| HS Code | 738510 |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.9 g/10 min |
| Melt Flow Ratio I21 I2 | 28 |
| Comonomer | Butene |
| Melting Point | 123 °C |
| Vicat Softening Point | 101 °C |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 9.65 MPa |
| Tensile Strength At Break Md | 30.3 MPa |
| Tensile Strength At Break Td | 26.2 MPa |
| Elongation At Break Md | 630 % |
| Elongation At Break Td | 780 % |
| Tensile Modulus Md | 179 MPa |
| Tensile Modulus Td | 200 MPa |
| Dart Drop Impact | 180 g |
| Elmendorf Tear Strength Md | 5.5 g/µm |
| Elmendorf Tear Strength Td | 11.0 g/µm |
| Haze | 11 % |
| Gloss 45 | 65 % |
| Test Film Thickness | 50.8 µm |
As an accredited LyondellBasell Icorene 1869 NAT 0000 US Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically supplied in 25 kg polyethylene-lined bags; 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | Loading LyondellBasell Icorene 1869 NAT 0000 US Polyethylene, Linear Low Density into a 20′ FCL container, palletized in 25-kg bags. |
| Shipping | LyondellBasell Icorene 1869 NAT 0000 US Polyethylene, Linear Low Density is a non-hazardous solid LLDPE resin. Ship in original sealed bags, boxes, or bulk containers. Store dry, away from heat, sunlight, and incompatible materials. No DOT/UN hazard class; follow SDS, local regulations, and maintain clean transport equipment. |
| Storage | Store LyondellBasell Icorene 1869 NAT 0000 US Polyethylene, Linear Low Density in a cool, dry, well-ventilated area. Keep containers closed, away from direct sunlight, heat, sparks, flames, and incompatible materials. Prevent moisture pickup and dust accumulation. Maintain clean, labeled packaging; avoid excessive stacking or temperatures that may cause degradation. Follow applicable local regulations and facility safety procedures. |
| Shelf Life | Shelf life: 24 months from manufacture when stored in original unopened packaging under cool, dry, ventilated conditions, away from direct sunlight. |
Single-piece rotomoulded water storage tanks in the 500–10,000 L range are produced from Icorene 1869 NAT 0000 US linear low-density polyethylene powder without weld seams, an advantage under cyclic hydrostatic loading. The powder is charged directly into a machined aluminium mould mounted on a shuttle or carousel rotomoulding machine with a primary-secondary rotation ratio of 4:1; primary axis speed is typically held at 2–5 rpm and secondary axis speed at 8–20 rpm. Oven air temperature is set between 260–300 °C, and the internal air temperature inside the mould must reach 190–210 °C for sufficient particle coalescence before cooling begins. Wall thickness is specified at 4.0–8.0 mm depending on tank height; fabricators measure wall thickness at the top corner, sidewall midpoint, and bottom corner because these locations exhibit the largest thinning during rotation. For potable water service, the finished tank is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers in food-contact articles, NSF/ANSI/CAN 61 for drinking water system components, and EU Regulation (EU) No 10/2011 as amended for plastics intended to contact food. Formulation is maintained at 100 wt% virgin Icorene 1869 NAT 0000 US in the contact layer; if a multilayer tank is moulded, the same-grade regrind level is limited to 0–5 wt% in the non-contact outer layer only. UV-stabiliser masterbatch addition is set at 0.5–2.0 wt% in the exterior layer, with the carrier resin selected from the same LLDPE family to avoid melt-freezing mismatches. Cooling sequence is process-critical: after the oven dwell, the mould is cooled in ambient air for 10–15 min, then water mist is applied in 30–60 s pulses until the mould surface reaches 70–90 °C, and the tank is demoulded only after stable geometry is confirmed. Terminal product types include vertical water storage tanks, rainwater harvesting cisterns, emergency water reservoirs, and transport tank liners. Long-term chlorinated water exposure above 3 mg/L free chlorine at elevated service temperature should be validated by ASTM D1693-15b environmental stress-crack testing because NSF/ANSI/CAN 61 does not fully quantify oxidative embrittlement after years of hot water contact.
