| HS Code | 489210 |
| Polymer Type | Metallocene Linear Low Density Polyethylene (mLLDPE) |
| Catalyst | Metallocene |
| Comonomer | Hexene |
| Form | Pellets |
| Color | White |
| Density | 0.917 g/cm³ |
| Melt Index | 1.6 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 234 MPa |
| Vicat Softening Point | 95°C |
| Melting Point | 122°C |
As an accredited LyondellBasell Icorene 1761 WHI 1008 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; each pallet holds 1,000 kg (40 bags) for shipping. |
| Container Loading (20′ FCL) | 20′ FCL: LyondellBasell Icorene 1761 WHI 1008 metallocene LLDPE loaded on pallets, 25 kg bags, securely stowed, weight-optimized for shipment. |
| Shipping | Icorene 1761 WHI 1008 is a non-hazardous metallocene linear low-density polyethylene resin supplied as free-flowing pellets. It ships in 25 kg polyethylene bags, 1000 kg bulk bags/octabins, or bulk trucks/railcars. Store dry, away from direct sunlight and heat. No special hazardous-materials handling required. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and oxidizing agents. Keep in original unopened bags or sealed containers on pallets to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Protect bags from physical damage. Maintain good housekeeping to prevent slipping from spilled pellets. Use first-in, first-out stock rotation. |
| Shelf Life | Generally 24 months from manufacture when stored dry, cool, and in original unopened packaging, away from direct sunlight and heat. |
Above-ground storage of aggressive aqueous chemicals, dosing solutions, and UN-regulated intermediate bulk containers is specified with Icorene 1761 WHI 1008 as the as-supplied white metallocene linear low density polyethylene rotomoulding powder. The material is assessed against EN 13575:2012 for unpressurised thermoplastic tanks, ASTM D1998-21 for polyethylene upright storage tanks, and UN 31H1/Y where the finished article is intended as a rigid plastics IBC for dangerous goods. A typical starting-point charge contains 100 parts by weight Icorene 1761 WHI 1008, 0.3–0.8 wt% of a HALS/benzotriazole UV stabiliser masterbatch, 0.05–0.12 wt% of a phenolic/phosphite antioxidant package, and 0.02–0.05 wt% of an acid neutraliser when chlorine-donor chemistry is excluded. The powder is pulverised to 100% pass 500 µm with a d50 of 250–300 µm measured by ASTM D1921-18, then charged into cast-aluminium moulds at ambient temperature. In a shuttle-type rotational moulding machine with a 2.8 m swing arm and 4:1 primary/secondary rotation ratio, oven set point is held at 270–290°C, and internal air temperature is maintained at 195–205°C for 6–10 minutes at peak. For a 1,000 L tank, nominal wall thickness is 4.5–6.0 mm; the demoulding criterion is a part surface temperature below 70°C after forced-air and water-mist cooling at 6–10°C/min. Finished article types include 500–10,000 L vertical storage tanks, 1,000 L UN-certified IBC units with integral pallet bases, double-wall dosing cabinets, and cylindrical process vessels. The principal process conflict observed on production-scale equipment is internal void formation at moulded-in bosses when peak internal air temperature falls below 193°C or when powder packing in the boss cavity is below 0.92 g/cm³ apparent density before heating; boss radii below 4.0 mm increase this failure rate. Chemical resistance verification follows ISO 16101:2004 compatibility testing for dangerous goods packaging, with retention values based on the actual filled chemical. The operational boundary for continuous chemical exposure is not resin-only; it must be qualified with the final part thickness and stress-cracking environment. In concentrated nitric acid above 20%, stress cracking resistance becomes the limiting factor, and published data for this specific configuration is limited. Where UN certification is specified, the rotomoulded IBC is tested at 1.5 times design pressure per the applicable UN test schedule, and wall-thickness readings are recorded at the four lowest ultrasonic measurement points.
