Lyondellbasell Icorene 1761 Gry 7907 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 466442
    Density 0.918 g/cm³
    Meltindex 1.0 g/10 min at 190°C/2.16 kg
    Tensilestrengthatyield 10.0 MPa
    Tensilestrengthatbreak 25.0 MPa
    Elongationatbreak 600%
    Flexuralmodulus 240 MPa
    Dartdropimpact 180 g
    Elmendorftearstrengthmd 130 g
    Elmendorftearstrengthtd 400 g
    Haze 6%
    Gloss 85%
    Meltingpoint 120°C
    Vicatsofteningpoint 95°C
    Processingtemperature 200°C
    Sealinitiationtemperature 90°C
    Color Grey
    Form Pellets

    As an accredited LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 GRY 7907 is typically supplied in 25 kg polyethylene bags, palletized at 1,000 kg per pallet (40 bags).
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of LyondellBasell Icorene 1761 GRY 7907 metallocene LLDPE resin, securely shrink-wrapped for export.
    Shipping LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene is a non-hazardous thermoplastic resin. Transport in dry, sealed bags, boxes, or octabins. Protect from moisture, contamination, and excessive heat. Not DOT, IMDG, or IATA regulated; no UN number, hazard class, or packing group required.
    Storage Store LyondellBasell Icorene 1761 GRY 7907 polyethylene in a cool, dry, well-ventilated warehouse, away from heat, ignition sources, and direct sunlight. Keep original containers closed, palletized, and protected from moisture, dust, and contamination. Avoid strong oxidizers and use first-in, first-out rotation. Follow the SDS and local regulations for safe handling and storage. Do not store outdoors or near open flames.
    Shelf Life Shelf life is two years when stored in original unopened packaging, cool and dry, away from direct sunlight and moisture.
    Application of LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene

    In rotational moulding of grey technical enclosures, Icorene 1761 GRY 7907 powder is conditioned in a desiccant hopper at 65–75°C for 2–4 h when storage relative humidity exceeds 60%. Incoming particle size distribution is screened on a 35 mesh (500 µm) sieve, and bulk density is checked according to ASTM D1895 Method A. Prior to charging, 0.05–0.15 wt% of phenolic antioxidant masterbatch is tumbled for 10–15 min in a low-shear ribbon mixer. Oven air temperature is set between 270°C and 300°C, while internal air temperature is logged with a Type K thermocouple until 190°C is recorded for 3 mm nominal wall sections. A lower peak internal air temperature yields partially coalesced particles on the inner free surface; a value above 220°C increases void formation from surface moisture or low-molecular-weight fractions. Demoulding is delayed until the mould-side surface drops below 70°C, because earlier removal increases edge warpage in flat-based enclosure designs. Compliance for electrical housings is limited to low-voltage installations, since unfilled polyethylene grades typically classify as HB under IEC 60695-11-10, not V-0. Finished components are used as machine guards, hydraulic tank covers, telemetry housings, and air-handling shrouds.

    What Oven Air Temperature Ramp Controls Warpage in Large Grey Agricultural Water Tanks?

    Differential cooling between the mould-side surface and the inner air interface remains the primary source of warpage when moulding 300–600 L vertical water tanks. The mould surface is prepared with a semi-permanent release agent cured at 120°C for 20 min before the first cycle. The oven ramp is programmed to reach 290°C within 12–15 min and hold until the internal air temperature reaches 195–210°C; this plateau is held for 4–6 min to complete sintering at 5–6 mm wall thickness. Rotational speed ratio is set at 4:1 primary to secondary, with the minor axis reversed for the final 2 min to reduce ski-jump formation near the tank shoulder. Outdoor grades are dry-blended with 0.15–0.3 wt% hindered amine light stabilizer and 0.05–0.1 wt% phenolic antioxidant prior to moulding. The grey-pigmented feedstock is specified for non-potable water storage; potable water contact requires separate migration testing under EU 10/2011 or equivalent national legislation. End products include agricultural sprayer tanks, animal feed hoppers, and chemical dosing tanks tested under ASTM D1998-21.

    For rotational lining of steel chemical vessels, the metal substrate is blasted to Sa 2.5 according to ISO 8501-1:2007 and preheated in an oven to 220–260°C before the grey powder is applied in successive passes. The liner thickness is built to 4–6 mm; after cooling, pinhole detection is carried out with high-voltage spark testing according to ASTM D4787 at 5–15 kV depending on the final thickness. Chemical resistance is evaluated by immersion in selected media for 28 days at 23°C and 60°C under ISO 175:2010, with a typical acceptance criterion of ≤ 1% mass change. Stainless steel fittings can be encapsulated during the second pass, but the differential thermal contraction between the metal insert and the mLLDPE liner requires a post-cure slow cool at ≤ 5°C/min to prevent stress cracking around the flange. The lining is not specified for concentrated nitric acid above ambient temperature or for aromatic solvents above 40°C without validated chemical resistance data. End products include wastewater dosing vessels, electroplating rinse tanks, and transportable diesel storage cells.

