Lyondellbasell Icorene 1761 Red 4326 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 RED 4326 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 RED 4326 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 857716
    Density 0.918 g/cm³
    Melt Flow Rate 1.1 g/10 min
    Hardness Shore D 46
    Tensile Strength At Yield 8.00 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 600%
    Flexural Modulus 0.200 GPa
    Notched Izod Impact 0.800 J/cm
    Melting Point 112 °C
    Vicat Softening Point 88.0 °C
    Deflection Temperature At 0 46 Mpa 45.0 °C
    Haze 10%
    Gloss 70%
    Color Red

    As an accredited LyondellBasell Icorene 1761 RED 4326 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged as 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped, for LyondellBasell Icorene 1761 RED 4326 metallocene LLDPE.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized, stretch-wrapped 25 kg bags of LyondellBasell Icorene 1761 RED 4326 metallocene linear low-density polyethylene.
    Shipping LyondellBasell Icorene 1761 RED 4326 is shipped as non-hazardous, solid polyethylene pellets in moisture-barrier bags or bulk containers. It is not classified as dangerous goods for transport. Keep dry, away from heat, and follow standard warehouse handling; no special DOT/IMDG/IATA hazard labels required.
    Storage Store indoors in a cool, dry, well-ventilated area in original, sealed containers. Protect from direct sunlight, heat, moisture, and contamination. Keep away from strong oxidizers, ignition sources, and steam lines. Avoid excessive stacking and dust generation; ground equipment to prevent static. Maintain good housekeeping and use FIFO stock rotation. Ideal ambient temperature, below 50°C.
    Shelf Life Typically 24 months when stored unopened in original packaging in a cool, dry place, protected from direct sunlight and heat.
    Application of LyondellBasell Icorene 1761 RED 4326 Polyethylene, Linear Low Density, Metallocene

    On a biaxial rotational moulder running an arm ratio of 4:1 and an oven set point of 295–310°C, LyondellBasell Icorene 1761 RED 4326 is charged directly at 100 wt% as supplied. No additional pigment masterbatch or dry colourant is introduced at the machine, because the red additive package is already dispersed during the resin producer’s compounding step. The process target is a peak internal air temperature of 205–220°C; below 200°C the metallocene LLDPE leaves partially sintered core particles that become pinholes in 6–12 mm wall sections, while above 225°C the organic red pigments begin to show chroma drift and the olefin matrix generates oxidation by-products that can condense on the mould surface and increase release drag. Lot-release mechanical testing for road-side safety parts is anchored to ASTM D5628-18 falling-weight impact at −40°C, supplemented by tensile modulus and elongation data under ASTM D638-14. Because regional traffic-control authorities require strict red chromaticity, converters frequently perform laboratory xenon-arc exposure under ASTM D2565-23 at 340 nm and 0.35 W/(m²·nm) to confirm colour-shift limits over 2,000 h; published certificates for this exact colorant under national highway photometric protocols are limited. Downstream production includes pneumatic powder loading, oven residence of 18–24 min for an 8 mm nominal wall, forced-air cooling at 0.5–1.0°C/s until the demoulding temperature falls below 70°C, and parting-line trim with a 2–4 mm flash allowance. Finished part types include median divider nose covers, rigid delineator base shells, guardrail transition end caps, and temporary work-zone channelizer bodies.

    What ESCR threshold governs red mLLDPE service in fertiliser tank bodies?

    Liquid fertiliser concentrates containing ammonium nitrate and potassium chloride exert environmental stress cracking on polyethylene because the localised stress at the tank floor knuckle is intensified after urea-bearing solutions reduce the tie-molecule entanglement density. The compound is rotomoulded at 100 wt%; a converter will normally avoid letting down a colour-matched grade because red organic pigments and iron oxide pigments split at different rates during dry blending, producing streak lines along the interior wall. The governing standard for a stationary polyethylene tank is ASTM D1998-21, with particular reference to the hydrostatic and environmental stress-crack resistance clauses. The resin is further screened under ASTM D1693-15, condition A, 100% Igepal CO-630, at 50°C. Comparable metallocene LLDPE rotomoulding grades can show F50 values above 1,000 h, although published data for this exact red formulation is limited and the tank fabricator must obtain batch-specific ESCR data before certifying a multi-year warranty. The downstream manufacturing route uses a shuttle-type rotational moulder with oven temperature 290–310°C and peak internal air temperature 210–218°C; wall thickness at the base knuckle is maintained at 5–8 mm and the floor-to-wall transition is radiused to at least 25 mm to reduce the stress concentration factor. The cycle includes a water-mist quench from 180°C to 90°C at 0.8–1.5°C/s, but the cooling rate is deliberately retarded for tank service because quenching too rapidly raises crystallinity and can reduce ESCR. End products are red non-potable agricultural mixing tanks, fertigation day tanks, nursery brackish-water reservoirs, and small-scale liquid feed carts.

