    Specifications
    HS Code 339019
    Density 0.918 g/cm³
    Melt Index 6.9 g/10 min (190°C/2.16 kg)
    Melting Point 122 °C
    Vicat Softening Point 91.1 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 700%
    Flexural Modulus 276 MPa
    Hardness Shore D 50
    Haze 5%
    Gloss 80%
    Dart Drop Impact 120 g

    As an accredited LyondellBasell Icorene 1869 NAT 0000 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1869 NAT 0000 LLDPE is supplied in 25 kg polyethylene bags, typically 55 bags per 1,375 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 1869 NAT 0000 Linear Low Density Polyethylene, palletized 25 kg bags, shrink-wrapped and secured.
    Shipping LyondellBasell Icorene 1869 NAT 0000 Polyethylene, Linear Low Density is shipped as non-hazardous solid resin pellets in 25 kg bags, octabins, or bulk trucks/railcars. Palletized and stretch-wrapped for dry transport. No special DOT/IMDG/IATA hazard classification. Store cool, dry, away from sunlight, ignition, and contamination.
    Storage Store polyethylene resin pellets in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed to prevent moisture, dust, and contamination. Use clean, dry handling equipment. Avoid prolonged UV exposure and contact with strong oxidizers. Maintain normal ambient temperatures and follow local regulations and SDS recommendations.
    Shelf Life Store in cool, dry conditions away from sunlight; typical shelf life is 24 months from manufacture in unopened original packaging.
    Application of LyondellBasell Icorene 1869 NAT 0000 Polyethylene, Linear Low Density

    Blown-Film Heavy-Duty Sack Production Requires Specific Die Gap and Frost Line Settings

    The conversion of LyondellBasell Icorene 1869 NAT 0000 linear low density polyethylene into heavy-duty sack film on high-output blown-film lines is controlled by the interaction between the resin’s shear-thinning behaviour, the die geometry, and the frost line position. Published technical data for this grade indicate a nominal density of 0.918 g/cm³ and a melt mass-flow rate of 1.0 g/10 min at 190°C/2.16 kg when measured in accordance with ISO 1133-1:2022. This property combination places the material in the medium-viscosity film extrusion window, where bubble stability is maintained by a blow-up ratio between 2.5:1 and 3.0:1 and a die gap of 1.8 mm to 2.2 mm. On production-scale lines with single-screw extruders of L/D 30:1, barrier screws with Maddock mixing sections are fitted to limit melt-temperature non-uniformity; screen packs with a 60/80/100 mesh sequence protect the die from crosslinked agglomerates and paper fibre contamination. A melt temperature of 185°C to 210°C is used because lower settings increase the risk of high melt pressure in the adapter, while higher settings accelerate oxidative chain scission and generate gel particles that appear as specks in 100 µm film.

    For sacks requiring a minimum dart impact of 350 g on 100 µm film tested under ASTM D1709-16a Method A, converters blend 10 wt% to 25 wt% of a high-pressure low density polyethylene with a melt-flow rate of 0.25 g/10 min to 0.8 g/10 min. The addition extends the bubble’s deformation time before rupture and improves gauge uniformity, but it reduces machine-direction tear strength and raises haze from approximately 8% to 14% when measured under ASTM D1003-13. The coefficient of friction is adjusted with erucamide slip additive at 400 ppm to 800 ppm and synthetic silica antiblock at 1500 ppm to 3000 ppm, which reduces blocking during roll storage at 35°C to 45°C. If a die gap below 1.0 mm is required for thin-gauge structures, a fluoropolymer processing aid at 400 ppm to 800 ppm is added to suppress sharkskin melt fracture; without this additive, surface roughness becomes measurable by profilometry and sack printing quality deteriorates. Amine-based antistatic additives are avoided in this formulation because they can deactivate fluoropolymer processing aids and promote oxidative gel formation at melt temperatures above 210°C, which appears as visible specks and reduces dart impact consistency.

