Lyondellbasell Icorene 1761 Yew 2171 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 285444
    Density 0.917 g/cm³
    Melt Index 1.6 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 650%
    Flexural Modulus 200 MPa
    Vicat Softening Temperature 95°C
    Melting Temperature 115°C
    Haze 4%
    Gloss 90%
    Coefficient Of Friction 0.20
    Dart Drop Impact 200 g
    Elmendorf Tear Strength 300 g

    As an accredited LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped; bulk quantities available in 1,000 kg octabins or big bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): typically palletized 25 kg bags of LyondellBasell Icorene 1761 YEW 2171 metallocene LLDPE, dry container, securely stowed.
    Shipping LyondellBasell Icorene 1761 YEW 2171 LLDPE metallocene is typically shipped in moisture-resistant 25 kg PE bags or 500–1,000 kg FIBCs, on pallets, by truck or rail. It is non-hazardous, requires dry conditions, and should be kept away from direct sunlight and ignition sources. Store in a cool, dry, ventilated area.
    Storage Store LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers closed and palletized in original packaging to prevent moisture and contamination. Protect from prolonged elevated temperatures and UV exposure. Avoid strong oxidizers. Use good housekeeping and grounding/bonding for bulk handling. Follow local regulations and manufacturer recommendations.
    Shelf Life Shelf life is 24 months when stored in original, unopened packaging under dry, cool conditions, away from direct sunlight.
    Application of LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene

    Within the rotational moulding sector, Icorene 1761 YEW 2171 is classified as a metallocene-catalysed linear low density polyethylene powder whose narrow molecular weight distribution alters the relationship between peak internal air temperature, cooling rate, and low-temperature impact retention. Rheological control is verified by melt flow rate according to ISO 1133-1:2022 at 190 °C/2.16 kg, and the downstream scenarios below are limited to documented rotary moulding applications rather than extruded film or injection moulded packaging.

    When Icorene 1761 YEW 2171 is charged into a single-wall chemical storage tank mould, the first processing constraint is not melt flow stability but the retention of environmental stress crack resistance after wall thickness exceeds 6 mm. The formulation used in this sector typically consists of 100 parts of the neat powder, 0.05–0.15 parts of a hindered phenolic antioxidant, 0.20–0.50 parts of a high-molecular-weight HALS, and 1.0–2.5 parts of a UV-stabilised carbon black masterbatch where outdoor black tanks are specified. Industry compliance is anchored to EN 13575:2012, ASTM D1998-21, and NSF/ANSI 61 Section 4 for potable water contact when applicable. Downstream production uses a carousel or shuttle rotomoulding machine with a biaxial rotation ratio near 4:1 on the primary axis; the powder is sintered to a peak internal air temperature of 210–220 °C, held for a time determined by wall thickness, and then cooled by forced air before demoulding. A processing conflict arises when the internal air temperature is pushed above 220 °C to shorten oven residence time: impact strength and elongation degrade through oxidative chain scission even though the outer powder layer appears fully fused. Conversely, premature removal at below 200 °C leaves residual porosity and lowers ESCR measured per ASTM D1693-15e1. Finished products include vertical cylindrical chemical dosing tanks, sodium hypochlorite day tanks, and double-wall spill-containment basins without steel reinforcement. Published chemical compatibility data for this exact grade in concentrated oxidising media is limited, so EN 13575:2012 Annex B compatibility testing should be performed for each specific chemical concentration and service temperature.

    What changes when the same metallocene LLDPE is rotated into insulated food transport boxes?

    Compliance for direct food contact is not conferred by resin selection alone; it requires additive formulation discipline and migration control during processing. The relevant regulatory anchor is FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011, with the overall migration limit set at 10 mg/dm² under Annex II for most food simulants. The sector-recognised formulation for this grade is 100 parts powder, 0.05–0.10 parts of an acid neutraliser such as calcium stearate, 0.05–0.10 parts of a phenolic antioxidant, and 0.5–2.0 parts of a pigment masterbatch formulated exclusively from monomers and additives listed in the applicable food-contact regulation. Amine-based antistatic additives and unlisted secondary stabilisers are not used in this formulation because they are outside the positive list and can raise migration values in fatty-food simulants. Regrind addition is generally excluded in direct food contact unless the recyclate is fully traceable to the same grade and supported by migration verification. The downstream production process uses fabricated aluminium moulds with a semi-permanent mould-release system applied and cured to avoid contaminant transfer. A biaxial rotational moulding machine is operated at an oven set temperature of 280–300 °C, with the peak internal air temperature held within the supplier-specified envelope and the mould cooled in forced air before part extraction. Terminal finished products include insulated fish boxes, ice bins, food transport containers, and freezer storage bins where the narrow molecular weight distribution contributes to more uniform wall thickness across corners and rib intersections.

