| HS Code | 372865 |
| Density | 0.918 g/cm³ |
| Melt Flow Rate | 1.0 g/10 min (190°C/2.16 kg) |
| Melting Point | 115 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 9.0 MPa |
| Tensile Strength At Break | 30.0 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Dart Drop Impact | 200 g |
| Haze | 5% |
| Gloss | 80% |
| Coefficient Of Friction | 0.20 |
| Color | White |
As an accredited LyondellBasell Icorene 1761 WHI 1400 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg bags, palletized and stretch-wrapped; LyondellBasell Icorene 1761 WHI 1400 Linear Low Density Metallocene Polyethylene. |
| Container Loading (20′ FCL) | Standard 20′ FCL loading of LyondellBasell Icorene 1761 WHI 1400 metallocene linear low density polyethylene, palletized and secured for ocean transport. |
| Shipping | LyondellBasell Icorene 1761 WHI 1400 Polyethylene, Linear Low Density, Metallocene is shipped as non-hazardous thermoplastic resin pellets. Not regulated as dangerous goods for DOT/IMDG/IATA/ADR. Typically packaged in 25 kg bags, octabins, or bulk trucks/railcars. Store dry, away from ignition sources, moisture, and contaminants. Use standard freight; avoid puncturing bags and environmental release. |
| Storage | Store LyondellBasell Icorene 1761 WHI 1400 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep original packaging closed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain normal ambient temperatures and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months under recommended storage in original, unopened packaging; keep cool, dry, away from direct sunlight. |
The transformation of Icorene 1761 WHI 1400 from compacted rotational-moulding powder into a homogeneous potable-water tank wall is governed by peak internal air temperature PIAT, not by oven set point alone. In three-arm carousel machines with swing radii from 2.0 m to 3.5 m, heating is generally run at oven temperatures of 285 °C to 300 °C until internal air reaches 190 °C to 205 °C. Below approximately 180 °C, partially sintered particles persist as pinholes at weld lines and undercut ribs; above 210 °C, oxidative degradation accelerates, producing yellowing and measurable loss of Charpy notched impact strength under ISO 179-1:2010. The narrow molecular weight distribution associated with metallocene catalysis shortens the sintering plateau relative to conventional Ziegler-Natta LLDPE, which is why production-scale operators track real-time internal air temperature with Rotolog or equivalent data-logging probes and terminate the heating cycle as soon as the lower threshold is crossed at all probe locations. Potable-water contact compliance is evaluated under NSF/ANSI 61-2023 Section 4 and AS/NZS 4020:2018; formulations intended for EU markets must also satisfy organoleptic and specific migration requirements of Regulation (EU) No 10/2011 as amended. Typical dry-blend additions remain lean: 0.15 wt% to 0.30 wt% of a hindered phenolic antioxidant masterbatch and 0.25 wt% to 0.50 wt% of a high-molecular-weight HALS UV stabiliser concentrate. The carrier resin for these masterbatches should itself be metallocene LLDPE to avoid differential melt viscosities that generate surface pitting. Cooling after oven exit is controlled to 6 °C/min to 10 °C/min in the recrystallisation window between 120 °C and 90 °C; faster air or mist cooling increases crystallinity but raises warpage in flat side panels, while excessively slow cooling improves impact but extends cycle time on multi-arm carousels. Terminal products in this segment include 500 L to 30,000 L vertical and horizontal potable-water storage tanks, distribution troughs, and rainwater harvesting cisterns with wall thicknesses from 4 mm to 12 mm depending on hydrostatic head and installation depth.
