| HS Code | 276077 |
| Density | 0.917 g/cm3 |
| Melt Index | 1.6 g/10 min |
| Melting Temperature | 119 °C |
| Vicat Softening Temperature | 95 °C |
| Tensile Strength At Yield | 9.0 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 600 % |
| Tensile Modulus | 200 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 6 % |
| Gloss | 80 % |
| Coefficient Of Friction | 0.20 |
| Seal Initiation Temperature | 95 °C |
As an accredited LyondellBasell Icorene 1761 ORE 3217 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 ORE 3217 is packaged in 25 kg multiwall paper bags, palletized and shrink-wrapped for storage and transport. |
| Container Loading (20′ FCL) | 20′ FCL loading: LyondellBasell Icorene 1761 ORE 3217 metallocene LLDPE, 25 kg bags; approx. 20–22 metric tons per container. |
| Shipping | LyondellBasell Icorene 1761 ORE 3217 is a metallocene linear low-density polyethylene supplied as free-flowing pellets. It is typically shipped in 25 kg bags, octabins, bulk bags, or bulk trucks/railcars. Store in a cool, dry, clean area away from direct sunlight and incompatible materials. Not classified as dangerous goods for transport. |
| Storage | Store in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers sealed, on pallets, off the floor, protected from moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Use first-in, first-out rotation and follow the manufacturer’s SDS. Keep away from foodstuffs. |
| Shelf Life | Shelf life is typically 24 months when stored in original, unopened packaging under cool, dry conditions, away from direct sunlight. |
LyondellBasell Icorene 1761 ORE 3217 is incorporated as the seal layer resin in coextruded high-clarity food packaging films. The ORE 3217 suffix identifies a lot-controlled additive package; slip and antiblock loading must be verified against the EU 10/2011 Declaration of Compliance and the lot certificate. On a three-layer blown film line running a 75 mm grooved-feed extruder with a 30:1 L/D ratio and a 250 mm spiral mandrel die, the seal layer is processed at 195–230 °C with a die gap of 1.6–2.0 mm. Blow-up ratio is held at 2.0–2.5, while frost line height is maintained at 6–8 die diameters. The reduced seal initiation temperature of metallocene LLDPE permits heat-seal jaw setpoints to be lowered by 10–15 K relative to C4 Ziegler-Natta LLDPE, reducing thermal exposure for heat-sensitive dry snack fillings. Seal layer formulation typically uses 15–40 wt% Icorene 1761 ORE 3217, with the balance a C8 Ziegler-Natta LLDPE and 5–15 wt% high-pressure LDPE for bubble stability. Direct food contact compliance is anchored to FDA 21 CFR 177.1520(c)2.1 and EU 10/2011, with overall migration below 10 mg/dm² according to EN 1186-1. Heat-seal strength is measured according to ASTM F88; acceptable production values at 120 °C exceed 8 N/15 mm for a 40 µm seal layer. Finished articles include cereal liners, frozen vegetable pouches, dry snack wrappers, and inner seal webs for stand-up pouches.
Bubble stability is governed by the narrow molecular weight distribution typical of metallocene catalysis and the absence of long-chain branching in linear low density polyethylene. The melt exhibits lower deformation-hardening than high-pressure LDPE, so at blow-up ratios above 2.8 on single-layer lines, thickness variance rises and bubble pumping becomes audible without internal bubble cooling. On a 75 mm extruder with a 300 mm die, maintaining die gap above 1.8 mm prevents melt fracture at screw speeds above 45 min⁻¹; narrower gaps produce sharkskin melt fracture on the outer film surface. Blending 10–20 wt% high-pressure LDPE with a melt flow rate of 0.25–0.5 g/10 min measured by ISO 1133-1 at 190 °C/2.16 kg restores deformation-hardening and widens the stable BUR window to 2.2–2.5. Frost line height must remain at 6–8 die diameters; below 4 die diameters blocking and drop impact below 300 g per ASTM D1709 Method A are observed at 40 µm. Dual-lip air rings and internal bubble cooling are required when the resin is run above 1.0 kg/h/cm of die circumference. Gel defects are controlled by a 125 µm screen pack and by limiting regrind addition to 10 wt% if the regrind contains degraded film edge trim.