Lot-specific melt flow index should be measured by ISO 1133-1:2022 and density by ISO 1183-1:2019 before campaign start because variations in melt flow index alter bubble removal and wall thickness distribution in necks. The main processing conflict is demoulding temperature: pulling at 90 °C shortens cycle time but increases thermal shrinkage after cooling, while pulling at 70 °C improves dimensional stability but can produce condensation marks on the inner surface. Fabrication shops therefore run a 10–20 tank capability study with ultrasonic thickness mapping and ASTM D1998-15 top-corner and bottom-corner measurements before releasing a tool.
In double-wall chemical containment, the inner tank is rotomoulded first and the outer containment skin is moulded around it, using the same Icorene 1869 NAT 0000 US powder in both skins. The inner contact layer is kept at 100 wt% natural powder to permit visual crack inspection, while the outer bund skin receives 2.0–4.0 wt% of a 50 wt% carbon black masterbatch in an LLDPE carrier for ultraviolet absorption. Secondary containment in the United States is qualified under U.S. EPA 40 CFR 264.193 when the tank is used at hazardous waste storage sites, while static above-ground chemical tanks in the European Union are fabricated to EN 13575:2012 for rotationally moulded polyethylene tanks. Wall thickness is measured after moulding with an ultrasonic gauge at 12 or more fixed grid points per skin; the inner tank wall is held at 4.5–8.0 mm and the outer bund at 3.0–5.0 mm, with no point below 3.0 mm on the outer skin. The oven air temperature is set at 270–310 °C, and the peak internal air temperature is allowed to reach 200–215 °C for the inner skin. A key failure mode is incomplete fusion at the inner tank and outer bund interface: if the inner tank surface is allowed to cool below 120 °C before the outer powder is charged, interlayer adhesion becomes dependent on surface oxidation and release-agent migration rather than melt fusion. Chemical compatibility is not inferred from density or melt flow index alone; fabricators conduct immersion screening per ISO 175:2010 at the service temperature and measure tensile strength retention per ISO 527-2:2012 after 1,000 h exposure to the specific chemical. Terminal products include acid and alkaline dosing tanks, air-gap bunded static tanks, portable containment units, and replacement liners for intermediate bulk containers. Venting design must prevent negative pressure during discharge; a 50–75 mm manway or vent port is typical on tanks above 1,000 L, but the exact opening is determined by filling and pumping rates.
When the outer bund is moulded over the inner tank, the interface temperature is controlled by injecting a small amount of compressed air through the vent to prevent the outer powder from cooling the inner wall below its re-melt threshold. The oven dwell time for the outer skin is shorter than for the inner skin; operators monitor the peak internal air temperature rather than wall time alone. Dimensional tolerance on outer bund capacity is checked by filling with water to the overflow line at 25 °C and recording the overflow volume, then comparing against the nominal bund capacity required by secondary containment regulations.
For rotomoulded kayaks and sit-on-top watercraft shells, wall thickness is specified at 2.8–5.0 mm to maintain hull stiffness without excessive mass. Icorene 1869 NAT 0000 US is dry-blended with a marine-grade pigment or UV masterbatch at 0.5–1.5 wt% before charging; the blend is not melt-compounded, so high-shear dry mixing in a turbomixer is required to prevent streaking and low-impact zones. Aluminium kayak moulds with large flat hull panels are mounted on a three-axis rotomoulding machine with a rotation ratio between 3:1 and 5:1, and oven air temperature is reduced to 250–290 °C to avoid overheating the thinner bow and stern sections. Peak internal air temperature is limited to 190–205 °C; exceeding 205 °C in a thin-wall mould creates bubble entrapment because the polymer melt travels farther before densification. The dominant manufacturing defect is not sink marks but warpage after demoulding: the hull bottom cools faster than the deck when the mould is opened, producing a concave deviation along the keel line. To control this, cooling is staged—ambient air for 5–10 min, then pulsed water mist for 10–30 s intervals until the mould surface falls to 120 °C, then air to 65–75 °C demoulding temperature. The still-warm hull is placed in a cooling jig for 10–15 min to hold the designed rocker profile. Regulatory compliance for non-motorised plastic watercraft is fragmented: the EU General Product Safety Directive 2001/95/EC applies, and in the United States the U.S. Coast Guard flotation rules under 33 CFR Part 183 apply to the finished watercraft, not directly to the resin. Manufacturers typically generate internal acceptance criteria using instrumented Charpy impact testing at -20 °C per ISO 179-1/1eA and drop tests from 1.0 m onto concrete. Published burst-strength data for Icorene 1869 NAT 0000 US in a 400 L kayak hull configuration is limited; process capability studies across 50–100 consecutive mouldings are therefore required before locking the cooling recipe. Terminal products include sit-on-top kayaks, recreational paddleboard blanks, canoe body shells, and small watercraft seat modules.
