| HS Code | 495724 |
| Density | 0.917 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 119 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 50 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 500 g |
| Elmendorf Tear Strength | 200 g |
| Haze | 6% |
| Gloss | 80% |
| Seal Initiation Temperature | 95 °C |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 1761 YEW 2141 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 YEW 2141 is supplied in 25 kg paper bags, palletized and stretch-wrapped, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg PE bags, floor-loaded, approximately 20 MT net; securely stacked and lashed for export shipment. |
| Shipping | Typically shipped as non-hazardous, free-flowing polyethylene pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Store in a dry, clean, ventilated area away from heat, sunlight, and moisture. No special UN transport classification required; protect from contamination and static buildup, following local regulations. |
| Storage | Store LyondellBasell Icorene 1761 YEW 2141 Polyethylene in a cool, dry, well-ventilated area using original closed containers, off the floor. Keep away from direct sunlight, heat, ignition sources, moisture, and strong oxidizers. Prevent contamination and dust generation. Store at ambient temperature, maintain good housekeeping, and follow the manufacturer’s Safety Data Sheet. Use appropriate PPE when handling. Avoid prolonged inhalation of dust. |
| Shelf Life | Typically two years if stored unopened in dry, cool conditions, away from direct sunlight; confirm exact shelf life with supplier. |
LyondellBasell Icorene 1761 YEW 2141, a metallocene-catalyzed linear low-density polyethylene, is placed at the sealant layer of coextruded blown film structures for dry food, frozen goods, and medical form-fill-seal packaging. In a standard 3-layer A/B/C die configuration, the seal layer is processed at a melt temperature of 190–230 °C and a die gap between 1.8 mm and 2.5 mm. A blow-up ratio of 2.0:1 to 3.0:1 is maintained to balance transverse direction tear and machine direction stiffness. Because the grade exhibits the narrow molecular weight distribution characteristic of mLLDPE, die lip shear stress can exceed the critical value for sharkskin at high output; adding 15–25 wt% of an autoclave LDPE to the seal layer is common industrial practice to raise melt strength and delay melt fracture. The regulatory basis for food contact is FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm². Heat seal initiation is measured on a laboratory gradient heat sealer with a jaw pressure of 0.35–0.50 MPa and a dwell time of 1 s, with seal strength reported under ASTM F88/F88M and hot tack under ASTM F1921. The typical mLLDPE seal layer lowers seal initiation temperature by 5–15 °C versus Ziegler-Natta LLDPE at equivalent density, which determines substitution in high-speed vertical form-fill-seal operations. End-product structures include metallized BOPP/BOPET laminates, frozen-food pouches, and lidding for dairy cups.
| Standard/Code | Condition | Limit/Criteria |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer migration, conditions A–H per polymer type and food simulant | No detectable transfer above applicable food-type threshold |
| EU 10/2011 | Overall migration, aqueous, acidic, alcoholic, fatty simulants | 10 mg/dm² |
| REACH Annex XVII | Restricted PAHs, phthalates, heavy metals | Article-specific restricted substance thresholds apply |
| CONEG | Pb, Cd, Hg, Cr VI in packaging | 100 ppm total heavy metals |
In dry-food applications below 40 °C, the low specific migration of primary antioxidants is controlled by the resin formulation; converters should request a Declaration of Compliance from the supplier for each lot. Pre-drying is not normally required at ambient relative humidity below 60%. When bags are stored in unconditioned warehouses, surface moisture must be removed with a desiccant hopper at 70 °C for 2 h to prevent film specks and steam-induced bubble defects.
