| HS Code | 512109 |
| Polymer Type | Polyethylene, Linear Low Density, Metallocene |
| Density | 0.916 g/cm³ |
| Melt Flow Rate | 1.0 g/10 min |
| Tensile Strength At Yield | 9.0 MPa |
| Tensile Strength At Break | 28.0 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 6.0% |
| Gloss | 80% |
| Melting Point | 118 °C |
| Vicat Softening Point | 94.0 °C |
| Brittleness Temperature | < -70.0 °C |
As an accredited LyondellBasell Icorene 1761 YEW 2911 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 YEW 2911 is supplied in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped for shipment. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 1761 YEW 2911 metallocene linear low-density polyethylene (LLDPE), 25 kg bags, palletized, approx. 18–20 metric tons. |
| Shipping | LyondellBasell Icorene 1761 YEW 2911 Polyethylene, Linear Low Density, Metallocene is shipped as non-hazardous resin pellets in sealed 25 kg bags or bulk, palletized and stretch-wrapped. Transport in dry, covered containers/trucks. Store away from heat, moisture, sunlight, and incompatible materials. Not regulated for transport. |
| Storage | Store LyondellBasell Icorene 1761 YEW 2911 Polyethylene, Linear Low Density, Metallocene in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep bags/containers closed to prevent moisture and contamination. Avoid dust and static; ground equipment. Store below 50°C, use first-in, first-out rotation, and follow supplier SDS. Protect from UV exposure and incompatible materials. |
| Shelf Life | Shelf life: 12 months from date of delivery when stored unopened in original packaging in a cool, dry, well-ventilated area. |
LyondellBasell Icorene 1761 YEW 2911 is specified for rotationally moulded components in which metallocene linear low-density polyethylene must combine ultraviolet stabilization, low-temperature ductility, and environmental stress-crack resistance. The application scenarios below are restricted to downstream sectors where these properties are exploited in production-scale rotational moulding; each segment records the controlling compliance framework, dry-blend addition level, rotational moulding process window, and finished article categories. Published data for unchanged long-term weathering of this exact stabilisation package in all installation chemistries are limited; accelerated weathering evaluations should be treated as screening data rather than service-life guarantees.
Rotational moulding of cylindrical fertiliser tanks from metallocene LLDPE imposes a narrow window between complete powder densification and oxidative degradation at the inner wall. The powder is dry-blended at 80–100 wt% virgin Icorene 1761 YEW 2911, 0–20 wt% clean in-house regrind, and 0.5–1.5 wt% UV or carbon black masterbatch for opacity. When the stored liquid is a chelated micronutrient solution below pH 4.0, the regrind level is held at or below 15 wt% to preserve environmental stress-crack resistance measured by ASTM D1693-21. Tooling is typically fabricated from rolled steel or CNC-machined cast aluminium, with a biaxial rotation ratio of 4.5:1 primary to secondary. Oven air temperature is maintained at 260–280 °C, peak internal air temperature at 190–205 °C, and total cycle time at 28–35 min for a nominal 8 mm wall section. Forced-air cooling to 80 °C followed by demoulding near 50 °C reduces warpage at the top rim and outlet boss.
Compliance is governed by ASTM D1998-21 for upright polyethylene storage tanks, with chemical resistance testing per ASTM D543-21 Method B against the intended fertiliser formulation. Finished articles include 500–15,000 L vertical storage tanks, cone-bottom fertigation tanks, and chemical dosing tanks for agricultural injection systems. Continuous service is not recommended above 40 °C or with oxidising chemistries above 5% available chlorine; aromatic solvent contact must be excluded from the installation specification.
For public playground shells, repetitive impact and variable outdoor weathering—not continuous hydrostatic stress—dominate the design verification plan. The formulation is set at 90 wt% virgin metallocene LLDPE powder, 10 wt% post-industrial regrind of the same grade, and 1.0–2.5 wt% UV-stabilised color masterbatch. No external process aid is added when powder moisture is below 0.05 wt%. Processing uses cast aluminium tooling and a 4:1 biaxial rotation ratio; oven set point is 250–275 °C, peak internal air temperature is 195–215 °C, and cycle time is 22–30 min for a 4–6 mm shell wall. Compressed-air pre-cooling followed by a short water mist shortens demoulding without inducing the differential shrinkage observed at thick moulded-in slide rail bosses.