Published burst-strength data for this exact grade in a watercraft hull configuration is limited; fabricators therefore run instrumented drop tests from 1.0 m onto concrete at -10 °C and section the hull to map thickness. If the bow thickness falls below 2.8 mm, the machine ratio is adjusted by reducing the secondary-axis speed relative to the primary axis. The mould surface roughness is maintained at Ra 0.8–1.6 µm; rougher surfaces increase demoulding friction and favour localised tensile stress at the keel.
| Application scenario | Oven air temperature (°C) | Peak internal air temperature (°C) | Wall thickness (mm) | Demould temperature (°C) | Key process control |
|---|---|---|---|---|---|
| Potable water tanks | 260–300 | 190–210 | 4.0–8.0 | 70–90 | Pulsed water mist after 10–15 min ambient cooling |
| Chemical double-wall | 270–310 | 200–215 | inner 4.5–8.0, outer 3.0–5.0 | 70–85 | Ultrasonic gauge at 12 grid points per skin |
| Kayak hulls | 250–290 | 190–205 | 2.8–5.0 | 65–75 | Cooling jig 10–15 min after demould |
| Agricultural hoppers | 260–320 | 195–215 | 5.0–8.0 | 75–85 | 5 min oven fan reduction before cooling |
| Insulated fish tubs | 260–300 | 190–210 | 3.5–5.0 each skin | 70–80 | Polyurethane foam injection after shell assembly |
| DEF reservoirs | 260–300 | 195–210 | 4.0–7.0 | 65–80 | Compressed-air leak test at 30 kPa |
When seasonal pesticide spraying and harvest handling require bins that tolerate fork-tine impact, agricultural fabricators rotomould Icorene 1869 NAT 0000 US at 5.0–8.0 mm wall thickness to tolerate repeated abrasive produce contact. Formulation for outdoor agricultural service uses 100 wt% powder as the base, with a hindered amine light stabiliser masterbatch added at 0.3–1.0 wt% and a UV absorber masterbatch at 0.2–0.5 wt%; regrind generated from trimmed bin openings and rejected parts is incorporated up to 10 wt% because agricultural service does not carry the same extraction limits as potable water. The powder blend is charged into steel or cast aluminium moulds and processed on a carousel rotomoulding machine at an oven air temperature of 260–320 °C. Peak internal air temperature is held between 195–215 °C for 10–20 min after the powder reaches tack temperature to densify the inner surface. Large flat sidewalls on rectangular hoppers present a wall-uniformity risk; the mould rotation ratio is set at 4:1 with a brief 5 min oven fan-speed reduction before cooling to allow corner sections to achieve the same heat history as sidewall centres. Cooling is performed in ambient air for 15–25 min followed by forced air at 20–30 °C until demoulding at 75–85 °C. Compliance for pesticide and liquid fertilizer contact is based on EN 13575:2012 when the unit is a static above-ground tank; if the bin is marketed for direct animal feed contact, the food-contact olefin requirements of FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 apply. Mechanical acceptance after moulding uses tensile testing per ASTM D638-14 on sections cut from the bin and visual inspection of corner thickness with ultrasonic gauging. Terminal products include portable liquid fertilizer tanks, pesticide induction hoppers, animal feed troughs, salt spreader hoppers, and vineyard picking lugs.