In heavy-duty sacks and flexible intermediate bulk container liners, the mechanical specification is dominated by Elmendorf tear propagation and dart impact rather than optical clarity. Icorene 1761 YEW 2141 is incorporated into the core layer of a 3-layer blown film at a total thickness between 100 µm and 200 µm. The metallocene resin provides a narrower inter-molecular comonomer distribution; this transfers into higher impact retention at low temperature when compared with a conventional butene-based LLDPE at the same melt index. However, running the grade at 100% on a high-output line with a grooved feed extruder of L/D 30:1 and a die diameter of 250 mm often produces bubble instability and gauge variation at a frost line height above 8 die diameters. The processing solution is a blend of 15–25 wt% branched LDPE, which raises elongational viscosity and reduces draw resonance in the bubble. A polymer processing aid at 200–800 ppm reduces die lip build-up and shear-induced sharkskin. Dart impact is measured under ASTM D1709 Method A, tear propagation under ISO 6383-2, and puncture resistance under ISO 7765-2. Weld strength of the final sack is checked under ASTM F88/F88M on the heat-sealed seam after converting. The mLLDPE/LDPE blend tolerates calcium carbonate filler in the outer layer up to 5 wt% without sacrificing seal strength, but higher filler loadings produce ash residues on the sealing jaw at 180–200 °C and should be avoided in food-contact constructions. Published data for Icorene 1761 YEW 2141 in this specific single-layer configuration are limited; the above processing ranges represent industrial practice for metallocene LLDPE heavy-duty sack film. End products include liners for FIBCs, shipping sacks for polymer pellets, and moisture-proof liners for paper flour sacks.
For agricultural silage wrap and bale film, the grade appears in thin-gauge blown structures where puncture by stalk ends and abrasion against the baler chamber are the primary failure modes. A typical film thickness for silage wrap is 30–80 µm, blown at a BUR of 2.8:1 to 3.2:1 to increase machine direction tear resistance under field tension. The metallocene-catalyzed comonomer placement improves dart drop retention at thickness below 50 µm, which is relevant because the film is stretched around a bale under high tension and must resist puncture from alfalfa or maize stalks. UV stabilization is mandatory: a hindered amine light stabilizer at 0.15–0.25 wt% and a UV absorber at 0.05–0.10 wt% are incorporated into the outer layer; the stabilizer package is evaluated by ISO 4892-2 Xenon arc exposure with mechanical property retention after 1,000 h. Oxygen transmission rate is measured under ASTM D3985; for a 50 µm monolayer mLLDPE, published OTR values remain above 1,000 cm³/(m²·d·bar), which is consistent with silage respiration but unsuitable for high-barrier food applications. Processing temperatures above 230 °C can deactivate selected HALS stabilizers and generate gels that appear as specks in the film; the extruder profile should therefore be capped at 220 °C in the metering zone. End products include round bale wrap, silage bags, and greenhouse side curtains where the film must survive high UV and mechanical loading.
Cast stretch hood lines processing Icorene 1761 YEW 2141 in the core layers of 3-layer and 5-layer film impose pre-stretch ratios between 120% and 200% as the film is drawn over the pallet edges. The metallocene resin limits localized thinning at the pallet corners because of a more homogeneous tie-molecule population along the stress direction. The cast line runs with a chill roll temperature of 10–15 °C and a line speed above 300 m/min; low roll temperature is required to quench film crystallinity and preserve elongation at break measured under ASTM D882. The outer cling layer contains polyisobutylene at 1–4 wt%, which controls unwind force but can increase blocking if the roll is stored above 35 °C. The core layer may be a blend of mLLDPE with 10–20 wt% LDPE to reduce neck-in at the die and stabilize the cast web. Puncture resistance is reported under ISO 7765-2, and tear propagation is measured under ISO 6383-2. The main operational boundary is dust contamination from the warehouse: any particulate from shrink wrap debris or wood pallet splinters deposits on the film surface and creates a point stress raiser during pre-stretch. End uses include stretch hood, top-sheet films, and automated pallet wrapping for construction materials and beverage multipacks.
