Lyondellbasell Icorene 1761 R Whi 1400 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 R+ WHI 1400 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 R+ WHI 1400 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 168580
    Density 0.918 g/cm³
    Specific Gravity 0.918
    Melt Mass Flow Rate Mfr At 190 C 2 16 Kg 1.7 g/10 min
    Tensile Strength At Yield 9.00 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 500%
    Tensile Modulus 0.150 GPa
    Flexural Modulus 0.200 GPa
    Dart Drop Impact 150 g
    Elmendorf Tear Strength 120 g
    Haze 7.0%
    Gloss 80%
    Melting Point 116°C
    Vicat Softening Temperature 100°C
    Crystallization Temperature 100°C

    As an accredited LyondellBasell Icorene 1761 R+ WHI 1400 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 R+ WHI 1400 is supplied in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg total).
    Container Loading (20′ FCL) 20′ FCL container loading for LyondellBasell Icorene 1761 R+ WHI 1400 metallocene LLDPE; 25 kg bags, palletized, cargo securely stowed.
    Shipping LyondellBasell Icorene 1761 R+ WHI 1400 is shipped as solid metallocene LLDPE resin in 25 kg polyethylene bags, palletized, stretch-wrapped, and labeled. It is non-hazardous for transport. Store cool, dry, and ventilated, away from heat, sparks, and direct sunlight. Avoid dust; use standard PPE.
    Storage Store LyondellBasell Icorene 1761 R+ WHI 1400 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers or bags closed to prevent moisture, dust, and contamination. Use appropriate PPE when handling. Maintain ambient temperature, avoid prolonged UV exposure, and follow local safety regulations.
    Shelf Life Polyethylene resin is stable under normal storage conditions; protect from heat, moisture, UV light. No specific shelf life generally assigned.
    Application of LyondellBasell Icorene 1761 R+ WHI 1400 Polyethylene, Linear Low Density, Metallocene

    Stationary liquid storage tanks for water treatment, chemical dosing, and pump skid reservoirs are rotomoulded as single-wall shells with integrally formed flanged nozzles, baffle supports, and lifting lugs. A production formulation for this segment is built on 100 parts by weight of LyondellBasell Icorene 1761 R+ WHI 1400, with 0.20–0.50 phr high-molecular-weight hindered amine light stabiliser, 0.05–0.15 phr primary antioxidant, 0.05–0.10 phr secondary phosphite antioxidant, and 0.5–1.5 phr white or light-blue pigment concentrate. Potable-water contact parts are evaluated under NSF/ANSI 61 after moulding; resin-level food-contact suitability is defined by FDA 21 CFR 177.1520 for olefin polymers, and industrial chemical tank construction is tested under EN 13575 and ASTM D1998 where applicable. On a three-arm carousel rotational moulding line, the mould is charged with the dry-flowing powder, closed, and rotated biaxially with a primary-axis speed of 6–8 min⁻¹ and a primary-to-secondary speed ratio of 4:1 for cylindrical vertical tanks; oven chamber air temperature is held at 260–300 °C, and peak internal air temperature is raised to 190–205 °C before forced-air cooling at 5–10 m/s. Wall thickness for chemical containment is specified in the range 4–8 mm, with the upper dome and threaded bosses receiving the least thickness in field measurements. Terminal finished products include vertical and horizontal storage tanks from 500 L to 20,000 L, conical-bottom dosing tanks, and pump skid reservoirs. The critical processing boundary is peak internal air temperature: exceeding 210 °C has been associated with inner-surface oxidative embrittlement, and subsequent microcracking at threaded bosses after 3–6 months of dilute sodium hypochlorite contact; falling below 190 °C leaves partially coalesced powder at the dome-to-sidewall junction. Batch-to-batch dry-flow variation outside ±2 s/100 cm³ measured by ASTM D1895 has shifted wall-thickness distribution at the upper dome by more than 10% on production-scale carousels, increasing pinhole frequency along the mould parting line. Published data for every additive combination are limited; the final article must be tested with the actual process settings and contact fluid rather than relying on base resin values alone.

    Why Do Rotational-Moulded Marine Buoy Shells Fracture at the Foam Filling Port?