Post-mould annealing is not routinely used; if corner warpage exceeds 3 mm on a 1.2 m side panel, the cooling jig is adjusted rather than increasing demould temperature because higher demould temperature increases sidewall bow after free-standing cooling.
Across cold-chain seafood and pharmaceutical distribution, insulated tubs and totes are assembled from two rotomoulded Icorene 1869 NAT 0000 US skins with a rigid polyurethane foam core injected between them. The food-contact inner skin is run at 100 wt% natural powder, while the outer skin receives 2.0–3.0 wt% high-opacity colour masterbatch and 0.5–1.0 wt% UV masterbatch; no post-consumer recycled material is used in the inner skin because extractable levels must be evaluated under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 for food contact. The two skins are rotomoulded separately at 3.5–5.0 mm wall thickness using oven air temperatures of 260–300 °C and a peak internal air temperature of 190–210 °C. After demoulding at 70–80 °C, the inner and outer shells are located on a steel assembly jig and the annulus is injected with a low-pressure rigid polyurethane foam system at a target core density of 40–60 kg/m³. The foam exotherm is controlled by maintaining mould shop ambient temperature at 20–25 °C and limiting shot mass to the cavity volume; excessive foam pressure can separate the outer shell from the inner shell at the rim lip. A critical manufacturing boundary is the foam cure: the assembly is held at 50–70 °C for 15–30 min, and the rim is inspected for foam bleed-through because any crack in the inner skin creates a direct food-contact failure. Mechanical testing is performed on the assembled tub using drop-impact at -10 °C and corner compression per ASTM D638-14 or internal finite-element-derived load cases. Terminal products include insulated fish boxes, e-commerce cold-chain totes, pharmaceutical transport containers, and seafood distribution bins. Published long-term thermal insulation data for this exact grade in foam-filled tubs is limited; fabricators should verify thermal conductivity of the foam core separately according to ISO 8301:1991 or the applicable regional equivalent.
The foam injection step is the main source of scrap: if the polyurethane system is metered before the LLDPE shell has fully cooled to below 50 °C, the foam exotherm can soften the inner wall and cause blow-out at the rim. Jigs must support both sidewalls during injection because low-pressure foam expansion can distort unsupported flat panels; published pressure ceilings for this exact tooling configuration are limited. The finished tub is inspected for foam bleed-through by filling with water and observing the outer skin for leakage under 24 h static head.
| Application scenario | U.S. compliance basis | EU compliance basis | Mechanical/chemical test method | Resin formulation note |
|---|---|---|---|---|
| Potable water tanks | FDA 21 CFR 177.1520(c), NSF/ANSI/CAN 61 | EU Regulation (EU) No 10/2011 | ASTM D1693-15b, ASTM D1998-15 | Contact layer 100 wt% virgin; regrind 0–5 wt% outer layer only |
| Chemical double-wall | U.S. EPA 40 CFR 264.193 | EN 13575:2012 | ISO 175:2010, ISO 527-2:2012 | Outer bund 2.0–4.0 wt% carbon black masterbatch |
| Kayak hulls | 33 CFR Part 183 | GPSD 2001/95/EC | ISO 179-1/1eA at -20 °C | UV masterbatch 0.5–1.5 wt%; dry turbomixer blending |
| Agricultural hoppers | FDA 21 CFR 177.1520(c) if feed contact | EU Regulation (EU) No 10/2011, EN 13575:2012 | ASTM D638-14 | Regrind up to 10 wt%; HALS 0.3–1.0 wt% |
| Insulated fish tubs | FDA 21 CFR 177.1520(c) | EU Regulation (EU) No 10/2011 | ISO 8301:1991, ASTM D638-14 | Inner skin 100 wt% natural; no PCR in food-contact layer |
| DEF reservoirs | ASTM D1693-15b, ISO 22241-1 | REACH Regulation (EC) No 1907/2006; RoHS Directive 2011/65/EU if applicable | ASTM D1693-15b | Outer carbon black 2.0–3.0 wt%; fitting insert ion screening |
