| HS Code | 199529 |
| Density | 0.917 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 35 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 240 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g/mil |
| Elmendorf Tear Strength Td | 300 g/mil |
| Haze | 5% |
| Gloss | 80% |
| Coefficient Of Friction | 0.2 |
As an accredited LyondellBasell Icorene 1761 RED 4328 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 RED 4328 is supplied in 25 kg moisture-resistant polyethylene bags, palletized, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL loading of LyondellBasell Icorene 1761 RED 4328 metallocene LLDPE, palletized bags, securely stowed and braced for ocean transport. |
| Shipping | LyondellBasell Icorene 1761 RED 4328 (metallocene linear low-density polyethylene) ships as non-hazardous solid pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. It is not regulated by DOT, IMDG, IATA, or ADR. Store cool and dry; keep containers closed; avoid moisture, heat, ignition, and UV. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original containers or bags closed to prevent moisture, dust, and contamination. Place on clean, dry pallets; avoid excessive stacking. Protect from weather and physical damage. Maintain good housekeeping. Follow the manufacturer’s SDS and local regulations for safe handling and storage. |
| Shelf Life | Shelf life is 24 months when stored in a cool, dry, well-ventilated area in original unopened packaging. |
LyondellBasell Icorene 1761 RED 4328 Polyethylene, Linear Low Density, Metallocene is charged as a pre-pigmented rotational molding powder into cast aluminium or fabricated steel molds mounted on carousel, shuttle, or rock-and-roll machines. In agricultural sprayer tanks, induction hoppers, and industrial liquid containment units, the nominal wall is set between 5 mm and 8 mm, with local bosses, threaded inserts, and baffle intersections increased by 40% to 60% to prevent shrinkage-induced leak paths. Oven air temperature is held at 260–290 °C, peak internal air temperature (PIAT) is controlled at 190–205 °C, and the primary/secondary arm ratio is typically 4:1 for cylindrical geometries, with primary rotation at 8–12 rpm and secondary rotation at 2–4 rpm. Demolding is initiated at a mold surface temperature of 70–80 °C, and forced-air cooling is applied at 8–12 °C/min to preserve flange flatness; water quenching is avoided on asymmetric tanks because differential shrinkage distorts the fill neck threads. Because RED 4328 is supplied pre-pigmented, dry-blending of red masterbatch is eliminated, which reduces colour streaking and pigment dust exposure; if additional UV stabilizer masterbatch is required, the carrier resin melt flow rate should be within 20% of the base resin to avoid variegation, and total addition should not exceed 4 wt% without first-article Charpy testing under ISO 179-1:2023. The powder should be stored in sealed packaging below 70% relative humidity; if exposed to humid air, drying at 60 °C for 2 h in a dry-air hopper is used to reduce surface moisture and pinhole risk. Stress cracking resistance is qualified by ASTM D1693-21 Condition B in 10% Igepal CO-630 at 50 °C; published data for metallocene LLDPE systems typically exceed 1,000 h without notched failure, but the specific RED 4328 lot should be checked against the release certificate. Chemical resistance is evaluated by ISO 175:2010 for dilute acids, alkalis, alcohol-water mixtures, and aliphatic hydrocarbon solutions at ambient temperature; continuous contact with aromatic hydrocarbons, chlorinated solvents, esters, ketones, or oxidizing acids above 20% concentration is outside the operational boundary, particularly at weld-line or threaded boss regions. When the tank is used as UN transport packaging for dangerous goods, the finished container must be type-tested under the applicable UN packaging scheme, such as UN 1H1 for non-removable-head plastics drums or UN 31H1 for composite IBCs; the resin grade alone does not confer UN certification.
