| HS Code | 784013 |
| Density | 0.917 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Temperature | 95 °C |
| Tensile Strength At Yield | 9 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 600 % |
| Flexural Modulus | 220 MPa |
| Dart Drop Impact | 120 g |
| Haze | 10 % |
| Gloss | 60 % |
| Coefficient Of Friction | 0.20 |
| Tear Strength Md | 200 g |
| Tear Strength Td | 300 g |
| Brittleness Temperature | < -70 °C |
As an accredited LyondellBasell Icorene 1761 ORE 3220 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 ORE 3220 metallocene LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): LyondellBasell Icorene 1761 ORE 3220 metallocene LLDPE polyethylene, typically 25 kg palletized bags, securely stowed. |
| Shipping | LyondellBasell Icorene 1761 ORE 3220 is shipped as non-hazardous LLDPE metallocene resin pellets, typically in 25 kg bags, 500–1000 kg bulk bags, or octabins on stretch-wrapped pallets. Transport in clean, dry, covered trucks or containers at ambient temperature. Protect from moisture, heat, and direct sunlight; no special dangerous-goods documentation required. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep material in original sealed bags or containers on pallets, protecting it from moisture, UV exposure, dust, and contamination. Avoid contact with strong oxidizers. Maintain moderate temperatures and use first-in, first-out stock rotation. Ensure good housekeeping to prevent slips and static buildup. |
| Shelf Life | Shelf life is typically 24 months when stored unopened in a cool, dry, well-ventilated area, protected from direct sunlight and moisture. |
In blown-film coextrusion, the grade is used as the sealant layer at 12–25 µm within a total web of 45–80 µm on lines with die gaps of 1.6–2.2 mm and blow-up ratios of 2.2:1–3.0:1. The seal initiation temperature is typically 10–15 °C below that of a conventional C8-LLDPE of equivalent density; on horizontal form-fill-seal equipment, dwell times below 0.4 s at 110–120 °C produce seal strengths exceeding 15 N/25 mm when measured by ASTM F88. Hot tack measured per ASTM F1921 remains above 1.5 N/25 mm at 110 °C when the sealant layer constitutes at least 30% of the total structure. Haze per ASTM D1003 on a 40 µm monolayer remains between 3% and 7% only when the die temperature is kept above 190 °C and the frost line height is at least 3 die diameters. Slip and antiblock masterbatches above 1.5 wt% suppress coefficient of friction below 0.1 per ASTM D1894, but degrade seal strength by 20–35% through erucamide migration. Horizontal form-fill-seal applications include frozen vegetable bags and dry snack pouches, where the sealant layer must survive grease and low-temperature flexing. The following table links process-control responses to applicable test methods.
| Control response | Test method | Relevant process parameter |
|---|---|---|
| Melt mass-flow rate | ASTM D1238 / ISO 1133-1:2022 | 190 °C, 2.16 kg |
| Density | ASTM D792 / ISO 1183-1:2019 | 23 °C |
| Hot tack force | ASTM F1921 | 0.4 s dwell, 0.3 N/mm² seal pressure |
| Seal strength | ASTM F88 | 300 mm/min peel |
| Haze | ASTM D1003 | 40 µm blown film |
| Coefficient of friction | ASTM D1894 | metal sled, 150 mm/min |
Rotational moulding with the metallocene linear low density grade uses a free-flowing powder ground to 95% below 500 µm (35 mesh) and 10% maximum below 150 µm (100 mesh), because excessive fines create pinholes and reduce air release. Apparent density measured by ASTM D1895 typically remains between 0.45 g/cm³ and 0.55 g/cm³ for uncompounded metallocene powder; values below 0.42 g/cm³ indicate excessive fines or moisture uptake. Peak internal air temperature is held at 190–205 °C for 20–30 min in a forced-air oven; lower peak internal air temperature leaves partially fused powder at the mold parting line, while higher peak internal air temperature accelerates antioxidant depletion and yellowing. Mold rotation ratio is set at 4:1 with a primary axis speed of 8 rpm. Internal air pressurization at 0.2–0.4 bar during cooling from 180 °C to 80 °C reduces shrinkage voids in wall sections above 8 mm. The grade is used for seamless tanks, containment basins, and agricultural storage vessels; drinking-water contact parts require 21 CFR 177.1520(c) and NSF/ANSI/CAN 61. Outdoor service requires a hindered amine light stabilizer package at 0.2–0.4 wt%, and lot-to-lot dry flow must be verified before charging to the mold.