In agricultural sprayer and fertiliser tank production, the controlling material property is environmental stress-cracking resistance ESCR, typically reported under ASTM D1693-21 Method B in 10% Igepal CO-630 solution, because tanks are exposed to organic acids, ester solvents, and high-pH cleaners at intermittent temperatures up to 45 °C. Icorene 1761 WHI 1400 is processed with wall thicknesses of 4 mm to 8 mm for 600 L to 5,000 L sprayer tanks, induction hoppers, and rinse-water containment units. Metallic inserts are preheated to 120 °C before mould charging to prevent localised cold spots at threaded ports. Oven settings on shuttle machines are generally 290 °C to 310 °C, with a peak internal air temperature of 200 °C to 210 °C held for 3 min to 5 min to densify outer skins. Chemical storage compliance is evaluated under EN 13575:2012 for static thermoplastic tanks and, when the tank is used for transport of dangerous goods, under ADR 6.8.2.1.13 with appropriate UN packaging type testing. The powder is dry-blended rather than melt-compounded; concentrate loadings are kept below 2.5 wt% for colour and below 0.8 wt% for antistatic additives, because higher additions of low-viscosity carrier resins create localised plasticisation and reduce ESCR at moulded-in thread bosses. Field teardowns of cracked sprayer tanks repeatedly show crack initiation at internal air-fitting bosses where wall thickness dropped below 3.2 mm; increasing local thickness by 1.5 mm and slowing cooling to 7 °C/min resolved the failure mode without changing resin selection. Fabricators also report that powder stored at relative humidity above 70% entrains surface moisture that causes microbubbles in the outer skin, so pre-drying at 70 °C for 2 h is required before charging in tropical plant environments. Terminal products include side-mounted saddle tanks, front-mounted spray tanks, chem-farm batch mixers, and secondary containment basins for agricultural chemical transfer stations.
| Application scenario | Standard or regulation | Test method or clause | Typical acceptance condition |
|---|---|---|---|
| Potable water tanks | NSF/ANSI 61-2023 | Section 4 water contact | Maximum contaminant concentrations per standard |
| Potable water tanks | AS/NZS 4020:2018 | Full battery | No significant taste, odour, or cytotoxicity |
| Agricultural chemical tanks | EN 13575:2012 | Static thermoplastic tank requirements | Hydrostatic and ESCR verification per standard |
| Marine floats | ISO 4892-3:2016 | Cycle 1 UVA-340 exposure | ≥80% elongation retention after 2,000 h |
| Playground components | EN 71-3:2019+A2:2024 | Soluble element migration | Pb ≤ 2.0 mg/kg, Cd ≤ 1.3 mg/kg in Category III |
| Food-contact bins | FDA 21 CFR 177.1520(c) | Olefin polymer clearance | Conforms to paragraph (c) 3.1 conditions of use |
| Vehicle interior parts | ISO 3795:1989 | Burn rate, horizontal | Class A or FMVSS 302 equivalent |
Field maintenance logs from marine aquaculture installations frequently identify nut-and-bolt failure, not polymer fracture, as the reason flotation buoys are retired after five to seven years. For Icorene 1761 WHI 1400 mouldings, however, the long-term UV exposure route is the critical design variable. Marine flotation parts such as mooring buoys, dredge pipe collars, and fish cage floats are rotationally moulded as double-walled hollow shells with wall thicknesses of 5 mm to 10 mm; closed-cell polyurethane foam may be injected through a secondary port at 0.8 MPa to 1.2 MPa after the shell cools, depending on the required buoyancy reserve. Weathering compliance is evaluated through accelerated exposure per ISO 4892-3:2016 Cycle 1 with UVA-340 lamps, and retention of at least 80% of initial elongation at break under ISO 527-2:2012 after 2,000 h is a typical acceptance gate; published data for this specific marine formulation is limited, so fabricators validate each colour masterbatch lot rather than relying on generic UV guarantees. Additive loadings in this segment are heavier than in potable water: 0.5 wt% to 1.0 wt% of a high-molecular-weight HALS masterbatch plus 0.3 wt% to 0.6 wt% of a benzotriazole UV absorber, with the total additive package held below 2.0 wt% to preserve low-temperature impact strength. Process temperatures are lowered to an oven set point of 270 °C to 290 °C and a peak internal air temperature of 185 °C to 195 °C because thick foam-filled structures retain heat and can over-crystallise the inner wall. Moulders using all-electric or direct gas-fired shuttle machines with IR pyrometers report that the inner wall surface must remain above 150 °C until demoulding to avoid shrink marks around lifting eyes. Finished products include 100 kg to 2,000 kg mooring buoys, encapsulated navigation floats, aquaculture pen corner floats, and sub-sea pipeline buoyancy modules with moulded-in galvanised bolt plates.