    Agricultural sprayer and fertiliser tanks are charged with the same metallocene LLDPE powder under a different risk profile: the service environment combines ultraviolet exposure, agrochemical surfactant stress cracking, and seasonal temperature cycling. Industry compliance in this segment is governed by EN 13575:2012 for static thermoplastic storage tanks, with chemical compatibility assessment performed according to ISO 16101:2004 for packaging and transport tanks when the tank carries hazardous preparations. The formulation addition ratio for outdoor agricultural service is 100 parts Icorene 1761 YEW 2171, 0.3–0.8 parts of a high-molecular-weight HALS, 0.05–0.15 parts of a hindered phenolic antioxidant, and 0.5–2.0 parts of a UV-stabilised pigment masterbatch matched to the final colour. For horizontal sprayer tanks, production commonly uses a drop-arm or rock-and-roll rotomoulding machine rather than a fixed carousel, because the long axis of the mould requires asymmetric heating and cooling control. The powder is sintered to a peak internal air temperature of 210–220 °C, followed by staged cooling with compressed air and intermittent water mist only after the part surface falls below 90 °C to reduce warpage. Terminal finished products include tractor-mounted sprayer tanks, tow-behind fertiliser hoppers, seed storage boxes, and rectangular chemical induction vessels with integrally moulded ribs and sump areas.

    Impact and weathering thresholds in rotomoulded playground components

    Loading of an aluminium playground-component mould with Icorene 1761 YEW 2171 around 20–30 °C avoids electrostatic clumping and improves powder flow into deep parting-line cavities. The governing standards for this downstream segment are EN 1176-1:2017 for playground equipment safety and ASTM F1487-21 for public-use playground equipment in North America; material-specific mechanical verification relies on ASTM D256-23 for notched Izod impact and ISO 4892-3:2016 for UV ageing. The formulation addition ratio is 100 parts powder, 1.0–3.0 parts of a pigmented UV masterbatch, 0.3–0.6 parts of HALS, and 0.05–0.15 parts of a phenolic antioxidant; mineral fillers are not used because they reduce low-temperature impact retention and increase notch sensitivity. Production is carried out on biaxial rotomoulding equipment with fabricated aluminium moulds, an oven set temperature of 280–300 °C, and a rotation ratio of 4:1 to distribute the powder across curved slide and tunnel sections. Peak internal air temperature is held to the lower end of the supplier-defined envelope to preserve surface gloss and limit differential shrinkage in parts with wall-thickness transitions from 4 mm to 10 mm. Finished products include straight and helical slide segments, tunnel sections, climbing panels, and independently certified spring rocker seats.

    Compliance and formulation checklist by downstream segment
    SegmentPrimary compliance anchorFormulation addition ratioProcessing window
    Chemical storage tanksEN 13575:2012, ASTM D1998-21100 parts resin, 0.05–0.15 parts AO, 0.20–0.50 parts HALS, 1.0–2.5 parts carbon black masterbatchPIAT 210–220 °C, rotation ratio 4:1
    Insulated food transport boxesFDA 21 CFR 177.1520, EU No 10/2011100 parts resin, 0.05–0.10 parts acid neutraliser, 0.05–0.10 parts AO, 0.5–2.0 parts compliant pigment masterbatchOven set 280–300 °C, forced-air cooling to below demoulding temperature
    Agricultural sprayer and fertiliser tanksEN 13575:2012, ISO 16101:2004100 parts resin, 0.3–0.8 parts HALS, 0.05–0.15 parts AO, 0.5–2.0 parts pigment masterbatchPIAT 210–220 °C, post-cooling water mist below 90 °C
    Rotomoulded playground componentsEN 1176-1:2017, ASTM F1487-21100 parts resin, 1.0–3.0 parts UV masterbatch, 0.3–0.6 parts HALS, 0.05–0.15 parts AOOven set 280–300 °C, wall thickness 4–10 mm
    Marine flotation unitsISO 4892-3:2016, ASTM D256-23100 parts resin, 0.3–0.8 parts HALS, 0.1–0.3 parts UV absorber, 1.0–2.0 parts white pigment masterbatchPre-dry powder at 60 °C for 1–2 h if RH exceeds 70%, PIAT 210–220 °C
    Material-handling pallets and process binsISO 8611-1:2011, ASTM D638-14100 parts resin, 0.05–0.15 parts AO, 0.2–0.5 parts HALS, 0.5–1.5 parts carbon black masterbatchFloor section thickness above 8 mm, cooling rate controlled to avoid sink marks

