Lyondellbasell Icorene 1761 Ore 3218 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 759561
    Density 0.917 g/cm³ (typical)
    Melt Mass Flow Rate 190 C 2 16 Kg 1.0 g/10 min (typical)
    Melting Temperature 118 °C (typical)
    Vicat Softening Temperature 95 °C (typical)
    Tensile Strength At Yield Md 10 MPa (typical)
    Tensile Strength At Yield Td 10 MPa (typical)
    Tensile Strength At Break Md 38 MPa (typical)
    Tensile Strength At Break Td 32 MPa (typical)
    Tensile Elongation At Break Md 500 % (typical)
    Tensile Elongation At Break Td 600 % (typical)
    Flexural Modulus 200 MPa (typical)
    Dart Drop Impact F50 200 g (typical)
    Elmendorf Tear Strength Md 200 g (typical)
    Elmendorf Tear Strength Td 300 g (typical)
    Haze 8 % (typical)
    Gloss 80 % (typical)

    As an accredited LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 ORE 3218 supplied in 25 kg moisture-resistant bags, stacked on 1,000 kg stretch-wrapped pallets.
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell Icorene 1761 ORE 3218 metallocene LLDPE in 25 kg bags, palletized, floor-loaded, secured for overseas shipment.
    Shipping LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene is typically shipped as non-hazardous resin pellets in 25 kg bags, 1,000 kg FIBCs, or bulk containers. Store in cool, dry, ventilated areas away from direct sunlight and ignition sources. Follow carrier and local regulations; avoid moisture and contamination.
    Storage Store in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, sparks, and open flames. Maintain closed original packaging or lined containers to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out. Store on pallets, away from oxidizing agents. Ground handling equipment to control static. Consult the SDS for specific local requirements.
    Shelf Life Shelf life typically 24 months when stored unopened in a cool, dry place, away from sunlight and moisture.
    Application of LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene

    Application assessment for LyondellBasell Icorene 1761 ORE 3218, a metallocene linear low density polyethylene (mLLDPE), must be verified against the lot certificate for melt index, density, and additive package. The conversion behaviour of mLLDPE with a narrow molecular weight distribution differs from Ziegler-Natta LLDPE in shear viscosity, seal initiation, crystallisation kinetics, and cooling-induced shrinkage. The downstream routes covered below are restricted to established industrial processes where metallocene LLDPE is used as a sealant, impact modifier, or monolayer structural resin. When a numeric processing window is grade-dependent, the datasheet value replaces the class-typical range.

    Where Rotational Moulding Uses a Narrow Sintering Window

    Rotational moulding of large storage tanks and intermediate bulk containers subjects the polymer to a two-stage thermal history in a biaxial oven. On a shuttle-type rotational moulding machine with a swing diameter of 1.5 m and a 4:1 arm ratio, oven setpoints between 260 °C and 300 °C are common. Peak internal air temperature (PIAT) is measured inside the mould; metallocene LLDPE with a narrow comonomer distribution generally consolidates when PIAT reaches 195–215 °C. If PIAT remains below 190 °C, partially melted particles remain at the inner wall and appear as pinhole defects after demoulding. Temperatures above 230 °C may lead to discoloration and surface oxidation, especially in poorly vented cavities. The exact PIAT window for Icorene 1761 ORE 3218 should be taken from the grade datasheet.

    Cooling determines flatness. Forced air is applied after removal from the oven until the mould surface falls below 80 °C before any water mist is introduced. Early water contact creates differential shrinkage that appears as sidewall bowing and vacuum collapse in flat panels. Venting of the cavity is required; for tanks below 1,000 L, a vent internal diameter of at least 20 mm is standard field practice, but the required vent area should be calculated from the mould cavity volume and peak air temperature. Mechanical property qualification follows ASTM D638-22 for tensile yield, ASTM D256-23 for notched Izod impact, and ASTM D1693-21 for environmental stress crack resistance. Food-contact construction relies on FDA 21 CFR 177.1520(c) 3.1a and 3.2a and on EU No 10/2011 with an overall migration limit of 10 mg/dm².

    What Limits Draw Resonance in High-Speed Metallocene LLDPE Cast Film?

    Draw resonance in cast film is influenced by air gap, melt tension, chill roll temperature, and the flat shear-thinning response of mLLDPE. On a three-layer cast line with a feedblock and edge encapsulation, a die gap of 1.8–2.5 mm and an air gap of 8–15 cm provide a stable starting window for mLLDPE with a melt index in the 4–7 g/10 min range measured by ISO 1133-1:2022. Chill roll temperature between 15 °C and 25 °C stabilises the web and reduces neck-in. If the melt temperature at the die exit is below 210 °C, sharkskin surface melt fracture can appear; if it exceeds 240 °C, gel formation and odour increase. Addition of 10–30 wt% high-pressure LDPE introduces strain hardening, which suppresses draw resonance but raises haze measured by ASTM D1003-21 and lowers dart impact measured by ASTM D1709-22.

