Lyondellbasell Icorene 1761 Ore 3222 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 795744
    Density 0.917 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 9.65 MPa
    Tensile Strength At Break 24.1 MPa
    Tensile Elongation At Break 600 %
    Tensile Modulus 241 MPa
    Flexural Modulus 207 MPa
    Vicat Softening Point 94.0 °C
    Melting Point 116 °C
    Haze 6.0 %
    Gloss 75 %
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Coefficient Of Friction 0.2

    As an accredited LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 ORE 3222 metallocene linear low-density polyethylene supplied in 25 kg polyethylene bags on pallets.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Icorene 1761 ORE 3222 metallocene linear low-density polyethylene, palletized and secured for ocean freight.
    Shipping LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene is a non-hazardous polymer resin. It is not regulated for transport by DOT, IMDG, IATA, or ADR/RID. Ship in clean, dry, sealed bags, octabins, or bulk containers, protected from moisture, contamination, and excessive heat.
    Storage Store this resin in a cool, dry, well-ventilated warehouse. Keep containers tightly closed, labeled, and off the floor. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, acids, and bases. Use grounding and bonding to control static. Avoid generating dust. Follow supplier SDS for shelf life, stacking limits, and emergency procedures. Store separately from incompatible materials.
    Shelf Life Typical shelf life is 24 months when stored in original, unopened packaging in a cool, dry place away from sunlight.
    Application of LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene

    At cast-film line speeds above 600 m/min, LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene is processed on a three-layer cast film line with a 2.6–3.0 m wide roll face and single-screw extruders having L/D 30:1 barrier screws. Melt temperature is held at 240–260 °C, and the die gap is set between 0.6 mm and 0.8 mm; wider gaps at this speed produce neck-in above 80 mm, while narrower gaps raise back pressure beyond 28 MPa and trigger sharkskin melt fracture at the die lip. The A/B/A layer distribution is 15/70/15, with skin layers containing 1.0–1.5 wt% erucamide slip masterbatch and 0.3–0.6 wt% synthetic silica antiblock with a median particle size of 3–5 µm. Core layer remains additive-free to preserve puncture propagation resistance. Primary chill roll temperature is controlled at 18–22 °C; if it exceeds 28 °C, the cling layer develops tack stability failure after 48 h as erucamide bloom becomes uneven. A vacuum box at −35 mbar and an air knife positioned 25–40 mm from the die exit are required to maintain gauge variance within ±5% on 12–18 µm film. Finished pallet wrap is tested for cling per ASTM D5458, with acceptable values of 60–150 g, and for tensile elongation per ASTM D882, with machine-direction elongation above 300%. For direct food contact, the film must comply with FDA 21 CFR 177.1520(c) 3.1/3.2 and EU 10/2011; overall migration into fatty-food simulant D2 must not exceed 10 mg/dm².

    What Happens When Metallocene LLDPE Replaces Conventional LLDPE in High-Clarity Frozen Food Blown Film?

    The first observable difference in a 300 mm blown film die is loss of bubble stability when the blow-up ratio exceeds 2.2:1 because the polymer has a narrow molecular weight distribution and limited strain-hardening melt strength. A converter using 100% Icorene 1761 ORE 3222 at a die gap of 1.4 mm and melt temperature of 200–210 °C must often reduce frost line height to 5 die diameters to prevent bubble vibration, but this causes machine-direction tear resistance to drop below 50 g/25 µm per ASTM D1922. The practical correction is a press-side blend of 15–20 wt% LDPE with a melt flow index of 0.25–0.8 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022. Extruder temperature zones range from 170 °C at the feed throat to 200 °C at the die; die-lip crystallisation is avoided by keeping the adapter and die at 205–210 °C. The frost line is held at 6–8 die diameters and the BUR at 2.0–2.2:1, producing a 50 µm film with haze below 8% by ASTM D1003. Stabilisation for frozen-food packaging uses 500–1000 ppm octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate and 400–800 ppm tris(2,4-di-tert-butylphenyl) phosphite; these loadings prevent gel formation at die-lip stagnation zones during 24 h continuous runs. Amine-based antifog additives are avoided in this system because they compete with the slip package and produce measurable seal-strength loss after 7 days of conditioned storage. The terminal lamination or premade bag is sealed at 120–135 °C; seal strength must exceed 12 N/15 mm per ASTM F88. Direct food contact under frozen or refrigerated conditions falls under FDA 21 CFR 177.1520(c) 3.2 and EU 10/2011 Annex I, with phosphite stabiliser migration below the specific migration limits listed therein.