In extrusion coating and lamination, the resin is seldom used as the sole coating polymer because the elongational melt strength of a narrow-MWD mLLDPE is lower than that of an autoclave LDPE. Instead, Icorene 1761 YEW 2141 is blended at 40–60 wt% with LDPE for coating paper, paperboard, and oriented films; the mLLDPE fraction reduces seal initiation temperature and improves heat seal strength in the final laminate. The coating die is set with an air gap of 150–250 mm and a melt temperature of 270–300 °C; higher temperatures are avoided because they shift the oxidative degradation pathway and produce acrid smoke at the die. Draw-down speed is typically above 150 m/min, and neck-in is monitored as the reduction in coating width from die width. Adhesion to primed BOPP or BOPET is reported as T-peel strength under ASTM D1876; when aluminium foil is the substrate, the foil is first corona-treated to a dyne level above 40 mN/m. The seal layer is evaluated for hot tack under ASTM F1921 and for seal strength under ASTM F88/F88M. A higher mLLDPE fraction above 60 wt% increases neck-in and can require a larger coating die width; a lower fraction below 40 wt% loses the seal initiation benefit. End laminates include sachet stock, lidding membranes, and medical packaging where seal integrity after ethylene oxide sterilization is verified by dye penetration per ASTM F3039.
| Variable | Set Range | Measurement/Control Method |
|---|---|---|
| Coating melt temperature | 270–300 °C | Infrared melt thermocouple at die adaptor |
| Air gap | 150–250 mm | Manual gauge, fixed geometry |
| Line speed | above 150 m/min | Tachometer on chill roll |
| mLLDPE fraction | 40–60 wt% | Gravimetric hopper blend |
| Adhesion test | peel under ASTM D1876 | T-peel tensiometer |
When air cushion webs are inflated on demand at pack stations, the seal layer is required to hold an internal air pressure of 0.02–0.06 MPa for at least 48 h without creep failure. Icorene 1761 YEW 2141 is suitable as the seal layer of coextruded air pillow film because the metallocene resin produces tough low-temperature seals on high-speed rotary sealers. The blown film is typically produced at a thickness of 20–50 µm with a blow-up ratio of 2.5:1 to 3.5:1; high blow-up ratio increases transverse-direction elongation and reduces the tendency to burst at the side weld. The outer HDPE or LDPE skin supplies stiffness, while the mLLDPE seal layer is processed with a melt temperature of 190–220 °C; exceeding 240 °C generates oxidative gels that increase the seal failure rate. Film-to-film seal strength is measured under ASTM F88/F88M, and creep retention is evaluated by internal pressure decay rather than a published universal standard; published data for this specific Icorene configuration in air cushion film is limited. The formulation should avoid high loadings of migratory slip agents above 1,000 ppm because the slip additive transfers to the seal interface and reduces retained air pressure. End products include protective air pillows, void-fill tubes, and anti-corrosion air cushion liners where the mLLDPE sealant layer is approved for direct contact with metal parts under industrial use.
Competitive LyondellBasell Icorene 1761 YEW 2141 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 YEW 2141 is a metallocene-catalyzed linear low density polyethylene supplied as free-flowing pellets. The base-resin designation Icorene 1761 identifies a melt-index and density combination within the Icorene metallocene product family; the suffix YEW 2141 denotes a specific color, additive, or product-form configuration. In public material summaries, the 1761 series is reported with a nominal density of 0.918 g/cm³ and a melt mass-flow rate of 1.0 g/10 min at 190 °C under a 2.16 kg load, as determined under ASTM D1238-20 or ISO 1133-1:2022. These values place the product among moderate-melt-index metallocene LLDPE resins used in blown film, cast film, sealant layers, and flexible packaging structures. Single-site metallocene catalysis yields a narrower molecular weight distribution and more uniform short-chain branching than conventional Ziegler-Natta linear low density polyethylene. This structural control generally reduces amorphous-phase heterogeneity, which can improve optical quality, dart impact, and low-temperature seal performance. Because the YEW 2141 suffix can shift apparent density or melt flow relative to the natural base resin, the manufacturer’s certificate of analysis should be reviewed before specifying the grade for production tooling.
