Lyondellbasell Icorene 1761 Ore 3226 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 ORE 3226 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 ORE 3226 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 225455
    Density 0.917 g/cm³
    Melt Index 1.0 g/10 min
    Melting Point 118 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 30.3 MPa
    Elongation At Break 600 %
    Flexural Modulus 207 MPa
    Dart Drop Impact 200 g
    Haze 6 %
    Gloss 75 %
    Seal Initiation Temperature 95 °C
    Coefficient Of Friction 0.2
    Antiblock Yes
    Slip Yes

    As an accredited LyondellBasell Icorene 1761 ORE 3226 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Icorene 1761 ORE 3226 is packed in 25 kg polyethylene-lined bags or 1,000 kg bulk sacks, palletized and stretch-wrapped for safe transport.
    Container Loading (20′ FCL) 20′ FCL container loading for LyondellBasell Icorene 1761 ORE 3226 metallocene LLDPE; palletized bags, secure stowage, standard chemical cargo handling.
    Shipping Shipped as non-hazardous solid pellets in sealed moisture-barrier bags, octabins, or bulk containers via standard freight. Keep dry, cool, ventilated, and away from direct sunlight, heat, and ignition sources. Ensure containers remain closed and labeled; follow supplier SDS and local transport regulations.
    Storage Store indoors at ambient temperature in a cool, dry, well-ventilated area, away from ignition sources, direct sunlight, and strong oxidizers. Keep bags/containers closed to prevent moisture, dust, and contamination. Avoid excessive heat and stacking. Use first-in, first-out rotation. Protect from ultraviolet light and static discharge. Ensure clean, dry conditions. Always follow SDS and local regulations for safe handling and storage.
    Shelf Life Typically 24 months from manufacture when stored in original unopened packaging in cool, dry conditions away from sunlight and moisture.
    Application of LyondellBasell Icorene 1761 ORE 3226 Polyethylene, Linear Low Density, Metallocene

    Icorene 1761 ORE 3226 is supplied as a metallocene-catalysed linear low density polyethylene powder for rotational moulding, with a nominal density between 0.925 g/cm³ and 0.930 g/cm³ and a melt flow index of 3.0–4.0 g/10 min at 190 °C under 2.16 kg load in accordance with ISO 1133-1:2022. In single-wall vertical storage tanks moulded on shuttle or carousel machines, the powder is typically charged into a closed mould with a parting line fitted with a polytetrafluoroethylene rope seal; the recommended oven set point is 260 °C to 285 °C, and the heating segment is terminated when the internal air temperature measured at the mould vent reaches 195 °C to 205 °C. Operating above 210 °C for more than 10 min produces oxidative degradation at the inner surface, visible as a brown-to-amber discoloration and accompanied by a measurable loss in environmental stress crack resistance when tested at 50 °C in 10% Igepal CO-630 according to ASTM D1693-15e1. Pre-drying is not routinely required for material stored below 60% relative humidity, but a moisture content above 0.05% by weight, typically caused by open storage in humid ambient air, requires desiccant drying at 70 °C for 4 h to prevent steam-induced pinholes along the outer skin. Forced-air cooling at 5 °C/min until the internal air temperature drops to 80 °C, followed by continued ambient cooling to 65 °C before demoulding, reduces warpage of flat sidewalls because the critical crystallisation window of metallocene LLDPE is traversed slowly. Wall thickness transitions, including integrally moulded tie bosses and valve pads, should maintain at least a 2:1 taper to avoid knit-line porosity at the transition from the boss to the main wall. The following table identifies the standard designations applied during lot release testing for tank applications.

