket depth of 8 mm and a 3 mm shoulder. Peak internal air temperature is 195°C to sinter the powder around the insert knurl; premature demoulding below 85°C causes insert pull-out load to fall below the 500 N retention threshold specified by the end user. The assembled enclosure is tested to IEC 60529 for IP65 dust and water ingress protection, and the polymer portion is evaluated to UL 94 HB for flammability. REACH compliance is documented under Regulation (EC) No 1907/2006, and the grade is screened against the current candidate list of substances of very high concern. If RoHS compliance is claimed, the black pigment and UV stabiliser system must be checked for restricted heavy metals under Directive 2011/65/EU, Annex II. The terminal article is a black pedestal base of 22 kg empty mass with integrally moulded cable entry knockouts, drainage channels, and a flat sealing surface for a neoprene gasket.
For 120 L side-loading refuse containers, the black grade is processed to a 5 mm wall at the base and a 4 mm wall at side panels. A charge weight of 2.9 kg/m² is used for the base-heavy design. The mould is rotated at a 4:1 ratio with 6 min⁻¹ primary and 1.5 min⁻¹ secondary. The heating cycle reaches 190°C internal air temperature and holds for 10 minutes; the drop impact test is performed after conditioning at -20°C for 24 hours. Per ISO 6603-2:2023, a 5 kg striker is dropped from 1.5 m, and the part must not show through-cracks or structural failure. EN 840-2:2020 is used for dimensional interchangeability with comb-lift equipment. Surface finish is controlled to a 60° gloss level because ultraviolet exposure causes microcracking on untextured high-gloss black surfaces; the mould is vapour-blasted to produce a matte finish with Ra 6.3 µm. That finish also reduces visible scuffing on collection routes. The terminal product is a 120 L two-wheel refuse container with side-lift trunnion pockets, a 4 mm sidewall, a 5 mm base wall, and ultraviolet-stable black pigment distributed through the full wall thickness.
Competitive LyondellBasell Icorene 2550 BLK 9001 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 2550 BLK 9001 is a black-pigmented linear low density polyethylene powder supplied primarily for rotational molding. The base polymer is an ethylene/α-olefin copolymer, and the short-chain branching architecture is controlled to balance environmental stress-crack resistance, low-temperature impact, and mold-surface reproduction. The designation 2550 identifies the base-resin melt-flow/density combination within the Icorene portfolio; BLK indicates carbon black pigmentation for ultraviolet screening; 9001 denotes the commercial formulation or packaging variant. Because suffix variants can share base-resin chemistry while differing in additive loading, particle-size control, or lot-acceptance limits, specification values should be taken from the current manufacturer certificate of analysis rather than inferred from the trade designation alone.
The product is supplied as a ground powder. Rotational molding powders require a controlled particle-size distribution that balances fine particles for surface reproduction against coarser particles for dry-flow and venting. If the fraction below 150 µm becomes excessive, electrostatic clumping and uneven venting can produce wall-thickness variation on multi-cavity tools. Incoming inspection programs for this product class often include sieve analysis according to ASTM D1921 and bulk density or pourability evaluation according to ASTM D1895. The supplier’s certificate of analysis should be used to set control limits because grind parameters may vary among production campaigns without changing the trade name.
For Icorene 2550 BLK 9001, universal time-temperature recipes are limited because mold mass, wall thickness, oven airflow, and charge weight shift the thermal response. The governing fusion sequence is well characterized: powder particles sinter above the crystalline melting range, densify against the mold wall, and coalesce into a void-free layer. Peak internal air temperature below 190 °C can leave partially fused powder at the inner wall or produce knit lines around inserts. Peak internal air temperature above 210 °C accelerates chain scission and antioxidant depletion. The processing window is therefore narrow in comparison with oven setpoint control alone. On 6 mm steel tooling in a forced-air carousel oven set at 280 °C, mold-surface thermocouples commonly lag internal air temperature by 20 °C to 40 °C. Process control based on oven temperature can therefore produce under-fused or over-oxidized parts even when the machine setting appears stable.
Cooling rate controls crystallinity, shrinkage, and warpage in rotational molding. A forced-air cooling stage followed by a short water mist or spray stage is common for medium-walled LLDPE parts, but the part should remain on the mold until ejection temperature is sufficiently low to maintain dimensional stability. For large panels, removing the part below 70 °C can reduce immediate warp, although the exact ejection temperature depends on part stiffness and mold geometry. Rapid quenching of a black part can create residual stresses at the mold side that later relax as out-of-flatness in outdoor service. The cooling sequence should be locked after impact testing because a visually acceptable surface does not guarantee retained toughness.