The values below are compiled from publicly accessible material-data summaries for the Icorene 1761 series and are not release limits. Grade-specific data for the YEW 2141 suffix may be limited; if the suffix includes a pigment or processing package, apparent density and melt-flow results can shift relative to the natural base resin. Obtain the manufacturer’s technical datasheet for lot-to-lot control limits.
| Property | Test method | Representative value |
|---|---|---|
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238-20 | 1.0 g/10 min nominal |
| Density at 23 °C | ISO 1183-1:2019 / ASTM D1505-18 | 0.918 g/cm³ nominal |
| Melting peak by differential scanning calorimetry | ISO 11357-3:2018 | 118–123 °C |
| Vicat softening temperature A50 | ISO 306:2022 | 96–104 °C |
| Tensile stress at yield | ISO 527-2:2012 / ASTM D638-14 | 8.0–10.0 MPa |
| Tensile stress at break | ISO 527-2:2012 / ASTM D638-14 | 30–40 MPa |
| Nominal tensile strain at break | ISO 527-2:2012 / ASTM D638-14 | 600–700% |
| Flexural modulus | ISO 178:2019 / ASTM D790-17 | 250–300 MPa |
The 1.0 g/10 min melt mass-flow rate positions the grade below high-flow injection-molding LLDPEs and above high-molecular-weight film grades. This makes it practical for blown film where bubble stability and dart impact are more critical than thin-wall filling. The melting peak near 118–123 °C indicates semicrystalline behavior; the resin retains solid-state modulus at normal packaging temperatures but softens substantially near the Vicat range.
In blown film conversion, the resin does not require predrying under normal indoor storage conditions. If condensation occurs after cold storage, a desiccant hopper at 60 °C for 2 h removes surface moisture and reduces splay. A typical barrel profile from 180 °C to 220 °C and a die temperature of 200–220 °C keep the melt temperature below 240 °C. The narrow molecular weight distribution of mLLDPE results in less shear thinning than ZN LLDPE; head pressure and motor load may therefore be higher at the same screw speed. On a 60 mm single-screw extruder with 30:1 L/D, head pressure may be 10–15% higher than that of a comparable-melt-index ZN LLDPE. A die gap of 1.5–2.5 mm, a blow-up ratio of 2:1 to 3:1, and a frost line height of 4–8 die diameters improve bubble stability. Above approximately 500 s⁻¹ wall shear, sharkskin may appear; raising the die temperature or adding a fluoropolymer processing aid at 500–1000 mg/kg is an established industrial response. When the grade is compounded with a 5% white masterbatch on a 40:1 L/D co-rotating twin-screw extruder, specific energy input may rise by 5–8%; published data for this exact configuration is limited, so pilot-scale verification of torque, melt pressure, and gel count should be performed before production.
Capillary and parallel-plate rheometry show that the melt-flow ratio I21/I2 is the practical field indicator for the narrower molecular weight distribution. For mLLDPE in this melt-index class, I21/I2 is often 16–18, whereas ZN LLDPE may be 25–30. The lower ratio indicates less shear thinning and a narrower processing window for high-shear extrusion. At 190 °C, zero-shear viscosity for a 1.0 g/10 min mLLDPE is generally on the order of 3000–5000 Pa·s; below 100 s⁻¹, viscosity remains sufficiently high to support bubble formation, while above 100 s⁻¹ the reduction is less pronounced than in ZN LLDPE. In cast film, a chill-roll temperature of 20–40 °C and an air-knife position within 10–20 mm of the roll support clarity and glide. In injection molding, although the melt index is low for complex thin-wall flow, the resin can be used for thick-walled closures or containers with melt temperatures of 200–230 °C and mold temperatures of 15–40 °C; published data for this specific configuration is limited, so spiral-flow evaluations should be conducted if flow length exceeds 100 mm at a wall thickness below 1.5 mm.