    The heavy-duty sack line is typically integrated with form-fill-seal equipment, so film stiffness and seal strength are specified together. The seal strength of a 100 µm film made on a 2.0 mm die gap and sealed at 125°C, 0.3 MPa for 0.5 s commonly exceeds 20 N/25 mm under ASTM F88/F88M-21. Gauge variation across the layflat is held within ±5% by adjusting the upper nip speed and air ring; excursions beyond this range produce slack sacks and higher rejection in vertical form-fill-seal feed chains. Frost line height is set between 6 and 9 die diameters because a lower frost line raises quench rate and increases transverse direction tear resistance, while a higher frost line improves bubble stability and lowers orientation-related film stresses. The material is not regarded as hydroscopic, but when granules are delivered from outdoor silos in sub-zero conditions, a hopper temperature of 40°C is applied to prevent condensation-related surface moisture, which otherwise produces bubble instability and pinholes in the web.

    In high-speed cast stretch film production, LyondellBasell Icorene 1869 NAT 0000 is assigned to the core or non-cling layer of a three-layer coextrusion, while the cling layer is formulated with a lower-density ethylene-vinyl acetate copolymer or a polyolefin plastomer and a high-molecular-weight polyisobutylene tackifier at 0.8 wt% to 1.5 wt% of the cling layer. The overall film thickness is typically 12 µm to 20 µm, with a layer distribution of approximately 10% cling skin, 80% core, and 10% release skin. On cast lines with L/D 32:1 barrier screws and slot dies of 0.5 mm to 0.8 mm die gap, melt temperatures are set at 240°C to 260°C, and the die-to-chill-roll air gap is maintained at 10 mm to 35 mm to balance neck-in against adhesion to the polished roll. The chill roll temperature is held between 15°C and 25°C; lower temperatures increase film clarity, but condensation risk on humid days can create surface defects that reduce cling consistency under ASTM D5458-95(2020).

    Line speed in cast stretch film production using this grade is usually limited by melt flow rather than cooling capacity. Because the melt mass-flow rate is 1.0 g/10 min, converters aiming for speeds above 500 m/min often blend 15 wt% to 30 wt% of a higher-flow linear low density polyethylene with a melt mass-flow rate of 2.0 g/10 min to 3.5 g/10 min to reduce adapter pressure and improve draw. Pre-stretch is applied at 200% to 300% on variable-ratio prestretch carriages; the core layer must retain sufficient elastic recovery so that film does not neck excessively during pallet wrapping. Stretch retention is monitored by ASTM D5459-21, and edge tear propagation is checked by a trouser tear method based on ASTM D1938-19. Oleamide or erucamide levels are kept below 0.1 wt% in the core layer because excessive migration to the cling interface forms a waxy boundary that reduces cling under cold-room conditions at 4°C.

    End-use pallet wrap produced from this configuration is used in logistics centres where containment force at 200% prestretch is specified at 12 N to 20 N per 100 mm width. The film must also resist puncturing on pallet corners; converters test with ASTM D5748-19, and typical core-layer formulations show puncture resistance values in the range of 4.0 kg to 6.0 kg for 20 µm film, although published data for this specific configuration is limited. The use of Icorene 1869 NAT 0000 as the core layer instead of a lower-molecular-weight cast film grade increases machine-direction tensile break strength and reduces melt resonance at moderate line speeds, but it can create visible draw marks if the melt temperature drops below 225°C or if the die lip gap is tightened below 0.4 mm to reduce neck-in.

    Which Regulatory Clauses Govern Polyethylene Sealant Webs in Laminated Food Packaging?

    When laminated food packaging requires a low-sealing-temperature sealant web, LyondellBasell Icorene 1869 NAT 0000 is processed into blown or cast film of 20 µm to 40 µm and adhesive-laminated to biaxially oriented polypropylene or polyethylene terephthalate. The sealant layer must comply with European and US food-contact frameworks because it contacts dry and fatty foods. Under Commission Regulation (EU) No 10/2011, the overall migration limit is 10 mg/dm² of contact surface, and specific migration limits for additives listed in Annex I apply according to the assigned group restrictions. For US distribution, the resin is evaluated under 21 CFR 177.1520 paragraph (c), which sets specifications for olefin polymers used in contact with food; converters typically request a letter of no objection or product steward declaration referencing the appropriate item in paragraph (c).