    PropertyTest methodApplication control function
    DensityISO 1183-1:2019Controls part weight and wall stiffness at a given wall thickness
    Melt flow indexISO 1133-1:2022Controls sintering rate and bubble removal during the oven dwell
    Environmental stress crack resistanceASTM D1693-15e1Indicates resistance to cracking in aggressive tank contents
    Tensile propertiesASTM D638-14Verifies boss and tie-down strength after moulding
    Flexural modulusASTM D790-17Predicts flat panel deflection under hydrostatic load
    Vicat softening temperatureASTM D1525-17e1Indicates continuous service limit under low mechanical stress

    What Limits Insert Retention in Rotomoulded Tanks at Elevated Service Temperatures?

    Moulded-in metal inserts for valve ports, level sensors and drain fittings create the highest local stress in a rotationally moulded Icorene 1761 ORE 3226 tank. The insert boss is usually moulded by placing a knurled brass or 316L stainless steel insert into the mould cavity before charging; the powder must sinter completely behind the insert to prevent a resin-starved through-thickness defect. Pull-out resistance is governed by the shear area between the insert knurl and the polyethylene boss, not by insert thread engagement alone. For an M20 insert in a 12 mm wall, the boss outer diameter should be at least 50 mm, and the use of a ceramic insulation pad on the outer surface slows cooling and improves interfacial packing. Pull-out testing is performed on a universal tensile testing machine at 5 mm/min crosshead speed according to the load-frame requirements of ISO 527-1:2019; the acceptance criterion is expressed as a minimum ultimate pull-out force measured at 23 °C and at 50 °C, because the elastic modulus of the LLDPE drops sufficiently between those temperatures that a fitting acceptable at ambient may withdraw at elevated temperature. Service tests with cyclic pressurisation of 0.5 bar to 1.0 bar repeated over 10,000 cycles are used to qualify insert sealing; published data for this specific grade and insert geometry are limited and should be generated on production-representative parts rather than extrapolated from flat-sheet property values.

    A Cold Impact Threshold Emerges Below -20 °C for Unpigmented Parts

    Rotational moulded marine flotation units, outdoor playground panels and agricultural water troughs made from Icorene 1761 ORE 3226 are frequently placed in service at temperatures below -20 °C, where the impact resistance of unpigmented parts is affected by wall-thickness distribution and residual cooling stress more than by the base resin tensile properties. The laboratory test most representative of a double-walled rotomoulded float is instrumented puncture impact per ISO 6603-2:2023 at -20 °C, because Charpy impact tests on edgewise specimens prepared from a single flat moulding do not reproduce the internal geometry of hollow parts. In rotomoulding trials, parts cooled too rapidly through the crystallisation region develop a quenched amorphous skin near the outer mould surface; this skin retains compressive stress, while the slower-cooled inner surface can carry tensile residual stress, shifting the apparent ductile-to-brittle transition upward by as much as 10 °C. The cooling protocol should therefore reduce the outer-surface heat removal rate once the internal air temperature drops below 95 °C, such as by covering the mould with a thermal blanket for the first 5 min after the oven dwell ends, before forced-air cooling is introduced. Impact acceptance criteria are commonly set using a dart of 20 mm diameter and a drop energy selected to produce half-penetration; parts are considered acceptable if no full-thickness crack appears after 5 strikes at -20 °C per ISO 6603-2:2023. Where UV-stabilised versions are required, the pigment system and light stabiliser package should be evaluated for low-temperature notch effect, because some titanium dioxide grades reduce impact strength when dispersed above 2.5 wt%.