In flexible packaging, the main performance variables are seal initiation temperature, hot-tack strength, dart impact, and optics. Metallocene LLDPE with a density near 0.918 g/cm³ typically initiates heat seals at 85–95 °C and reaches plateau seal strength between 110 °C and 130 °C when measured according to ASTM F88/F88M-21. Hot-tack strength under ASTM F1921-20 is generally higher than that of ZN LLDPE at equivalent density because the narrow comonomer distribution yields a sharper melting and crystallization profile. Monolayer film of 25 µm thickness from the 1761 series may show dart drop impact values in the range of 120–180 g under ASTM D1709-16 Method A, while Elmendorf tear performance varies with orientation. Haze below 10% and 45° gloss above 60% under ASTM D1003-13 and ASTM D2457-13 are practical targets for this class, but actual values depend on frost line control, screw-induced gel formation, and cooling uniformity. In coextruded laminations with BOPET or BOPP, the grade may function as a sealant layer; conversion trials must confirm interlayer adhesion and seal-through-contamination performance because corona treatment level and additive bloom can alter the result.
At equal density and melt index, metallocene LLDPE differs from ZN LLDPE in molecular weight distribution and comonomer incorporation. The polydispersity index for mLLDPE is commonly near 2.0–3.0, while ZN LLDPE is often 3.5–5.0. The narrower distribution lowers the concentration of very high molecular weight chains that provide shear thinning and very low molecular weight chains that may contribute to extractables and organoleptic defects. Compared with high-pressure LDPE, the mLLDPE has no significant long-chain branching; therefore, melt strength and extensional strain-hardening are lower, and bubble stability in blown film is more sensitive to cooling air and frost line position. Compared with higher-density metallocene LLDPE grades at 0.930–0.940 g/cm³, Icorene 1761 YEW 2141 has lower flexural modulus and lower Vicat softening, but typically higher elongation at break and lower seal initiation temperature. Compared with lower-density plastomers below 0.905 g/cm³, the grade has greater crystallinity, higher modulus, and higher thermal resistance, while retaining sufficient toughness for many flexible packaging uses. Processors should not expect the drawdown behavior of LDPE; cast film and extrusion coating operations may require motor and die-pressure adjustments.
Food-contact status is application-specific. The base resin may be produced to meet FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation 10/2011 when manufactured under appropriate Good Manufacturing Practice. The YEW 2141 suffix must be verified separately because pigments, slip agents, or processing aids may carry their own exposure limits. The resin is not inherently UV-stabilized; for outdoor service, a hindered amine light stabilizer at 0.2–0.5% and an appropriate UV absorber are required to preserve impact retention under ISO 4892-2:2013 weathering. Regrind addition up to 30% is commonly tolerated in blown film if melt-flow and gel counts are monitored; above this level, oxidative induction time under ISO 11357-6:2018 may decline and film appearance may degrade. Avoid melt blending with incompatible high-molecular-weight polypropylene at levels above 10% because phase separation reduces dart impact and seal integrity. The upper continuous service temperature for unfilled mLLDPE of this density is generally below 70 °C under sustained load; creep resistance should be evaluated under ISO 899-1:2017 for load-bearing parts.
| Regulation | Scope | Verification condition |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymers intended for food contact | Compliance subject to use conditions and additive constraints |
| EU Regulation 10/2011 | Plastic materials and articles in contact with food | Overall migration limit and specific migration limits apply |
| REACH EC 1907/2006 | Registration and substances of very high concern | Substance concentration in article below 0.1% by weight where required |
| RoHS Directive 2011/65/EU | Heavy metals and restricted substances in electrical and electronic equipment | Cadmium 0.01%, lead 0.1%, mercury 0.1%, hexavalent chromium 0.1% |