Because diesel exhaust fluid is a 32.5 wt% urea solution sensitive to metal-ion contamination, rotomoulded reservoirs on agricultural and construction equipment are produced from Icorene 1869 NAT 0000 US using fabricated steel moulds and compressed-air demoulding. The powder is charged at 100 wt% in the inner contact layer; the outer surface can receive 2.0–3.0 wt% carbon black masterbatch for UV resistance when the reservoir is exposed on a machine exterior. Diesel exhaust fluid is subject to ISO 22241-1; material selection must avoid introducing copper, zinc or calcium ions that degrade the fluid, so mould release agents and fitting inserts must be screened. Environmental stress-crack resistance is evaluated on moulded specimens after urea solution exposure using ASTM D1693-15b with the specimen thickness and notch depth recorded in the test report. In the European Union, the finished reservoir is assessed under REACH Regulation (EC) No 1907/2006 for substances of very high concern above 0.1 wt%; RoHS Directive 2011/65/EU applies only if the reservoir is part of an electrical or electronic device. Processing uses oven air temperatures of 260–300 °C and a peak internal air temperature of 195–210 °C; wall thickness is maintained at 4.0–7.0 mm around insertion bosses. The moulding is cooled to 65–80 °C before demoulding, then placed in a fixture for 5 min of forced-air purge to stabilize the fitting bore dimensions. Differential cooling around insert threads causes ovality; thread chase or post-mould machining is required for fittings with sealing surfaces. Each reservoir is leak-tested with compressed air at 30 kPa under water or soap film according to the fabricator’s internal procedure, and terminal products include diesel exhaust fluid tanks for agricultural and construction machinery, hydraulic oil reservoirs, toolbox enclosures, fender extensions, and battery boxes.
Insert bosses are often preheated to 80–100 °C before charging to reduce cooling rate mismatch around threads. Metal fittings are not overmoulded; they are installed after moulding with gaskets to allow replacement. For diesel exhaust fluid service, copper-containing alloys are excluded from both the mould release and fitting assembly because copper ions catalyze urea decomposition. Published long-term aging data for this specific reservoir geometry is limited; automotive-grade validation programs require thermal aging, vibration, and pressure cycling tests defined by the off-highway original equipment manufacturer.
Competitive LyondellBasell Icorene 1869 NAT 0000 US Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1869 NAT 0000 US is a linear low-density polyethylene resin supplied under the Icorene grade family for injection moulding and high-speed compounding. The NAT field identifies a natural, unpigmented presentation, not an additive-free system; processing stabilizers and catalyst neutralizers are normally present in the commercial formulation. The 0000 US field identifies the US regional specification and packaging stream. The material is placed in the ethylene-alpha-olefin LLDPE class with a nominal density of 0.918 g/cm³ and a melt flow rate of 6.9 g/10 min at 190 °C under 2.16 kg load when tested to ASTM D1238 or ISO 1133-1:2022. Public data for this exact NAT 0000 US configuration is limited, so the current certificate of analysis and technical datasheet should be used for lot-level values.
Commercial listing data for the grade generally places it at the 0.918 g/cm³ / 6.9 g/10 min node. The surrounding LLDPE class from 0.916 g/cm³ to 0.920 g/cm³ and 6.5 g/10 min to 7.5 g/10 min exhibits the property envelope shown in Table 1. These ranges are not independent specifications; they represent the typical interval for stabilized, natural-color injection moulding LLDPE with the same density and flow architecture.