    Film gauge in food and hygiene overwrap typically ranges from 20 µm to 50 µm. Sealing performance is tested by ASTM F88/F88M-21 for heat-seal strength and ASTM F1921-12(2018) for hot tack. Tensile properties of cast film follow ASTM D882-18; Elmendorf tear follows ASTM D1922-23. For direct food contact, the sealant layer is evaluated under FDA 21 CFR 177.1520(c) 3.2a and EU No 10/2011. Processors using thin gauges below 30 µm should confirm that the edge trim can be reground without exceeding the gel limit in the final film.

    Extrusion coating of paper, aluminium foil, and metallised substrates uses mLLDPE as the sealant layer in aseptic beverage cartons and dry food sachets. The resin is processed through a 90-mm single-screw extruder with a barrier screw and a slot die at melt temperatures between 270 °C and 300 °C. This temperature range balances adhesion and oxidation; mLLDPE exposed to ambient air for more than 20 s at the die lip can develop carbonyl species that reduce seal performance. Ozone treatment at the nip is applied at 0.5–1.0 kW/m of web width to increase aluminium foil adhesion. Paperboard is corona-treated to 40–44 mN/m immediately before coating. The structure is qualified by peel or heat-seal strength per ASTM F88/F88M-21 and hot tack per ASTM F1921-12(2018). Food-contact compliance relies on EU No 10/2011 and FDA 21 CFR 177.1520(c) 3.2a; migration certificates for fatty-food simulants are required because the sealant layer is in direct contact with product.

    Adhesion loss occurs when the web temperature at the nip is below the resin’s crystallisation onset. Infrared pyrometers positioned after the die are used to hold web temperature above 90 °C before lamination. For foil substrates, the chill roll finish and nip pressure influence bond strength; a nip pressure of 3–5 bar is often set as a starting point on a 140-mm diameter chill roll. Materials that are overtreated above 48 mN/m can show curl and blocking in reel storage.

    Balancing Impact and Stiffness When Compounding with Post-Consumer Polyethylene

    mLLDPE is added to recycled high-density polyethylene and mixed polyolefin regrind to improve impact and environmental stress crack resistance. On a co-rotating twin-screw extruder with an L/D ratio of 36:1 to 44:1 and a side feeder for ground flake, addition levels between 5 wt% and 20 wt% are common. Melt temperature is controlled at 180–210 °C. Local overheating above 230 °C creates gel particles when aggressive kneading blocks are used at screw speeds above 600 rpm. The extruder configuration should limit neutral kneading elements to two zones and use distributive mixing after the feed port.

    The trade-off is quantified by tensile modulus per ASTM D638-22 and notched Izod impact per ASTM D256-23. As the mLLDPE fraction increases, stiffness decreases; there is no single loading that satisfies both high-impact and high-modulus requirements. Environmental stress crack resistance is measured by ASTM D1693-21; the improvement is lot-dependent because recycled input melt flow index can vary by more than ±20% between batches. Long-term heat-aging compounds should limit metal stearate carryover from recycled packaging to below 500 ppm, because polyethylene oxidation accelerates in the presence of excess stearate during extended thermal exposure.

    Thin-wall lids and caps are produced on accumulator-assisted injection moulding machines with clamp forces from 150 tonnes to 350 tonnes. The melt is injected through hot runner valve gates. mLLDPE has a flatter shear-thinning curve than LDPE, so injection pressure and holding pressure are higher for the same flow length. Barrel settings are typically 40–60 °C in the feed zone, 190–200 °C in the compression zone, 210–230 °C in the metering zone, and 220–240 °C at the nozzle. If the gate freezes before the packing phase ends, part mass varies by more than 0.5% shot-to-shot and warpage increases. Holding pressure is increased until gate freeze time exceeds 0.8 s for a lid thickness of 0.45 mm; this value is mould-specific and must be confirmed by short-shot and gate-seal studies. Mould cooling water at 10–15 °C reduces cycle time. Dimensional stability is checked by ASTM D955-21. For food-contact closures, compliance is established under FDA 21 CFR 177.1520 and EU No 10/2011; organoleptic testing is part of release for filled product.

    Mould design must account for the higher coefficient of linear thermal expansion of metallocene LLDPE relative to high-density polyethylene. Demoulding taper angles below 0.5° on core surfaces may require additional ejection force. Purge with a conventional LDPE after production runs prevents accumulation of degraded gel in the hot runner manifold. Nozzle back pressure is held at 5–10 bar to avoid excessive shear heating.