Potable water expansion vessels and atmospheric storage tanks molded from Icorene 1761 RED 4328 require a reduced PIAT of 190–200 °C and an extended post-fusion hold at 200 °C for 10–15 min to minimize residual low-molecular-weight species at the internal food-contact surface. The resin falls within the olefin polymer scope of FDA 21 CFR 177.1520 when the finished article is tested for extractives under the condition-of-use simulation specified in 21 CFR 176.170(c); for the EU market, finished parts are assessed under Commission Regulation (EU) 10/2011 with an overall migration limit of 10 mg/dm² for aqueous simulants over 10 days at 40 °C. The red pigment package must also be verified against the applicable positive list for colourants in food-contact materials, because pigment migration is product-specific and cannot be inferred from base resin compliance alone. Municipal water component approvals in North America are governed by NSF/ANSI 61, while German and UK installations reference DVGW W 270 or WRAS testing for taste and odour, and these are completed on the molded article, not on the raw resin powder. Internal wall thickness should not fall below 3.5 mm on any water-bearing surface, and sharp internal corners must be radiused to at least 6 mm to prevent stress concentration and microbial adhesion. Continuous hot water exposure above 60 °C is not recommended because creep modulus decreases with temperature; published long-term hydrostatic strength data for this specific pre-pigmented formulation is limited, so hydrostatic testing under ASTM D1998-21 or EN 13341:2005 should be conducted for each tank geometry at 25 °C and 60 °C. Chlorine resistance in potable water depends on inner-surface skin integrity and antioxidant package; where free chlorine exceeds 2 mg/L, lot-specific accelerated oxidative aging should be reviewed according to the resin supplier’s published test protocol, because published third-party data for this specific pre-pigmented formulation is limited.
| Segment | Regulatory or test instrument | Test designation / clause | Operational boundary |
|---|---|---|---|
| Potable water contact | FDA 21 CFR 177.1520 / 21 CFR 176.170(c) | Extractives simulation | Continuous water contact ≤ 60 °C |
| EU food contact | Regulation (EU) 10/2011 | Overall migration, aqueous simulant | 10 mg/dm² at 40 °C / 10 days |
| UN dangerous goods transport | UN 1H1 / UN 31H1 | Drop, leakproofness, hydraulic pressure | Resin does not replace component certification |
| Chemical resistance | ISO 175:2010 | Immersion, mass and dimensional change | No aromatics, chlorinated solvents, esters, ketones, or > 20% oxidizing acids |
Rotational molded play panels, tunnel sections, and climb-through rings are molded with a wall thickness of 4–6 mm and include molded-in drain slots to prevent water accumulation and freeze cracking. Impact absorption is evaluated by ISO 8256:2004 Type II tensile-impact or ISO 6603-2:2000 puncture impact at -20 °C; playground equipment must also meet the structural requirements of EN 1176 and, where applicable, ASTM F1487 for entrapment and protrusion hazards. The red surface of RED 4328 provides high visibility without post-molding painting, but UV weathering must be qualified by ISO 4892-2:2021 Xenon-arc exposure; after 3,000 h of artificial weathering, retention of tensile elongation per ISO 527-2:2012 should be established for the part geometry. Because the red surface absorbs a higher fraction of solar radiation, black panel temperature under full sun can reach 55–65 °C even at 25 °C ambient; this thermal load must be included when calculating expansion clearances and selecting attachment points. The outer surface should not be flame-treated solely for colour correction; if attachment of anti-slip coatings is required, a plasma or corona pre-treatment with a surface energy of at least 42 mN/m is used, and adhesion is checked by cross-cut adhesion testing according to ISO 2409:2020.
Cold chain insulated container liners for pharmaceutical and food distribution are rotationally molded as hollow double-wall shells with a polyurethane foam core injected after demolding. The inner liner is made from Icorene 1761 RED 4328 with a wall thickness of 3–5 mm, the outer wall is molded at 4–6 mm, and the foam gap is maintained at 25–50 mm by molded-in stand-offs. Bonding between polyethylene and rigid PUR foam is mechanical rather than chemical, so the inner and outer shells must include dovetail ribs or undercut anchors at 150–200 mm spacing to prevent delamination during thermal cycling. The process uses a PIAT of 190–200 °C and slow forced-air cooling at 8–12 °C/min to limit warpage in large flat panels; water quenching is avoided because differential shrinkage in double-wall structures causes corner buckling. Food-contact certification of the inner surface follows EU 10/2011 and FDA 21 CFR 177.1520 extraction testing; where insulated containers transport biologics, foam blowing agent and liner permeation should be reviewed under applicable cold chain transport protocol ISTA 7E. Published data for this specific red-pigmented mLLDPE under frozen storage at -40 °C is limited; low-temperature impact behaviour should be confirmed by ISO 179-1/1eA Charpy with notched specimens at -30 °C on molded test plaques.