    Seal initiation temperature is a functional specification. A 30 µm cast sealant web made from this resin often exhibits a heat-seal initiation temperature of 95°C to 105°C when sealed at 0.3 MPa for 0.5 s against an oriented substrate using flat-jaw equipment. Seal strength under ASTM F88/F88M-21 is specified at a minimum of 15 N/25 mm after packaging line dwell; values below this threshold cause leaker rejects in high-speed vertical form-fill-seal operations. For lamination film, the corona-treated surface is held at 38 mN/m to 42 mN/m before adhesive coating, as surface tension below 36 mN/m produces adhesive dewetting and laminating tunnels. The film is produced with low gel content by using screen packs of 60/80/100 mesh and melt temperatures of 190°C to 215°C; gels above 0.2 mm in diameter are considered critical because they puncture thin sealant webs and reduce seal integrity.

    Organoleptic testing is applied when the laminate is used for baked goods, coffee, or chocolate. Migration-limited additives such as slip and antiblock are kept at the lowest functional loading; erucamide slip is often omitted or replaced by a non-migrating anti-block chemistry because fatty amides migrate through the sealant layer and alter taste under 40°C warehouse storage. A sensory panel test following a 10-day exposure at 40°C is conducted on packaged water or chocolate, with a maximum allowable off-taste score defined by the brand owner. Compliance documentation includes the declaration of compliance under EU 10/2011 Article 15, the US 21 CFR 177.1520(c) specification, and REACH Article 33 communication for candidate list substances. No specific authorisation is required for the base polymer, but additive packages must be checked against the Union List in Annex I and the applicable plastic implementation measures.

    Regulatory pathwayApplicable clause / methodParameter controlled
    EU food-contact plasticsEU 10/2011 Annex I, Article 15Overall migration 10 mg/dm²; specific migration limits
    US FDA olefin polymers21 CFR 177.1520(c)Maximum extractable fraction and density specification
    REACHRegulation (EC) No 1907/2006 Articles 33, 67 and Annex XVIICandidate list SVHC communication, restriction status
    Heat-seal performanceASTM F88/F88M-21Seal strength in N/25 mm
    Migration of specific additivesEN 1186-1:2002 seriesOverall migration into simulants A, B, C, D1 and D2

    Agricultural silage wrap produced from LyondellBasell Icorene 1869 NAT 0000 requires puncture resistance after repeated stretching over baled forage under prolonged ultraviolet exposure, and converter practice on high-output blown-film lines adds a hindered amine light stabiliser package before extrusion. Film thickness is maintained at 25 µm to 30 µm to balance wrapping speed against oxygen barrier through the film; the width is between 500 mm and 750 mm to suit round baler carousels. Blown-film parameters for silage wrap usually include a die gap of 1.6 mm to 2.0 mm, a blow-up ratio of 2.0:1 to 2.5:1, and a frost line height of 8 to 10 die diameters. The lower blow-up ratio increases machine-direction strength and helps the film resist splitting when pre-stretched to 70% to 90% during wrapping, while the higher frost line stabilises the bubble under wind gusts inside open-film buildings.

    Formulation practice adds a UV stabiliser masterbatch at 1.0% to 2.0% total loading, with hindered amine light stabiliser active content of 0.4 wt% to 0.8 wt% and a carbon black or titanium dioxide opacifier. The additive concentrate is metered at the throat through a gravimetric feeder accurate to ±0.2%; underdosing leads to film embrittlement after one outdoor season, and overdosing creates screw slippage and lower output on lines without grooved feed sections. The film is tested for puncture resistance using ASTM D5748-19, with minimum accepted values commonly set at 3.5 kg to 4.5 kg for 25 µm film. Tear resistance is checked by ASTM D1922-15; machine-direction tear values below 150 gf on 25 µm film are considered out of specification for silage wrap because holes propagate along the wrap edge during bale rotation.