Governing standards are EN 1176-1:2017 for public playground equipment and ASTM F1487-21 for the corresponding U.S. installations. Material acceptance records include tensile yield per ASTM D638-14, notched Izod impact per ASTM D256-23, and accelerated UV exposure per ASTM G154-23 Cycle 1. Finished components include tube slide sections, roof panels, climbing tunnel modules, and spring rocker seat bodies. Regrind above 15 wt% is not permitted without high-speed puncture validation, and post-consumer recyclate is excluded from load-bearing EN 1176 applications unless independently tested.
In marine sanitation holding tanks, tensile yield is less decisive than leakage resistance after installation in a vibrating hull environment and exposure to ammonium-rich waste. ISO 8099:2000 governs small craft toilet waste retention systems, and the rotomoulded shell is formulated at 100 wt% virgin Icorene 1761 YEW 2911 to avoid micropitting and odor carryover due to regrind contamination. The addition of 0.5–1.0 wt% carbon black masterbatch is restricted to deck-exposed installations; below-deck tanks are processed without pigment to eliminate surface inclusions near outlet threads. Tooling is steel or CNC-machined aluminium, with oven set point 270–290 °C, peak internal air temperature 195–210 °C, and a cycle time of 30–40 min for an 8 mm nominal wall. After demoulding and a 24 h normalisation period, the tank is pneumatically tested at 20–30 kPa internal pressure to detect pinholes at corners and inserts.
The resulting parts include 15 L, 40 L, and 80 L holding tanks, pump-out basins, and maceration tank shells. Brittleness temperature is verified by ASTM D746-20, water absorption by ASTM D570-22, and accelerated weathering for deck installations by ASTM G154-23. The material is not rated for solvent-based toilet cleaning agents, gasoline, or pressurised fuel service; published data for continuous seawater submersion of this specific YEW 2911 stabilization package are limited and must be supplemented with application-specific testing.
Chemical secondary containment basins require wall integrity after contact with mixed corrosive liquids, but the failure mode most often observed on production lines is stress cracking adjacent to moulded-in inserts rather than bulk wall failure. The dry blend is set at 95 wt% virgin metallocene LLDPE and 5 wt% clean in-house regrind for neutral runoff applications; aggressive containment duties at pH < 2.0 or oxidising mixtures require 100 wt% virgin material. A 1.0 wt% colour-coding masterbatch is added only when the basin must signal a specific hazard class. Steel tooling is used, with oven set point 280–300 °C, peak internal air temperature 195–210 °C, and cycle time 35–45 min for 6–10 mm walls. Demoulding is delayed until the part is below 50 °C, and insert bosses are leak tested by static pressure decay at 15–20 kPa after cooling.
Regulatory compliance references 40 CFR 264.175, requiring secondary containment volume of at least 10% of the largest primary tank or 100% of the largest vessel, whichever is greater. Chemical resistance is evaluated by ASTM D543-21 Method A, and stress-crack resistance by ASTM D1693-21. Finished parts include spill pallets, secondary containment basins, chemical sumps, and acid dilution trays for water treatment skids. Concentrated nitric acid, aromatic hydrocarbons, and strong oxidising acids above normal industrial concentrations are outside the documented operating boundary.
When industrial bulk handling bins store granular fertilizer for extended periods, phosphatic dust combined with storage humidity forms a weakly acidic surface film that can initiate stress cracking at flat-bottom corners. The powder compound is therefore dry-blended at 85 wt% virgin Icorene 1761 YEW 2911 and 15 wt% post-industrial regrind, with 1–2 wt% color masterbatch for inventory coding. Tooling is steel or cast aluminium, rotation ratio is 4:1, oven set point is 260–280 °C, peak internal air temperature is 190–205 °C, and cycle time is 30–38 min for 5–8 mm shell walls. Corner radii are maintained above 25 mm during tool design to reduce stress concentration, and loaded drop performance is verified by ASTM D5276-19.