Twin-screw compounding of color concentrates and additive masterbatches using this metallocene LLDPE as carrier resin requires specific energy input between 0.18 kWh/kg and 0.24 kWh/kg on a co-rotating twin-screw extruder with 40:1 L/D and screw speeds of 400–600 rpm. Lower energy input leaves pigment agglomerates above 5 µm; higher energy input generates chain scission and raises the melt flow rate by 15–30%, shifting the carrier viscosity outside the target for downstream film dilution. Dispersion quality is evaluated according to ISO 18553:2002 by counting pigment agglomerates in a 0.1 mm film; accepted concentrates limit agglomerates above 10 µm to fewer than 5 per 100 cm². Screen-pack filtration across 30/60/120 mesh screens maintains pressure rise below 0.5 bar/h; faster pressure increase indicates agglomeration or metal contamination. The carrier can be diluted at 2–4% letdown in blown film without forming melt fracture. End products include masterbatches for lamination sealants, stretch hoods, and rotational molding tinting; carrier compliance for indirect food contact follows 21 CFR 177.1520(c).
Frozen-food bags and heavy-duty ice packaging are coextruded with the metallocene grade in the outer or core layer at 60–100 µm total gauge. The absence of long-chain branching in mLLDPE lowers melt strength, so the film line uses a low frost line height and a blow-up ratio not above 2.5:1 to maintain bubble stability. Dart drop impact per ASTM D1709 Method A after 48 h conditioning at -20 °C is the critical release criterion; converter acceptance protocols require no splitting or pinhole formation after the dart drop. Replacing 20 wt% EVA with the metallocene LLDPE reduces cold-cracking defects at -40 °C, although exact values for this grade must be confirmed on the target line. A core layer containing 10–20 wt% HDPE raises flexural modulus without reducing low-temperature puncture resistance, but HDPE content above 20 wt% introduces brittle failure at the layer interface. Tear resistance is tracked by ASTM D1922, and gauge uniformity is measured at 10 mm intervals across the web. End products include frozen vegetable packaging, meat bags, and ice cube bags.
Extrusion coating with the metallocene linear low density is constrained by neck-in and draw resonance, so the grade is run as a coextruded sealant skin over an LDPE or polypropylene tie layer at coat weights of 12–20 g/m². Melt temperatures of 290–310 °C are maintained at the die; a valved die and edge encapsulation reduce neck-in below 30 mm at 200 m/min. Adhesion to aluminum foil requires a solventless primer or a coextruded maleic anhydride-grafted polyethylene tie layer; peel strength is measured according to ASTM D903 at 300 mm/min, and delamination must occur within the sealant layer rather than at the foil interface. Acidic or oxygen-sensitive contents require an aluminum or EVOH barrier, and the metallocene sealant is separated from EVOH by a tie layer to prevent interfacial failure. The sealant layer is used in aseptic liquid packaging, pharmaceutical moisture barriers, and snack laminations, where seal integrity after flex-cracking is verified by ASTM F392.
Competitive LyondellBasell Icorene 1761 ORE 3220 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 ORE 3220 is a metallocene-catalyzed linear low-density polyethylene supplied as a rotational molding powder. The grade combines a nominal density of 0.940 g/cm³ with a nominal melt mass-flow rate of 5.0 g/10 min at 190 °C/2.16 kg. The single-site catalyst system produces a narrower molecular weight distribution and more homogeneous intermolecular comonomer placement than conventional Ziegler-Natta LLDPE. The resulting crystalline morphology has thinner, more uniform lamellae, which influences sintering, densification, impact resistance, and environmental stress crack resistance. The product is typically specified for rotationally molded tanks, containers, and hollow parts requiring low-temperature toughness and resistance to environmental stress cracking in service. The suffix ORE 3220 forms part of the manufacturer’s commercial grade designation and should be cited in full when ordering.