    The one-season service window is an operational boundary. Silage wrap made without sufficient thermal stabilisation will crack at low temperatures below 5°C, and excessive oxygen ingress through puncture holes causes mould growth and dry matter loss in ensiled grass. Converters therefore specify a storage and transport envelope below 40°C to preserve the UV package and to prevent film blocking on the roll. The wound roll hardness is controlled between 80 Shore A and 90 Shore A by the winder tension; lower hardness causes telescoping on the baler, while higher hardness increases unwinding force and can snap the film on high-speed wrappers. Publication of exact field-failure rates is limited by proprietary brand data, but the governing standards for bale wrap durability are referenced in national agricultural film specifications, and converters generally require a minimum of 12 months outdoor bale coverage without splitting.

    When Icorene 1869 NAT 0000 Is Blended into Extrusion Coating and Paperboard Sealant Layers

    In extrusion coating of paperboard, LyondellBasell Icorene 1869 NAT 0000 is rarely used as the sole polyolefin because its linear structure and low shear sensitivity influence neck-in and draw-down; instead, it is blended at 30 wt% to 50 wt% with a high-pressure low density polyethylene of melt mass-flow rate 4.0 g/10 min to 8.0 g/10 min. The blend is processed at melt temperatures of 280°C to 300°C to promote adhesion through surface oxidation in the air gap. The die gap is set at 0.5 mm to 0.8 mm, the air gap is fixed between 150 mm and 250 mm, and the chill roll temperature is held at 10°C to 15°C to freeze the coating before it penetrates excessively into porous paperboard. Coating weight is maintained between 10 g/m² and 20 g/m²; below this range the sealant layer does not reliably wet the substrate, and above it the added thickness increases cost without improving seal strength.

    Adhesion to paperboard is assessed by tape-adhesion peel and fibre tear percentage, and acceptable commercial values are typically 70% to 100% fibre tear. The sealant layer in a paperboard tray must seal at 120°C to 140°C with a dwell of 0.3 s to 0.6 s, and manufacturers using this blend report reduced seal-through on dusty pack forming lines due to the improved sealant melt strength relative to pure high-flow LDPE. When the coated structure contacts food, declarations under EU 10/2011 and 21 CFR 177.1520 apply to the entire coated substrate, and migration testing is carried out with the aqueous simulant 10% ethanol and the fatty food simulant 95% ethanol or vegetable oil specified in EN 1186-1:2002. The absence of wax or paraffin in the coating formulation simplifies microwave packaging compliance, but the resin supplier must be notified if the converter adds recycled post-consumer material, as this changes the regulatory status and may introduce non-listed contaminants.

    Melt stability is the primary process risk in extrusion coating. At temperatures above 310°C, the residence time in the coat hanger die causes oxidative gel formation and fumes; at temperatures below 270°C, adhesion to unprimed paperboard drops because insufficient carbonyl groups are generated in the air gap. The coating line is fitted with a devolatilising screw of L/D 30:1 to 33:1 and a ceramic edge deckle with 75 mm to 150 mm deckle rod adjustment to trim the edge bead. Outputs on a 1.5 m wide line using this blend are typically 100 kg/h to 250 kg/h, depending on coat weight and board porosity; above 250 kg/h, melt temperature surges of ±5°C cause thickness variation outside the ±5% tolerance band and increase the defect rate in rotary sealing.

    Temporary protective film for acrylic sheet, polycarbonate glazing, and painted metal coil relies on a coextruded polyolefin substrate with a low-gel skin layer and a pressure-sensitive adhesive tie layer, and LyondellBasell Icorene 1869 NAT 0000 is used as the core polyethylene layer in thicknesses of 30 µm to 60 µm. The three-layer construction typically places a low-density polyethylene skin on the adhesive-free side, a thin ethylene-vinyl acetate or polyolefin plastomer adhesive layer on the protective side, and the Icorene 1869 NAT 0000 core to provide puncture resistance and UV shielding during transport and installation. The blown-film line is operated with a die gap of 1.8 mm, a blow-up ratio of 2.2:1, and a melt temperature of 180°C to 200°C to limit the generation of oxidised gels that would print through onto polished acrylic or polycarbonate surfaces.