    Rotational moulding of Icorene 1761 ORE 3222 begins not with virgin pellets but with a micropulverised powder because consistent wall thickness requires that 95% of the feed pass a 35 mesh (500 µm) sieve and that fines below 100 µm remain under 10% to prevent bridging in the mould. Published data for this specific grade in rotational moulding is limited; the following processing window is derived from mLLDPE grades with a melt flow index of 1.0–2.5 g/10 min and density of 0.912–0.918 g/cm³ and must be validated against the LyondellBasell technical bulletin. Because the micropulverised powder picks up moisture under relative humidity above 60%, pre-drying at 60–70 °C for 4–6 h is required to prevent steam pinholes. The powder is dry-blended with 0.15–0.35 wt% hindered amine light stabiliser and 0.08–0.12 wt% phenolic antioxidant before the mould is charged. Oven temperature is set at 270–290 °C, while peak internal air temperature is controlled to 185–195 °C to avoid oxidative discolouration and pinholing. Rotational speed ratio is 4:1 with primary axis rotation of 6–8 rpm; the secondary axis is 1.5–2 rpm. A nominal wall thickness of 3–6 mm must remain within ±15% at corners and ribs. Environmental stress crack resistance is evaluated per ASTM D1693 Condition B in 10% Igepal CO-630 at 50 °C; mLLDPE grades in this class typically exceed 1000 h without cracking. Low-temperature impact of the moulded part is tested with a 9.0 kg striker at −40 °C following ASTM D1998; brittle failure or visible delamination is not permitted. The terminal component is a rotationally moulded chemical dosing tank or water treatment vessel in which cross-sectional microscopy must show no voids greater than 1% of the wall-thickness area.

    Adhesion and Heat Seal Integrity in Extrusion-Coated Liquid Packaging Structures

    Extrusion coating of Icorene 1761 ORE 3222 onto aluminium foil, paperboard, or oriented PET operates under a melt temperature window of 300–320 °C; below 290 °C, peel adhesion to unprimed foil measured at a 180° angle falls below 1.5 N/15 mm, and above 330 °C the polymer begins emitting acrid fumes and may suffer surface oxidation that reduces heat-seal strength. The coating line uses a single-screw extruder with L/D 26:1–30:1 and a barrier screw, feeding a coat-hanger die with a 0.4 mm die gap. Air gap is set at 200–250 mm; longer gaps increase neck-in beyond 50 mm and destabilise coat weight at line speeds above 150 m/min. Chill roll surface temperature is controlled at 10–18 °C, and the rubber nip roll applies 0.25–0.40 MPa pressure to force the melt into the substrate pores. When line speed exceeds 150 m/min, a blend of 15–30 wt% LDPE is added to suppress draw resonance; without it, edge tearing and gauge variance can exceed ±10% at the substrate edges. The resulting aseptic carton inner liner or liquid pouch is tested for water vapour transmission rate per ASTM F1249 at 38 °C/90% RH; values above 7 g/(m²·day) are unacceptable for extended-shelf-life milk cartons. Heat-seal strength after 1 s dwell at 150–170 °C and 0.2 MPa is measured per ASTM F88 and must exceed 15 N/15 mm. Regulatory compliance of the polyethylene coating is established under FDA 21 CFR 176.170(c) for paperboard in contact with aqueous and fatty foods, and under EU 10/2011 for the finished multilayer structure.