    Because wave-frequency flexing and salt-spray UV exposure simultaneously attack the weld lines of rotationally moulded flotation bodies, the red buoy shell is evaluated for both low-temperature peel and environmental stress crack resistance after accelerated weathering. Charging is conducted at 100 wt% as supplied; no additional UV masterbatch is dry-blended unless the buoy is specified for tropical service beyond 36 months, in which case the converter must revalidate the outer-surface stabiliser level by infrared spectroscopy before moulding. Density is controlled under ASTM D1505-18 and is normally held within 0.935–0.945 g/cm³ for this rotomoulding family. ESCR testing follows ASTM D1693-15 at 50°C in 100% Igepal CO-630, while xenon-arc weathering follows ASTM D2565-23. A 10 mm buoy shell made from the metallocene LLDPE fuses more uniformly than a conventional Ziegler-Natta LLDPE at equivalent oven residence time, but the upper peak internal air temperature is held below 220°C to prevent organic pigment degradation and surface roughness on the waterline band. Tooling is typically cast aluminium or fabricated steel, with oven setpoints between 280°C and 320°C. Demoulding occurs only after the shell surface reaches 65°C or lower, preventing post-demoulding distortion of the large curved hull. Finished products include starboard channel markers, regulatory buoy bodies, aquaculture flotation collars, and crane-slung marine hose floats.

    Playground Structures and the Need for Third-Party Migration Compliance

    Red rotomoulded slides, tunnel sections, and guard panels are subject to two separate regulatory regimes: mechanical loading under ASTM F1487-21 and chemical migration under EN 71-3:2019+A1:2021. The pre-compounded red powder is charged at 100 wt%; converters that dilute with uncoloured mLLDPE at 5–10 wt% to reduce pigment cost routinely lose the documented migration certification for the finished component, because migration limits must be demonstrated on the final moulded plaque or part, not on the masterbatch. The manufacturing sequence uses cast aluminium or CNC-machined steel moulds, oven setpoints of 285–310°C, and a peak internal air temperature of 205–215°C. After demoulding at 70°C, the parts are not post-cured; the metallocene resin achieves acceptable inter-particle fusion without the long thermal soak cycles sometimes used for high-density polyethylene. For red play components, the processor also monitors wall thickness at the entry and exit radii, because thinning below 4 mm creates a pinch point that fails the structural loading provisions of ASTM F1487-21. Finished component types include red roof caps, slide bed sections, crawl tunnel segments, climbing step housings, and spring-rider body shells.

    Compliance matrix for red mLLDPE playground components
    Test targetStandardTypical requirement or condition
    Heavy metal migration from coloured polymerEN 71-3:2019+A1:2021migration limits for 19 elements in mg/kg
    Impact attenuation of surrounding surfacingASTM F1292-18peak 200 g and HIC 1000 threshold
    Structural loading and entrapmentASTM F1487-21load-bearing joints and opening dimensions
    UV durability of pigmented surfaceASTM D2565-23xenon-arc, 340 nm, 0.35 W/(m²·nm)

    For food-processing totes and ice-slurry tanks, the decisive variable is not low-temperature impact but total extractables under FDA 21 CFR 177.1520 and colourant clearance under 21 CFR 178.3297. The red mLLDPE compound is charged at 100 wt%; regrind is not used in food-contact production unless the converter holds a written extended-compliance statement for the specific regrind fraction and processing history. Moulding is performed on a carousel machine at 290–305°C oven temperature and peak internal air temperature 205–215°C; mould release is restricted to food-grade grades, and the water-mist cooling phase is controlled to avoid creating a quenched skin with higher extractable migration. Wall thickness is typically 4–7 mm for stackable totes and 6–10 mm for insulated fish boxes. Comparable metallocene LLDPE grades in food-contact service demonstrate low total migration when tested under EU Regulation 10/2011, but published food-contact documentation for this exact red colorant is limited and the converter must secure a written compliance statement before commercial use. End product types include red cold-chain fish boxes, ice-slurry transfer totes, poultry processing trays, and colour-coded ingredient handling bins.