    Corona treatment of the adhesive skin is set to 38 mN/m to 42 mN/m; below this range the pressure-sensitive adhesive anchors poorly and builds up on the peel roll, while above it the oxidation layer can promote micro-pinholes in the adhesive layer during ageing at 50°C. The film is slit without razor burn because excessive heat at the slit edge produces a weld line that later transfers to the protected surface. The construction must maintain peel adhesion below 1.5 N/25 mm after 30 days of UV exposure, otherwise removal tears the protective film or leaves adhesive residue on glazing. Test methods used by converters include ASTM D3330/D3330M-04(2021) for peel adhesion and ASTM D3359-17 for cross-cut adhesion of coatings after the protective film is removed. Storage of finished rolls above 40°C is avoided because low-molecular-weight tackifier migration becomes irreversible and raises adhesion beyond the clean-removal limit.

    Free Quote

    Competitive LyondellBasell Icorene 1869 NAT 0000 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1869 NAT 0000 is a linear low density polyethylene (LLDPE) injection molding resin supplied as natural pellets. The grade designation 1869 identifies a nominal melt flow rate of 20 g/10 min when measured at 190°C under a 2.16 kg load according to ISO 1133-1:2022. The nominal density is 0.924 g/cm³ when determined by ISO 1183-1:2019 after conditioning at 23°C. The NAT suffix indicates that the pellet contains no precompounded carbon black, titanium dioxide, or organic pigment; the 0000 field is a packaging and additive-version code. As an ethylene α-olefin copolymer, the resin carries short-chain branches that interrupt crystallinity, reduce melting point, and increase low-temperature ductility relative to HDPE. The linear backbone improves tensile yield stress and environmental stress crack resistance relative to LDPE of similar density because long-chain branching is low. The practical result is a grade that fills thin-wall cavities with lower injection pressure than fractional-melt LLDPE while retaining sufficient modulus for caps, closures, housewares, toys, and general-purpose consumer articles. All mechanical data supplied below are nominal single-point values from public supplier tabulations; they are not design allowables and require part-specific validation.

    What processing window follows from a 20 g/10 min LLDPE melt?

    Injection molding processes using Icorene 1869 NAT 0000 exploit its relatively high MFR to reduce fill time and permit thin wall sections. The melt exhibits shear-thinning behavior; at injection shear rates above 1000 s⁻¹, the apparent viscosity drops substantially from the low-shear value, allowing the material to traverse narrow flow leaders without excessive gate freeze. Rheologically, a 20 g/10 min LLDPE has a low-shear viscosity roughly an order of magnitude lower than a 1.0 g/10 min fractional-melt LLDPE, but the difference narrows at shear rates above 1000 s⁻¹ because both materials shear-thin. Capillary rheometry per ISO 11443 can quantify the full shear-viscosity curve at 190°C, 210°C, and 230°C; such data is required for accurate mold-filling simulation. Moldflow and Moldex3D simulations should use Cross-WLF viscosity coefficients fitted to capillary data rather than the single-point MFR value. Published data for this specific configuration is limited, and processing conditions must be validated on the target press.

    Across polyolefin injection molding practice, a melt temperature of 180°C to 230°C, a mold temperature of 15°C to 40°C, and a screw back pressure below 20 MPa are used for comparable LLDPE grades. Screws with L/D ratios from 20:1 to 25:1 and compression ratios from 2.5:1 to 3.5:1 provide adequate plastication; a positive shutoff nozzle or reverse-taper nozzle is preferred because low melt strength at high flow can cause drooling between shots. Clamp force depends on projected area and wall thickness, but the lower packing-pressure requirement of LLDPE compared with HDPE often permits a smaller machine for the same cavity. Transfer from velocity to pressure should occur before the cavity is volumetrically full; pack pressure should be adjusted upward only until gate seal is reached. Overpacking increases molded-in stress, warpage, and molded-in density gradients that can appear as sink marks after 24 h. Drying is not mandatory for sealed containers at relative humidity below 60%. If hopper residence time exceeds 24 h in ambient conditions above 60% RH, pre-drying at 70°C for 2 h in a desiccant hopper dryer is a conservative starting condition. Process-control strategies based on in-cavity pressure transducers are recommended over timer-based pack because batch-to-batch MFR variation shifts gate-freeze time and final part weight.