| Property | Nominal Published Value | Test Method |
|---|---|---|
| Density | 0.940 g/cm³ | ASTM D1505 |
| Melt mass-flow rate | 5.0 g/10 min at 190 °C/2.16 kg | ASTM D1238 |
| Environmental stress crack resistance | > 1000 h | ASTM D1693 Condition B |
| Brittleness temperature | < -76 °C | ASTM D746 |
| Tensile yield strength | 18 MPa | ASTM D638 |
| Elongation at break | > 800% | ASTM D638 |
| Vicat softening temperature | 121 °C | ASTM D1525 |
Nominal values are derived from supplier literature and are based on compression-molded plaques. They are not design allowables for finished rotationally molded parts. Property values in molded walls are influenced by cooling rate, wall thickness, mold surface, pigmentation, and regrind addition. Final part testing is therefore required for load-bearing applications. The producer’s current technical data sheet should be consulted for exact test specimen geometry and conditioning protocol.
In Ziegler-Natta LLDPE, comonomer is incorporated preferentially in low-molecular-weight fractions, leaving high-density segments that melt at higher temperatures. This broad melting distribution can require higher peak internal air temperature to eliminate unmelted particles and can generate a heterogeneous crystalline network on cooling. In metallocene LLDPE, comonomer placement is more random along the chain, producing a narrower melting range and thinner average lamellae at equivalent density. The sintered wall may therefore develop a more uniform crystalline structure. However, the narrower melting transition also reduces the thermal cushion between full consolidation and thermal oxidation. Operators on carousel equipment with oven setpoints in the range 260 °C to 300 °C have observed that Icorene 1761 ORE 3220 can achieve complete surface replication at lower internal air temperature than some Ziegler-Natta grades of equivalent melt index, but published data for this specific configuration is limited.
Differences from other products are material at property level. At equivalent density, metallocene-catalyzed LLDPE typically provides higher instrumented dart impact resistance because the uniform branching distribution increases the number of inter-lamellar tie molecules. In contrast, a high-density polyethylene rotational molding grade with density above 0.945 g/cm³ may provide higher flexural modulus but generally lower ESCR and a higher ductile-brittle transition temperature. The Icorene 1761 ORE 3220 is therefore positioned for parts requiring low-temperature impact resistance and long-term contact with aqueous or mild oxidizing environments rather than maximum structural stiffness. Compared with lower-melt-flow metallocene grades, the 5.0 g/10 min melt mass-flow rate of this product may improve flow into complex mold features, although ESCR and impact resistance should be verified in the finished part because resin property rankings do not always transfer directly from plaque data to thick molded sections.
Closed-loop monitoring of internal air temperature is specified on rotational molding machines used for this product because oven setpoint alone does not capture the endotherm of the polymer or the thermal lag of the mold wall. Carousel machines with steel molds generally permit lower oven setpoints than aluminum molds because the thermal conductivity of steel is lower and heat transfer is slower. Peak internal air temperature should be established by iterative trials, with physical inspection of cut sections for voids and microtensile specimen acquisition from the wall. In multi-layer structures, layer thickness and sequence should be fixed before establishing the cycle because regrind layers have different particle morphology and may sinter at slightly different times.
For rotational molding, the powder is typically ground to a controlled sieve profile with a maximum particle size below 600 µm. Finer particle size distributions can reduce bubble entrapment but may increase dust and electrostatic handling issues. The resin should be stored in sealed containers at ambient temperatures not exceeding 50 °C. Contamination with foreign polymers, particularly polypropylene or polyamide, should be avoided because incompatible melts can form visible weld-line defects. Production-scale carousel machines with aluminum or steel molds and forced-air cooling have been used for tanks with wall thicknesses from 3 mm to 15 mm; published data for larger wall thicknesses is limited.
Process failures observed in rotational molding of metallocene LLDPE include pinholes when peak internal air temperature is insufficient to complete sintering, and orange peel or poor surface replication when oven residence time is too short. Warpage is more likely when demolding is performed at surface temperatures above 65 °C or when cooling is non-uniform across flat panels. Pre-drying is not generally required for this powder at relative humidity below 60%. Material exposed to condensation or stored in open containers should be dried before molding to avoid porosity in thick sections.