    If the mould is charged without pre-drying in a coastal plant above 70% relative humidity

    In coastal plants where relative humidity regularly exceeds 70%, condensation on the powder surface becomes a process defect generator for marine flotation unit production. The resin does not absorb water as a bulk polymer, but surface moisture is carried into the mould and vaporises during oven residence, leaving pinholes that violate the wall integrity requirements of closed-cell foam-filled parts. Pre-drying at 60 °C for 1–2 h in a desiccant hopper dryer is therefore specified before charging. The applicable durability verification for this segment is ISO 4892-3:2016 for accelerated weathering and ASTM D256-23 for low-temperature notched impact; there is no single global product standard that covers all marine buoy designs, so the original equipment purchase specification normally fixes wall thickness, impact energy, and UV retention limits. The formulation addition ratio is 100 parts Icorene 1761 YEW 2171, 0.3–0.8 parts of a high-molecular-weight HALS, 0.1–0.3 parts of a UV absorber, 1.0–2.0 parts of a white pigment masterbatch, and 0.05–0.15 parts of a phenolic antioxidant. Rotational moulding is performed with a wall thickness of 8–12 mm, a biaxial rotation ratio near 4:1, and a peak internal air temperature of 210–220 °C; after cooling and demoulding, the shell is filled with a closed-cell polyurethane foam to provide buoyancy even if the outer wall is punctured. Terminal finished products include mooring buoys, foam-filled fenders, pontoon floats, and channel marker shells with integrally moulded lifting eyes.

    Material-handling pallets and modular process bins represent the highest-abrasion downstream route for this grade, where the failure mode shifts from chemical attack to repeated impact, point loading, and warehouse racking deflection. The governing mechanical compliance standard is ISO 8611-1:2011 for flat pallet test methods, supplemented by ASTM D638-14 for tensile properties and ASTM D790-17 for flexural modulus. The formulation addition ratio for this segment is 100 parts powder, 0.05–0.15 parts of a hindered phenolic antioxidant, 0.2–0.5 parts of HALS for outdoor storage, and 0.5–1.5 parts of a carbon black masterbatch where warehouse UV exposure is intermittent. Production uses a shuttle-type rotomoulding machine with fabricated steel or aluminium moulds; the floor section is designed above 8 mm to resist pallet-jack wheel loading, and the cooling rate is controlled with forced air to prevent sink marks over internal steel tube inserts. A process conflict occurs when the wall thickness is increased without extending oven residence time: the densified outer layer insulates the inner powder bed, and the peak internal air temperature must still reach 210–220 °C or the inner surface retains a powdery, low-strength layer. Finished products include process pallets, modular bulk bins, dump hoppers, and flame-retardant-free cleanroom totes where metal surfaces cannot be introduced.

    Free Quote

    Competitive LyondellBasell Icorene 1761 YEW 2171 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 YEW 2171 is a metallocene-catalysed linear low density polyethylene supplied as pelletized resin for blown film extrusion and selected cast film structures. The grade designation couples a base resin, Icorene 1761, with an additive package identified by YEW 2171; the latter typically includes stabilisation components and may incorporate slip or antiblock additions depending on the packaging configuration. The base resin is specified in the supplier literature with a nominal density of 0.918 g/cm³ under ISO 1183-1 and a nominal melt flow rate of 1.0 g/10 min under ISO 1133-1:2022 at 190°C and 2.16 kg load. The product is used in coextruded sealant webs, high-speed form-fill-seal packaging, lamination films, and overwrap structures where low seal initiation temperature and optical uniformity of thin gauges are required.