    Shell fracture at the fill port is rarely explained by a single material defect. The more common production-scale sequence is local wall thinning at the port boss, followed by thermal softening when polyurethane foam exotherm exceeds the heat deflection resistance of the shell. Marine buoy and aquaculture float shells are formulated with 100 parts by weight of Icorene 1761 R+ WHI 1400, 0.30–0.60 phr high-molecular-weight HALS, 0.10–0.20 phr UV absorber, 0.05–0.10 phr secondary antioxidant, and 0.5–1.0 phr weather-fast pigment concentrate. The downstream process uses shuttle-type or rock-and-roll rotational moulding machines; for cylindrical floats the minor-to-major axis rotation ratio is typically 3:1 to 4:1, with oven residence of 22–35 min at 280–310 °C and forced-air cooling to below 70 °C before demoulding. After demoulding, the hollow shell is filled with two-component polyurethane foam at a core density of 45–60 kg/m³ through a separately moulded or machined fill port; the port is then closed by spin welding or hot-plate welding. Terminal finished products include navigation buoys, aquaculture pen flotation collars, harbour fenders, and mooring floats. The process boundary is the exotherm at the inner shell surface: when foam exotherm pushes the shell temperature above 80 °C, localised softening collapses the fill-port boss; field observations on filled floats show that a boss wall thickness below 3 mm fails disproportionately compared with a 5 mm boss, especially when the foam rise profile is too fast near the port. Weathering conformity for marine service is assessed by ISO 4892-2 xenon-arc exposure or ASTM G154 fluorescent UV exposure, with tensile elongation retention measured after ageing according to ISO 527-2:2012. No single ISO standard covers all aquaculture float configurations; project-specific verification against classification society rules may be required for mooring components. Published long-term thermal oxidation data for this exact pigmented lot are limited, so upper service temperature and UV lifetime should be taken from the supplier's technical data sheet and confirmed by part-specific weathering trials.

    Agricultural Saddle Tank Boss Cracking and Wall Thickness Scatter

    Large tractor-mounted sprayer tanks are deep-drawn rotational mouldings with moulded-in drain ports, sumps, and agitator bosses. These geometries expose the narrow molecular-weight distribution of metallocene LLDPE: the same melt characteristic that improves powder coalescence can reduce sag resistance near the upper peak internal air temperature, compressing the functional processing window to approximately ±5 °C on some rock-and-roll machines. The formulation in this segment is 100 parts by weight of Icorene 1761 R+ WHI 1400, 0.20–0.40 phr HALS, 0.05–0.10 phr primary antioxidant, 0.05–0.10 phr secondary antioxidant, and 1.0–2.0 phr blue, green, or orange pigment concentrate for fluid identification. The manufacturing process is typically rock-and-roll rotational moulding with a swing arc of ±45°, oven chamber temperature of 270–310 °C, peak internal air temperature of 195–210 °C, and slow forced-air cooling to minimise warpage at the flat saddle back. Saddle tanks, induction hoppers, and seed boxes from 200 L to 1,500 L are the terminal product types. Industrial conformity for agricultural sprayers is assessed under ISO 16119-1:2013 and the EU Machinery Directive 2006/42/EC when the tank is integrated into a complete sprayer; chemical resistance of the moulded article is evaluated by immersion testing under ISO 175 using the actual agrochemical mixture at the field dilution concentration. The operational boundary is boss geometry: a drain port boss with a wall thickness below 3 mm and an internal corner radius below 6 mm develops stress concentration under vibration and torque, and production failures have been recorded after 1,000–2,000 h of field service. Where wall-thickness scatter exceeds ±15% on the saddle back, the tank may also exhibit sink marks at the mould parting line; this is typically corrected by reducing the secondary-axis speed during the final 5 min of heating. Published data for every agrochemical formulation are limited, so chemical resistance tests should be repeated whenever the customer changes carrier solvent or concentration.