When cyclic partial-fill loading creates alternating hoop stress in agricultural water and fertigation tanks, Icorene 1761 WHI 1008 is specified because the metallocene linear low density structure permits graduated wall sections without excessive part distortion. The article is evaluated against AS/NZS 4766:2006 for polyethylene storage tanks and, where aggressive fertilisers are stored, ISO 16101:2004 chemical compatibility testing is applied. A starting formulation uses 100 parts by weight Icorene 1761 WHI 1008, 0.6–1.2 wt% high-molecular-weight HALS UV stabiliser masterbatch, 0.08–0.12 wt% phenolic/phosphite antioxidant, and 0.02–0.05 wt% acid neutraliser for acidified fertiliser solutions. The processing window for a 10,000 L vertical cylinder uses an oven set point of 265–280°C, peak internal air temperature of 190–200°C, and a biaxial rotation ratio of 3.5:1. Shell wall thickness is graduated from 5.0 mm in the upper cylinder to 8.0 mm in the conical bottom to manage hoop stress and hydrostatic head. Cooling is performed at 4–7°C/min with interrupted water fog, and demoulding occurs only below 75°C wall temperature to limit ovality. On a carousel machine with 2.4 m swing radius, batch-to-batch variance of ±3°C in peak internal air temperature has been observed to increase out-of-roundness to 1.5% or more when cooling is not indexed to the measured internal air temperature. Finished product types include 2,000–20,000 L vertical water tanks, conical-bottom mixing vessels, nurse tanks for fertigation, and dosing buffer tanks.
Mechanical entrapment, impact puncture, and migration of elements govern play-value structures moulded from Icorene 1761 WHI 1008. These articles are required to satisfy chemical migration limits under EN 71-3:2019+A1:2021, mechanical and physical requirements under EN 71-1:2014+A1:2018, and public playground equipment criteria under ASTM F1487-21. The as-supplied white pigmented grade is dry-blended with 100 parts by weight resin, 0.5–1.0 wt% HALS-based UV stabiliser masterbatch, and 0.05–0.10 wt% phenolic/phosphite processing antioxidant; secondary colour masterbatches are not normally required because the article is white. The rotomoulding process uses cast aluminium moulds with a 4:1 rotation ratio, oven set point 260–275°C, and internal air temperature 185–195°C for a nominal wall thickness of 2.5–3.5 mm. Forced-air cooling is controlled at 5–8°C/min to avoid differential shrinkage in ribbed panels, and demoulding below 75°C reduces strain whitening at load-bearing ribs. A known production failure mode on a multi-arm carousel with 2.4 m mould swing is puncture failure at tunnel rims below 2.0 mm wall thickness during impact testing; increasing the rim radius to 6.0 mm and wall thickness to 3.0 mm removes the fracture. Finished article types include slide bodies, tunnel modules, climbing panels, themed enclosures, and roofed playhouse sections. Published data for this specific Icorene grade under EN 71-3 migration testing is limited to final article qualification; extractable element testing must be performed on the moulded article rather than on resin powder alone.
Because skid-load transfer and abrasive contact dominate industrial material handling, pallet boxes and process bins are moulded from Icorene 1761 WHI 1008 under ISO 8611-1:2011 for flat pallet and pallet box load transfer, with additional drop and side-impact tests referenced by end-user specifications. The typical formulation includes 100 parts by weight Icorene 1761 WHI 1008, 0.2–0.5 wt% antioxidant masterbatch, 0.1–0.3 wt% internal process lubricant, and 0.3–0.8 wt% metallic stearate acid scavenger. Moulding is performed on cast-aluminium tools with a 4:1 rotation ratio, oven set point 270–285°C, and internal air temperature 195–205°C. Nominal wall thickness is 5.0–8.0 mm for load-bearing bases and sidewalls, with the base formulated to sustain rated static stacking of 1,000 kg when the bottom deck is fully supported. Cooling is conducted at 6–9°C/min and demoulding below 70°C. The mould cavity texture is specified at Ra 2.5–4.0 µm to permit predictable part release and to reduce skid-load friction. Processing experience on a shuttle machine with 2.8 m platen indicates that release agent film build-up increases ejection force when cavity roughness is below Ra 1.6 µm; periodic alkaline mould cleaning at 40–60°C is required to maintain cycle time. Finished product types include pallet boxes, distribution totes, process bins, nestable storage containers, and dividable material handling crates.