The metallocene structure that improves ESCR and low-temperature impact does not make the resin suitable for all chemical containment duties. The grade is a linear low-density polyethylene with limited barrier performance against nonpolar solvents, aromatic hydrocarbons, and chlorinated species. Permeation of these fluids can cause swelling and loss of mechanical strength. For aqueous acids, bases, and polar solutions at ambient temperature, the environmental stress crack resistance of the resin is relevant, but compatibility should be confirmed by immersion testing according to ISO 175 or ASTM D543 using the specific concentration and temperature. A mass increase greater than 3% after 7 days at the service temperature is commonly used as a screening criterion before prototyping large tanks. This threshold is not universal but is routinely applied in chemical tank qualification.
High-pressure vessels, pressurized gas cylinders, or containers above the design limits of monolayer polyethylene should not be manufactured from the resin without explicit mechanical design validation. Creep rupture behavior is not characterized in the supplier’s published data for this grade. In outdoor tank applications, ultraviolet exposure and long-term oxidation should be evaluated separately because the base resin’s stabilization package is specified for normal processing conditions and may not be sufficient for continuous exterior service without additional weatherable protection.
The linear low-density polyethylene structure contains only carbon-carbon and carbon-hydrogen bonds in the base polymer, which provides resistance to polar media such as aqueous salt solutions, dilute acids, and dilute alkalis at ambient temperature. Nonpolar liquids with solubility parameters close to polyethylene, including aliphatic and aromatic hydrocarbons, can penetrate the amorphous phase and cause swelling. The degree of swelling can be assessed by mass change after immersion under ASTM D543. The finished article must be qualified by the converter because processing additives, colorants, and regrind content can alter chemical resistance.
Low-temperature ductility is a primary selection criterion for rotationally molded tanks used in outdoor service. The reported brittleness temperature below -76 °C under ASTM D746 indicates that the resin remains ductile under low-temperature impact. However, the test is not a direct measure of performance of a finished molded part. Instrumented dart impact testing on 3 mm compression-molded plaques using ASTM D3763 provides a more useful comparison of puncture resistance, with published values for this metallocene grade often exceeding those of conventional Ziegler-Natta LLDPE at equivalent density. Environmental stress crack resistance greater than 1000 h under ASTM D1693 Condition B is significant because stress cracking in service is a common failure mode in polyethylene tank applications involving detergents, wetting agents, or cyclic thermal stress.
Compared with a typical Ziegler-Natta butene LLDPE rotational molding resin of similar melt flow rate, the metallocene base resin of Icorene 1761 ORE 3220 generally provides a narrower melting range and more uniform crystallite development. Compared with a premium hexene LLDPE grade, differences are smaller and often depend on additive formulation. Published data for this specific suffix is limited with respect to instrumented dart impact on molded parts, long-term creep, and ultraviolet exposure. Therefore selection against a competing grade should be based on prototype testing under the actual service environment rather than on pellet or plaque property sheets alone.
| Regulatory Reference | Condition or Scope |
|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for repeated food-contact articles, subject to end-use test temperature, density, and additive compliance. |
| EU 10/2011 as amended | Plastic materials and articles intended to come into contact with food; overall migration must be verified on the finished article. |
| REACH Regulation 1907/2006 | Material supplier documentation should be checked for substances of very high concern; polymers are exempt from registration but additives may be subject to obligation. |
| RoHS Directive 2011/65/EU | Lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE are not intentionally added; verification on the final compound is required. |
The base polyolefin chemistry is generally covered by FDA 21 CFR 177.1520 for articles intended for repeated food-contact use, subject to the density, maximum extractable fraction, and end-use temperature limitations specified in the regulation. Compliance with EU Regulation 10/2011 as amended must be demonstrated by the finished article through overall migration and specific migration testing with food simulants. The resin manufacturer may provide a statement of composition, but the converter is responsible for documenting compliance of the molded part because additives, pigments, and any post-molding surface treatment are outside the resin supplier’s certification.