| HS Code | 389158 |
| Polymer Type | Metallocene Linear Low Density Polyethylene |
| Density | 0.917 g/cm³ |
| Melt Mass Flow Rate | 1.0 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 9.0 MPa |
| Tensile Strength At Break | 30.0 MPa |
| Elongation At Break | 600 % |
| Flexural Modulus | 220 MPa |
| Vicat Softening Temperature | 95 °C |
| Melting Temperature | 122 °C |
| Haze | 8 % |
| Gloss | 70 % |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 300 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
| Color | Red 4339 |
As an accredited LyondellBasell Icorene 1761 RED 4339 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged as 25 kg polyethylene-lined paper bags, palletized, for LyondellBasell Icorene 1761 RED 4339 metallocene linear low density polyethylene. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell Icorene 1761 RED 4339 metallocene linear low-density polyethylene in 25 kg bags, palletized and secured. |
| Shipping | LyondellBasell Icorene 1761 RED 4339 is a non-hazardous polyethylene resin. It is not regulated for transport; no UN number, hazard class, or packing group. Ship in sealed bags, boxes, or bulk containers by truck, rail, or sea. Protect from moisture, contamination, and excessive heat. |
| Storage | Store in a cool, dry, well-ventilated warehouse using closed original bags or containers. Keep away from direct sunlight, heat, flames, strong oxidizers, and incompatible materials. Protect from moisture, contamination, and UV exposure. Maintain stable pallets, minimize dust and static discharge, and follow first-in, first-out stock rotation. Comply with the SDS and local regulations. |
| Shelf Life | Shelf life: 24 months from production date when stored unopened in original packaging under cool, dry conditions. |
LyondellBasell Icorene 1761 RED 4339 is a red-compounded metallocene linear low density polyethylene supplied as a rotational moulding powder. The metallocene polymerisation route produces a narrower molecular weight distribution and more uniform comonomer placement than conventional Ziegler-Natta LLDPE. These structural features reduce the concentration of high-molecular-weight tails that resist sintering at rotomoulding temperatures. The red pigment package is pre-dispersed in the powder matrix; dry blending with additional colour concentrates is possible only when the added pigment particle size is below 35 µm to avoid pinholing at thin-wall sections. Densification is completed at a peak internal air temperature between 195°C and 208°C, with an oven set point between 280°C and 310°C depending on wall thickness and mould metal. Internal air temperature is measured with an articulated thermocouple entering the mould cavity through the vent tube. Pre-drying at 80°C for 2 h is required when the powder has been exposed to relative humidity above 60% because absorbed moisture causes surface porosity and lowers tensile elongation at the inner mould surface.
Red-pigmented rotational moulding grades for diesel fuel tanks are required to meet impact and chemical compatibility limits set by fleet operators and equipment manufacturers. The primary mechanical acceptance criteria are a notched Izod impact value of at least 20 kJ/m² at -40°C according to ASTM D256-10 and an environmental stress crack resistance F50 value above 1,000 h under ASTM D1693-21 Method B using 10% Igepal CO-630. Diesel fuel contact testing is typically run at 60°C for 1,000 h with no visible delamination, blistering, or mass change greater than 1.0%. The metallocene architecture of Icorene 1761 RED 4339 can permit lower wall thickness than conventional LLDPE, but a reduction of 15–20% should not be assumed without destructive sectioning of the moulded part. Incomplete sintering is identified by a matte inner surface or by tensile elongation below 300% on cut samples; these conditions create fuel permeation paths and stress concentrations at moulded-in fittings. Overheating above 220°C should be avoided because the red pigment transitions toward a brown cast and the polymer embrittles through antioxidant depletion.