    Low Extractable Film Structures for Medical Device Pouch Stock

    Medical pouch film uses mLLDPE as the sealant layer coextruded with polyester or polyamide outer layers. The sealant layer thickness is typically 25–50 µm and the target seal initiation temperature is below 100 °C. Cytotoxicity is evaluated per ISO 10993-5:2009. Physicochemical suitability is assessed per USP <661.1>. Leachable testing follows ISO 10993-12:2021. Sterilisation by ethylene oxide is commonly performed at 55 °C and 50% RH for 2 h; gamma irradiation at 25 kGy requires an irradiation-stable stabilizer package to avoid discoloration.

    On a three-layer blown film line with a 75-mm extruder and a 200-mm die, bubble stability is maintained by a dual-lip air ring and internal bubble cooling. Frost line height is held between 2 and 3 die diameters. Seal strength is tested per ASTM F88/F88M-21; tensile behaviour per ASTM D882-18; puncture resistance per ASTM D5748-19. The resin and film should be stored below 50 °C and protected from ultraviolet exposure before pouch conversion.

    ApplicationRegulatory referenceTest methodControl note
    Rotational moulded food storageFDA 21 CFR 177.1520(c) 3.1a/3.2a; EU No 10/2011ASTM D1693-21Overall migration limit 10 mg/dm²
    Cast film sealant layerFDA 21 CFR 177.1520(c) 3.2a; EU No 10/2011ASTM F88/F88M-21; ASTM F1921-12(2018)Heat-seal strength per package specification
    Extrusion coatingEU No 10/2011; FDA 21 CFR 177.1520(c) 3.2aASTM F88/F88M-21Corona/dyne level 40–44 mN/m
    Medical pouch stockUSP <661.1>; ISO 10993-5:2009ISO 10993-12:2021Cytotoxicity negative; leachables per device

    Blown film conversion for agricultural silage covers and stretch hood packaging uses mLLDPE in an A/B/A coextruded structure to combine puncture resistance with sealability. On a high-stalk line with a 55-mm extruder and a die gap of 1.6–2.2 mm, a blow-up ratio of 2.0:1 to 3.0:1 and frost line height of 2–3 die diameters stabilise the bubble. Melt temperature is held at 190–215 °C; raising the die temperature above 215 °C reduces melt fracture but narrows the cooling window. The film is tested for dart impact per ASTM D1709-22 and Elmendorf tear per ASTM D1922-23. Outdoor service requires UV stabilizer masterbatch addition at 2–5 wt% and verification of stabilizer depletion by accelerated weathering per ASTM D4329-21. Stretch hood machines with a wrapping speed of 100 pallets/h demand film with sufficient elastic recovery. The elastic recovery of mLLDPE film is measured by ASTM D5459-22. If surface blocking develops during wind-up, recycled edge trim can be reduced or an anti-block masterbatch added at 2–4 wt%. Blown film lines without internal bubble cooling may need to reduce output by 15–20% compared with LDPE at the same die diameter. Stretch hood films require cling behaviour; mLLDPE alone may need a cling additive or an LDPE skin to maintain pallet load stability.

    Free Quote

    Competitive LyondellBasell Icorene 1761 ORE 3218 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 ORE 3218 is a metallocene-catalysed linear low-density polyethylene supplied as natural pellets for blown-film extrusion. The resin is classified under ISO 1043-1 as PE-LLD and carries a nominal density of 0.918 g/cm³ when measured according to ISO 1183-1. The melt mass-flow rate is reported as 1.0 g/10 min at 190°C/2.16 kg using ISO 1133-1. The metallocene catalyst system differs from conventional Ziegler–Natta technology by producing a narrower molecular weight distribution and a more homogeneous short-chain branch distribution. These molecular features influence solid-state crystalline morphology and melt rheology; published data for this specific ORE 3218 packaging variant are limited where full copolymer type and additive-package details are concerned, but the base resin properties are consistent with film-grade mLLDPE.

    The short-chain branch distribution is the primary structural difference between Icorene 1761 ORE 3218 and a Ziegler–Natta LLDPE of equivalent density. In Ziegler–Natta grades, comonomer is incorporated preferentially into the low-molecular-weight fraction, leaving a comparatively linear high-molecular-weight fraction that forms thicker lamellae. In metallocene-catalysed polyethylene, comonomer is distributed more uniformly along the molar-mass axis. Gel permeation chromatography against polystyrene standards generally reports polydispersity indices below 3.0 for metallocene grades, while many conventional butene-based LLDPE grades fall between 3.5 and 5.0. This difference reduces scattering from large spherulites, lowers haze measured by ASTM D1003, and increases the dart-drop impact threshold evaluated by ASTM D1709/A. The result is a different balance of stiffness, toughness, and optical performance at the same nominal density.