Marine floats, buoy shells, and dock fenders molded from RED 4328 are produced with wall thicknesses between 6 mm and 12 mm and are filled with closed-cell polyurethane foam rated for permanent immersion. The foam fill density is typically 60–100 kg/m³, and the fill hole is plug-sealed by hot-plate welding of a molded PE plug. Seawater ageing is assessed by ISO 4611:2010 cyclic salt spray and humidity exposure, with tensile property retention measured under ISO 527-2:2012 after 1,000 h; UV weathering is tested under ISO 4892-3:2021 QUV or ISO 4892-2:2021 Xenon-arc, and colour shift of the red surface is quantified by ISO 7724-3:2019. Impact after prolonged water immersion is evaluated by ISO 6603-2:2000 instrumented puncture at -20 °C to verify that plasticization or oxidation has not reduced energy absorption. Zinc stearate mold release residues must be fully removed before adhesive bonding of navigation brackets, because surface contamination below 38 mN/m causes bond failure; a water-break test is used as a field check. The supplied pre-coloured grade is not formulated for long-term immersion in aromatic fuel or bilge cleaner concentrates; immersion in such media is outside the operational boundary unless a chemical resistance barrier liner is used.
| Property evaluated | Method reference | Test condition | Application interpretation |
|---|---|---|---|
| Tensile yield | ISO 527-2:2012 | 23 °C, 50 mm/min | Molded part QC |
| Charpy impact | ISO 179-1:2023 | -30 °C, notched 1eA | Cold chain and marine impact |
| Puncture impact | ISO 6603-2:2000 | -20 °C, instrumented striker | Playground and automotive reservoir service |
| Tensile-impact | ISO 8256:2004 | Type II double notch | Dynamic tear of rotationally molded parts |
| ESCR | ASTM D1693-21 | 10% Igepal, 50 °C | Agricultural and industrial containment |
For automotive fluid reservoir bodies such as coolant surge tanks and diesel exhaust fluid (DEF) storage housings, Icorene 1761 RED 4328 is rotationally molded on shuttle machines with 3–5 mm wall sections using aluminium tooling that includes cavity pressure relief vents. Inserts for level sensors and filler necks are placed at indexed locations; post-molding leak testing is performed at 0.5 bar internal air pressure under water. DEF compatibility with 32.5% urea solution is checked by ISO 22241-2:2019 liquid exposure, with weight change held below 2% after 72 h at 60 °C; coolant reservoir performance is tested under pressure cycling from -40 °C to 95 °C, but continuous operation at the upper end exceeds the recommended long-term creep limit for metallocene LLDPE and requires derating and venting. Rock impact resistance is evaluated by ISO 6603-2:2000 at -30 °C, and the reservoir must pass a drop test from 1.5 m at -20 °C onto a granite impact surface. Because RED 4328 is pre-pigmented red, it is used for agricultural vehicle or aftersales reservoirs where colour indicates coolant or fluid type; it is not a drop-in replacement for multi-layer coextruded HDPE fuel tanks, and the resin must not be used for gasoline, diesel, brake fluid, or organic refrigerant contact.
Because RED 4328 enters the final part as a pre-pigmented powder, industrial material handling bins, hoppers, and security boxes are molded in single-step carousel machines without a separate dry-colour blending station, which shortens housekeeping and reduces cross-colour contamination. Wall sections are typically 6–10 mm, with corner radii not less than 8 mm to distribute forklift impact energy. Static compressive strength is evaluated by ASTM D642-20 on a full-size bin or representative panel, and repeated impact resistance is assessed by a 20 kg hemispherical striker drop from 1.0 m at -20 °C; first-article testing is required because published data for this specific grade in large welded or molded hoppers is limited. The red pigmented surface is suitable for safety-interlock zones, but it is not permanently antistatic; in flammable atmosphere areas, addition of conductive carbon black or insertion of a grounded steel frame is required to avoid surface charges above 10⁶ Ω/square. Continuous contact with hydrocarbon-based cutting fluids, ester-based hydraulic fluids, or solvent-based cleaning agents should be avoided unless a compatibility patch test has been performed under ISO 175:2010 on a molded plaque from the same lot.