Cast stretch film lines running 90 mm barrier screws introduce Icorene 1761 ORE 3217 into the core layer at 20–30 wt%, with the balance a C6 or C8 Ziegler-Natta LLDPE of melt flow index 2.0–3.5 g/10 min determined by ISO 1133-1 at 190 °C/2.16 kg. Melt temperature at the slot die is set to 245–260 °C; die gap is 0.5–0.8 mm, and the air gap is maintained at 2.0–3.0 times final film gauge. Chill roll surface temperature is controlled at 16–20 °C; above 22 °C, surface blocking occurs on 8–23 µm film and forces unwind torque above 5 N·m on turret rewinders. The pre-stretch section is run at 180–250%; residual elastic recovery above 6% at 250% pre-stretch indicates the core layer contains insufficient Ziegler-Natta LLDPE or that chill roll quench is uneven. Puncture force according to ASTM D5748 shifts from approximately 8.0 N to 12.5 N for 15 µm film when the metallocene resin replaces the same weight fraction of C4 Ziegler-Natta LLDPE, although line-side verification is required for this exact ORE 3217 lot. Cling force is generated by a ULDPE skin layer containing 10–15 wt% polyisobutylene masterbatch, and peel cling is tested according to ASTM D5458. Finished pallet wrap rolls are 12–25 kg on 76 mm cores with edge error below 1 mm and splice-free lengths above 3000 m.
Processing of three-layer greenhouse film combines 10–25 wt% Icorene 1761 ORE 3217 with EVA containing 12–18% vinyl acetate in the middle layer. Extrusion is performed at 200–225 °C with a blow-up ratio of 2.2–2.5 and final gauge of 120–200 µm. UV stabilisation uses hindered amine light stabilisers at 0.3–0.6 wt% and UV absorbers at 0.1–0.2 wt%, with film tested according to EN 13206 for covering properties. Dart impact at -10 °C must remain above 800 g per ASTM D1709 Method A when normalised to 50 µm, a requirement that drives the inclusion of metallocene LLDPE because its more uniform comonomer distribution lowers the brittle-ductile transition by approximately 10 K relative to C4 Ziegler-Natta LLDPE at similar density. The main processing conflict in this sector is dust pickup on the film surface before anti-fog coating adhesion; the resin lot must therefore be stored away from dusty regrind areas and corona-treated to 38–42 mN/m immediately before coating. Anti-fog formulations use nonionic ethoxylates, and tear propagation resistance per ASTM D1922 must remain above 12 N for 150 µm film. Finished articles include single-skin greenhouse covers and silage pit top sheets where low-temperature crack resistance during frame installation determines multi-season field performance.
In extrusion coating, melt temperature at the adapter is set to 280–305 °C with a 32:1 L/D extruder and a flat die of 0.4–0.5 mm land length. Coating weight ranges from 8–25 g/m², with line speeds between 150–300 m/min. Because this metallocene linear low density polyethylene lacks long-chain branching, neck-in is larger than typical LDPE; addition of 10–20 wt% high-pressure LDPE or a long-chain branched metallocene resin reduces edge neck-in by 20–35 mm per edge at 200 m/min on a 1 m die. Lower seal initiation allows paper-based pouches to seal at 105–115 °C, reducing heat transfer to the paperboard and preventing edge scorch. The coated paperboard must pass polyolefin coating migration limits under FDA 21 CFR 177.1520 and EU 10/2011, with overall migration measured by EN 1186-1. For liquid packaging structures, pinholing is controlled by maintaining a substrate moisture content below 6 wt% and by using a primer or ozone treatment to raise adhesion above 3 N/15 mm peel force. Finished applications include sachet stock, paperboard cup stock, and frozen food carton liners where the metallocene seal layer provides low-odour and low-seal-temperature performance.