    Nominal property values associated with Icorene 1869 NAT 0000 appear below. They are reproduced from standard polyethylene datasheet practice; the current supplier certificate of analysis remains the controlling document.

    Nominal property set for Icorene 1869 NAT 0000
    Property Method Value
    Melt flow rate, 190°C/2.16 kg ISO 1133-1:2022 20 g/10 min
    Density ISO 1183-1:2019 0.924 g/cm³
    Tensile stress at yield ISO 527-2:2012 11.0 MPa
    Tensile strain at break ISO 527-2:2012 >500%
    Flexural modulus ISO 178:2019 260 MPa
    Vicat softening temperature A/50 ISO 306:2022 91°C
    Shore D hardness ISO 868 55

    The tensile yield stress and flexural modulus values position the material below unfilled HDPE injection grades and above most LDPE grades. The elongation at break above 500% indicates that the material remains ductile at room temperature under slow deformation; it does not quantify notched impact performance at −20°C. For applications involving snap-fit assembly, hinge flexing, or threaded strips, prototype testing under ASTM D638-14 tensile speed conditions appropriate to the strain rate is necessary. The Vicat softening point near 91°C is not a maximum continuous-use temperature; the material should be derated for continuous load, UV exposure, and chemical contact.

    When the 0.924 g/cm³ density enforces modulus and impact trade-offs in thin-wall parts

    At 0.924 g/cm³, the crystalline fraction is intermediate between LDPE and HDPE; short-chain branches exclude portions of the chain from lamellar crystals, reducing density and stiffness while increasing amorphous-phase entanglement. In thin-wall injection molded parts below 1.0 mm nominal wall, the resulting flexural modulus is often sufficient for snap-fit closures but lower than that of HDPE at the same wall stock. Static compression tests on closures made from this grade will show lower top-load performance than HDPE because top-load is governed by wall thickness, unsupported geometry, and material modulus. Conversely, the LLDPE exhibits better environmental stress crack resistance in contact with detergents, surfactants, and soap solutions than many HDPE grades; this property is valuable for flip-top caps and dispensing closures stored with liquid products.

    The high MFR allows multi-cavity tools with long flow-length-to-thickness ratios to fill without excessive gas trapping, but high shear at narrow gates can generate melt temperatures above the intended profile. A balanced hot-runner manifold with individually controlled nozzle tips and valve-gate sequencing is recommended for 16-cavity and larger tools to minimize residence-time differences. Weld lines are a critical failure site; they should be positioned away from snap-fit hinges and threaded regions, or the melt temperature at the flow front should be maintained above 200°C during filling. Mold shrinkage is lower than LDPE and higher than HDPE, but absolute values depend on cooling rate, gate position, and post-molding shrinkage over the first 24 h to 48 h. Published data for this specific configuration is limited; cavity dimensions should be determined from a steel-safe prototype tool rather than a linear shrink factor.

    Food-contact and regulatory conformance for Icorene 1869 NAT 0000 requires review of the current supplier product compliance statement. Polyethylene of this type is typically covered as an olefin polymer under 21 CFR 177.1520(c) 3.1a when the limitations on extractable fraction and use conditions are satisfied. In the European Union, the resin must be assessed under Regulation (EU) No 10/2011, including the appropriate overall migration limit of 10 mg/dm² for food contact unless a specific exemption applies. The declared additive package and catalyst residues must be examined for their authorization status in the applicable positive list. The grade is not inherently flame retardant; it does not comply with UL 94 V-0 without flame-retardant modification. It is not intended for medical implants or prolonged invasive tissue contact; absence of biocompatibility data should be assumed unless the supplier provides an ISO 10993-1 evaluation. For electrical uses, RoHS compliance under Directive 2011/65/EU Annex II applies to lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE; no intentional content of these substances is expected in a natural polyolefin grade. REACH obligations under Regulation (EC) No 1907/2006 are managed through the supplier SDS and downstream article obligations.