Oven residence time on a 4.0 m shuttle machine with forced-air circulation is not directly transferable to a carousel machine with lower air velocity. The peak internal air temperature is the controlling process variable. Cooling rates between 5°C/min and 12°C/min provide the most reproducible balance of warpage and crystallinity. Faster cooling suppresses spherulite growth but can freeze in residual stress near metal inserts. Slower cooling increases flexural modulus but reduces low-temperature impact resistance. Mould release of red-pigmented mLLDPE parts requires that mould surfaces be kept free of pigment plate-out; zinc stearate mould release at 0.2–0.5 wt% dry blend is compatible. Diesel fuel has lower vapour pressure and less aggressive swelling than gasoline, but aromatic content above 10% in diesel can increase mass uptake. Direct gasoline or oxygenated fuel contact is not recommended unless the rotomoulded tank receives an internal fluorination or sulfonation barrier treatment to meet evaporative emission limits.
| Parameter | Lower Control Limit | Upper Control Limit | Out-of-Limit Failure Mode |
|---|---|---|---|
| Peak internal air temperature | 195°C | 208°C | Porosity below lower; pigment darkening above upper |
| Oven set point | 280°C | 310°C | Incomplete sintering; thermal degradation |
| Cooling rate | 5°C/min | 12°C/min | Warpage; impact loss |
| Mould rotation ratio | 3.5:1 | 4.5:1 | Non-uniform wall thickness |
Agricultural chemical storage vessels have a different failure hierarchy. The red pigment package performs a secondary function as a visual indicator of tank contents or site safety, but the critical resin property is environmental stress crack resistance at the base radius. Moulded-in inserts for fill pipes and drain fittings are made from stainless steel or polypropylene. The difference in thermal expansion between the insert and the mLLDPE wall creates residual hoop stress. Stress cracking occurs at the knit line where two powder layers densified at different temperatures. In field trials, tanks moulded from Icorene 1761 RED 4339 are tested with ASTM D1693-21 Method B plaques cut from the moulded wall, not from compression-moulded sheet. The acceptance criterion for a liquid fertiliser tank is an F50 value above 500 h in 10% Igepal CO-630 at 50°C. Chemical resistance to urea ammonium nitrate is evaluated by immersion for 90 d at 23°C; a mass change above 0.5% or a reduction in tensile elongation below 50% of the unexposed value indicates unacceptable absorption. The metallocene resin has lower extractables than Ziegler-Natta LLDPE, which minimises the release of short-chain oligomers into recirculating fertiliser solution. Contact with strong oxidisers such as concentrated nitric acid is not recommended without specific chemical resistance testing on the moulded part.
Red-pigmented mLLDPE is used for rotationally moulded buoys, fenders, and flotation elements because the colourant retains visibility in water. Cyclic wave loading applies low-frequency flexural stress to the shell. The relevant test is not single-point notched Izod from ASTM D256-10 alone; fatigue crack growth under alternating stress is assessed with ISO 18489 for slow crack growth or ASTM F1473 for polyethylene pipe notch tests adapted to moulded specimens. Field experience with rotomoulded buoys shows that failure initiates at the mould parting line where pigment concentration is higher due to localised flow. The parting line should be located away from the mooring eye and the maximum flexural strain region. UV stabilisation is mandatory. Although the red pigment screens part of the visible spectrum, UV absorbers and hindered amine light stabilisers are still required at 0.2–0.4 wt% total additive loading. Outdoor exposure in marine environments combines UV with chloride stress; the material should be tested for 5,000 h under ISO 4892-2 Method A xenon-arc ageing. A retention of tensile elongation at break of at least 60% after 5,000 h is considered acceptable for marine service. The red colourant should not shift the CIELAB a* value by more than 5 units during that exposure.