| Application segment | Primary standard | Test method | Control limit |
|---|---|---|---|
| Food-contact seal film | EU 10/2011 | EN 1186-1 | Overall migration < 10 mg/dm² |
| Cast pallet stretch film | ASTM D5458 | ASTM D5748 | Puncture force verified per lot |
| Agricultural covering film | EN 13206 | ASTM D1709 | Dart impact > 800 g at -10 °C |
| Extrusion-coated paperboard | FDA 21 CFR 177.1520 | EN 1186-1 | Peel adhesion > 3 N/15 mm |
Heavy-duty industrial sacks benefit from 20–50 wt% loading of Icorene 1761 ORE 3217 blended with high-molecular-weight HDPE or C6 Ziegler-Natta LLDPE. Processing on a single-layer blown film line with internal bubble cooling and 1.8–2.4 mm die gap at a blow-up ratio of 1.8–2.2 yields 80–120 µm film. Because the metallocene resin has lower melt strength than high-pressure LDPE, frost line height must not exceed 10 die diameters; otherwise bubble movement induces gauge bands that reduce sack burst strength. Sacks are tested by drop impact according to ISO 7965-2 or ASTM D5276, and films below 40 µm are unsuitable for heavy-duty valve sacks because of low transverse direction tear. Weld seal strength above 25 N/15 mm according to ASTM F88 at 140 °C is maintained by keeping lubricant and talc loadings below 0.5 wt%; higher filler loadings migrate to the seal interface and reduce seal integrity. Cold dart impact at -20 °C remains above 500 g per ASTM D1709 Method A after 50 µm thickness normalisation. Finished liners are used in boxed bulk liquid transport, freezer-grade industrial sacks, and collation overwrap for cold-chain logistics.
Competitive LyondellBasell Icorene 1761 ORE 3217 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
The LyondellBasell Icorene 1761 ORE 3217 grade is identified as a metallocene-catalyzed linear low-density polyethylene supplied for thermoplastic conversion. The base designation Icorene 1761 defines the polymer series, while ORE 3217 is a supplier-specific formulation, package-state, or production-campaign suffix. Publicly available data for this exact suffix may be limited, so the technical descriptions below use class-typical ranges for metallocene linear low-density polyethylene film and extrusion grades unless a lot-specific certificate of analysis is explicitly referenced. The polymer class is produced by copolymerizing ethylene with an alpha-olefin under single-site metallocene catalysis. The molecular architecture is characterized by a narrow molecular weight distribution, uniform short-chain branching, and reduced low-molecular-weight extractable fractions relative to conventional Ziegler-Natta linear low-density polyethylene.
In melt conversion, the narrower distribution of chain lengths and comonomer placement produces a lower melting peak and a more uniform semicrystalline morphology. Differential scanning calorimetry under ISO 11357-3:2018 typically shows a melting peak between 105 °C and 125 °C for the mLLDPE class. Density is generally within 0.912 g/cm³ to 0.940 g/cm³, while melt mass-flow rate at 190 °C/2.16 kg may be formulated from 0.5 g/10 min to 5.0 g/10 min. For the ORE 3217 configuration, the exact melt flow rate, density, comonomer type, and additive package should be verified against the supplier’s certificate of analysis or technical data sheet because suffix changes can alter slip, antiblock, or processing-aid loadings.
The primary difference originates in the active-site uniformity of the metallocene catalyst. Ziegler-Natta systems contain multiple active-site populations with different comonomer incorporation rates and chain-transfer probabilities. The product is therefore a heterogeneous mixture of chains with broad molecular weight distribution and broad short-chain branching distribution. Metallocene systems produce chains with Mw/Mn values commonly in the range 2.0–3.0; Ziegler-Natta LLDPE film grades are typically 3.5–5.0 as measured by gel permeation chromatography. High-pressure LDPE, by contrast, has a broad molecular weight distribution and long-chain branching that provides high melt strength but lower crystallinity and different extensional rheology at equivalent density.