    In dry food handling and hygienic logistics, rotationally moulded bins and trays are used where post-mould cleaning at high temperature or aggressive detergent is required. Food-contact articles produced from this metallocene LLDPE powder must be formulated with 100 parts by weight of Icorene 1761 R+ WHI 1400 and an additive package restricted to substances positively listed for food contact: typically 0.03–0.08 phr primary antioxidant, 0.02–0.05 phr neutraliser, and 0.3–0.8 phr high-purity white pigment whose components comply with EU 10/2011 Annex I and Annex II. The relevant regulatory framework is FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 on plastic materials intended to come into contact with food, with an overall migration limit of 10 mg/dm² for the final article; manufacturing hygiene is controlled under EC 2023/2006 on good manufacturing practice. Downstream production uses cast aluminium moulds because the higher thermal diffusivity of aluminium produces smoother inner surfaces that reduce food residue retention and allow cleaning at 75–80 °C in industrial washing tunnels. The rotational moulding cycle uses oven air at 260–300 °C, peak internal air temperature of 190–205 °C, and forced-air cooling until the inner surface drops below 70 °C before demoulding. Terminal products include 200–1,200 L hygienic bins, dolly bases, dough troughs, and dry-ingredient process totes. The operational limitation is that the final article must be tested under the exact food simulant, time, and temperature assigned by EU 10/2011; fatty food contact may require simulant D1 testing at 40 °C for 10 days, which cannot be assumed from resin certification alone. EU REACH Annex XVII restrictions apply to any intentionally added substance in the concentrate, and RoHS is not applicable unless an electrical component is inserted during assembly.

    When UV Stabiliser Loading Approaches the Upper Rotomoulding Window in Outdoor Playground Components

    Outdoor playground components require long-term colour retention and impact strength retention after years of sunlight, while the rotomoulding process itself limits how much stabiliser can be carried before surface deposits degrade mould release and weld-line strength. The starting formulation for LyondellBasell Icorene 1761 R+ WHI 1400 in this segment is 100 parts by weight of resin, 0.35–0.70 phr high-molecular-weight HALS, 0.10–0.20 phr UV absorber, 0.05–0.12 phr primary antioxidant, 0.05–0.10 phr secondary antioxidant, and 0.5–1.5 phr high-opacity pigment concentrate. The manufacturing process is carousel rotational moulding with textured steel or cast aluminium moulds; oven chamber temperature is held at 270–310 °C, peak internal air temperature is controlled between 195–210 °C, and cooling is conducted without water quench to avoid differential shrinkage on large slide shells and tunnel sections. Terminal products include rotomoulded slides, crawl tunnels, playhouse roofs, climbing panels, and spring toy seats. Safety conformity is assessed at the assembled equipment level under EN 1176-1 and ASTM F1487-17; material-level weathering is evaluated by ISO 4892-2 or ASTM G154, and retained tensile elongation is measured by ISO 527-2:2012 after the exposure period. The processing boundary is stabiliser overload: above 0.70 phr total HALS and UV absorber, the risk of surface deposit formation on the mould and poor hot-tack at the tool split line increases on multi-cavity carousel machines, while below 0.35 phr HALS the outer surface can develop microcracking after extended tropical UV exposure. Published data for this exact white-pigmented lot under all playground-specific UV cycles are limited, so accelerated weathering data should be generated on a moulded test plaque rather than the raw powder.

    Free Quote

    Competitive LyondellBasell Icorene 1761 R+ WHI 1400 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 R+ WHI 1400 is supplied as a white-pigmented, UV-stabilized metallocene linear low-density polyethylene (mLLDPE) powder for biaxial rotational moulding. The designation contains the additive/release modifier R+ and the colour index WHI 1400; the tinted formulation therefore differs from unpigmented Icorene 1761 base resin in pigmentation density, weathering package, and mould-release behaviour. The base resin is produced by single-site metallocene catalysis, which gives a narrow molar-mass distribution and a controlled short-chain branch distribution. Nominal base-resin values include a density of 0.940 g/cm³ determined in accordance with ISO 1183-1 and a melt flow rate of 6.5 g/10 min at 190 °C under a 2.16 kg load determined in accordance with ISO 1133-1:2022. The grade is intended for medium-to-large hollow parts requiring low-temperature impact resistance, environmental stress-crack resistance, and outdoor UV stability; application-specific values for the pigmented white compound must be confirmed against the certificate of analysis.