The LLDPE architecture of 2550 BLK 9001 differs from LDPE and HDPE in branching structure, processing behavior, and service properties. LDPE carries long-chain branches, which reduce shear viscosity and ease flow in some processes, but do not provide the same environmental stress-crack resistance as LLDPE at equivalent density. HDPE offers higher modulus and hardness but generally requires a higher peak internal air temperature and can exhibit lower low-temperature impact in thick sections. The linear low density classification places the product in the density band from 0.915 g/cm³ to 0.940 g/cm³, which supports a better ESCR-stiffness compromise for chemical-contact parts than typical LDPE at equivalent wall thickness. Actual ESCR performance depends on comonomer type, comonomer distribution, and molded-in residual stress.
| Polymer class | Density range under ISO 1183-1:2019 | Branching architecture | Typical rotomolding consequence |
|---|---|---|---|
| LDPE | 0.910–0.925 g/cm³ | Long-chain branched | Lower stiffness, lower ESCR, easier flow into complex recesses |
| LLDPE | 0.915–0.940 g/cm³ | Linear backbone with short-chain branches | Higher ESCR, improved toughness, greater sensitivity to cooling rate |
| HDPE | 0.940–0.970 g/cm³ | Linear, low branch content | Higher modulus, higher oven demand, lower low-temperature impact in thick sections |
Within the Icorene rotomolding range, 2550 BLK 9001 is positioned as a pre-compounded outdoor grade. This removes the need for post-molding painting or separate dry-blend UV stabilizer addition, but it also fixes the carbon black concentration. Molders requiring custom colors cannot switch to a natural grade without revalidating the thermal processing window because carbon black increases infrared absorption and can reduce the time required to reach a given internal air temperature. The same oven recipe that works for a natural LLDPE powder may overheat the black grade in thin sections or under high-velocity airflow.
Carbon black particles in the 20–50 nm range absorb ultraviolet radiation and convert it to heat, but protection depends on dispersion quality. Poor dispersion creates agglomerates that act as stress concentrations and reduce low-temperature impact. ISO 18553:2002 is used to assess carbon black dispersion in polyolefin compounds by image analysis of microtomed sections. For outdoor service, a dispersion rating sufficient for a decorative part may be inadequate for a load-bearing agricultural tank. Accelerated weathering under ISO 4892-2:2013 with xenon arc exposure and wet/dry cycles evaluates gloss retention, chalking, and embrittlement, but correlation to real outdoor life is geometry-dependent. Carbon black screening does not protect the polymer matrix from thermal oxidation during processing or long-term heat exposure, so weathering performance cannot be inferred from pigmentation alone.
For chemical storage, the material’s environmental stress-crack resistance under ASTM D1693-15 can be used as an initial screen. Long-chain-branched LDPE typically fails earlier in the same stress-crack test, while HDPE may show higher tensile modulus but lower ESCR in notched specimens when density exceeds 0.945 g/cm³. Coupon testing in the actual chemical medium at the upper service temperature is required because ESC failure depends on surfactant concentration, temperature, and molded-in stress. Parts designed under ASTM D1998 for polyethylene upright storage tanks require minimum wall thickness based on hydrostatic stress; no material designation can guarantee performance without accounting for weld-line quality and residual stress generated in the rotational mold.
The processing tolerance for LLDPE rotomolding is often described as a plateau rather than a single point. Once internal air temperature enters the fusion window, the part may appear acceptable over a range of oven residence times. However, extended residence above 210 °C consumes the antioxidant package and can produce a brittle inner surface layer. Field evidence from carousel machines processing black LLDPE shows that parts molded at the same oven setpoint but with different load masses can shift peak internal air temperature by 10 °C or more because mold mass and part surface area change heat absorption. Validation should use a pyrometer or internal air probe to lock oven time, rotation speed, and cooling sequence for each mold family. If oven airflow is unbalanced, mold corners can overheat while the center remains below fusion temperature, producing warpage and impact scatter on multi-cavity tools.
| Attribute | Test method | Relevance to incoming inspection or qualification |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | Process control at 190 °C/2.16 kg |
| Density | ISO 1183-1:2019 | Part mass and stiffness estimation |
| Tensile properties | ASTM D638-14 | Design data for wall sections |
| Flexural modulus | ASTM D790-17 | Stiffness comparison with HDPE and LDPE |
| ESCR | ASTM D1693-15 | Chemical tank service screening |
| Accelerated weathering | ISO 4892-2:2013 | Outdoor aging evaluation |
| Carbon black dispersion | ISO 18553:2002 | Compound quality and impact retention |
Bags should be stored indoors at relative humidity below 60% and allowed to reach shop temperature before opening if condensation is visible. Although polyethylene is hydrophobic, condensation on powder surfaces can introduce water into the mold and cause pinholes or steam venting defects at the inner wall. Adding regrind from trimmed parts changes the particle-size distribution and can increase the fines fraction; regrind levels above 20 wt% in the final powder blend may alter dry-flow and wall-thickness uniformity. No universal limit exists for this specific grade, so each blend ratio must be validated on the target machine. Regulatory status for potable-water, food-contact, or toy applications must be confirmed through current supplier documentation because the presence of carbon black does not itself establish compliance with application-specific standards such as NSF/ANSI 61 or regional food-contact regulations.