    Specifications
    HS Code 178558
    Density 0.918 g/cm³
    Melt Mass Flow Rate 190 C 2 16 Kg 18 g/10 min
    Tensile Strength At Yield 8.5 MPa
    Tensile Strength At Break 10 MPa
    Tensile Elongation At Break 700%
    Flexural Modulus 200 MPa
    Notched Izod Impact Strength 80 kJ/m²
    Vicat Softening Temperature 80 °C
    Melting Temperature 120 °C
    Heat Deflection Temperature 0 45 Mpa 45 °C
    Shore D Hardness 45
    Water Absorption <0.01%
    Ul 94 Flame Rating HB
    Color Black

    As an accredited LyondellBasell Icorene 1869 BLK 9907 Polyethylene, Linear Low Density factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1869 BLK 9907 is supplied in 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) LyondellBasell Icorene 1869 BLK 9907 LLDPE loaded in 20′ FCL; 25 kg bags, palletized, stretch-wrapped, secured for sea transport.
    Shipping LyondellBasell Icorene 1869 BLK 9907 is a non-hazardous, black linear low-density polyethylene pellet. It typically ships in 25 kg bags, octabins, or bulk hopper trucks/railcars. No UN number, hazard class, packing group, or labels are required. Store dry, away from heat, sunlight, and contaminants.
    Storage Store in original packaging in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed and sealed to prevent moisture, dust, and contamination. Palletize at ambient temperature, avoid stacking damage, and segregate from strong oxidizers and incompatible chemicals. Follow local fire codes and the manufacturer’s SDS recommendations.
    Shelf Life Shelf life is typically 24 months from manufacture when stored unopened in original packaging, dry, away from sunlight, below 50°C.
    Application of LyondellBasell Icorene 1869 BLK 9907 Polyethylene, Linear Low Density

    In rotational moulding operations producing vertical agricultural liquid storage tanks, LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene is charged as 100 phr single-layer feed, with clean post-industrial rotomoulding regrind restricted to 10 wt% in the outer wall and 20 wt% in the inner wall of two-layer constructions because the outer wall must retain the compounded carbon black ultraviolet package. The material is processed on four-arm carousel rotational moulding machines with aluminium or cast steel tooling, oven set-point 265–285 °C, internal air temperature monitored via Rotolog to reach a peak internal air temperature of 185–190 °C before cooling, primary-to-secondary axis rotation ratio 4:1, forced air cooling to 90 °C followed by water mist to 60 °C demoulding. Tanks are produced in flat-bottom vertical configurations from 500 L to 20,000 L for fertigation storage and rainwater retention, with wall thicknesses from 4 mm to 15 mm depending on hydrostatic load. Conformity is assessed against ASTM D1998-06 for polyethylene upright storage tanks and FDA 21 CFR 177.1520(c) 3.1a where potable-water contact is declared; the rotomoulder bears responsibility for migration testing on the finished article because resin certification alone does not guarantee food-contact conformity after processing.

    What Limits Wall Thickness Uniformity in Foam-Filled Marine Aquaculture Float Shells?

    Wall thickness deviation in single-seam float shells arises from non-uniform heat transfer at the mould parting line and from powder bridging in narrow neck regions. Rotomoulding of LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene for marine aquaculture collar floats and fender shells uses a two-piece clamshell mould with an internal mandrel for through-hole formation; the powder charge is 100 phr virgin compound for the outer shell, and the shot weight is calculated to give a nominal wall thickness of 10–14 mm at a tolerance of +0/-1 mm. Peak internal air temperature is held at 190 °C for 8–12 min to sinter the powder fully, with secondary axis rotation speed not exceeding 3 rpm to avoid centrifugal thinning at the equator. After demoulding, closed-cell polyurethane foam is injected into the hollow void at 1.05:1 volume fill ratio relative to the void volume; overfill beyond 1.10:1 generates hoop stress sufficient to split the shell at the mould parting line, while underfill below 0.95:1 reduces hydrodynamic stiffness. Conformity for floating aquaculture structures is reviewed against NS 9415:2009 and IALA Recommendation E-108 where surface colour and signal marking are specified. Terminal products are black aquaculture cage float collars, mooring fender bodies, and marker buoy shells, all exposed to 3,000 h accelerated QUV aging under ASTM G154-23 before field deployment.