    Silage wrap conversion places an unusual combination of high outdoor UV exposure, low-temperature cling, and puncture resistance on the same film. The structure is blown at 15–25 µm thickness as an A/B/A coextrusion; the outer skin contains 1.2–2.0 wt% carbon black masterbatch or 0.8–1.5 wt% titanium dioxide white masterbatch to block UV radiation and reduce film surface temperature. The cling layer is formulated with 1.5–3.0 wt% polyisobutene having a number-average molecular weight of 1,200–2,500 g/mol; full cling development requires 24–72 h post-production migration, and the cling value is specified at 40–80 g per ASTM D5458. Bubble parameters for Icorene 1761 ORE 3222 include a blow-up ratio of 2.0–2.2:1, die gap of 1.1–1.3 mm, and melt temperature of 195–210 °C. Puncture resistance is measured with a 19 mm diameter probe at 500 mm/min; films below 30 N fail during cylindrical bale wrapping due to stubble penetration. Elmendorf tear strength in both machine and transverse directions must exceed 450 g/25 µm per ASTM D1922. Amine-based antifog packages are incompatible with the high-cling formulation because they compete for the film surface and reduce cling below 40 g. Although silage wrap is not direct food contact, REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons in carbon black and the requirements of DIN EN 13206 for agricultural films apply. The terminal roll is 750 mm × 1500 m on a round baler; edge curl must remain below 3 mm per 100 m to prevent telescoping during high-speed wrapping.

    When 20 wt% LDPE Is Added to Restore Bubble Stability in Stretch Hood Film

    With the addition of 20 wt% LDPE, stretch hood film made from Icorene 1761 ORE 3222 gains sufficient melt strength at blow-up ratios above 2.5:1 on a 400 mm die without the bubble flutter observed with the unmodified metallocene resin. The LDPE used for this correction has a density of 0.923–0.924 g/cm³ and a melt flow index of 0.25–0.8 g/10 min. Raising LDPE above 25 wt% depresses elastic recovery below 80% after 50% stretch per ASTM D5459. The three-layer blown film line uses a die gap of 1.2 mm, BUR of 2.5–3.0:1, and extruder zone temperatures from 180 °C to 210 °C, with the die head at 205–215 °C. Final film gauge is 50–120 µm, and the layflat width is gusseted to 1,800–2,400 mm for pallet hoods. Puncture resistance is tested according to ASTM D5748; values of 8–15 N at 23 °C and 4–8 N at −20 °C are required to survive pallet corners. The hooding machine pre-stretches film at 1.3–1.6:1; pre-stretch above 1.8:1 causes localised thinning and corner failures. Outdoor pallet storage requires 0.20–0.40 wt% hindered amine light stabiliser and 0.10–0.20 wt% phenolic antioxidant. Regulatory oversight for industrial packaging falls under REACH; where the hood is used as secondary packaging for food contact articles, only indirect contact under EU Regulation 1935/2004 applies.

    Thin-wall drip irrigation tubing with a nominal wall thickness of 0.3–0.5 mm is extruded at 150–250 m/min from a blend of 30–50 wt% metallocene LLDPE and 50–70 wt% HDPE; the Icorene 1761 ORE 3222 component contributes environmental stress crack resistance at barbed fittings and during mechanical coiling. Extrusion temperatures are set between 200 °C and 230 °C, with the die head held at 210–225 °C. The compound requires 2.0–2.5 wt% carbon black with an average primary particle size of 20–50 nm to meet outdoor UV resistance, plus 0.10–0.20 wt% phenolic antioxidant for processing stability. Hydraulic pressure resistance is evaluated by ISO 1167 in a 60 °C water bath under a hoop stress of 2.5 MPa; ductile failure is not permitted before 1,000 h. Dimensional tolerance for the integrated dripper labyrinth must be held within ±0.02 mm, which requires melt viscosity homogeneity at the die inlet and minimal gel content. Tensile yield strength of the blend per ASTM D638-14 must exceed 18 MPa, and elongation at break must exceed 600%. The terminal product is an integral drip line or tape for row crops; the metallocene LLDPE fraction reduces the kinking radius to below 50 mm without stress whitening or cracking.