Flat-bottom static load capacity is assessed under ISO 8611-1:2011 pallet-load test protocols or the equivalent customer block-load specification, with environmental stress-crack resistance screened by ASTM D1693-21. Terminal articles are 200–1,000 L bulk bins, seed hoppers, granular fertilizer tote liners, and mobile feed carts for agricultural distribution. These containers are not rated for liquid service or for direct exposure to aromatic solvents; phosphoric acid-rich dust environments should limit regrind to 10 wt% if high-humidity storage exceeds 75% RH.
| Application segment | Governing standard or regulation | Controlling test method | Key condition or acceptance boundary |
|---|---|---|---|
| Agricultural liquid storage | ASTM D1998-21 | ASTM D1693-21; ASTM D543-21 | pH 4.0 chelated solutions limit regrind to 15 wt% |
| Public playground shells | EN 1176-1:2017; ASTM F1487-21 | ASTM D256-23; ASTM G154-23 | Post-industrial regrind limited to 10 wt% without puncture validation |
| Marine sanitation tanks | ISO 8099:2000 | ASTM D746-20; ASTM D570-22 | 100 wt% virgin shell; pneumatic test at 20–30 kPa |
| Chemical secondary containment | 40 CFR 264.175 | ASTM D543-21; ASTM D1693-21 | 100 wt% virgin required below pH 2.0 |
| Industrial bulk bins | ISO 8611-1:2011 | ASTM D5276-19; ASTM D1693-21 | Corner radii above 25 mm; regrind below 10 wt% above 75% RH |
| Outdoor furniture | EN 581-1:2017 | ASTM D790-17; ASTM G154-23 | Air quench to 80 °C; fixture held below 45 °C |
| Segment | Oven set point | Peak internal air temperature | Regrind limit | Nominal wall thickness | Representative cycle time |
|---|---|---|---|---|---|
| Agricultural liquid storage | 260–280 °C | 190–205 °C | 0–20 wt% | 8 mm | 28–35 min |
| Public playground shells | 250–275 °C | 195–215 °C | 10 wt% | 4–6 mm | 22–30 min |
| Marine sanitation tanks | 270–290 °C | 195–210 °C | 0 wt% | 8 mm | 30–40 min |
| Chemical secondary containment | 280–300 °C | 195–210 °C | 5 wt% or 0 wt% | 6–10 mm | 35–45 min |
| Industrial bulk bins | 260–280 °C | 190–205 °C | 15 wt% | 5–8 mm | 30–38 min |
| Outdoor furniture | 250–270 °C | 190–210 °C | 12 wt% | 4–7 mm | 25–32 min |
After air-quench cycles are selected to minimise internal stress, outdoor furniture shells require dimensional stabilisation before demoulding and secondary router work. The dry blend comprises 88 wt% virgin UV-stabilised metallocene LLDPE, 12 wt% clean post-industrial regrind, and 2–3 wt% UV-stabilised masterbatch for colour saturation. Cast aluminium tooling is operated at 250–270 °C oven set point and 190–210 °C peak internal air temperature, with a 4:1 rotation ratio and 25–32 min cycle for 4–7 mm wall thickness. Air quench to 80 °C is used rather than water spray, and the part is held in a cooling fixture until it drops below 45 °C to prevent warp at long bench seat spans.
Seating compliance is evaluated against EN 581-1:2017, while flexural modulus is recorded by ASTM D790-17 and weather resistance by ASTM G154-23. Finished products include park benches, picnic table seat and top components, waste receptacle lids, planter liners, and bollard covers. Air-quench processing increases overall cycle time compared with water mist but reduces stress-crack initiation around through-holes and fixture points. The material is not intended for structural members beyond the load levels defined in EN 581-1 or for continuous contact with strong organic solvents.
Competitive LyondellBasell Icorene 1761 YEW 2911 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 YEW 2911 is a metallocene-catalysed linear low density polyethylene. The grade identifier 1761 distinguishes the melt viscosity, density and additive package; the suffix YEW 2911 identifies the commercial formulation, colour and stabiliser configuration. Because the base resin is classified as linear low density polyethylene, its density at 23 °C is below 0.940 g/cm³ when tested under ISO 1183-1:2019. The material is supplied as a powder or compounded pellet for rotational moulding, compounding, and selected injection-moulding operations. The exact melt flow rate, powder particle-size distribution and stabiliser loading must be read from the lot certificate of analysis; they are not established by the product-class description alone.
Incoming quality-control measurements for this resin class should include melt flow rate at 190 °C and 2.16 kg according to ISO 1133-1:2022 or ASTM D1238-23, density by ISO 1183-1:2019, tensile yield stress and elongation at yield from ISO 527-2:2012 type 1B specimens, flexural modulus from ISO 178:2019, Charpy notched impact from ISO 179-1:2023, and oxidative induction time from ISO 11357-6:2018. The supplier certificate of analysis should be compared against these methods because different conditioning histories and specimen preparation routes can shift the reported values by several per cent.