    Industrial Secondary Containment Pallets and Sump Floor Integrity

    For portable chemical containment pallets, the sump floor is moulded as a monolithic, weld-free basin from LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene at 100 phr virgin compound; regrind is excluded from the sump floor and sidewall bottom 25 mm because stress cracking at corner radii is the dominant failure mode under static hydrochloric acid and sodium hydroxide exposure. The process is biaxial rotational moulding on shuttle machines with steel tooling, peak internal air temperature 192–195 °C, dwell 18–22 min, and slow cooling in quiescent air at 1.5–2.0 °C/min to minimise warpage across the 1,200 mm span. A galvanised steel load frame is inserted into integrally moulded pockets after demoulding; load rating is verified at 250 kg to 2,500 kg uniformly distributed load. Chemical compatibility is tested by ASTM D543-20 for 30 day immersion in candidate chemicals at 23 °C, with tensile retention required above 80% of unexposed values. Secondary containment sizing follows 40 CFR 112.7(c), where the sump volume must equal or exceed 110% of the largest container volume stored on the platform. Terminal products include spill pallets, drum caddies, and floor-scale bunds with sump capacities from 50 L to 1,200 L.

    When municipal utilities specify non-metallic pull boxes for underground power and telecommunications distribution, LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene is rotomoulded at 100 phr for load-bearing covers and at 80 phr virgin compound with 20 phr matched in-house regrind for vertical sidewalls up to a Tier 22 rating, while regrind is excluded from Tier 33 covers subject to heavy vehicular loading. Oven residence time for a 6 mm nominal wall is 22–28 min at a peak internal air temperature of 188–193 °C, with internal air temperature confirmation by radio thermocouple rather than oven temperature alone. Threaded brass inserts for grounding lugs are moulded in place under 8–10 kN insert retention force testing. Compliance is verified against ANSI/SCTE 77 2017 for underground enclosure integrity, including Tier 15, Tier 22, and Tier 33 load classifications, and tensile properties are determined by ASTM D638-14 using Type IV specimens cut from moulded panels. Terminal configurations are single- and double-lid signal pull boxes, streetlight junction enclosures, and handholes with internal clear openings from 300 mm × 600 mm to 900 mm × 1,200 mm.

    When Post-Consumer Regrind Is Reintroduced Into Three-Layer Rotomoulded Play Panels

    Three-layer playground panel constructions require careful shot sequencing because post-consumer LLDPE regrind reduces the sinter-fusing window of the core layer. In this configuration, the outer skins each consist of 30 wt% LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene and the core consists of 40 wt% post-consumer LLDPE regrind, giving a total regrind fraction of 40 wt%; the first skin shot is dropped at 175 °C internal air temperature, the core shot at 140 °C, and the second skin shot at 120 °C during cooldown to maintain discrete layers. Peak internal air temperature is capped at 185 °C for 8 min, because temperatures above 190 °C produce oxidative embrittlement at regrind-rich layer boundaries and temperatures below 180 °C leave unmelted core particles. Mechanical acceptance is assessed under EN 1176-1:2017 for structural integrity and entrapment, with Izod impact at -20 °C required above 15 kJ/m² using ISO 180:2023; carbon black loading is verified by ash method in the outer skins only to ensure the regrind core is not exposed to ultraviolet irradiation. Terminal products include climbing panels, tunnel segments, and activity panels that are surface-textured during moulding rather than post-machined.

    Carousel rotational moulding lines producing wheeled refuse container bodies use LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene at 85 phr virgin compound with 15 phr closed-loop rotomoulding regrind for the outer shell, while the comb lift receiver and axle bosses are shot from the same material at 100 phr virgin to prevent hinge tear-out. The process is conducted on a six-arm carousel with oven set-point 270–290 °C, peak internal air temperature 190–195 °C, and oven dwell 20–25 min for a 5 mm nominal wall. Forced air cooling at 4 m/s is applied until the mould surface reaches 70 °C, followed by jig demoulding to limit shrinkage-induced sidewall bow. Dimensional and performance conformity is tested under EN 840-1:2020 for mobile waste containers up to 400 L, and environmental stress cracking resistance is evaluated by ASTM D1693-15 Condition B on notched specimens, with failure time recorded above 1,000 h. Terminal products are two-wheeled refuse containers from 80 L to 360 L with integrated comb lift receivers and black UV-stabilized exteriors.