    How Does the Single-Site Metallocene Catalyst Architecture Modify Comonomer Distribution and Sintering Behaviour?

    Conventional Ziegler-Natta LLDPE is produced using multi-site catalysts with different propagation and termination rates. This generates a broad molar-mass distribution and preferential comonomer incorporation in lower-molar-mass chains. Metallocene single-site catalysis removes most of that active-site heterogeneity. The resulting mLLDPE exhibits a molar-mass polydispersity typically in the range of 2.0–3.0, compared with 4.0–8.0 for conventional Ziegler-Natta LLDPE. Short-chain branches from the alpha-olefin comonomer are distributed more uniformly across chain lengths, reducing low-molecular-weight soluble fractions and lowering hexane extractables. The more uniform branch distribution also produces a narrower crystalline lamellae thickness distribution relative to heterogeneous Ziegler-Natta resins.

    Rotational moulding densification occurs at very low shear rates, typically below 1 s⁻¹. In this regime, zero-shear viscosity, melt elasticity, and particle coalescence control bubble removal and wall densification. Metallocene LLDPE of this melt-flow class shows less shear thinning than a Ziegler-Natta LLDPE of equivalent melt flow rate. Consequently, melt flow rate alone does not predict rotational moulding behaviour. The homogeneous short-chain branching lowers crystallinity and melting onset compared with high-density polyethylene, and differential scanning calorimetry under ISO 11357-3 generally records a primary melt endotherm near 121 °C. The lower zero-shear viscosity assists sintering of powder particles in thin walls, but large flat panels may require additional mould support because melt elasticity is lower than that of long-chain-branched low-density polyethylene.

    Pigmented, UV-Stabilised Formulation and Specification Context

    The WHI 1400 white formulation incorporates titanium dioxide pigment for opacity and long-term UV screening. Titanium dioxide raises as-moulded density by approximately 0.01–0.02 g/cm³ depending on pigment loading and dispersion, and it increases flexural modulus while potentially reducing impact resistance if dispersion is poor. The R+ additive package provides internal mould release and weathering stabilization, typically employing hindered amine light stabilizers in combination with phenolic and phosphite antioxidants. The exact formulation is proprietary, and the manufacturer’s certificate of analysis should be used for batch-specific colour, density, and stability data.

    For outdoor applications, accelerated weathering comparisons are typically performed under ISO 4892-2 or ASTM D2565. Those tests rank relative weathering resistance but do not directly predict service life in a specific climate. Food-contact use of pigmented rotomoulding parts is not automatically covered by the unpigmented base-resin listing under FDA 21 CFR 177.1520(c); end-use migration testing according to EU Regulation (EU) No 10/2011 Annex III is required. Compliance with REACH SVHC restrictions and RoHS Directive 2011/65/EU should be verified with the supplier for the final tinted compound.

    PropertyMethodNominal Value
    DensityISO 1183-10.940 g/cm³
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20226.5 g/10 min
    Tensile yield stressISO 527-220 MPa
    Tensile elongation at breakISO 527-2>800 %
    Flexural modulusISO 178900 MPa
    Shore hardnessISO 86860 D
    Vicat softening temperatureISO 306121 °C
    Environmental stress-crack resistance, 100 % Igepal, Condition BASTM D1693>1000 h

    The table reflects nominal values published for the unpigmented metallocene LLDPE base resin. The white-pigmented WHI 1400 variant may show measurable shifts in density, impact, and weathering-related properties; pre-production qualification on the intended moulding machine is required.

    On shuttle-type biaxial rotational moulding machines with a 4:1 arm-speed ratio, the powder is typically processed at oven air temperatures between 260 °C and 290 °C. The target peak internal air temperature for a 6 mm wall section is generally controlled between 190 °C and 200 °C, measured by in-mould thermocouple or infrared pyrometer. The white pigmentation can alter radiative heat absorption relative to natural powder, so oven set-points may require adjustment. Production-scale colour-dependent heating rate differences should be mapped before full-rate operation.