    Nominal thermal and film data from producer technical literature indicate a melting peak near 121°C by ISO 11357-3 and a Vicat softening point near 100°C using ISO 306/A50. Blown-film evaluations at 25 µm thickness typically report tensile strength at yield in the range of 8 MPa to 12 MPa and tensile elongation at break above 700% when tested according to ISO 527-3 or ASTM D882. Dart-drop impact values above 1500 g and haze values below 10% are frequently cited for Icorene 1761-series film samples under ASTM D1709/A and ASTM D1003. These values are grade-class benchmarks rather than lot guarantees; final values depend on die gap, draw ratio, frost-line height, and additive package.

    Blown-film processing of Icorene 1761 ORE 3218 is typically performed on single-screw extruders with an L/D ratio of 25:1 to 30:1. A barrier screw with a Maddock mixing section is recommended to reduce melt-temperature variation. Die gaps between 1.6 mm and 2.4 mm are used because mLLDPE has lower die swell and lower melt strength than high-pressure LDPE; a narrow die gap can produce excessive shear stress and melt fracture. Blow-up ratios from 2.2:1 to 2.8:1 and melt temperatures from 190°C to 210°C are common. Bubble stability is maintained with a dual-lip air ring and internal bubble cooling when gauges below 25 µm are run. Published data for the minimum stable gauge of this exact ORE 3218 designation is limited; comparable metallocene grades are processed to 12 µm to 15 µm on equipment configured as described.

    Relative to high-pressure LDPE, Icorene 1761 ORE 3218 exhibits higher tensile strength, puncture resistance, and elongation at break, but lower melt strength and less shear thinning. LDPE has a highly branched long-chain structure that allows high melt tension and easier bubble formation; mLLDPE requires a wider die gap and more precise air-ring control. In coextruded films, the metallocene LLDPE is commonly used as a surface or core layer to improve mechanical performance, while an LDPE layer contributes melt strength and process stability. The seal-initiation temperature of metallocene LLDPE is typically lower than that of Ziegler–Natta LLDPE of the same density, which permits faster packaging-line seal cycles. Seal-strength data for this specific grade should be generated using ASTM F88 on the actual film gauge and seal-bar geometry.

    Primary application areas are food-contact films, freezer films, heavy-duty sacks, and lamination layers where puncture resistance and optical performance are specified. The grade is not intended for injection molding or rotational molding; its melt flow rate of 1.0 g/10 min is too low for most injection-molding cycles and its density is outside the typical rotomolding window of 0.930 g/cm³ to 0.940 g/cm³. In food-contact applications, the base polyethylene can be assessed under FDA 21 CFR 177.1520 in the United States and Regulation (EU) No 10/2011 in the European Union. Overall migration testing is performed according to EN 1186-1. The ORE 3218 suffix may identify a specific antioxidant or processing-stabilizer formulation; compliance documentation for the final fabricated article must be obtained from the producer or converter.

    In film structures, Icorene 1761 ORE 3218 may be blended with LDPE at 20 wt% to 40 wt% to retain bubble stability while improving dart-drop impact. Above 40 wt% mLLDPE, melt tension declines and the frost-line height typically must be reduced. The addition of a fluoropolymer polymer-processing aid at 200 ppm to 500 ppm can extend extrusion run time by reducing die-lip buildup and melt fracture. The exact additive level depends on screw design, throughput, and die pressure; production trials on the target line are required because laboratory rheology under ISO 11443 at 190°C cannot fully reproduce bubble dynamics.

    Pellets are not hygroscopic; predrying is generally unnecessary when storage is below 40°C and relative humidity below 60%. If surface moisture is present from outdoor storage, a dehumidified-air dryer at 60°C to 70°C for 2 h to 4 h removes surface water without antioxidant depletion. The resin should not be exposed to melt temperatures above 250°C for extended periods; oxidative degradation accelerates and creates carbonyl byproducts detectable by infrared spectroscopy at 1715 cm⁻¹. Avoid contact with oxidizing agents and avoid blending with amine-based additives that can interfere with the phenolic antioxidant system. Published data for long-term heat-aging performance specific to Icorene 1761 ORE 3218 is limited; users should request oxidative induction time data by ISO 11357-6.

    Compared with other metallocene LLDPE grades in the Icorene series, Icorene 1761 ORE 3218 is positioned at the lower-density end with a nominal density of 0.918 g/cm³ and an MFR of 1.0 g/10 min. Higher-density mLLDPE grades with densities of 0.923 g/cm³ to 0.930 g/cm³ provide greater stiffness and barrier, while lower-density grades below 0.915 g/cm³ offer higher impact and lower puncture resistance. The choice of comonomer, if hexene or octene, affects tear and dart-drop properties relative to butene-based mLLDPE; producer datasheets for ORE 3218 may not specify the comonomer type. Users should request the full technical datasheet and certificate of analysis for the specific lot.