Where visual inspection, low particulate retention, and controlled surface cleanliness govern cleanroom solid handling, Icorene 1761 WHI 1008 is rotomoulded into solid dosage transfer bins and process totes. The material is assessed against FDA 21 CFR 177.1520 olefin polymer composition and, for final article qualification, USP <87> in vitro cytotoxicity and USP <88> Class VI systemic reactivity. A starting formulation uses 100 parts by weight Icorene 1761 WHI 1008, 0.05–0.10 wt% phosphite antioxidant, 0.05–0.10 wt% acid neutraliser, and 0.05–0.15 wt% boron nitride release agent when silicone-based external release agents are excluded to minimise particulate contamination. Moulding is carried out in an ISO 14644-1:2015 Class 7 post-mould handling environment, with oven set point 265–280°C, internal air temperature 190–200°C, and rotation ratio 4:1. Filtered-air cooling at 5–8°C/min and demoulding below 65°C are specified to reduce dust attraction and electrostatic surface charging. A defined production risk is the migration of processing aids to the surface at internal air temperatures above 200°C, which can alter the contact angle and particulate retention of the finished bin; internal air temperature is therefore kept below 200°C for this application. Finished articles include solid dosage transfer bins, tablet collection totes, granulation feed hoppers, and washable process totes. Data for extractables and leachables on this specific configuration are limited; the final part is qualified per the end-user's pharmaceutical validation protocol.
For roadside traffic barriers, the assembled shell is moulded from Icorene 1761 WHI 1008 when the white pigmented outer shell must resist weathering-induced colour shift and maintain ballast integrity under impact. The assembled article is assessed under EN 1317-1:2010 for road restraint system terminology and performance, and under MASH 2016 Test Level 2 for vehicle impact acceptance in relevant jurisdictions. The formulation uses 100 parts by weight Icorene 1761 WHI 1008, 0.8–1.5 wt% high-molecular-weight HALS stabiliser masterbatch, and 0.1–0.2 wt% phenolic/phosphite antioxidant. The rotomoulding process uses a 4:1 rotation ratio, oven set point 275–290°C, and internal air temperature 195–205°C; walls around ballast compartments are moulded to 6.0–10.0 mm. Cooling is conducted at 5–7°C/min, with slower cooling through the baffle intersections to prevent sink marks and internal voids. A production failure mode occurs at the baffle-to-shell junction when peak internal air temperature is below 195°C or cooling exceeds 8°C/min; this is corrected by increasing oven residence time until the junction surface temperature reaches 200°C before cooling. Finished article types include water-filled longitudinal barriers, channeliser ballast bases, barricade shells, and crash-cushion submodules. Impact performance is a system-level property of the filled and assembled barrier, not of the polyethylene shell alone; full-scale crash testing is required for final certification.
Compliance matrix for rotomoulded application scenarios.