    Thermal Bridging Occurs at the Foam-Injection Port in Double-Wall Insulated Fish Tubs

    Double-wall insulated fish tubs suffer local wall thinning at the foam-injection port when the polyurethane foam shot introduces exothermic heat after demoulding. The food-contact inner shell is rotomoulded from LyondellBasell Icorene 1869 BLK 9907 Linear Low Density Polyethylene at 100 phr virgin compound, while the outer shell is produced from the same material at 70 phr virgin compound plus 30 phr matched rotomoulding regrind; the insulating cavity is then filled with rigid polyurethane foam at 35–45 kg/m³ core density and a shot weight ratio of 1.05:1 relative to cavity volume. The inner layer is fusion-bonded at peak internal air temperature 190 °C for 7–9 min, then the outer layer is shot during cooldown at 125 °C to avoid collapse at the injection port. Food-contact compliance is supported by FDA 21 CFR 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011 with overall migration testing according to EN 1186-1:2002; surface smoothness is measured by profilometry at Ra 0.8 µm to minimise biofilm retention. The rotomoulder must verify specific migration limits on the finished tub because the resin supplier does not guarantee food-contact conformity after processing. Terminal products are 600 L and 1,000 L chilled fish transport tubs and insulated seafood handling bins used in cold-chain distribution with internal cavity temperatures maintained below 4 °C.

    Free Quote

    Competitive LyondellBasell Icorene 1869 BLK 9907 Polyethylene, Linear Low Density prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1869 BLK 9907 is a black-pigmented linear low-density polyethylene powder supplied for rotational molding. The designation Icorene 1869 identifies the unfilled ethylene/α-olefin copolymer; the suffix BLK 9907 identifies a combined carbon black and UV-stabilizer package. Under ISO 1872-1, the base material is classified as an ethylene-based thermoplastic. The powder form is intentional: rotational molding requires controlled particle size distribution and low-shear melt coalescence rather than the pellet mass flow used in extrusion or injection molding. Nominal density is 0.936 g/cm³ per ISO 1183-1, and nominal melt mass-flow rate is 5.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1 in published trade literature. These values position the product as a medium-flow rotational molding LLDPE with a balance of stiffness, low-temperature toughness, and environmental stress-crack resistance.

    The grade is not a high-density homopolymer. The short-chain branching produced by α-olefin comonomer reduces density and crystallinity compared with HDPE rotational molding grades, lowering flexural modulus but improving ESCR and low-temperature ductility. In contrast to low-density polyethylene, which contains long-chain branching, this LLDPE has a more linear backbone and higher tensile strength at equivalent melt index. The result is a resin that is typically selected when a black outdoor part must resist cracking in service but does not require an HDPE-level modulus. Natural Icorene 1869 without the black package may be prescribed when translucency, lower surface temperature, or colour-matching of the final product is required.

    Black 9907 differs from a natural Icorene 1869 in three operational respects: opacity, weathering resistance, and solar heat absorption. Carbon black attenuates ultraviolet radiation and reduces photo-oxidative chain scission at the part surface; it also increases solar absorptance compared with unpigmented polyethylene. A black part installed outdoors may therefore reach a higher wall temperature than an identically shaped natural part. The UV stabilizer and carbon black package is proprietary. Quantitative xenon-arc or outdoor exposure retention figures must be confirmed from the supplier lot certificate rather than transferred from natural-grade data.

    How does the 9907 black package alter weathering resistance and solar heat absorption?

    Black pigmentation in polyolefins acts primarily as a UV screener. Incident radiation is absorbed by carbon black aggregates rather than transmitted into the polymer matrix, limiting initiation of free-radical chain scission. The mechanism depends on dispersion quality and aggregate size; incomplete dispersion can create localized UV protection failure. Weathering tests for this product family are normally performed under ISO 4892-2 or ASTM G154. Published test hours for retention of tensile elongation in Icorene 1869 BLK 9907 are limited in regional trade literature, so designers should require lot-specific weathering data when the part warranty exceeds 3 years of outdoor exposure.