| Property | Test method | Typical range for the 0.918 g/cm³ / 6.9 g/10 min LLDPE class |
|---|---|---|
| Density | ISO 1183-1:2019 / ASTM D792 | 0.916–0.920 g/cm³ |
| Melt flow rate | ISO 1133-1:2022 / ASTM D1238 | 6.5–7.5 g/10 min |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638-14 | 11–13 MPa |
| Elongation at break | ISO 527-2:2012 / ASTM D638-14 | >800% |
| Flexural modulus | ISO 178:2019 / ASTM D790 | 320–420 MPa |
| Vicat softening temperature | ISO 306:2022 / ASTM D1525 | 94–102 °C |
| Melting temperature | ISO 11357-3:2018 / ASTM D3418 | 120–124 °C |
Molecular architecture in this density interval is controlled by a linear polyethylene backbone with short-chain branches introduced through an alpha-olefin comonomer. The 1869 grade class is commonly associated with hexene comonomer, but the trade name alone does not disclose the exact alpha-olefin; the technical datasheet should be consulted. Short-chain branches disrupt lamellar crystallization and lower density below the 0.940 g/cm³ threshold that separates linear low-density material from high-density polyethylene. Differential scanning calorimetry of the 0.916–0.920 g/cm³ class typically indicates a crystalline fraction between 45% and 55%, with a broad melting endotherm from 105 °C to 125 °C and a peak near 120–124 °C under ISO 11357-3:2018 or ASTM D3418.
Melt rheology in this flow class is characterized by linear chain architecture and short-chain branching. A capillary rheometer at 190 °C typically records apparent shear viscosities of 150–250 Pa·s at 100 s⁻¹, with additional shear thinning at 1000 s⁻¹. The flow rate ratio measured at 21.6 kg and 2.16 kg loads is an indirect indicator of molecular weight distribution; for Ziegler-Natta LLDPE in this viscosity class, the flow rate ratio is commonly 16–20, although the exact value depends on catalyst type and finishing process. This broader distribution supports shear thinning during cavity filling but may produce lower gloss than metallocene LLDPE grades.
Semicrystalline solidification produces mould shrinkage that depends on wall thickness, mould temperature, packing time, and gate freeze. For unfilled LLDPE at 0.918 g/cm³, linear mould shrinkage is typically 1.5–2.5% in both flow and transverse directions, but differential shrinkage can increase with highly oriented thin-wall parts. Shrinkage should be measured after 24 h at 23 °C and 50% RH according to ASTM D955 or ISO 294-4. Warpage in caps and closures is controlled by uniform cooling, balanced gates, and adequate packing pressure. If mould temperature is raised above 40 °C, cycle time increases, but crystallinity and dimensional stability may improve.
For thin-wall packaging, caps, closures, and general-purpose containers, the grade is typically processed at melt temperatures of 210–230 °C and mould temperatures of 15–40 °C. A general-purpose screw with 20:1 to 24:1 L/D, compression ratio 2.5:1 to 3.5:1, and a check-ring non-return valve is an appropriate baseline. Injection pressure is set to fill 95–98% of the cavity volume, and pack pressure is commonly 40–60% of peak pressure. Holding time should be set to gate seal; for a 1.5 mm wall, gate seal often requires 3–8 s. Gate thickness should not fall below 0.8 mm at this wall stock if jetting and sink are to be limited. A cavity pressure of 300–400 bar and a projected area of 500 cm² correspond to an estimated clamp force of 150–200 tonnes, but gate freeze and runner balance determine the actual process window.
Compared with high-pressure LDPE, the linear backbone of this LLDPE class gives higher tensile yield stress, improved environmental stress-crack resistance, and better puncture resistance at equivalent density, but lower melt strength and higher shear viscosity at equal melt index. Against HDPE, the 0.918 g/cm³ density class shows lower flexural modulus, lower Vicat softening temperature, and better low-temperature impact. Within LLDPE, butene comonomer versions at the same density and melt flow rate tend to show lower ESCR and lower dart impact than hexene-derived grades; the exact comparison for Icorene 1869 NAT 0000 US requires comonomer identification from the datasheet. Metallocene LLDPE grades often provide a narrower molecular weight distribution and lower extractables, but they may require higher injection pressure or faster screw recovery because of higher melt viscosity.