| Application scenario | Leading compliance standard or code | Verification test method or condition |
|---|---|---|
| Chemical storage tanks and IBCs | EN 13575:2012; UN 31H1/Y | ASTM D1998-21 hydrostatic test |
| Agricultural water and fertigation tanks | AS/NZS 4766:2006 | ISO 16101:2004 chemical compatibility |
| Playground and recreational structures | EN 71-3:2019+A1:2021; ASTM F1487-21 | Element migration and impact puncture |
| Material handling bins and pallet boxes | ISO 8611-1:2011 | Payload and rack-load transfer |
| Cleanroom pharmaceutical handling | USP <87>; USP <88> Class VI | Cytotoxicity and systemic reactivity |
| Roadside traffic barriers | MASH 2016; EN 1317-1:2010 | Full-scale vehicle impact assembly test |
Competitive LyondellBasell Icorene 1761 WHI 1008 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Under ASTM D883-23 and ISO 1872-1:2018, LyondellBasell Icorene 1761 WHI 1008 is classified as a metallocene-catalysed linear low-density polyethylene supplied in white-pigmented powder form. The base designation 1761 defines the molecular weight, density target and narrow-comonomer-distribution architecture; the suffix WHI 1008 identifies the white pigment and additive package supplied for rotational moulding. The material is specified for hollow articles such as chemical storage tanks, agricultural sprayer bodies, recreational watercraft components and industrial enclosures, where low-temperature ductility assessed by instrumented puncture testing under ISO 6603-2 and environmental stress-crack resistance assessed by ASTM D1693-15 are more important than the high modulus of a dense HDPE. The powder is intended for low-shear biaxial-sintering processes and should not be treated as a film-grade LLDPE or as a high-shear injection-moulding compound.
Conventional Ziegler–Natta LLDPE contains a broad distribution of short-chain branches: some chains are highly branched and barely crystallise, while others are nearly linear and crystallise early. Metallocene catalysis narrows the distribution of hexene or butene incorporation and produces more uniform crystallisable sequence lengths. The practical consequence in a rotational mould is a narrower sintering window. The powder transitions from solid to fully sintered over a smaller temperature interval, which can improve surface replication but demands tighter internal air-temperature control. Published representative values for Icorene 1761 WHI 1008 include density of 0.933 g/cm³ by ISO 1183-1:2019 and a melt flow rate of 6.0 g/10 min at 190 °C/2.16 kg by ISO 1133-1:2022. The molecular weight distribution is narrower than a Ziegler–Natta powder of equivalent melt flow rate, normally with polydispersity below 3.0 compared with 3.5 to 5.0 for conventional linear-low resins. That difference lowers melt elasticity and reduces residual orientation in thick sections, but it also reduces shear thinning during any downstream compounding step.
| Property and test method | Icorene 1761 WHI 1008 | Conventional ZN-LLDPE reference |
|---|---|---|
| Density, ISO 1183-1:2019 | 0.933 g/cm³ | 0.935 g/cm³ |
| Melt flow rate, 190 °C/2.16 kg, ISO 1133-1:2022 | 6.0 g/10 min | 5.2 g/10 min |
| Flexural modulus, ISO 178:2019 | 550 MPa | 480 MPa |
| ESCR, F50, 100% Igepal, ASTM D1693-15 | >1000 h | 300–700 h |
| Tensile elongation at break, ISO 527-2:2012 | 800 % | 600 % |
The conventional ZN-LLDPE column is a comparative literature range for a non-metallocene powder of similar density and melt flow rate, not a single commercial reference. Batch certificates for the specific silo lot govern final acceptance.
On production-scale carousel or shuttle-type biaxial rotational moulding machines, the powder is charged into thin-wall steel or cast aluminium moulds. Oven cavities for mLLDPE powders in the 0.933 g/cm³ density envelope typically operate between 260 °C and 310 °C, with mould internal air temperature reaching 180 °C to 200 °C before cooling begins. Rotation ratios of 4:1 to 6:1 are common for asymmetric hollow parts. Because the grade’s narrower melting range shortens the time between initial particle coalescence and full densification, timer-based process control can result in porosity at low internal air temperature or local yellowing at the thickest corners. Process development should therefore use internal air temperature probes in the mould and verify wall stock by ultrasonic gauge rather than by visual gloss alone.