Compliance with EN 71-3:2019+A2:2024 becomes the controlling constraint when rotomoulded Icorene 1761 WHI 1400 is used for playground slide shells, tunnel sections, and spring-rider bodies, because the migration limits for soluble elements apply to the final pigmented coating and the substrate polymer alike. In this segment, the rotational moulding cycle runs at an oven temperature of 280 °C to 295 °C with a peak internal air temperature of 190 °C to 200 °C, followed by forced-air cooling at 8 °C/min to 12 °C/min because rapid cooling improves surface gloss retention and reduces tack for subsequent graphic decal adhesion. Wall thickness is typically 3.5 mm to 6.0 mm, with local thickening to 8 mm at handgrip edges and bolt-through points. Pigment masterbatch loadings of 1.0 wt% to 3.0 wt% are common for high-chroma playground colours, but only heavy-metal-free organic pigments should be used; antimony, cadmium, and lead are excluded because EN 71-3:2019+A2:2024 Category III limits are lower than legacy compounds can meet at these addition ratios. A 0.1 wt% to 0.3 wt% slip/antiblock masterbatch reduces nesting friction during automated demoulding and prevents surface scuffing during assembly. Dry powder flow should be checked under ASTM D1895-96 Method A after storage, because humidified powder charged above 65% RH can bridge in deep slide tools; moulds with slide or tunnel geometries longer than 1.8 m should include vents at the blind end to prevent air entrapment. Production-scale experience shows that demoulding temperatures above 75 °C cause part distortion when the mould is opened without support frames; cooled to 60 °C, the same parts retain their intended geometry within ±1.0 mm across a 1.2 m span. Finished products include outdoor playground slides, crawl tunnels, balance-beam shells, and institutional play components certified under ASTM F963-23 and EN 1176-1:2017 for structural integrity.
At -30 °C, the ductile-to-brittle transition behaviour of thin-wall rotomoulded mLLDPE determines whether an insulated fish tub can be dropped from a forklift tine without outer-shell fracture. Icorene 1761 WHI 1400 in this segment is used for double-wall insulated containers in food processing and cold-chain logistics, where the outer and inner shells are rotationally moulded separately and then filled with polyurethane foam at a free-rise density of 32 kg/m³ to 45 kg/m³. Shell wall thickness is held between 4 mm and 8 mm, with the load-bearing base thickened to 10 mm to 12 mm and reinforced by moulded-in ribs at 250 mm spacing. Food-contact compliance for the inner shell follows FDA 21 CFR 177.1520(c) paragraph 3.1 and Regulation (EU) No 10/2011 Annex I Table 1, with migration testing conducted under the intended time-temperature conditions for fish, meat, and dairy products. The rotational moulding cycle differs from thin-wall commodity production: oven temperature is 295 °C to 310 °C, peak internal air temperature is 205 °C to 215 °C, and the inner shell is cooled slowly at 5 °C/min to 8 °C/min to reduce post-foaming delamination. Production-scale operators note that insulation foam exerts an internal pressure of 0.2 MPa to 0.4 MPa on the outer shell during curing, so moulded-in vent holes must remain open until after the foam rise is complete or the part will bulge beyond dimensional tolerance. Formula modifications are minimal; 0.5 wt% to 1.5 wt% of a linear-low-density PE-based slip masterbatch improves release from aluminium tools, and 0.2 wt% to 0.5 wt% of a HALS stabiliser is retained for freezer washdown environments where alkaline detergents and hot-water sprays reach 80 °C. Terminal products include 20 L to 1,000 L insulated fish tubs, meat lug boxes, bakery ingredient totes, and temperature-controlled pharmaceutical transport containers.