    The black surface has higher solar absorptance than an unpigmented grade. This raises wall temperature under solar load, which can accelerate post-shrinkage and reduce creep modulus at the affected surface. In high-insolation installations, surface temperatures above 60 °C are possible. The operational boundary does not preclude outdoor use, but design calculations must include thermal movement and reduced stiffness. If the part is used as a tank or hitch cover with mechanical attachments, thermal expansion must be accommodated by slotted holes or flexible mounts. Carbon black does not protect against oxidation at these elevated service temperatures; the stabilizer package only delays radical propagation under weathering.

    On shuttle and carousel rotational molding lines, the powder is charged into steel or aluminum molds and heated in forced-air ovens with set temperatures typically between 260 °C and 320 °C. The controlling process variable is peak internal air temperature, not oven setting. For the LLDPE powder family containing Icorene 1869, peak internal air temperature is commonly held between 190 °C and 205 °C to complete sintering, eliminate gas bubbles, and avoid oxidative degradation. Published data specific to Icorene 1869 BLK 9907 may narrow this window; instrumented mold trials with internal thermocouples are therefore required before volume production. Heating above 210 °C can drive rapid melt-flow increase, odour development, and surface defects in black parts.

    Heat transfer into the powder bed occurs through the mold wall. During heating, particle surface melting begins near the crystalline melting peak of the LLDPE, typically 124–128 °C by differential scanning calorimetry. Rotational molding requires heating well above the melting peak to reduce melt viscosity and allow particle coalescence. Incomplete densification leaves granular boundaries at the inner wall; these boundaries reduce ESCR and can initiate crack propagation under stress. Entrapped air and moisture must dissolve and diffuse from the melt. Peak internal air temperature therefore controls both cycle time and final through-thickness morphology. Melt mass-flow rate alone is insufficient to predict bubble removal because the process is low-shear; published shear viscosity data for this specific grade is limited.

    Demolding temperature is as important as oven residence time. Slow air cooling at 8–12 °C/min minimizes residual stress, while forced-air or water-mist cooling improves cycle time at the risk of higher shrinkage variation and warpage. Carbon black may act as a nucleating agent in LLDPE, altering crystallization kinetics relative to natural 1869 and producing a finer spherulitic texture. This can change shrinkage and warpage when a mold is transferred from natural to black powder. Incoming powder should be inspected for bulk density and particle size distribution. Powders in the 150–600 µm range are generally favored for rotational molding; excessively fine fractions increase dust explosion sensitivity, while coarse fractions slow melting and create pinholes. Powder that has been exposed to storage relative humidity above 60% should be pre-dried at 70–80 °C for 1–2 h before charging to reduce moisture-induced pinholes.

    On production-scale shuttle machines, the largest source of lot-to-lot variability is not melt index shift but changes in powder bulk density and dry flow. A lower bulk density can cause undercharging by mass if a volumetric fill station is used, producing thin wall sections and lower collapse resistance. Field experience with black rotomolding powders shows that carbon black dispersion quality can vary by concentrate let-down ratio and grinding history; poor dispersion may appear as grey streaks in thin sections and as local losses in ESCR. Incoming inspection should therefore include sieve analysis and a dispersion check, not solely melt flow rate.

    Mechanical and environmental stress-crack response under published test conditions

    Published typical properties for Icorene 1869 BLK 9907 are summarized below. These values are representative, not specification limits, and should be verified against the manufacturer’s lot certificate before design release.

    PropertyTest methodTypical value
    DensityISO 1183-10.936 g/cm³
    Melt mass-flow rateISO 1133-15.0 g/10 min at 190 °C/2.16 kg
    Tensile yield stressISO 527-218 MPa
    Elongation at breakISO 527-2450%
    Flexural modulusISO 178700 MPa
    ESCR, condition BASTM D1693-15>1000 h
    Brittleness temperatureASTM D746-20−76 °C
    Vicat softening temperatureISO 306/A50118 °C

    The ESCR result greater than 1000 h under ASTM D1693-15 condition B, 10% Igepal CO-630 at 50 °C, is a key differentiator from LDPE and many HDPE homopolymer rotomolding powders. LDPE rotomolding grades may fail below 100 h under identical conditions, while HDPE homopolymers may show shorter ESCR in the same test. The trade-off is flexural modulus: at 700 MPa, this LLDPE is less stiff than typical HDPE rotomolding grades, which can exceed 900 MPa. Therefore, a load-bearing wall made from Icorene 1869 BLK 9907 requires thicker geometry or ribbing to meet deflection limits.