Metallocene catalysis produces an ethylene-α-olefin copolymer with a narrow molecular weight distribution and a uniform short-chain branching distribution. In contrast, Ziegler-Natta linear low density polyethylene contains a heterogeneous distribution of comonomer across molecular weights: lower-molecular-weight chains are typically more branched, and higher-molecular-weight chains are more linear. The metallocene architecture reduces the fraction of highly linear, high-molecular-weight chains that can nucleate large crystalline domains. Consequently, the melting peak is lower, the crystalline lamellae are thinner, and the resin exhibits higher slow-crack-growth resistance at equivalent density. These differences are measurable by gel permeation chromatography with infrared detection, differential scanning calorimetry at 10 °C/min under ISO 11357-3:2018, and environmental stress crack resistance under ASTM D1693-15e1. The same narrow distribution lowers shear thinning in the melt; capillary rheometry per ISO 11443:2021 typically shows a power-law index closer to 1 than that of a broad-molecular-weight-distribution Ziegler-Natta grade. This is a processing liability in blown-film and extrusion-coating, where melt strength and bubble stability are critical, but it is less severe in rotational moulding.
The following tendencies summarise differences between the metallocene LLDPE class represented by Icorene 1761 YEW 2911 and a conventional Ziegler-Natta LLDPE. They are comparative expectations, not substitutes for grade-specific data from the certificate of analysis.
| Property or processing characteristic | Metallocene LLDPE class | Conventional Ziegler-Natta LLDPE | Reference method |
|---|---|---|---|
| Molecular weight distribution | Narrow | Broad | ISO 16014-2:2019 |
| Short-chain branching placement | Uniform across molecular weight | Heterogeneous, higher in low-molecular-weight fraction | TREF / GPC-FTIR |
| Melting peak temperature | Lower at equal density | Higher at equal density | ISO 11357-3:2018 |
| Environmental stress crack resistance | Higher at equal density | Lower at equal density | ASTM D1693-15e1 |
| Dart impact resistance | Improved | Lower | ISO 6603-2:2023 |
| Extractable fraction | Lower | Higher | Food-contact extraction under EU Regulation 10/2011 |
| Melt shear-thinning | Lower | Higher | ISO 11443:2021 |
Rotational moulding powder behaviour is governed by particle-size distribution, bulk density and dry flow. A practical sieve target for metallocene LLDPE rotomoulding powders in this class is 35 mesh to 150 µm; coarser fractions retard sintering, while an excess of fines lowers bulk density and creates dust-control problems. Bulk density is measured by ISO 60:2023 or ASTM D1895-17, and dry flow by ISO 6186:2023. Incoming lots should be sampled from multiple silo depths because pneumatic transfer can stratify coarse and fine particles, and the resulting segregation can produce wall-thickness variation in production parts.
During heating, the powder particles coalesce by viscous sintering. The zero-shear viscosity of a metallocene LLDPE is lower than that of a density-matched Ziegler-Natta grade at the same melt flow rate; this accelerates neck formation and densification. However, the low melt strength of the narrow molecular weight distribution reduces the stability of the molten film through which air bubbles must escape. In practice, the oven air temperature should not be raised aggressively to remove bubbles; instead, the peak internal air temperature is held at a moderate plateau to allow bubble diffusion while limiting oxidative consumption of the primary antioxidant. The practical processing window for a rotomoulded metallocene LLDPE part is frequently ±5 °C when the peak internal air temperature is above 180 °C; below the lower limit, pinhole voids remain at the inner wall. Above the upper limit, yellowness index rises and impact strength declines because the antioxidant package is depleted. Published data for this specific configuration is limited; in-plant trials with internal air temperature loggers are required to fix the window for each mould geometry and wall thickness.
Cooling after densification controls shrinkage and warpage. Fast forced-air cooling reduces the development of secondary crystallinity and lowers part shrinkage measured by ISO 294-4:2018, but it can lock in residual thermal stress and reduce environmental stress crack resistance in thick sections. Slow cooling increases crystallinity and stiffness but can produce sink marks and increase cycle time. Production-scale machines should monitor the temperature difference between the mould outer surface and the internal air; when the difference exceeds 15 °C, non-uniform wall thickness or internal voids are more likely. These operational limits are drawn from standard rotomoulding practice rather than from a supplier-published process curve for this single grade.