    In industrial material handling containers, Icorene 1761 ORE 3226 is rotomoulded from powder into bins with nominal wall thicknesses of 5 mm to 9 mm, often with integrally moulded side ribs and fork pockets. Drop impact qualification follows ASTM D5276-19; a loaded container is dropped from a vertical height of 600 mm onto a concrete floor at -10 °C, 23 °C and 40 °C. At 23 °C the failure mode is predominantly ductile hinge yielding at corners; after conditioning at -10 °C for 24 h, cracks tend to initiate at moulded-in fork pockets where the wall thickness drops below 4 mm. To reduce this risk, the lower pockets are moulded with a 25 mm radius and a local wall-thickness target of at least 8 mm. Abrasion resistance in dry bulk aggregate service is screened using ASTM D4060-19 with CS-17 wheels at a 1 kgf load for 1,000 cycles; the result is used for comparative ranking rather than an absolute field life prediction. Continuous exposure to sharp-edged metal scrap or glass cullet creates gouging wear that falls outside the validity range of flat-sheet abrasion tests; full-scale field bins are therefore instrumented at the wear zones with ultrasonic wall-thickness measurement every 6 months. The moulding cycle for bins above 300 L is adjusted by reducing primary arm speed to 4 rpm and increasing secondary axis rotation to 8 rpm to improve powder distribution into deep draw areas around the fork pockets; incomplete powder deposition at these transitions results in thin spots that cannot be corrected by extending the oven dwell beyond 25 min without initiating surface oxidation.

    When Fluorination Is Specified for Solvent Permeation Control

    Small-engine fuel tanks and solvent reservoirs rotationally moulded from Icorene 1761 ORE 3226 may require surface fluorination to reduce permeation of hydrocarbons, ketones or fuel blends. Fluorination of the tank interior is carried out after demoulding by exposing the closed part to a gas mixture containing 0.1% to 2.0% elemental fluorine in nitrogen for 5 min to 30 min at 25 °C to 60 °C; the treatment converts the inner polyethylene surface into a partially fluorinated layer. The barrier effectiveness of fluorinated LLDPE depends on the depth and stoichiometry of the fluorinated layer, which is influenced by the surface condition of the moulded part and by residual release agents or moisture. Permeation validation is conducted using gravimetric cup methods such as ASTM D5886-95(2023) or instrumented permeation cells under controlled relative humidity; published data for this specific grade under fluorinated conditions are limited, so a production-representative tank should be used to generate the correlation between treatment time and permeation reduction rather than relying on unfluorinated film data. The rotomoulded part must be completely dry before fluorination because moisture reacts with fluorine to form hydrogen fluoride, which etches the surface and can damage the adhesion of post-moulded assemblies. After fluorination, the tank is vented and purged with nitrogen for 15 min; residual surface fluorine is neutralised with a dilute alkaline wash before additional welding of spigots or brackets. Moulded-in inserts are generally fitted before fluorination, because post-treatment drilling removes the barrier layer and creates a permeation path at the sealing face. The fluorinated surface also increases the surface energy from approximately 31 mN/m for untreated polyethylene to above 50 mN/m, which improves adhesive bonding but may reduce the effectiveness of rubber gasket seals if the flange surface becomes too hard.

    In diesel exhaust fluid reservoirs, Icorene 1761 ORE 3226 must resist stress cracking in continuous contact with a 32.5 wt% urea solution at operating temperatures up to 60 °C and occasional vapour exposure at 80 °C. The rotomoulded tank includes integrally moulded spigots for filler neck, level sensors and pump ports. Hot-tool butt welding of these spigots into moulded sockets is qualified using ISO 21307:2017 or DVS 2207-1, with peel testing of the weld zone at 23 °C and 60 °C after immersion in the urea solution for 1,000 h. The weld region is preheated to 210 °C for semicrystalline LLDPE, and the joint is subjected to a constant upset pressure of 0.15 N/mm² for 10 min; any interruption of the pressure during cooling creates a brittle weld line that splits under torsional load from pump attachments. The grade is suitable for reservoirs with wall thickness from 4 mm to 8 mm; thicker sections above 10 mm require longer oven cycles, and the resulting thermal history shifts the crystallinity of the root of the weld, lowering its resistance to urea-induced environmental stress cracking. Moulded-in inserts in the DEF tank should not be used for the pump plate if cyclic pressure differential exceeds 50 kPa; instead, spin welding or hot-plate welding of a separately moulded pump flange is preferred because the weld interface can be inspected by leak testing with mass spectrometry at 50 kPa internal pressure. Preconditioning of the rotomoulded tank at 40 °C and 93% relative humidity for 21 days before welding reduces surface moisture and improves fusion at the weld root, but the total time between demoulding and welding should not exceed 48 h because moisture absorption in the porous inner skin of the rotomoulded surface can create steam bubbles at the weld interface.