Traffic safety barriers and delineator bases made from Icorene 1761 RED 4339 are filled with ballast water or sand on site. The processing requirement is not high mechanical strength but consistent wall thickness at the fill port. A moulded wall that varies by more than ±10% from the nominal thickness creates localised flexing when the barrier is impacted. Impact test requirements for work-zone barriers are jurisdiction-specific; many North American procurement specifications reference NCHRP 350 or MASH crash test protocols for full-scale devices rather than resin-level tests. Material-level acceptance often uses ASTM D790-17 flexural modulus and ASTM D256-10 notched Izod at -20°C. The red pigmentation provides daytime visibility without the high surface temperature of black-pigmented polyethylene. Published data for the specific surface temperature differential between red and black rotomoulded LLDPE is limited; however, black-pigmented polyethylene surfaces commonly exceed 70°C under 1,000 W/m² solar irradiance, and red pigments reflect a larger fraction of visible light than black. However, the grade is not suitable for crash-rated barriers unless the full device has been tested. The resin alone provides no certification for impact attenuation.
Rotomoulded agricultural produce bins and aquatic harvest totes use the grade for impact resistance and washdown chemical resistance. The smooth densified inner surface reduces crevice contamination during cleaning with diluted sodium hypochlorite solution. Cleaning agents are used at 0.5–1.0% available chlorine; contact time should not exceed 30 min at 40°C because chlorinated oxidisers attack the polymer surface and deplete antioxidants. A drop test from 1.2 m at -20°C onto a concrete floor is the standard field acceptance criterion. Weight of the filled tote should be limited to 800 kg when the wall thickness is 6 mm, based on rotational moulding wall stress calculations. The narrow molecular weight distribution of metallocene LLDPE gives a smoother inner surface than conventional LLDPE, which reduces bacterial attachment in food handling. The red pigment, however, is not automatically compliant with food-contact indirect additive requirements. Before use in aquaculture or produce handling, the specific colourant package must be cleared under FDA 21 CFR 177.1520 or EU 10/2011, and migration testing must cover the red colourant.
Competitive LyondellBasell Icorene 1761 RED 4339 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 RED 4339 is supplied as a pre-compounded rotational moulding powder based on a metallocene-catalysed linear low-density polyethylene. The grade identifier separates the 1761 base resin from the 4339 red colour and stabilizer formulation. Compared with conventional Ziegler-Natta LLDPE, the metallocene architecture provides a narrower molecular weight distribution and a more uniform short-chain branching distribution. Published nominal values for the base resin include a melt mass-flow rate of 5.0 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022 and an unpigmented density of 0.938 g/cm³ per ISO 1183-1:2019. The red compound typically produces a rotomoulded part density near 0.939 g/cm³, with the exact value dependent on pigment loading, peak internal air temperature, and cooling rate. The product is intended for hollow parts formed in biaxial rotational moulding equipment such as shuttle, carousel, and rock-and-roll machines.
Process control is governed by peak internal air temperature rather than oven set point alone. In shuttle or carousel machines operating at a biaxial rotation ratio of 4:1 to 5:1, oven set points between 260 °C and 320 °C are common for metallocene LLDPE. The powder densifies after the mould wall crosses the crystalline melting range; for this grade the practical peak internal air temperature target lies between 190 °C and 210 °C. The tolerance around the selected peak internal air temperature set point is typically no more than ±5 °C because the narrower melting range of metallocene LLDPE creates a smaller thermal gap between incomplete sintering and thermo-oxidative degradation. Peak internal air temperature is measured with a grounded thermocouple or infrared pyrometer inserted through the vent, not inferred from oven air temperature.
Inadequate heating below the lower target produces porous walls, pinholes, wormholes, and poor drop-impact resistance. Overheating above 230 °C in air accelerates carbonyl formation, reduces elongation at break, and can shift the red surface colour. The powder particle size distribution also controls bubble removal; rotomoulding grades are typically ground to a maximum particle size of 500 µm (35 mesh). The fine fraction fills interstices and assists sintering, but excess fines can reduce bulk density and increase dust during charging. Lot-specific dry-flow time and bulk density should be obtained because the red pigment package can alter powder flow relative to the unpigmented base resin.