    Low-temperature ductility is another differentiating property. The brittleness temperature of −76 °C under ASTM D746-20 indicates that the material retains impact performance below the freezing point of water. This supports outdoor service in cold climates, provided the part design avoids sharp notches and molded-in stresses. Published charpy or notched Izod data for this specific formulation are limited; do not transfer un-notched impact data to notched part features. Flexural modulus and tensile yield should be used as short-term design inputs only. Long-term creep, stress relaxation, and chemical exposure require separate testing under the actual service fluid and temperature.

    If regulatory approval is required for potable-water or food-contact service

    Compliance for black-pigmented rotomolding grades is not automatic. The base ethylene/α-olefin copolymer may be covered by FDA 21 CFR 177.1520 in the United States and EU Regulation (EU) No 10/2011 as amended for plastic food-contact materials. The carbon black and UV-stabilizer package, however, must satisfy 21 CFR 178.3297 in US formulations and the EU positive lists with specific migration limits. For Icorene 1869 BLK 9907, the supplier’s regulatory declaration for the exact colour code is required; published data for this specific configuration is limited in general compilations.

    Regulatory areaApplicable referenceVerification required
    EU food-contact plasticsRegulation (EU) No 10/2011 including amendmentsSupplier declaration with migration test data for the specific stabilizer and carbon black package
    US food-contact olefin polymersFDA 21 CFR 177.1520Grade-specific confirmation; carbon black compliance under 21 CFR 178.3297
    REACH SVHCRegulation (EC) No 1907/2006Declaration for substances above 0.1% w/w in the article
    RoHSDirective 2011/65/EUConfirm absence of restricted heavy metals in black colorant

    Potable-water tank service may require additional NSF/ANSI 61 or regional approvals. These are end-product tests and cannot be replaced by resin-level declarations alone. If the part must meet ISO 9080 hydrostatic design stress for pressure pipe or pressurized vessels, separate long-term creep-rupture data must be generated from the molded part, not transferred from ESCR results. Black pigment does not automatically confer suitability for outdoor potable water storage; microbiological surface behavior, taste and odour migration, and UV screening must be considered together.

    Powder handling on a production line requires attention to minimum ignition energy and static dissipation. Polyethylene powder in the rotomolding size range can form explosible dust-air mixtures. Equipment should be bonded and grounded; air conveying should be designed with adequate velocity to avoid dust accumulation. The carbon black content in BLK 9907 may reduce surface resistivity relative to natural polyethylene, but this does not eliminate static control requirements under IEC 61241 or regional dust explosion standards. Bulk storage should be in sealed containers away from direct sunlight and heat sources. Outdoor storage of opened containers should be avoided because surface moisture uptake can lead to pinholes even if the resin itself is not hygroscopic.

    Chemical resistance is not uniform across all end-use fluids. Prolonged exposure to aromatic hydrocarbons, chlorinated solvents, or strong oxidizing acids may swell the polyethylene matrix and accelerate environmental stress cracking, particularly at molded-in stresses or weld lines. The black UV package improves outdoor weathering but does not provide protection against continuous hot-air oxidation above the published service temperature. For applications involving sustained load at temperatures above 60 °C, creep modulus and stabilizer consumption should be evaluated under the actual fluid and stress state. Processing or service contact with incompatible mold release agents can migrate into the surface and reduce adhesion of foamed insulation or gaskets applied to the molded part. Published data for this specific configuration is limited in multi-layer assemblies. If the grade is used for playground surfaces or public furniture, the final molded part must be evaluated for heavy metals and phthalates under the relevant regional product safety standards, regardless of resin-level REACH or RoHS declarations.

    Top