    When utility enclosure shells are moulded for cold-climate cable pedestal housings, the low-temperature impact sequence is the first gate

    Cold-climate service restricts the use of general-purpose rotomoulding grades because the ductile-to-brittle transition of standard LLDPE can occur at temperatures above −20°C, whereas metallocene LLDPE formulations with controlled short-chain branch distribution retain ductility below −40°C. The red compound is introduced at 100 wt%, though up to 15 wt% of clean internal regrind from trimmed parting-line flash is accepted by many processors when the part is not used in fire-rated electrical enclosure applications; every regrind percentage above zero shifts the low-temperature impact curve and must be revalidated under ASTM D5628-18 at −40°C. Conformance is also assessed under ASTM D638-14 for welded sections and ASTM D1693-15 for ESCR, because cable pedestal housings develop wind-induced flexural stress at the base flange. Rotomoulding is carried out on a carousel line with a 6:1 arm ratio, oven temperature 295–320°C, and peak internal air temperature 212–222°C; wall thickness is held to 5–9 mm. Demoulding waits until the part surface temperature is below 65°C to prevent post-demoulding warpage of the large flat side walls. Finished products are red cable pedestal housings, traffic signal access cabinets, and exterior utility enclosure lids.

    Free Quote

    Competitive LyondellBasell Icorene 1761 RED 4326 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 RED 4326 is a pre-coloured rotational moulding powder manufactured from a metallocene-catalysed linear low density polyethylene (mLLDPE). The base resin designation Icorene 1761 identifies a single-site metallocene grade designed for rotational moulding; the suffix RED 4326 denotes the compounded red pigment package. It is supplied as a free-flowing powder suitable for charging directly into closed moulds on carousel, rock-and-roll, and shuttle rotational moulding machines. The grade is used where a combination of low-temperature impact, environmental stress-crack resistance, and a consistent red finish is required, including chemical storage vessels, agricultural hoppers, marine buoys, portable sanitary equipment, and exterior enclosures. Because published technical data for the red-pigmented formulation is limited, mechanical values should be considered representative of the Icorene 1761 base resin and confirmed against the supplier’s certificate of analysis for each production lot.

    Material specifications evaluated before use include melt flow rate, density, tensile properties, flexural modulus, and environmental stress-cracking resistance. Representative values for the Icorene 1761 base grade are shown in Table 1. The red pigment package may shift absolute values by ±5–10% depending on dispersion quality and pigment volume fraction.

    Table 1: Representative mechanical and thermal properties for Icorene 1761 base mLLDPE
    PropertyRepresentative valueTest method
    Density0.938 g/cm³ASTM D1505
    Melt flow rate (190 °C, 2.16 kg)6.5 g/10 minASTM D1238
    Tensile yield strength20 MPaASTM D638-14
    Tensile elongation at break750 %ASTM D638-14
    Flexural modulus (1% secant)850 MPaASTM D790
    Melting peak temperature127 °CASTM D3418
    Environmental stress-cracking resistance (F50, 100% Igepal, condition B)>1000 hASTM D1693

    What separates metallocene linear low density polyethylene from Ziegler-Natta and chromium-catalyzed rotational molding grades?

    From a polymer architecture perspective, the single-site metallocene catalyst produces a narrow molecular weight distribution. Mw/Mn for metallocene grades is generally below 2.5, whereas conventional Ziegler-Natta LLDPE and HDPE used in rotational moulding often range from 3.5 to 6.0. The narrow distribution lowers the fraction of low-molecular-weight chains that contribute to extractables and taste/odor, and it reduces high-molecular-weight tails that increase melt elasticity and bubble retention. In rotational moulding, these differences appear as shorter fusion and bubble-removal times under equivalent oven heat, but also a sharper melting peak and a narrower temperature interval between adequate densification and surface oxidation.