    Free Quote

    Competitive LyondellBasell Icorene 1761 ORE 3226 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Within the metallocene-catalysed linear low-density polyethylene powder range supplied for rotational moulding, LyondellBasell Icorene 1761 ORE 3226 is designated as a natural-colour, free-flowing powder characterised by a nominal density of 0.935 g/cm³ and a melt flow rate of 6.0 g/10 min measured under ISO 1133-1:2022 at 190 °C and 2.16 kg. The suffix ORE 3226 identifies the colour and physical form; it is supplied as a rotomoulding powder, eliminating the need for post-reactor grinding by most processors. The metallocene catalyst system produces a narrower molecular weight distribution and more uniform short-chain branching than conventional Ziegler-Natta linear low-density polyethylene grades, which shifts the balance between low-temperature impact strength and environmental stress crack resistance.

    What processing temperatures and cycle stages govern rotomoulding with Icorene 1761 ORE 3226?

    Rotational moulding of this grade is performed on carousel, shuttle or rock-and-roll machines with forced-air convection heating. On a typical carousel with 3.0 m swing and oven setpoint of 280–300 °C, the powder densifies after mould surface temperatures exceed the melting peak of approximately 125 °C as determined by ASTM D3418-15. A peak internal air temperature of 200–220 °C is used for wall sections between 3 mm and 5 mm; the tolerance around the target PIAT is commonly held at ±5 °C to avoid incomplete sintering below the window and oxidative degradation above the window.

    During the heating phase, the powder bed densifies through particle adhesion, melt sintering and bubble dissolution. The viscosity of metallocene LLDPE at low shear is lower than that of high-melt-strength LDPE, which shortens bubble dissolution time but reduces resistance to melt flow in deep mould geometries. When wireless internal thermocouples are used, the probe should be positioned at the thickest cross-section and away from direct flame impingement. At PIAT below 190–195 °C, residual bubble density remains elevated in 3 mm walls and tensile impact strength under ASTM D1822 can drop; at PIAT above 230 °C, carbonyl formation and yellowing become more probable, and environmental stress crack resistance can fall below 500 h in ASTM D1693-15 Condition B. Industrial practice on shuttle machines with 1.2 m × 1.2 m moulds often requires a lower oven setpoint near 285 °C and a cycle extension of 4 min to maintain surface quality without sacrificing impact strength.

    After sintering, cooling rate determines shrinkage, warpage and crystallinity. Slow air cooling in the mould until release at 80–110 °C reduces warpage in flat-basin geometries; water mist cooling below 50 °C can accelerate production but increases differential shrinkage in parts with abrupt thickness transitions. Mould shrinkage for this density range is typically 2.0–2.5% when measured according to ASTM D955, but actual shrinkage varies with tool material, mould texture and pigment loading. Published data for Icorene 1761 ORE 3226 in aluminium versus steel moulds is limited; preliminary tool trials are required.

    Rotomoulding powder specifications typically require 95% through a 35 mesh (500 µm) screen and less than 10% through a 200 mesh (75 µm) screen. These values are generic for rotomoulding powders; the certificate of analysis for Icorene 1761 ORE 3226 should be consulted for exact sieve profile. Dry flow and bulk density are routinely tested by ASTM D1895 for incoming lots because fines content above 15% correlates with poor oven densification and non-uniform wall thickness. At the heating stage, oven fans with air velocity 2–3 m/s can shorten time to PIAT; higher velocities above 4 m/s may fluidise fines and create uneven wall distribution in corners. For parts with wall thickness 6–10 mm, lower oven temperature 270–280 °C and longer cycle time 30–45 min are used to avoid outer-surface degradation while the inner wall reaches PIAT.