Competitive LyondellBasell Icorene 1761 RED 4328 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The grade designation LyondellBasell Icorene 1761 RED 4328 identifies a pre-colored linear low density polyethylene produced with a metallocene catalyst system. The base resin, Icorene 1761, belongs to the metallocene LLDPE class in which the catalyst permits a narrow molecular weight distribution and uniform short-chain branching distribution across the molecular weight range. The suffix RED 4328 is understood from the grade nomenclature to denote an integrated red colorant system compounded into the polyethylene matrix. Published data for this specific pre-colored formulation are limited; therefore, the processing parameters and property boundaries stated herein are drawn from the general behavior of metallocene LLDPE film grades and from documented interactions between polyolefin matrices and red pigments. Any production qualification must be confirmed against the current LyondellBasell technical data sheet and the applicable food-contact compliance documentation.
The metallocene catalyst architecture yields a polyethylene with a polydispersity index, Mw/Mn, typically between 2.0 and 3.0 when measured by gel permeation chromatography according to ISO 16014-4. A conventional Ziegler-Natta linear low density polyethylene of equivalent melt index and density often exhibits Mw/Mn in the range of 3.5 to 5.0. The narrower distribution reduces the concentration of very high molecular weight chains, which lowers melt elasticity at shear rates relevant to blown film and cast film extrusion. The more homogeneous comonomer placement in mLLDPE generates a greater fraction of tie chains and lowers the seal initiation temperature by approximately 5–15°C relative to a Ziegler-Natta resin of the same density and melt index, as determined by ASTM F1921 or ASTM F88 heat seal testing. In a lamination sealant web, that characteristic permits jaw sealing temperatures between 110°C and 140°C, depending on film thickness, seal dwell time, and pressure.
Specification of the base resin is defined by melt index, density, and film mechanical properties. Melt index is measured under ISO 1133-1:2022 at 190°C and 2.16 kg; metallocene LLDPE blown film grades of this architecture generally fall between 0.5 g/10 min and 2.0 g/10 min. Density is reported under ISO 1183-1:2019; the typical range for linear low density film grades lies between 0.915 g/cm³ and 0.925 g/cm³. Tensile yield and elongation at break on 25 µm film are measured by ISO 527-3:2018 or ASTM D882-18. Elmendorf tear propagation is tested under ISO 6383-2 or ASTM D1922; dart impact is tested under ASTM D1709 method A or B. The pre-colored variant RED 4328 may exhibit reduced dart impact values relative to the natural base resin; organic red pigments can reduce impact strength by 5–15% depending on pigment particle size, dispersion quality, and loading. The exact tensile, tear, and impact values for this grade must be verified from the manufacturer’s datasheet, because the red pigment type influences crystalline nucleation and film solidification.
| Property | Test method | Metallocene LLDPE typical | Ziegler-Natta LLDPE typical |
|---|---|---|---|
| Molecular weight distribution, Mw/Mn | ISO 16014-4 | 2.0–3.0 | 3.5–5.0 |
| Melt index | ISO 1133-1 | 0.5–2.0 g/10 min | 0.5–2.0 g/10 min |
| Density | ISO 1183-1 | 0.915–0.925 g/cm³ | 0.915–0.925 g/cm³ |
| Seal initiation temperature | ASTM F1921 | 5–15°C lower | Reference |
| Dart impact, 25 µm film | ASTM D1709 | 50–100% higher | Reference |
| Haze, 25 µm film | ASTM D1003 | 3–10% | 5–15% |
Data are typical ranges for film grades; exact Icorene 1761 RED 4328 values require the LyondellBasell technical data sheet.
Organic red pigments used in polyolefin masterbatches can undergo thermal degradation at sustained melt temperatures above 240–260°C. Iron oxide red pigments are more thermally stable but may act as heterogeneous nucleating agents and can catalyze polyethylene oxidation if the pigment surface is not adequately passivated. For the RED 4328 formulation, the recommended melt temperature range in blown film extrusion should not exceed 230°C unless verified by color shift measurements and melt flow stability tests. A screen pack of 100–250 µm mesh is typically installed upstream of the die to remove pigment agglomerates and to raise backpressure for improved dispersive mixing. Melt pressure variations greater than 5% over a 30-minute run may indicate filler or pigment agglomeration in the feed throat or screw wear. The narrow molecular weight distribution of the metallocene base resin imparts low melt elasticity, which reduces die swell and permits use of a die gap of 1.0–2.0 mm for blown film at blow-up ratios between 2.0:1 and 2.5:1.