    Moisture uptake above approximately 0.02 % by mass can create steam-induced porosity. Storage at relative humidity above 60 % may therefore require sealed containers or conditioning of the powder. Dry flow and particle-size distribution are batch-controlled. Particles coarser than 500 µm reduce surface quality and sintering homogeneity, while excessive fines below 150 µm increase dust and can cause fluidisation inside the mould. The powder is not intended for injection moulding, blown film, or filament extrusion in its supplied form.

    Cooling rate after demoulding is a primary process lever. Forced-air cooling increases productivity but can increase residual stress and warpage; slower cooling improves dimensional stability but extends cycle time. White pigmented parts can show differential cooling because of wall-thickness variation, so wall thickness should be maintained within ±10 % of nominal in critical regions to reduce sink marks and post-mould distortion.

    When Peak Internal Air Temperature Exceeds 200 °C in Thick-Section Rotational Moulding

    Overheating of metallocene LLDPE accelerates thermo-oxidative chain scission. Visible yellowing, low-temperature impact loss, and reduced environmental stress-crack resistance are the common failure signatures. Oxidation induction time measured by ISO 11357-6 or ASTM D3895 is used as a quality-control indicator; a drop below a pre-established control limit, typically 20 min at 200 °C, indicates antioxidant depletion. This is especially relevant when regrind is re-used, because stabilizer package consumption is cumulative.

    In thick sections above 12 mm, the temperature difference between the inner air surface and the mould surface can exceed 15 °C. Peak internal air temperature control alone is insufficient under these conditions; mould-surface thermocouples or infrared measurement are required to confirm complete sintering without over-cure. Published data for this specific white formulation in very thick sections is limited, and pre-production trials should establish the relationship between oven temperature, internal air temperature, mould-surface temperature, and wall porosity.

    Storage tanks and outdoor containers produced from this grade are often qualified under ASTM D1998-15, which specifies minimum wall thickness, hydrostatic pressure testing, and environmental stress-crack resistance requirements. Playground components and recreational parts are evaluated for low-temperature impact under ISO 6603-2 or ASTM D3763. Marine buoys and pontoons require UV stability testing under ISO 4892-2 and salt-spray exposure under ISO 9227. Food-contact containers require migration testing according to EU 10/2011 Annex III because the pigment and stabilizer system are not automatically covered by the base-resin listing under FDA 21 CFR 177.1520. Long-term outdoor weathering data for this exact white formulation are limited; accelerated weathering results should be correlated with field exposure before extended service commitments.

    Molecular Architecture Distinctions Are Not Thermodynamic Trivialities

    ParameterMetallocene LLDPE, this grade classZiegler-Natta LLDPEHigh-pressure LDPE
    Catalyst typeSingle-siteMulti-siteFree-radical initiator
    Molar-mass distribution, Mw/Mn2–34–85–9
    Short-chain branch distributionUniformHeterogeneousRandom with long-chain branches
    ESCR at equivalent densityHigherModerateLower to moderate
    ExtractablesLowerHigherIntermediate
    Low-shear viscosity at equal melt flow rateLower to moderateHigherHigh due to long-chain branching

    The practical consequence is that a part moulded from Icorene 1761 R+ WHI 1400 can achieve higher environmental stress-crack resistance at a given density and wall section than a Ziegler-Natta LLDPE of similar melt flow, but may require higher oven set-points in deep-draw sections because the metallocene polymer has lower zero-shear viscosity and less shear thinning. Compared with high-pressure LDPE, the grade provides higher flexural modulus and hardness but may show poorer melt elasticity; thin-walled parts with severe undercuts should be evaluated for demoulding stress. The white pigmentation further modifies mechanical balance: titanium dioxide increases modulus and opacity but can act as a stress concentrator that reduces impact and ESCR if dispersion is inadequate. Pigmented rotomoulding grades are therefore not direct drop-in replacements for natural grades; process and design adjustments are required when converting from Ziegler-Natta or LDPE formulations. The product should not be melt-blended with amine-based antistatic additives or peroxide masterbatches used for crosslinking unless specifically validated, because residual peroxide can initiate chain scission and discoloration of white parts.

    Top