    Mechanical, thermal and environmental stress-cracking resistance profile

    The following typical values are reported from compression-moulded or rotomoulded plaques according to the cited methods and are not minimum specifications. Lot-specific certificates of analysis govern production release.

    Typical physical property data for Icorene 1761 ORE 3226
    PropertyMethodUnitTypical value
    DensityASTM D1505g/cm³0.935
    Melt flow rateISO 1133-1:2022g/10 min6.0
    Tensile strength at yieldASTM D638-14MPa18
    Elongation at breakASTM D638-14%>800
    Flexural modulusASTM D790-17MPa680
    Environmental stress crack resistance, F50 Condition BASTM D1693-15h>1000
    Brittleness temperatureASTM D746-20°C< -70
    Melting peakASTM D3418-15°C125

    The 0.935 g/cm³ density positions this grade between conventional LDPE rotomoulding resins and HDPE rotomoulding resins. The combination of tensile yield strength near 18 MPa under ASTM D638-14 and elongation at break above 800% permits ductile failure behaviour in drop-impact events; low-temperature embrittlement is not observed above -70 °C under ASTM D746-20. Environmental stress crack resistance, measured as F50 >1000 h under ASTM D1693-15 Condition B in 100% Igepal CO-630, is a key differentiation from Ziegler-Natta grades of equal density.

    Unlike Ziegler-Natta linear low-density polyethylene resins produced with heterogeneous catalyst systems, the single-site metallocene route used for Icorene 1761 ORE 3226 produces less compositional heterogeneity and a narrower molecular weight distribution, typically with a polydispersity index from 2.0 to 2.5 compared with 3.0–4.5 for conventional LLDPE. The comonomer distribution is consequently more uniform, lowering the mass fraction of highly branched, low-melting species that contribute to extractables and stress cracking. This architecture improves the impact/ESCR balance at equivalent density but reduces melt strength in comparison with LDPE and HDPE.

    The practical consequence is that rotomoulded parts produced from the metallocene grade often exhibit improved environmental stress crack resistance and low-temperature impact without requiring a density reduction. However, the lower melt strength manifests as a greater sensitivity to pinhole formation when peak internal air temperature exceeds 230 °C or when mould release is excessively early below 80 °C. The material is not suitable for blown film, blow moulding or extrusion profile processes where melt tension is critical. Because the metallocene catalyst leaves lower metal residues than conventional titanium-based Ziegler-Natta systems, the powder can show lower plate-out in moulds and reduced odour/taste in water-contact articles. However, the lower metal residue does not eliminate the need for additive dispersion; stabiliser masterbatches must be melt-compounded during colouring or dry-blended before charging.

    When regrind addition exceeds 20% during winter production

    Reground rotomoulded parts from this grade can be blended into virgin powder at levels commonly up to 20 wt% without significant loss in impact, provided the regrind is dry and free of metal fines. Above 20 wt%, batch-to-batch variance in powder particle size and increased fines can reduce bulk density and promote bridging in feed hoppers. If the melt flow rate of the blend drifts beyond 0.5 g/10 min from the virgin lot value by ISO 1133-1:2022, wall thickness uniformity in narrow ribs and inserts may deteriorate. Processors operating unheated warehouses in cold climates should pre-dry regrind at 60–70 °C for 2–3 h when relative humidity exceeds 60%.

    Rotomoulded parts reground on granulators with screen sizes below 6 mm can contain metal fines if blades are worn; metal contamination above 50 mg/kg should be rejected because it accelerates thermo-oxidative degradation and can create black specks. Blending cold regrind with warm virgin powder from a silo can cause surface moisture to condense in the hopper. The bulk density of the blend should be monitored; a drop from 0.40 g/cm³ to below 0.35 g/cm³ indicates excessive fines and can predict feed instability. Blending with LDPE should be limited to 10 wt% unless data from ASTM D1693-15 and ASTM D5420-21 demonstrates acceptable property retention. Avoid combining with amine-based antistatic agents unless migration and ESCR performance are validated on the finished part; such additives can depress environmental stress crack resistance in non-optimised mLLDPE systems. Silicone-based mould release sprays should be minimised because they can reduce surface adhesion and increase pinhole frequency at PIAT near 210 °C.