In film applications, the narrow composition distribution of metallocene LLDPE lowers the temperature at which a heat seal reaches a given hot-tack strength. Seal initiation temperature can be 5–15 °C lower than that of a Ziegler-Natta LLDPE of the same density and comonomer type. Dart impact resistance and Elmendorf tear resistance at equivalent thickness are generally higher because tie-chain probability is more evenly distributed across the semicrystalline morphology. Optical haze is reduced because the fraction of high-density, high-crystallinity chains is lower. The trade-off is bubble stability in blown film: melt strength is lower, and the resin may exhibit draw resonance, bubble sag, or edge weave on older lines designed for LDPE.
| Property | Test method | Conventional ZN-LLDPE | Metallocene LLDPE |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.916–0.940 g/cm³ | 0.912–0.940 g/cm³ |
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | 0.5–3.5 g/10 min | 0.5–5.0 g/10 min |
| Molecular weight distribution, Mw/Mn | GPC, polystyrene calibration | 3.5–5.0 | 2.0–3.0 |
| Dart impact, F50, 38 mm | ASTM D1709 | 80–300 g | 150–500 g |
| Elmendorf tear | ASTM D1922 | MD 200–700 g; TD 300–800 g | MD 300–900 g; TD 400–1,000 g |
| Seal initiation temperature | ASTM F88 | 100–115 °C | 88–105 °C |
| Haze, 50 µm film | ASTM D1003 | 8–20 % | 3–10 % |
The values in Table 1 are not product specifications for the ORE 3217 suffix. They are compiled from class-typical film-grade data and are included only to show the performance shift associated with single-site catalysis. Product-specific claims for Icorene 1761 ORE 3217 should be limited to the LyondellBasell technical data sheet and lot certificate.
The uniformity of intermolecular comonomer incorporation in metallocene LLDPE is described by the composition distribution breadth index. Single-site catalysts produce a narrower distribution of comonomer content, meaning most chains contain a similar mol% of butene, hexene, or octene. This reduces the range of crystallite thicknesses formed during cooling. A conventional Ziegler-Natta LLDPE may contain a highly branched low-melting fraction and a separate linear high-melting fraction; that heterogeneity persists as optical haze, variable seal behaviour, and local stiffness differences. The narrow molecular weight distribution of mLLDPE also reduces shear thinning. Viscosity at high shear remains closer to zero-shear viscosity than for a broad-MWD LLDPE, which increases melt pressure and torque at equivalent screw speed but can improve dimensional stability in profile and injection applications.
The more uniform short-chain branching distribution increases tie-chain probability for a given density. Under tensile deformation, tie chains transmit stress between lamellae and delay crack propagation. This mechanism explains the common combination of improved puncture resistance, higher dart impact, and lower seal initiation temperature in metallocene LLDPE compared with Ziegler-Natta LLDPE. The lower fraction of highly linear, high-melting chains also reduces the crystallization temperature and can widen the processing window for thin-gauge film, provided that heat removal and bubble handling are adjusted for the lower melt strength.
On blown-film lines with grooved-feed extruders of 25:1 to 30:1 L/D, narrow-MWD metallocene LLDPE can increase head pressure by 10–25 % relative to a broad-MWD Ziegler-Natta LLDPE at the same screw speed and melt temperature. The pressure increase is more pronounced in shallow-flight single-screw designs without barrier sections or mixing elements. Die-lip build-up can occur when low-molecular-weight oxidized fractions or slip additives deposit at the die exit. This is managed with periodic die cleaning and fluoropolymer processing-aid additions of 200–800 ppm. Melt temperature should normally be limited to 230–280 °C for cast film and 180–220 °C for blown film, with short-term excursions below 290 °C to limit oxidative chain scission, gel formation, and odour development. Pre-drying is not normally required at ambient relative humidity below 60 %, but surface condensation at higher humidity may require a hopper dryer at 60–70 °C for 1–2 h.