Moisture uptake is a known failure source. Factory-sealed containers can usually be processed without drying, but open storage at relative humidity above 60% for more than 48 h can produce surface bubbles from steam volatilisation. A forced-air hopper dryer at 80 °C for 2 h to 4 h is used when moisture pickup is suspected. The white pigment in WHI 1008 changes heat absorption relative to natural grades; a pigmented powder may need slightly shorter oven dwell than a natural mLLDPE of the same base melt flow rate because white reflects infrared radiation differently from dark colours. Oven settings should be re-established after switching from natural to WHI 1008, not copied from a natural-grade recipe.
At a melt flow rate of 6.0 g/10 min, the zero-shear viscosity is sufficiently low for particle coalescence, but the narrow molecular weight distribution reduces strain hardening. The sintered layer can drain away from vertical walls if the oven dwell is excessive or if the mould surface exceeds 250 °C before the full wall stock has sintered. Parts with deep ribs or kiss-off features may exhibit thinning because the melt has lower melt strength than a long-chain-branched LDPE. That is a fundamental difference from low-density polyethylene produced by high-pressure autoclave polymerisation: LDPE retains long-chain branching and better sag resistance at low shear, but it lacks the same ESCR at equivalent density.
Regulatory clearance is not automatically transferred from the raw material to the moulded part. The base polyolefin can be evaluated under FDA 21 CFR 177.1520 for food-contact uses, but the WHI 1008 colour and stabiliser system requires separate confirmation that the specific pigments and additives are cleared for the intended end use. For the European market, final-article migration testing under EU Regulation 10/2011 is required at the actual surface-to-volume ratio. Potable-water tanks require article-level certification to NSF/ANSI 61 or equivalent national rules; a resin datasheet alone cannot satisfy that requirement. Outdoor service life depends on UV-stabiliser concentration and wall thickness. Accelerated weathering comparisons should follow ISO 4892-2 or ASTM D2565-16, with mechanical retention measured after exposure.
Chemically, the polymer resists many aqueous salt solutions, mild acids and non-oxidising alkalis. Aromatic hydrocarbons, chlorinated solvents and strong oxidisers are outside the recommended service envelope unless specific immersion testing demonstrates acceptable mass change and crack resistance. ESCR data generated by ASTM D1693-15 is a screening indicator, not a substitute for full-scale tank stress testing.
| End-use requirement | Standard or regulation | Typical test article |
|---|---|---|
| Food contact, United States | FDA 21 CFR 177.1520 plus colourant clearance | Moulded plaques, extraction cells |
| Food contact, European Union | EU Regulation 10/2011 | Final article or representative coupon |
| Potable water contact | NSF/ANSI 61 | Finished tank or pipe fitting |
| Outdoor weathering | ISO 4892-2 / ASTM D2565-16 | Injection- or compression-moulded plaques |
| ESCR screening | ASTM D1693-15 | Notched test bars in 100% Igepal |
This matrix is a qualification checklist; it does not imply that the grade has been certified under every listed scheme. Certification status must be confirmed against the supplier’s compliance statement and the final article’s independent test report.
Compared with high-density polyethylene rotomoulding powders of similar melt flow rate, Icorene 1761 WHI 1008 gives up flexural modulus in exchange for higher environmental stress-crack resistance and lower warpage after cooling. HDPE parts often require a mould release agent or a higher internal air temperature to achieve an acceptable surface; the mLLDPE grade can generally be moulded at lower peak temperature because of its lower zero-shear viscosity. Compared with film-grade LLDPE, the rotational moulding powder is coarser and contains a stabiliser package selected for long oven dwell times, not for high-shear single-screw film extrusion. It is not recommended for blown-film or cast-film processes because the additive system and particle size do not match the shear heating and bubble-stability requirements of those lines. Dry-blending with external masterbatches or regrind should be limited to systems with a compatible polyethylene carrier. Amine-based antistatic or antifog additives can interfere with the metallocene stabiliser package and should not be introduced without extended oven-ageing trials at the maximum anticipated wall thickness.