Because small-series vehicle reservoirs are processed without high-volume injection tooling, the melt-flow latitude of Icorene 1761 WHI 1400 allows a single aluminium mould to fill hydraulic-fluid reservoirs, cab interior cowlings, and wheel-arch splash shields with wall stocks from 3 mm to 7 mm. In this segment, the material must satisfy flammability requirements under ISO 3795:1989 and FMVSS 302 where interior surfaces are involved; when the neat resin cannot reach the required burn rate at 3 mm thickness, a halogen-free phosphate-based flame-retardant masterbatch is added at 4 wt% to 8 wt%, with the trade-off of a 6% to 10% reduction in tensile strength at yield under ISO 527-2:2012. The rotational moulding process uses a two-axis biaxial speed ratio between 4:1 and 5:1, with oven temperature set at 280 °C to 295 °C and peak internal air temperature at 190 °C to 200 °C; moulded-in brass or stainless-steel inserts are preheated to 130 °C and held in place with silicon magnets during the heating cycle. For chemical-carrying reservoirs used with hydraulic oil or urea solutions, compatibility is screened under ISO 175:2010 by immersion in the actual fluid at 60 °C for 1,000 h, with a maximum allowable weight gain of 0.5% to prevent wall swelling and threaded-port loosening. Fabricators report that the narrow molecular weight distribution of metallocene LLDPE reduces warpage in large flat cowling faces, but the same characteristic narrows the cooling window: cooling rates above 12 °C/min produce sink marks at ribs, while rates below 4 °C/min increase cycle time without measurable property gain. Terminal products in this segment include 5 L to 80 L hydraulic oil reservoirs, urea solution tanks, cab interior shroud panels, and agricultural tractor roof liners made in annual volumes from 500 to 20,000 units.
Competitive LyondellBasell Icorene 1761 WHI 1400 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 WHI 1400 is a metallocene-catalysed linear low density polyethylene supplied as a white-coloured powder for rotational moulding. The grade is classified within the manufacturer’s Icorene metallocene polyethylene product family and is specified when a pre-coloured material with controlled melt flow and narrow molecular weight distribution is required for shell-tool charging. Property release for this product class normally includes melt flow rate measured under ASTM D1238-23 at 190 °C/2.16 kg, density measured under ASTM D792-20, tensile yield and ultimate elongation under ASTM D638-22, flexural modulus under ASTM D790-17, and environmental stress cracking resistance under ASTM D1693-21. Published data for this specific configuration is limited; therefore, lot-specific values for melt flow rate, density, antioxidant loading, and pigment dispersion are controlled by the LyondellBasell certificate of analysis rather than by generic family averages.
The metallocene single-site catalyst architecture produces a narrower molecular weight distribution, commonly in the range of 2.0–3.5 polydispersity index, compared with 4.0–8.0 for conventional Ziegler-Natta linear low density polyethylene. A uniform short-chain branching distribution reduces the high-molecular-weight tail and lowers melt elasticity during sintering. This is relevant in rotational moulding because the powder bed must densify without high shear; rheological differences therefore affect bubble removal time and final wall-thickness uniformity more than in injection moulding.
Rotational moulders running shuttle-type machines with arm radii of 2.0 to 3.5 m observe that pre-coloured metallocene LLDPE powders densify at a lower peak internal air temperature than Ziegler-Natta powders of equivalent melt index because the metallocene melting peak is narrower and the crystalline lamellae are more uniform. Typical oven chamber settings of 260–290 °C and peak internal air temperatures of 190–205 °C are used in production; excursions beyond 210 °C can promote yellowing of the white pigment package and loss of low-temperature ductility. Powder moisture uptake is generally low, but storage at relative humidity above 60% can produce surface condensation that should be removed by low-temperature air drying before charging to the mould. Processors who replace a Ziegler-Natta rotomoulding powder with Icorene 1761 WHI 1400 should anticipate a shorter oven residence time and a slightly lower peak internal air temperature requirement; however, local wall sections below 3 mm may require tooling adjustments to maintain uniform heat transfer.
Sieve distribution and bulk density are important control parameters. Powder fines below 150 µm can bridge in drop arms, while coarse particles above 500 µm can increase surface porosity and pinhole frequency. Sieve analysis per ASTM D1921 and bulk density per ASTM D1895-17 are used to monitor dry-flow and hopper discharge. A typical rotomoulding powder should pour without ratholing; if the bulk density drops below the certified range, fines or moisture may have altered the flow behaviour.
Upstream, white rotomoulding grades are compounded by melt mixing in a corotating twin-screw extruder with L/D ratios of 32:1 to 40:1, followed by grinding and classification. Poor dispersive mixing of titanium dioxide can produce colour streaks and local impact variations. On the moulding line, batch-to-batch bulk density should be monitored because a drop in bulk density changes the mass delivered to the mould and can alter wall thickness. A similar check should be performed after regrinding trimmed parts; reground material may reduce low-temperature impact and should not exceed the proportion allowed by the application specification.