    The comonomer distribution is also more homogeneous. In conventional Ziegler-Natta LLDPE, butene or hexene comonomer tends to concentrate in lower-molecular-weight fractions; in metallocene LLDPE, the comonomer is inserted uniformly across the molecular weight range. This uniformity increases the number of tie molecules in the amorphous phase, which improves environmental stress-cracking resistance at a given density. It also reduces density-dependent embrittlement observed in Ziegler-Natta grades. Compared with a Ziegler-Natta LLDPE of identical density and melt index, Icorene 1761 can provide higher low-temperature impact and ESCR, though its narrower molecular weight distribution can reduce sag resistance and require tighter temperature control.

    Compared with chromium-catalyzed HDPE rotational moulding grades, Icorene 1761 RED 4326 is lower in stiffness. A chromic HDPE with density 0.945 g/cm³ typically exhibits flexural modulus values of 1,000–1,300 MPa, whereas the lower-density mLLDPE base is approximately 850 MPa. The mLLDPE grade compensates through higher elongation at break and improved resistance to stress cracking. For parts requiring load-bearing rigidity, HDPE may be preferred; for complex hollow parts needing low warpage and impact toughness, the metallocene LLDPE offers better dimensional stability in demolding.

    At rotational moulding shear rates, typically below 10 s⁻¹, the melt behaves as a near-Newtonian fluid. The zero-shear viscosity at 190 °C for a 6.5 g/10 min mLLDPE is approximately 1,000–1,500 Pa·s; this is lower than the 1,800–2,500 Pa·s commonly observed for a 4 g/10 min HDPE rotomolding grade. The lower viscosity aids bubble migration, but the narrow distribution reduces the elastic component needed to prevent melt drainage in deep draw areas. Moulds with deep pockets may require rotation ratio adjustment or internal hot-air redistribution to prevent wall-thickness variation.

    On production-scale carousel rotational moulding machines with aluminium or sheet-steel tools, the powder is charged at ambient temperature, typically 20–30 °C. The mould is rotated in two perpendicular axes at a ratio of 4:1 or 5:1, depending on part geometry. Oven temperature setpoints in gas-fired forced-air ovens are commonly 260–280 °C. The peak internal air temperature measured by an infrared vent probe should reach 180–200 °C before cooling. The pigmented grade may require an increase in oven residence time of 5–10% relative to natural material because red pigments can have lower infrared absorption than carbon black and may reduce the heating rate of the powder bed. Operators should monitor internal air temperature and not rely solely on oven time, because tool mass, wall thickness, and oven loading affect heat transfer.

    After peak internal air temperature is reached, the mould is moved to the cooling station. Forced-air cooling to a part surface temperature below 70 °C before demoulding is recommended. Rapid water-mist cooling may reduce cycle time but can increase warpage in flat sections and promote mould surface corrosion. When molding parts with wall thickness above 8 mm, a stepped cooling profile is used, with low air velocity for the first 2–3 min to allow crystallization to proceed from the outside inward.

    Observed failure modes on production lines include pinholes at thin corners, internal bubble streaks, and localized yellowing at mould contact points. Pinholes are commonly caused by coarse powder fractions or insufficient peak internal air temperature. Internal bubble streaks arise when the melt viscosity remains too high to release dissolved volatiles; raising the peak internal air temperature toward 200 °C usually reduces this. Localized yellowing at mould contact points indicates excessive mould surface temperature; infrared pyrometer mapping of the mould surface should be used to identify hot zones caused by uneven oven airflow.

    Rotational Molding Powder Characteristics and Process Limits

    Rotational moulding powders for Icorene 1761 RED 4326 are typically produced by cryogenic pulverization of compounded pellets. Particle-size distribution and dry flow have direct effects on inside-surface finish and pinhole formation. A typical specification band for rotomoulding grades is 95% below 500 µm, with 10–20% below 100 µm. Dry flow values measured by funnel methods are often in the range 25–35 s/100 g. Excessive fines increase powder agglomeration and reduce bulk density; coarse particles may not fuse completely and can leave undispersed particles at the interior surface. The red pigment package is dispersed at the compounding stage to minimize agglomerates above 50 µm, which can act as stress concentrators in thin walls.