Environmental stress-crack resistance in LLDPE is governed by tie-molecule concentration, crystalline morphology, comonomer type, and moulded-in stress. In the 0.916–0.920 g/cm³ density class, ESCR values under ASTM D1693, condition B, can range from 100 h to over 1000 h depending on comonomer type, molecular weight, sample preparation, and ageing medium. When a closure or container is exposed to surfactants, essential oils, or aggressive cleaning formulations, testing should be performed on the final part geometry rather than relying on compression-moulded plaques. Incompatibilities include strong oxidizing acids, chlorinated solvents, and aromatic hydrocarbons under elevated temperature. For outdoor service, a natural grade without a UV stabilizer system is not adequate; hindered amine light stabilizers and UV absorbers should be incorporated through masterbatch or a UV-stabilized compound.
Regulatory status for polyolefin food-contact applications is commonly addressed through FDA 21 CFR 177.1520, which covers olefin polymers under specified end-use conditions. European food-contact compliance is evaluated through Regulation (EU) 10/2011, including overall migration and specific migration testing on the final article. The grade may also be screened under Regulation (EC) 1907/2006 REACH Annex XVII and Directive 2011/65/EU RoHS for restricted substances. Table 2 lists the typical standards matrix, but it is not a certificate of compliance.
| Normative area | Standard or regulation | Clause or test method |
|---|---|---|
| Food contact, United States | FDA 21 CFR 177.1520 | Olefin polymers paragraphs (c) 3.1a and 3.1b, end-use restrictions |
| Food contact, European Union | Regulation (EU) 10/2011 | Overall migration under Annex III/IV; specific migration limits for additives |
| REACH | Regulation (EC) 1907/2006 | SVHC screening, Annex XVII restrictions |
| RoHS | Directive 2011/65/EU | Lead, cadmium, mercury, hexavalent chromium, PBB, PBDE limits |
| Toy safety heavy metals | ASTM F963 / EN 71-3 | Extraction limits for the final article |
LLDPE melt degradation accelerates above 260 °C; gel formation, yellowing, and odor can occur even at lower temperatures if residence time is excessive. Injection moulding operators should use the smallest barrel capacity consistent with shot size, ideally 25–75% of barrel capacity, to limit residence time. Purging after processing natural LLDPE should use a low-viscosity HDPE or LLDPE purge grade at 240–250 °C with moderate screw rotation for 5–10 min. If the next resin is a higher-viscosity HDPE, the purge should be followed by a brief high-speed short shot to displace remaining LLDPE from the check ring and hot-runner drops. Pre-drying is not normally required below 60% RH; however, cold pellet surfaces moved into a warm processing area can condense moisture and generate splay.
Masterbatch compatibility is improved when the carrier resin has a density and melt flow rate close to 0.918 g/cm³ and 6.9 g/10 min. Dry blending of 1–3 wt% color or additive masterbatch is common in injection moulding; higher loadings can reduce melt stability and increase nozzle drool. Post-industrial regrind from clean, single-material streams is often re-introduced at 20–30 wt% for non-critical parts. The regrind should be free of fines, moisture, and degraded gels, and it should be tested for melt flow rate shift and tensile property retention under ASTM D638-14 or ISO 527-2:2012. Published data for this specific Icorene configuration at elevated regrind loadings is limited, so process validation is required.
Incoming resin lots should be checked for melt flow rate, density, moisture, and visual contamination. Melt flow rate is determined under ASTM D1238 or ISO 1133-1:2022; density is measured by density gradient column or displacement according to ASTM D792 or ISO 1183-1:2019. Moisture content in polyethylene is normally low, but surface condensation should be avoided if pellets are stored at temperatures below the processing area dew point. A maximum screen pack of 250–400 µm in the feed throat or melt filter can protect hot-runner nozzles from degraded specks. The audit protocol should also verify that the documented NAT 0000 US designation matches the certificate of analysis, because pack size, lot number, and regional specification streams can affect traceability.