On a production-scale single-screw extruder with an L/D ratio of 25:1 to 30:1 and a barrier screw, barrel zone temperatures for metallocene LLDPE are frequently set 10–20°C lower than those for a Ziegler-Natta grade of the same melt index. Because the metallocene resin has a narrower molecular weight distribution, viscous heat generation is lower and the melt temperature measured at the adapter is more responsive to screw speed changes. A temperature profile of 160°C to 200°C from the feed zone to the metering zone is often adequate, with the adapter and die maintained at 200–220°C. The frost line height in blown film should be established above the die face at a distance that permits sufficient bubble cooling without excessive orientation; for 25–50 µm film, a frost line height of 100–200 mm is typical on lines with dual-lip air rings. The colorant in RED 4328 can increase melt viscosity slightly; therefore, the screw amperage may be 5–10% higher than that of natural Icorene 1761 under identical conditions.
In laminated flexible packaging, the red pre-colored grade can serve as the sealant web in a structure where a metallocene sealant layer is required for low seal initiation temperature and high hot tack. Hot tack strength measured per ASTM F1921 at 100–130°C is commonly specified because the seal region retains load-bearing capacity before cooling; the narrow comonomer distribution of mLLDPE improves hot tack relative to broad-MWD resins. The red colorant must comply with food contact additive restrictions. In the European Union, the overall migration limit for plastic food contact materials is 10 mg/dm² per Regulation (EU) 10/2011, and colorants are required to be evaluated for specific migration under the assigned simulant conditions. In the United States, olefin polymers may be used in contact with food under 21 CFR 177.1520, provided that the finished article meets extraction limitations and the colorant is covered by a suitable food additive regulation or colorant approval.
Typical downstream converting operations for the RED 4328 pre-colored mLLDPE include blown film extrusion for form-fill-seal packaging, lamination sealant webs, and heavy-duty sacks where a red side or red identification strip is required. The material differs from a C4-based Ziegler-Natta LLDPE in its lower seal initiation temperature, higher dart impact, and improved organoleptic properties, although the red pigment may offset some haze and gloss benefits. Compared with low density polyethylene produced by high-pressure radical polymerization, the metallocene LLDPE base resin exhibits higher tensile strength and elongation but lower melt strength, which restricts bubble stability at high blow-up ratios. Converters that require deep-draw thermoformability or high melt strength for large-diameter blown film should consider blending with LDPE or processing on equipment with internal bubble cooling.
| Requirement | Designation | Scope |
|---|---|---|
| US FDA food contact | 21 CFR 177.1520 | Olefin polymers used in contact with food; extraction limitations apply. |
| EU food contact | Regulation (EU) 10/2011 | Overall migration limit 10 mg/dm²; specific migration for colorants. |
| REACH | Regulation (EC) 1907/2006 | SVHC content below 0.1 wt% per article. |
| RoHS | Directive 2011/65/EU | Heavy metal restrictions for electrical and electronic applications. |
With the pre-colored grade, the extruder screw design should incorporate a Maddock or spiral mixer element to distribute the pigment without excessive shear heating. Specific energy consumption for mLLDPE blown film typically ranges from 0.20 kWh/kg to 0.30 kWh/kg on modern extruders; the addition of dispersed pigment may raise this value by 0.02–0.05 kWh/kg. At a die diameter of 100 mm and a die gap of 1.5 mm, an output rate of 80–120 kg/h is achievable for this resin class on a 60 mm extruder, but the exact output depends on screw geometry, melt temperature, and colorant loading. The melt wastage during purging should be monitored; red pigments can leave residue on the die lips and require longer purging than natural grades. Film haze and gloss are measured under ASTM D1003 and ASTM D2457; pigmented film typically reports higher haze values than unpigmented metallocene LLDPE of the same thickness.
The RED 4328 pre-colored resin should not be dry-blended with polypropylene or ethylene vinyl acetate at ratios above 10 wt% for sealant applications, because phase separation can reduce seal strength and create visible gels. Pre-drying is generally not required at ambient relative humidity below 60%; however, if the resin has been stored in unsealed containers in humid conditions, drying at 70–80°C for 2–4 hours may be necessary to prevent surface moisture defects. Reclaimed film trim of the pigmented grade can be re-extruded at levels up to 20 wt% without major property loss, but the red color intensity may shift with repeated heat history. The formulation should be protected from long-term UV exposure because organic red colorants can fade; outdoor film applications require the addition of hindered amine light stabilizers or the use of inorganic red pigments.