Test methodology for this material class is anchored to standardised specimens and conditioning protocols. Melt flow rate is compared under ISO 1133-1:2022 and ASTM D1238-23; density is determined by ASTM D792-20 Method B or ISO 1183-1:2019. Tensile yield and elongation are evaluated with Type IV specimens at 50 mm/min per ASTM D638-22. Low-temperature impact can be evaluated by instrumented puncture per ISO 6603-2:2021. For food-contact use, the base olefin polymer must satisfy FDA 21 CFR 177.1520, while the white colourant requires separate conformance to 21 CFR 178.3297 or 21 CFR 73.575 depending on pigment chemistry and end-use.
Regulatory compliance statements should not be transferred from unpigmented resin without testing. Titanium dioxide, if present, may be subject to purity limits for soluble metals; a white-pigmented rotomoulding powder should be confirmed against the final article’s migration test because pigment dispersion and polymer matrix interaction influence extractables. In the European Union, plastic food-contact evaluation requires overall migration testing under Regulation (EU) No 10/2011 using food simulants assigned to the intended contact class.
| Standard or regulation | Scope | Condition | Significance |
|---|---|---|---|
| ASTM D1238-23 | Melt flow rate | 190 °C / 2.16 kg | Controls sintering, bubble release, and wall-thickness distribution |
| ASTM D792-20 / ISO 1183-1:2019 | Density | 23 °C | Sets flexural stiffness, softening, and chemical resistance expectations |
| ASTM D638-22 | Tensile yield and elongation | Type IV, 50 mm/min | Confirms short-term load-bearing and ductility |
| ASTM D790-17 | Flexural modulus | Method 1 | Predicts part stiffness under bending |
| ASTM D1693-21 | Environmental stress cracking resistance | Condition B, 10% Igepal CO-630, 50 °C | Predicts detergent and agricultural chemical failures |
| ISO 6603-2:2021 | Instrumented puncture impact | Plaque at specified thickness | Measures energy absorption and ductile/brittle behaviour |
| FDA 21 CFR 177.1520 | Olefin polymer food-contact base | Conditions of use B–H | Base polymer compliance for food packaging |
| 21 CFR 178.3297 | Colourants for polymers | Food-contact safety | White pigment compliance in contact applications |
| Regulation (EU) No 10/2011 | Plastic food-contact materials | Overall migration 10 mg/dm² | EU food-contact verification |
For general industrial applications, documentation should address RoHS Directive 2011/65/EU Annex II heavy-metal limits, and REACH Regulation (EC) No 1907/2006 Article 33 communication obligations for substances of very high concern. These are not alternative property specifications but are commonly requested for rotomoulded articles exported to the European Union.
At equivalent density and melt index, a metallocene LLDPE differs from a Ziegler-Natta butene LLDPE principally in comonomer distribution and molecular weight distribution. The single-site catalyst yields a narrower molecular weight distribution and a more uniform short-chain branching distribution. This reduces the high-molecular-weight tail, lowers melt elasticity, and produces more uniform wall thickness in complex rotomoulded parts. Ziegler-Natta grades typically contain both highly branched and lightly branched chains, which can generate differential shrinkage and localised stress in closure areas.
Autoclave LDPE, by contrast, contains long-chain branching that increases shear thinning and melt tension; it is not directly interchangeable because the powder-bed densification and bubble-dissolution behaviour differ. A metallocene LLDPE does not reproduce the same melt strength as LDPE and should not be used in processing lines that depend on extensional hardening. For rotational moulding, this lower melt elasticity is not a processing disadvantage; it can improve powder coalescence, but the oven residence time must be revalidated whenever the feedstock is changed.
Within the LLDPE class, comonomer type and content are product-specific. Metallocene grades can be produced with butene, hexene, or octene; hexene and octene comonomers generally provide greater environmental stress cracking resistance and low-temperature toughness than butene at equivalent density. Direct substitution should not be made from a butene Ziegler-Natta LLDPE without comparing ESCR and impact because density and melt flow alone do not capture chain architecture.