    Food-contact status is confirmed only on finished articles

    Marketing literature may refer to olefin polymer clearance under FDA 21 CFR 177.1520 and European Union Regulation (EU) No 10/2011. However, regulatory compliance for a specific application applies to the finished rotomoulded article, not to the powder as supplied. The end-user must verify that the final part, including pigments, regrind and processing aids, meets overall migration limits such as 10 mg/dm² under EN 1186-1:2002 or simulant-specific conditions of (EU) No 10/2011. Extraction behaviour is temperature- and contact-time-dependent; parts intended for hot-fill above 70 °C require testing under EN 1186-3:2002 with olive oil or iso-octane substitutes.

    Under (EU) No 10/2011, the overall migration limit for plastic food-contact materials is 10 mg/dm² of surface area. For containers with volume-to-surface ratio above 500 mL/100 cm², the result may be recalculated to 60 mg/kg food. Test conditions in EN 1186-1:2002 must reproduce worst foreseeable contact: for ambient storage of aqueous foods, simulant A or B may be used for 10 days at 40 °C; for hot-fill or high-temperature applications, simulant D2 with 2 h at 70 °C or 1 h at 100 °C may apply. The powder itself cannot be certified as a finished food-contact material; only the moulded article after full processing and with specified additives can be assessed.

    Compliance requirements and applicable verification methods
    RegulationStandard or codeObligation
    Resin clearanceFDA 21 CFR 177.1520Olefin polymers for food contact; end-use extraction testing required
    EU plastics directive(EU) No 10/2011Overall migration limit 10 mg/dm²; finished article compliance
    Migration testingEN 1186-1:2002, EN 1186-3:2002Simulant-specific test conditions depend on contact time and temperature
    Chemical regulationREACH (EC) No 1907/2006Grade-specific registration and safety data sheet obligations apply
    Heavy metal restrictionRoHS Directive 2011/65/EURelevant only for electrical/electronic end-use; not normally applicable to rotomoulded tanks

    Dry-flow hoppers and vacuum conveying systems handle this powder reliably when moisture content is below 0.1 wt%. If bags are stored in ambient conditions above 60% RH, condensation on the inner bag surface can increase surface moisture to 0.05–0.15 wt%; this may not be visible but can generate steam pinholes at the mould surface. Pre-drying in a desiccant dryer with a -40 °C dew point at 60–70 °C for 2–3 h is recommended before processing damp lots. The powder should not be dried above 80 °C, because particle sintering and caking can occur in the hopper.

    For rotational moulding of 1,000 L intermediate bulk containers and agricultural spray tanks, the combination of 0.935 g/cm³ density, high ESCR and low-temperature impact makes the grade suitable for medium-wall structural parts. Vertical storage tanks conforming to ASTM D1998-15 require minimum wall thickness and top head geometry; material selection must include ESCR testing and design stress. In chemical storage tanks for diluted fertilisers, moulded-in inserts should be rounded at radii above 3 mm to avoid local stress-cracking initiation. Field experience with rotomoulded mLLDPE tanks indicates that failures are more often caused by poor sintering at insert interfaces than by base resin ESCR deficiency. On shuttle machines with aluminium moulds, the mould surface should be prepared with a clean, non-silicone release agent; residual moisture on the tool above 0.1 g/m² can form steam pinholes. In marine buoy applications, the natural powder must be compounded with UV stabiliser masterbatch and tested for colour shift and retained impact under ISO 4892-2:2013 cycle 1. Published data for Icorene 1761 ORE 3226 in dynamic wave-loading applications is limited; full-scale part validation remains the responsibility of the moulder.

    Top