    Free Quote

    Competitive LyondellBasell Icorene 1761 ORE 3222 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 ORE 3222 is a metallocene-catalysed linear low-density polyethylene supplied as a low-dust, free-flowing powder for rotational moulding of hollow, sealed, and double-wall components. The base resin is classified under ISO 1043-1 as PE-LLD. The Icorene 1761 model designation identifies the base resin and melt-flow class, while the ORE 3222 suffix identifies a producer-specific additive and stabiliser formulation. The additive package does not alter the fundamental polyethylene backbone but influences oxidative stability, regrind tolerance, colour retention, and surface finish during long rotational moulding cycles. Typical industrial uses include chemical storage tanks, agricultural water reservoirs, insulated transport boxes, marine buoys, air ducts, and industrial covers where low-temperature impact resistance and environmental stress-cracking resistance are required. Because publicly available data for this exact ORE 3222 configuration is limited, process parameters and part qualification should be based on the lot certificate and the current LyondellBasell product datasheet rather than class-level literature values alone.

    For metallocene rotational moulding LLDPE grades of this family, density is normally determined by ISO 1183-1:2019 or ASTM D1505, and melt mass-flow rate by ISO 1133-1:2022 at 190°C and 2.16 kg. Published class-level ranges for such powders commonly fall between 0.930 and 0.940 g/cm³ in density and between 3 and 8 g/10 min in melt flow rate. These intervals contextualise the product but do not constitute release specifications. Tensile, flexural, and impact values should be generated on rotomoulded specimens because mechanical performance is strongly influenced by mould surface temperature history, cooling rate, wall thickness, internal air temperature profile, and part geometry. Conditioning of test specimens should follow ISO 291 at 23°C ± 2°C and 50% ± 5% relative humidity unless the end-use specification requires otherwise.

    Molecular Architecture and Catalyst-Derived Comonomer Distribution

    The defining structural feature of this metallocene-catalysed linear low-density polyethylene is the narrow interchain comonomer distribution produced by single-site catalysis. In ethylene/α-olefin copolymers, metallocene active sites insert comonomer with less chain-to-chain heterogeneity than conventional Ziegler-Natta catalysts. This difference can be observed by temperature-rising elution fractionation or crystallisation analysis fractionation, and it directly affects solid-state morphology. A more controlled short-chain branching distribution increases the concentration of tie molecules at a given density, which translates into improved environmental stress-cracking resistance under ASTM D1693 and higher impact toughness under ISO 6603-2 or ASTM D256. The narrower molecular-weight distribution can reduce shear thinning in melt processing, but this effect is less relevant in rotational moulding than in extrusion because the powder is not pumped through a die. Instead, powder densification, bubble dissolution, and void elimination at the mould surface control final part quality.

    The melting range displayed by differential scanning calorimetry per ISO 11357-3 is typically sharper for metallocene LLDPE than for conventional LLDPE of equivalent density. This arises from a more uniform lamellar thickness distribution and lower fractional content of poorly crystallisable, highly branched chains. Oxidative stability of the ORE 3222 stabiliser package can be monitored by oxidation induction time per ISO 11357-6 at 200°C under oxygen; stabilised rotational moulding powders in this class are commonly specified to exceed 20 min. Sustained exposure to mould surface temperatures above 280°C may accelerate additive consumption, promote surface plate-out, and increase yellowness. Storage should be in sealed containers at ambient temperature below 30°C, with protection from direct sunlight and standing water. The zero-shear viscosity of metallocene LLDPE at a given melt index is often lower than that of a Ziegler-Natta LLDPE of equivalent density; this difference is minor in rotational moulding but becomes important if the same resin is diverted to compounding or extrusion operations.

    In rotational moulding cells with independently controlled oven zones, process development for this mLLDPE powder typically begins with oven air temperatures between 260°C and 320°C, with the peak internal air temperature at the mould cavity ranging from 180°C to 210°C. The optimum peak internal air temperature depends on mould gauge, oven residence time, cooling configuration, and the presence of bosses, ribs, or metal inserts. Powder flow and bulk density govern how evenly the material distributes into difficult-to-reach features. A powder with median particle size below 500 µm and controlled fines content reduces dusting and promotes densification. At relative humidity above 60%, pre-drying to below 0.05 wt% moisture is recommended to limit pinholes, internal bubbles, and surface porosity. Instrumented moulds with thermocouples sampling at 1 Hz are used to record the internal air temperature trace and identify the point of polymer sintering, melt coalescence, and void closure. Cooling rate significantly affects warpage and residual stress. Forced-air cooling is often continued until the part surface drops below 70°C before demoulding, while slower cooling can improve dimensional stability at the cost of longer cycle time.