    The metallocene catalyst system produces a narrow molecular weight distribution and more homogeneous comonomer placement than conventionally polymerised linear low density polyethylene. This structural feature affects crystallisation kinetics, optical haze, and the heat-seal response. The grade is positioned relative to Ziegler-Natta butene LLDPE and high-pressure low density polyethylene primarily through processing latitude and the balance between hot tack and seal strength on high-speed packaging lines.

    What Distinguishes the Sealing and Optics Profile from Conventional C4 LLDPE?

    The primary practical difference appears in the seal initiation window. In coextruded webs where Icorene 1761 YEW 2171 is used as the sealant layer, heat-seal strength is typically measurable at seal temperatures 8°C to 15°C below those required for conventional butene LLDPE of similar density, depending on film gauge, seal dwell, and jaw pressure. This shift is consistent with the narrower melting endotherm and lower fraction of high-melting crystalline species generated by uniform comonomer distribution. Seal strength should be measured under ASTM F88/F88M-21; hot tack is evaluated under ASTM F1921-18. Because the resin has a lower extractable fraction than some Ziegler-Natta grades, organoleptic performance in food packaging is favoured, but the film structure and any post-extrusion lamination or coating step determine the final migration profile.

    Optical haze differences are similarly linked to morphology. A 40 µm blown film from this resin class commonly shows haze below 5% when measured under ISO 14782, but this value is highly dependent on die gap, frost-line height, melt temperature, and surface roughness. Comparisons between products must therefore report processing conditions alongside the optical data. The narrow molecular weight distribution also reduces the amount of high molecular weight tail that can stabilise large bubbles and contributes to a more Newtonian shear-thinning response in the die. This has consequences for extrusion output and bubble stability.

    Because metallocene LLDPE generally exhibits lower melt strength and less shear-thinning than high-pressure LDPE, stable bubble formation with Icorene 1761 YEW 2171 depends on die gap, blow-up ratio, frost-line height, and cooling air control. On a 200 mm three-layer blown-film die operating with dual-lip air rings, the resin is typically processed in the skin layer at melt temperatures of 210°C to 230°C, while the core may be a high-pressure LDPE to maintain bubble stability. Die gaps between 1.2 mm and 2.0 mm are common, but the narrow molecular weight distribution can produce melt fracture at higher shear rates if the die is undersized; die lip polishing and application of fluoropolymer-based polymer processing aids are used when surface defects occur. The recommended extruder configuration includes a barrier screw with L/D of at least 24:1, screen pack with 60/100/60 mesh layers, and downward or upward haul-off depending on film gauge. Blow-up ratio is normally maintained between 2.0:1 and 2.8:1. Frost-line height is adjusted to avoid both excessive crystallisation before orientation and excessive MD shrinkage in the collapsed film. Process operators report that higher internal bubble cooling can raise output but narrows the stable processing corridor if the bubble is not adequately supported by cage geometry.

    Regulatory, Food-Contact and Antioxidant Package Boundaries

    Compliance with global packaging and electrical/electronics directives is governed by the exact formulation represented by the suffix YEW 2171. The base polyolefin is generally considered suitable for food-contact applications under 21 CFR 177.1520, but the final article must be tested for overall migration under Regulation (EU) No 10/2011, where the overall migration limit is 10 mg/dm². Additive package components may have specific migration limits; the converter must verify that the final film meets any applicable SML. REACH registration status applies to the substance or mixture as supplied; downstream articles are outside the scope of REACH registration but SVHC content below 0.1% w/w can be documented through supplier declarations. RoHS Directive 2011/65/EU Annex II restrictions apply only to electrical/electronic equipment, but the declaration for the grade usually confirms absence of cadmium, lead, mercury, hexavalent chromium, PBB and PBDE at the homogeneous material level. The product should not be used in medical implant applications without additional specification and validation under ISO 10993-1.