For injection-moulding or compounding operations, temperature control is the dominant safeguard. Barrel settings should keep the melt temperature below 220 °C unless the stabiliser package is explicitly approved for higher temperatures. When colour concentrates or carbon black are introduced, a corotating twin-screw extruder with an L/D of at least 32:1 and distributive mixing elements improves pigment dispersion while limiting shear heating. Carbon black dispersion can be assessed by ISO 18553:2002; poor dispersion reduces low-temperature impact and can create stress concentrations in service.
Field failure modes in rotomoulded parts made from metallocene LLDPE grades are classified by their fracture surface and thermal history. Pinhole voids near the inner wall indicate insufficient peak internal air temperature or short plateau time; discolouration and brittleness indicate antioxidant depletion; large radial cracks at sharp corners indicate excessive cooling rate or mould-release geometry. When a part is returned from the field, measurement of melt flow rate by ISO 1133-1:2022 and oxidative induction time by ISO 11357-6:2018 can distinguish between molecular degradation and a pre-existing processing defect. A significant reduction in oxidative induction time without a change in melt flow rate points to thermo-oxidative consumption of stabiliser, whereas a large increase in melt flow rate suggests chain scission from repeated melt processing.
When Icorene 1761 YEW 2911 is substituted for a conventional Ziegler-Natta LLDPE in an existing rotomoulded tank or lining tool, the metallocene grade enters full densification at a lower oven air temperature, but its lower melt strength can reduce the ability of trapped air to escape through the molten phase. Venting geometry may require modification, and the peak internal air temperature may need a longer plateau rather than a higher setpoint. Compared with chromium-catalysed high density polyethylene, the linear low density metallocene grade has lower flexural modulus but higher resistance to slow crack growth; for tanks exposed to aggressive aqueous media, the change can extend time-to-failure under full-notch creep test conditions such as ISO 16770:2019. Published data for this specific formulation is limited; qualification should include side-by-side moulding trials on the production tool rather than extrapolation from resin-family averages.
Compared with autoclave low density polyethylene, the linear metallocene product has no long-chain branching and therefore lower melt strength; however, its tensile yield stress and slow-crack-growth resistance are higher when tested under ISO 527-2:2012 and ISO 16770:2019. This distinction matters in extrusion coating and blow moulding; in rotational moulding, the lower melt strength is less limiting because the melt is not required to support a free web. Compared with high density polyethylene, density and flexural modulus are lower, but environmental stress crack resistance is generally higher. The trade-off shifts part design toward thicker wall sections when stiffness is governing and toward metallocene LLDPE when stress cracking is the lifetime-limiting mechanism.
Compliance status is package-dependent. The following checks apply to the final fabricated part, not to the raw resin alone.
| Compliance area | Requirement or method |
|---|---|
| European food-contact plastics | EU Regulation 10/2011; overall migration limit 10 mg/dm² or 60 mg/kg for most food simulants |
| United States food-contact olefin polymers | FDA 21 CFR 177.1520, with additive compliance under subpart B |
| Restriction of hazardous substances | Directive 2011/65/EU for the final article |
| Registration and substances of very high concern | Regulation (EC) No 1907/2006 |
| Melt flow rate | ISO 1133-1:2022 or ASTM D1238-23 |
| Density | ISO 1183-1:2019 |
| Environmental stress crack resistance | ASTM D1693-15e1 |
| Oxidative induction time | ISO 11357-6:2018 |
For storage and handling, polyolefin powders are not hydrolytically sensitive, but surface moisture can be introduced during transport through high-humidity environments. When relative humidity exceeds 60%, drying in a dehumidified-air hopper at 60 °C to 80 °C for 1 h to 2 h is applied before processing to prevent steam porosity. Avoid blending this grade with acid-functionalised polymers or with recycled polyolefin streams containing high residual metals unless oxidative induction time testing under ISO 11357-6:2018 confirms that the stabiliser package is adequate. The product should not be exposed to chromate-based pigments in acidic service because chromium ions can catalyse thermo-oxidative degradation of the polyethylene backbone; published data for this specific configuration is limited.