Cooling after densification determines shrinkage and residual stress. Slow cooling in still air reduces thermal shock but increases total shrinkage and warpage on large flat panels. Forced-air or water-mist cooling raises throughput but can lock in residual stresses at the outer skin. Because metallocene LLDPE has a narrower molecular weight distribution than high-pressure LDPE and broad-MWD HDPE, melt elasticity and mechanical integrity at the sintering stage are managed through peak internal air temperature control rather than through shear history.
Mechanical characterisation for quality control is preferably performed on rotomoulded plaques rather than compression-moulded sheet because cooling rate, inner-surface porosity, and pigment dispersion affect tensile and impact response. Under ISO 527-2:2012 at 50 mm/min, the base resin class typically shows a tensile yield stress near 18 MPa and elongation at break above 800%. Flexural modulus tested to ISO 178:2019 is commonly reported near 750 MPa. Drop-impact testing per ASTM D5276-19 at -40 °C is used to distinguish ductile from brittle failure; the material is expected to remain ductile if minimum wall thickness and curing are adequate. Environmental stress-crack resistance, tested with 100% Igepal CO-630 according to ASTM D1693-15ae1, exceeds 1000 h for the base resin class. The red colour package may increase modulus slightly through pigment volume fraction, while poorly dispersed pigment aggregates can reduce elongation. All values are typical and are not specification limits.
| Property | Method | Nominal value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | 5.0 g/10 min |
| Density | ISO 1183-1:2019 | 0.939 g/cm³ |
| Tensile yield stress | ISO 527-2:2012, 50 mm/min | 18 MPa |
| Elongation at break | ISO 527-2:2012, 50 mm/min | >800% |
| Flexural modulus | ISO 178:2019 | 750 MPa |
| Vicat softening point, A120 | ISO 306:2022 | 122 °C |
| Melting peak, DSC | ISO 11357-3:2018 | 127 °C |
| ESCR, 100% Igepal CO-630 | ASTM D1693-15ae1 | >1000 h |
| Drop impact, -40 °C | ASTM D5276-19 | Ductile/no break |
These values are drawn from class-typical mLLDPE rotational moulding data and the Icorene 1761 base resin datasheet; the RED 4339 package may shift specific values. Confirm against the current certificate of analysis before part qualification.
Differences from conventional Ziegler-Natta LLDPE rotomoulding powders become apparent at the molecular scale. Ziegler-Natta catalysts produce heterogeneous comonomer placement and a broader molecular weight distribution; this broadens the melting range and can create a wider processing exit, but it also yields lower ESCR and reduced low-temperature toughness at a given density. The metallocene base in Icorene 1761 RED 4339 provides a more uniform crystallisable sequence distribution, which raises ESCR and impact performance without increasing density. In comparison with HDPE rotomoulding powders of density above 0.945 g/cm³, the 0.939 g/cm³ density of this grade trades away flexural modulus and heat deflection capability but improves environmental stress-crack resistance and sub-zero ductility. Against high-pressure LDPE rotomoulding grades, the metallocene LLDPE offers higher modulus and better chemical resistance, but has lower melt elasticity and requires more controlled peak internal air temperature.
For moulded goods such as water storage tanks, agricultural chemical tanks, insulated boxes, and marine buoys, the design may need thicker ribs or more curvature than an equivalent HDPE part because of the lower flexural modulus. In exchange, the high ESCR of the metallocene LLDPE can extend service life when the part is exposed to detergents, polar solvents, or cyclic mechanical stress. Rotational moulders comparing this grade with other metallocene LLDPE powders should treat melt mass-flow rate and density as the primary specification boundaries; a lower-MFR variant may require a longer oven cycle but can offer a slightly higher impact response, while a higher-MFR variant may densify faster at the cost of some toughness.
Thermal analysis under ISO 11357-3:2018 records a single melting endotherm peaking near 127 °C, which is characteristic of an ethylene-hexene copolymer with a high degree of comonomer uniformity. The crystallisation exotherm during cooling appears near 107 °C at 10 °C/min in typical metallocene mLLDPE; the exact value depends on comonomer type and additive package. The narrow melting range means that heating rate and mould wall thickness have an amplified effect on the onset of densification. Thin-walled steel moulds may reach the peak internal air temperature target faster than thick aluminium moulds, and cycle development must be based on the actual mould plus part geometry rather than on resin data alone.