    Regulatory assessment boundaries for Icorene 1761 YEW 2171 film applications
    Regulation or standard Scope Typical exposure or limit Verification boundary
    FDA 21 CFR 177.1520 Olefin polymers for food contact Conditions A through H as designated by end use Final article migration testing
    EU 10/2011 Plastic materials and articles 10 mg/dm² overall migration Specific migration limits for additives
    REACH Substance and SVHC 0.1% w/w SVHC threshold Supplier declaration or article notification
    RoHS 2011/65/EU Electrical/electronic equipment Annex II restricted substances Homogeneous material analytical screening

    Storage and handling boundaries for Icorene 1761 YEW 2171 are set by the additive package and the need to avoid surface condensation after cold storage. Polyolefin pellets are not hygroscopic in the manner of polyamides or PET, but condensation on resin surfaces can introduce water into the melt and generate surface defects in monolayer film. Pellets should be allowed to reach ambient temperature in unopened packaging before feeding to a hopper. Long-term ultraviolet exposure should be avoided because the stabilisation system is not formulated for outdoor storage of the resin, even though the final film may exhibit acceptable weathering only after additional UV stabiliser addition. Antioxidant and process stabilisers in YEW 2171 are selected to protect melt processing at typical film extruder temperatures; however, long-term heat ageing should be evaluated under ISO 188 where service temperatures exceed 60°C.

    When Replacing High-Pressure LDPE in Sealant Layers or Downgauging Structures

    In coextruded structures where a blown film line currently uses high-pressure LDPE or traditional C4 LLDPE as the sealant web, Icorene 1761 YEW 2171 may permit a reduction in sealant layer gauge because the seal strength response is governed by the sealant surface melting and crystallisation rather than bulk stiffness. In trials on high-speed vertical form-fill-seal equipment with seal jaw temperature profiles between 110°C and 150°C, metallocene LLDPE sealant layers have maintained seal integrity at gauge reductions of 20% to 30% relative to conventional C4 LLDPE, but published data for this specific grade configuration is limited. The most sensitive defects are not low average seal strength but local cold-seal tail failures at package corners where film folding induces stress concentration. Therefore seal temperature mapping across the jaw and measurement of hot tack under ASTM F1921-18 at 0.5 s seal dwell are more informative than average seal strength alone. When downgauging, tensile impact in both machine and transverse directions should be monitored using ISO 8256 or ASTM D1822, while tear resistance is measured using ISO 6383-1. Because the narrow comonomer distribution reduces the crystalline fraction, stiffness falls more rapidly with gauge reduction; converter should verify that the package openability and deadfold are not controlled solely by the sealant layer.

    Replacement of high-pressure LDPE in a skin layer is not a drop-in substitution. LDPE contributes bubble stability, melt strength, and higher autoclave clarity in some structures. If Icorene 1761 YEW 2171 is used at 100% in a skin layer, the bubble may require reduced screw speed, higher frost-line residence time, or a narrower die gap to avoid instability. A practical approach is to blend the metallocene LLDPE with 10% to 20% high-pressure LDPE to preserve bubble stability while retaining most of the lower seal initiation and optical benefit. The ratio should be verified by pilot runs because excessive LDPE can reintroduce higher seal initiation and reduce the downgauging advantage.

    Crystallisation Proceeds Through a Narrow Lamellar Thickness Distribution

    Differential scanning calorimetry under ISO 11357-3 on the base resin identifies a narrower melting endotherm than conventional C4 LLDPE; the peak melting temperature is commonly reported near 122°C for the 0.918 g/cm³ density class. The crystallisation exotherm occurs at a lower temperature because uniform short-chain branching impedes lamellar thickening. A consequence of the lower lamellar thickness distribution is that the film surface reaches a tacky seal state at lower temperature, but the absence of a high-temperature crystalline tail also reduces the upper hot-tack plateau. For packaging requiring high-temperature dimensional stability, this resin is therefore not a direct substitute for homopolymer polypropylene or high-density polyethylene; the continuous use temperature should be limited to service conditions typical of polyolefin packaging. The optical haze of a 40 µm blown film measured under ISO 14782 is influenced by surface roughness and die-lip build-up. The lower haze and higher gloss of metallocene LLDPE arise from reduced spherulite size and less surface scattering, not from polymer refractive index. Waxy and particulate die-lip build-up can reverse this advantage; periodic purging with a dedicated purging compound or high-pressure LDPE transition is recommended on long runs.

    Published data for specialised configurations, including high-stalk extrusion of 10 µm webs on lines exceeding 60 m/min, is limited. Grade-specific mechanical values should be taken from the LyondellBasell technical data sheet for Icorene 1761 YEW 2171 rather than extrapolated from other metallocene LLDPE grades. Processing windows established on one line may not transfer directly to another because of differences in air ring design, die geometry, and haul-off configuration.

    Top