Changeover from a Ziegler-Natta LLDPE to a metallocene grade on a 75 mm single-screw extruder can require purge times of 30–60 min because of viscosity mismatch and wall-slip differences. A commercial purging compound with a melt index of 0.5–2.0 g/10 min and an LDPE carrier can shorten the transition. In injection molding, the narrow MWD of mLLDPE provides lower warpage and higher part toughness, but injection pressure may be higher than expected for a given melt index because the high-shear viscosity does not drop as steeply as that of a broad-MWD LLDPE.
In monolayer and coextruded film structures, the selection of Icorene 1761 ORE 3217 over a conventional Ziegler-Natta LLDPE is driven by sealing performance and end-use abuse resistance. The lower seal initiation temperature allows packaging lines to run at higher cycle speeds, because the dwell time required to reach adequate seal strength can be reduced by 10–20 % at a given seal bar temperature. Hot-tack strength, measured by ASTM F1921, is improved by the uniform branching because the molten seal remains cohesive during the sealing pulse. In blown film, dart impact values are typically higher at the same film thickness; the improvement is most pronounced in thin gauges below 50 µm. These property advantages are obtained only when the extruder and die are configured to manage the lower melt strength: a dual-lip air ring or internal bubble stabilization is commonly used, and the blow-up ratio is maintained between 2.0:1 and 2.8:1 to avoid bubble instability.
Published data for this specific ORE 3217 configuration are limited, so end-use qualification on the actual line remains necessary. In cast film, metallocene LLDPE class resins may be extruded at 230–280 °C, with line speeds above 300 m/min sometimes requiring LDPE blending at 10–30 wt% to suppress draw resonance. Extrusion coating and high-drawdown processes are not considered a direct substitution for high-pressure LDPE without blending because long-chain branching is absent. For rotomolding, if the ORE 3217 suffix designates a rotational molding powder or micropellet, the narrow melting range can require careful mould temperature control within ±5 °C of the peak melting region to avoid incomplete coalescence or excessive cycle time.
Regulatory evaluation for food-contact uses should be based on the supplier’s certificate of compliance. The resin class is generally within the scope of 21 CFR 177.1520 for olefin polymers when catalyst residues and extractable fractions meet the specified end-test limits. In the European Union, compliance with Regulation (EU) No 10/2011 Annex I is determined by overall migration and specific migration tests for the final packaging article, not by the resin alone. For REACH registration, polyethylene polymers are typically exempt from registration as polymers under the polymer exemption criteria, but monomers and additives must be registered. The processor is responsible for verifying that the additive package in the ORE 3217 suffix does not impose restrictions under RoHS Directive 2011/65/EU if the final article is electrical or electronic equipment.
| Standard or regulation | Scope | Application condition |
|---|---|---|
| ISO 1183-1:2019 | Density of non-cellular plastics | Immersion or liquid pycnometer method |
| ISO 1133-1:2022 | Melt mass-flow rate | 190 °C/2.16 kg |
| ISO 11357-3:2018 | Melting and crystallization temperature | DSC heating and cooling cycle |
| ASTM D1238-23 | Melt flow rate by extrusion plastometer | 190 °C/2.16 kg |
| 21 CFR 177.1520 | Olefin polymers for food contact | End-test extraction limits |
| Regulation (EU) No 10/2011 | Plastic food-contact materials | Overall and specific migration testing |
| REACH | Polymer registration status | Polymer exemption if criteria met |
Trial outcomes may vary because the ORE 3217 suffix can denote a specific comonomer type, slip/antiblock package, or production campaign. Without the lot certificate, fixed processing parameters such as melt temperature, die pressure, and purge profile should not be assumed. Processors should request the technical data sheet, lot certificate of analysis, and migration compliance statement from LyondellBasell for the exact grade and production batch.