Rotational moulding machines for this powder should be capable of maintaining oven temperature uniformity within ±10 °C across the working volume. Insufficient air circulation can produce side-to-side temperature differences that translate into uneven wall thickness and variable peak internal air temperature. Mould release and venting also influence quality: a blocked vent can create pressure fluctuations that deform the inner wall or cause part ejection difficulties. Moulds fabricated from 3 mm to 6 mm steel or 5 mm to 10 mm cast aluminium are common; thin-wall moulds reduce cycle time but require more careful thermal control because they track oven air temperature more quickly.
Depending on end use, part qualification may also include drop tests for transport packaging under UN/DOT 49 CFR 178.603 or the applicable IMDG mandate, internal pressure resistance for tanks under EN 12573-1, and insert integrity tests. Resistance to slow crack growth can be assessed on notched specimens using ISO 16770:2019 full notch creep testing; reported data for this specific red compound is limited. For water-contact applications, extraction and organoleptic testing may be required beyond standard mechanical data.
The 4339 package is incorporated by the supplier as a pre-compounded additive system rather than a dry-blended masterbatch. Outdoor qualification should use xenon-arc weathering per ISO 4892-2:2013 with a black-standard temperature of 65 °C ± 3 °C, water spray, and periodic colour measurement under ISO 11664-4:2008 to obtain CIELAB Delta E values. Gloss retention is tracked with ISO 2813:2014. Red organic pigments can absorb more near-infrared radiation than black pigments, raise surface temperature, and show more visible fading in long outdoor service. The product should not be considered a direct substitute for carbon-black UV-stabilised compounds unless comparative weathering data on the actual wall thickness and surface finish are generated. Publicly available accelerated weathering data for this specific red formulation is limited; outdoor Florida or Arizona exposure is therefore the final qualification step for critical outdoor parts.
Minimum wall thickness at corners and parting lines controls outdoor performance more than the stabilizer content alone. Ultrasonic wall-thickness mapping is required on production parts because large flat panels and deep draw regions can develop thin inner walls due to radius-to-depth constraints. Regrind levels above 20% should be validated for colour retention, impact, and ESCR because reground surfaces contain weathered polymer and additive-depleted layers.
The base polyolefin portion falls within the scope of FDA 21 CFR 177.1520 when the end-use conditions and the regulation’s specifications are met. Food-contact use in the European Union requires evaluation of the finished article under EU Regulation (EU) No 10/2011; the red colourant and stabilizer package must be listed and the overall migration limit of 10 mg/dm² plus any specific migration limits must be demonstrated on the final part. Under REACH, the base resin contains no substances of very high concern above 0.1% w/w. Directive 2011/65/EU RoHS restricted substances are not intentionally added. Storage should be in unopened packaging below 40 °C, protected from ultraviolet radiation, and material should be used within 12 months of delivery. If condensation is visible, dehumidified-air drying at 60 °C for a maximum of 2 h is permitted; prolonged thermal exposure can deplete the stabilizer package or alter powder flow.
| Requirement | Reference | Status/condition |
|---|---|---|
| Olefin polymer food contact | FDA 21 CFR 177.1520 | Conditional on end-use conditions |
| EU plastic food-contact material | Regulation (EU) No 10/2011 | Requires pigment/additive verification |
| REACH SVHC | EC 1907/2006 | Below 0.1% w/w |
| RoHS restricted substances | Directive 2011/65/EU | Not intentionally added |
| Storage temperature | Manufacturer handling data | Max 40 °C |
| Shelf life from delivery | Manufacturer handling data | 12 months |
Compliance statements apply to the base polymer and are not a substitute for testing of the finished moulded article under the specific food-contact or outdoor-use conditions.