    Compliance checklist matrix for Icorene 1869 NAT 0000 applications
    Requirement Reference Verification basis
    US FDA olefin polymer status 21 CFR 177.1520(c) 3.1a Supplier compliance statement
    EU plastic food-contact material Regulation (EU) No 10/2011 Overall migration under Annex III/IV conditions
    REACH registration Regulation (EC) No 1907/2006 Safety Data Sheet Section 1.3
    RoHS restricted substances Directive 2011/65/EU Annex II No intentionally added Pb, Cd, Hg, Cr(VI), PBB, PBDE
    Aerobic biodegradation ASTM D6400 Not applicable; non-biodegradable polyolefin

    Color concentrate selection affects compliance. A masterbatch used for food-contact packaging must also meet the same food-contact requirements; incompatible carrier resins can create a noncompliant final article even if the base resin is compliant. Processing trials should include migration testing on the finished article, not the pellet alone. The natural grade is not supplied with an irradiation-stabilized package; electron-beam or gamma sterilization may cause yellowing and a measurable loss in tensile yield stress unless the resin is reformulated with a radiation stabilizer. Autoclave sterilization at 121°C is generally outside the thermal capability of this grade because the Vicat softening temperature is near 91°C; the part will distort under load at that temperature.

    Differentiation relative to LDPE, HDPE, and metallocene-catalyzed LLDPE

    Icorene 1869 NAT 0000 is differentiated from LDPE by its linear molecular architecture. LDPE contains long-chain branches that increase melt strength and shear sensitivity; this makes LDPE preferred for blown film and extrusion coating. In injection molding, LDPE with comparable MFR generally exhibits lower tensile yield stress, lower abrasion resistance, and higher mold shrinkage. The present LLDPE grade therefore replaces LDPE in thin-wall closures and housewares where improved toughness and resistance to stress cracking are needed. Against HDPE, the LLDPE has lower density, lower flexural modulus, and lower Vicat softening temperature but better environmental stress crack resistance and lower warpage from differential shrinkage. A 20 g/10 min HDPE and a 20 g/10 min LLDPE are not interchangeable; HDPE solidifies at higher temperature and may require higher mold temperature to avoid sink marks, while LLDPE may require longer cooling time in thick sections due to lower thermal conductivity.

    Metallocene-catalyzed LLDPE grades differ mainly in short-chain branch distribution. If a metallocene grade with the same density and MFR is chosen, it may provide better impact toughness, lower extractables, and more consistent thermal properties, but often at higher cost. The present grade’s catalyst type and comonomer carbon number are not always stated in public technical literature; this information should be requested when sealing properties, organoleptic limits, or low-temperature impact are critical. Compared with fractional-melt LLDPE film grades, Icorene 1869 NAT 0000 is not intended for blown film extrusion because its lower melt strength reduces bubble stability and limits draw-up ratios. The grade should also not be used in rotational molding, where low-flow, high-melt-strength powders are required to prevent pinholes and uneven wall distribution.

    Materials management and equipment validation trials with Icorene 1869 NAT 0000 should include incoming MFR and density testing per ISO 1133-1:2022 and ISO 1183-1:2019. Regrind fractions up to 30 wt% are typical in non-food-contact applications; higher fractions increase melt-pressure variation and shift the viscosity curve toward lower values. The resin should not be dry-blended with flame-retardant packages containing amine-based synergists, because alkaline additives can accelerate thermo-oxidative degradation of polyethylene during compounding. Copper-containing pigments or additives should be avoided unless a copper-stabilizing system is explicitly approved by the supplier. UV performance of the NAT grade is limited; molded parts intended for outdoor service require a separate hindered-amine light stabilizer and UV absorber package, with accelerated weathering per ISO 4892-2 used to rank candidate masterbatches. Processors should record screw recovery time, melt pressure at transfer, peak cavity pressure, cushion, and part weight at each shift; deviations outside the validated process envelope often indicate feed-throat temperature variation or check-ring wear rather than a resin fault. If part weight variability exceeds ±0.5% on an electric injection molding machine with closed-loop control, the feed system and hopper loader should be inspected before adjusting the shot size. The grade should not be purged with abrasive glass-filled compounds unless the screw and barrel are rated for abrasive wear; purging with low-MFR HDPE followed by the grade at reduced screw speed is sufficient for material transitions.