    The powder should not be blended with high-density polyethylene or polypropylene regrind without a documented compatibility study, because inter-domain phase separation can reduce low-temperature impact and stress-crack resistance. Where masterbatch or compound preparation is carried out on a corotating twin-screw extruder with L/D ratio between 36:1 and 48:1, barrel feed-zone temperatures should remain below 160°C to avoid premature sticking of powder on the screw root and feed throat. The stabiliser package has a finite thermal budget; regrind levels above 20 wt% should be validated by melt flow rate shift, yellowness index per ASTM D1925, and notched impact testing. No release specification should be assumed without reviewing the production lot certificate, because melt flow rate and additive loadings may move within the producer’s allowed tolerance band.

    What Distinguishes Icorene 1761 ORE 3222 from Ziegler-Natta and Conventional LLDPE Grades?

    Compared with conventional Ziegler-Natta LLDPE, the metallocene catalyst used in Icorene 1761 ORE 3222 generates a narrower interchain copolymer composition distribution. The practical consequence in rotational moulding is a more uniform crystallite size distribution and lower residual stress in thick walls, which can reduce warpage and permit a lower part weight for the same burst or impact requirement. The trade-off is that the narrower molecular-weight distribution and lower melt elasticity can produce a slightly reduced sintering rate under some conditions; oven residence time may therefore need adjustment relative to a Ziegler-Natta powder of the same nominal melt index. This adjustment cannot be predicted solely from melt flow rate and should be established by moulding trials on the intended line.

    Environmental stress-cracking resistance of mLLDPE rotomoulded parts is generally superior to Ziegler-Natta LLDPE at equivalent density, as evaluated by ASTM D1693 condition B in 10 vol% Igepal CO-630 at 50°C. Low-temperature impact resistance tested by ISO 6603-2 shows a lower ductile-to-brittle transition temperature for metallocene LLDPE parts, which is relevant for outdoor service in cold climates. Permeation of aliphatic hydrocarbons is a function of density, wall thickness, and crystallinity rather than catalyst type alone; barrier performance must therefore be confirmed on the final rotomoulded article using ASTM D3985 or ISO 15105-2 as appropriate. The following comparison uses class-level data because published data for this specific ORE 3222 configuration is limited; lot certificates and current producer datasheets shall govern commercial specifications.

    Property axis Test method Metallocene LLDPE class Ziegler-Natta LLDPE class Implication for rotational moulding
    Density ISO 1183-1:2019 typically 0.930–0.940 g/cm³ typically 0.925–0.945 g/cm³ mLLDPE may meet toughness targets at lower density and weight
    Melt mass-flow rate ISO 1133-1:2022 typically 3–8 g/10 min at 190°C/2.16 kg often 2–10 g/10 min at 190°C/2.16 kg Cycle time depends more on peak internal air temperature than melt index alone
    Short-chain branching distribution TREF or CRYSTAF narrow interchain distribution broad interchain distribution Uniform crystallite size reduces thick-wall internal stress
    Environmental stress-cracking resistance ASTM D1693 commonly exceeds 1,000 h in class-level data often 100–700 h at equivalent density Improved chemical tank and container durability
    Low-temperature impact ISO 6603-2 lower ductile-to-brittle transition temperature higher ductile-to-brittle transition temperature Better cold-climate field service performance

    When process temperatures drift above 300°C for prolonged periods, oxidative degradation can cause discolouration, carbonyl formation, and loss of impact strength. The ORE 3222 stabiliser package is not unlimited in its thermal protection; extended cycles, high regrind content, or accidental contamination with transition metal oxides can exhaust the antioxidant package prematurely. Food-contact status, potable-water contact, and specific chemical resistance must be confirmed by LyondellBasell for the ORE 3222 additive package. Generic PE-LLD clearance under 21 CFR 177.1520 cannot be assumed for finished articles, and migration limits under 21 CFR 177.1520(c) must be verified on the final part. REACH compliance requires review of the safety data sheet for monomer and additive registrations. Published data for this specific configuration is limited; therefore mould-filling behaviour, sintering time, and mechanical design allowables should be developed from first-article testing on the intended production line.

    Top