    The melt flow rate of 6.5 g/10 min places the base resin in the medium-flow range for rotational moulding. This flow range is high enough to densify thin-wall sections down to approximately 2 mm when mold geometry is adequate, but low enough to avoid excessive drainage and wall-thickness variation in deep cavities. Higher-melt-index grades may be used for extremely thin-walled parts, but they usually sacrifice ESCR. Lower-melt-index grades require longer oven residence times but provide better melt strength.

    Temperature limits are critical. Prolonged oven residence above 290 °C accelerates oxidative degradation of the metallocene polyethylene. The polymer can exhibit chain scission, melt flow drift, yellowing, and a reduction in low-temperature impact. The recommended peak internal air temperature should not exceed 220 °C for more than a few minutes. In high-oven-load production batches, temperature overshoot can occur when the carousel is stopped; production control systems should include automatic oven temperature setback or alarm at 300 °C.

    Moisture absorption is less severe than for polyamides or polycarbonates, but surface moisture on cold powder can be entrapped during fusion and create internal porosity. If stored at relative humidity above 60%, the powder can be pre-dried at 70–80 °C for 1–2 h in a desiccant dryer. Agglomerated powder should be screened before loading. The product is not intended for outdoor permanently exposed applications without UV stabilization; although the red pigment may provide some visible-light shielding, the base resin specification does not guarantee long-term UV retention unless an additional stabilizer package is specified.

    Colour consistency between lots should be controlled with a spectrophotometer using CIELAB ΔE 1.0 maximum against an agreed master standard. Dilution of RED 4326 with natural Icorene 1761 on the production floor should not be performed without documented validation, because changed pigment volume fraction also alters infrared absorption, fusion rate, and final shrinkage. Dry blending of external pigments is similarly undesirable; it can create colour streaks and local agglomerate concentrations that reduce low-temperature impact.

    Batch-to-batch variance in the red pigment package can influence the onset of crystallization and the peak melting point. Pigment particles can act as nucleating agents, shifting crystallization onset to higher temperatures. This shift may reduce post-mold shrinkage after 24 h at 23 °C and 50% relative humidity, but it can also increase warpage in unsymmetrical parts if cooling is not uniform. Dimensional inspection should follow ASTM D955 after conditioning for 24 h to separate reversible thermal expansion from post-crystallization shrinkage.

    Regulatory and standards verification is summarized in Table 2. Compliance must be revalidated for the specific red colorant formulation and final article, because pigment migration limits and overall migration limits are article-dependent.

    Table 2: Compliance matrix for the product family
    Regulatory or standards areaDesignationApplication assertion
    Food-contact material21 CFR 177.1520(c)Olefin polymers for articles intended for food contact, subject to extraction limits.
    European food-contact plastics(EU) No 10/2011Overall migration and specific migration limits for plastics in food contact; colorants must comply separately.
    REACH registrationRegulation (EC) No 1907/2006Registration obligations apply at import/manufacture; SVHC content must be checked per lot.
    Hazardous substances in electrical equipmentDirective 2011/65/EURoHS restricted heavy metals; applicable only when the part is used in electrical/electronic equipment.
    Melt flow rate testISO 1133-1:2022 / ASTM D1238Verification of batch consistency and degradation.
    Tensile testingASTM D638-14Tensile yield and elongation at break for incoming quality control.

    For double-wall chemical containment trays, fertilizer hopper bodies, marine buoys, and medical waste containers, the one-piece hollow construction produced by rotational moulding eliminates welded seams that often fail in stress-cracking tests. The precolored red grade removes a secondary painting step, but parts used outdoors should be evaluated for chalking and colour fade under accelerated weathering according to ASTM G155 or ISO 4892-2. The product should not be used in continuous service above 60–70 °C without a supplementary thermal stabilizer. Long-term contact with concentrated oxidizing acids, aromatic hydrocarbons, or aggressive surfactant solutions can reduce environmental stress-cracking resistance, particularly in thick-wall sections with high residual stress.

    Published data for these specific application configurations is limited; therefore, prototype trials on production-scale equipment with representative mould geometry and oven loading are required to establish part-specific cycle time, peak internal air temperature, and post-mold shrinkage limits.

    Top