Compared with HDPE rotomoulding powders, Icorene 1761 WHI 1400 exhibits lower flexural modulus and lower Vicat softening point but greater ductility and improved environmental stress cracking resistance. The white pre-colouration removes the need for dry-blending pigment on the shop floor, reducing dust and lot-to-lot colour drift. However, titanium dioxide particles can act as stress concentrators and may lower instrumented puncture energy relative to unpigmented metallocene base resin. Sieve analysis per ASTM D1921 and bulk density per ASTM D1895-17 are used to control powder dry-flow.
Surface quality of white parts is sensitive to mould release agent thickness. Excessive semi-permanent release agent or contaminated mould surfaces produce gloss reduction and local surface roughness. The use of forced air cooling should be gradual; rapid cooling with water mist can improve impact but may promote shrinkage and warpage. Processors should establish a cooling curve that balances cycle time against dimensional stability.
Typical rotomoulded components produced from white metallocene LLDPE powders include agricultural holding tanks, secondary containment basins, playground enclosures, fresh-water tanks, and industrial covers. The colour package and catalyst package should be verified for UV stabilisation when the part is intended for outdoor service; titanium dioxide may provide surface protection, but hindered amine light stabilisers are required for long-term gloss and tensile retention. Chemical storage compatibility should be tested with the intended fluid because polyethylene is permeable to nonpolar hydrocarbons and is not recommended for continuous immersion with strong oxidising agents without evaluation.
Rotomoulded wall sections from this product family are usually designed between 3 mm and 12 mm; sections below 3 mm can produce poor powder flow-in and local thinning, while sections above 12 mm extend soak time and can develop sub-surface porosity. Critical service parts should be checked by sectioning and microscopy if internal voids are suspected. Pigment dispersion can be verified by optical microscopy on thin sections; agglomerates larger than 25 µm can indicate inadequate dispersion during compound manufacture.
Environmental stress cracking resistance is a critical design threshold in white rotomoulded tanks subjected to detergents, agricultural chemicals, or freeze-thaw cycles. The metallocene architecture of Icorene 1761 WHI 1400 reduces inter-crystalline tie-molecule unevenness, which contributes to improved resistance under ASTM D1693-21 Condition B, 10% Igepal CO-630 at 50 °C. The failure time measured in this test is not an absolute service life; it is a comparative indicator of resistance to cracking initiated by stress and active wetting agents.
Low-temperature ductility should be evaluated on rotomoulded plaques, not on compression-moulded laboratory specimens, because cooling rate and residual stress differ. Instrumented puncture testing per ISO 6603-2:2021 across −20 °C and −40 °C can reveal the brittle-to-ductile transition of the white-pigmented material. Published data for this specific configuration is limited, but titanium dioxide addition is known to shift the transition to a slightly higher temperature than that of the unpigmented metallocene base.
Processors should monitor internal air temperature and cooling rate as primary variables influencing ESCR. Rapid air quenching produces smaller spherulites and generally improves ductility; slow cooling can improve dimensional stability but may reduce ESCR because crystallinity increases. Parts intended for severe detergent service should avoid sharp internal corners, weld-line starvation, and local wall thickness below 4 mm, since those features concentrate stress and reduce time to failure in standard environmental stress cracking tests.
When the component must also meet food-contact or potable-water standards, white-pigment dispersion and antioxidant package selection must be considered together. Some hindered phenolic antioxidants and phosphite stabilisers may alter organoleptic behaviour; therefore, the final part should be subjected to sensory and migration testing where applicable. The polymer’s narrow molecular weight distribution also produces lower shear heating during grinding; however, high-throughput milling can generate fines that affect bulk density and should be controlled with closed-loop screen classification.
In applications requiring white colouration, low-temperature impact, and resistance to stress cracking, Icorene 1761 WHI 1400 is used as a pre-coloured metallocene LLDPE powder. It is not a high-temperature engineering resin and is not a barrier layer for hydrocarbons. The grade should be specified only after reviewing the certificate of analysis for melt flow rate, density, pigment dispersion, and antioxidant content against the exact wall-thickness and service environment of the rotomoulded part. Users must also verify that post-moulding operations such as deflashing, drilling, and insert installation do not introduce microcracks in stress-sensitive corners.