    Injection Moulding Gate Freeze-Off and Dimensional Stability at 2.1 mm Wall Stock

    When pelletized material is moulded in thin-wall industrial containers, barrel temperatures are maintained at 200–230°C, the nozzle at 210°C, and the mould surface at 20–40°C. The narrow molecular weight distribution of metallocene LLDPE shortens the gate freeze time compared with conventional Ziegler-Natta LLDPE at the same wall thickness; holding-pressure time is therefore limited to 5–10 s for a 2.1 mm nominal wall. Flow length-to-wall thickness ratios above 150:1 produce excessive pressure drop and short-shot at the end of fill. Dimensional stability after demoulding is documented through measurement at 24 h and 48 h post-moulding under ISO 294-4, because post-mould shrinkage continues as crystallinity approaches equilibrium. For stackable crates and waste containers, the grey pigmentation permits laser marking of polymer code under ISO 11469:2016. The grade is not intended for food-contact packaging unless migration testing under EU 10/2011 or FDA 21 CFR 177.1520 is supplied for the specific lot. End products include distribution totes, reusable dunnage trays, and municipal waste bins.

    The following compliance matrix identifies the test designations used in qualification of grey mLLDPE components in these sectors:

    ApplicationStandard designationVerification condition
    Rotational moulded non-potable water tanksASTM D1998-21Wall thickness, pinhole continuity under ASTM D4787
    Rotational lined steel vesselsISO 175:2010Immersion in selected media for 28 days at 23°C and 60°C
    Injection moulded industrial containersISO 11469:2016Material marking with polymer code and filler type
    Outdoor grey componentsISO 4892-2:2013Xenon-arc exposure; target agreed between supplier and moulder
    Electrical enclosure low-voltage useIEC 60695-11-10Flammability classification; polyethylene normally rated HB, not V-0

    Compounding of grey-pigmented metallocene LLDPE with post-consumer HDPE is performed on a co-rotating twin-screw extruder with 40:1 L/D and segmented screw elements. Barrel settings from 190°C to 210°C avoid oxidative chain branching; specific mechanical energy is typically logged at 0.18–0.24 kWh/kg for a 30 mm twin-screw extruder running at 300–600 rpm. The mLLDPE is added at 10–30 wt% to the recycled HDPE stream to increase notched impact strength and environmental stress crack resistance, with ESCR measured under ASTM D1693-15 at 50°C in 10% nonylphenoxy poly(ethyleneoxy) ethanol solution. A melt filtration system with 100–150 µm screens removes residual rigid contamination before strand pelletization. Published data for this specific grade in post-consumer HDPE blends is limited; pilot compounding must be conducted before specifying mechanical property guarantees. End products include dark grey drainage chambers, truck wheel arch liners, and industrial pallet stops.

    When the Powder Is Used as a Carrier Resin for Grey Masterbatch Extension

    Masterbatch extension with this powder requires a two-stage pigment dispersion protocol on a high-shear co-rotating twin-screw extruder, because the grey pigment already present acts as a dilution base for dark recycled compounds. In a first stage, a 50 wt% concentrate is prepared using the powder as carrier and a wetting agent at 0.5–1.0 wt%; in the second stage, the concentrate is let down at 20:1 into natural mLLDPE or HDPE extrusion compounds. Melt temperature at the die is held below 220°C; higher temperatures shift the grey tone due to oxidative yellowing of the stabilizer package. Let-down ratios above 25:1 may result in visible colour drift from metering errors on single-screw extruders without gravimetric dosing. Compatibility with outdoor exposure is evaluated under ISO 4892-2:2013, with the number of xenon-arc hours agreed between compounder and end user. End products include grey horticultural trays, construction shims, and protective packaging inserts processed on conventional sheet and profile lines.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7907 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    In rotational moulding operations, LyondellBasell Icorene 1761 GRY 7907 is classified as a metallocene-catalysed linear low-density polyethylene powder with an integral grey pigmentation package. The grade is specified where low-temperature impact strength, environmental stress crack resistance, and pin-hole-free thin-wall coalescence must be maintained in hollow parts. Grade-specific release limits are available on the manufacturer’s certificate of analysis; public batch certificates for the prefilled grey configuration are not always issued through regional distribution channels. When independent verification is required, density is determined by ISO 1183-1:2019 and melt flow rate by ISO 1133-1:2022 at 190 °C and 2.16 kg. Typical metallocene LLDPE rotational moulding powders of this class exhibit a density interval of 0.936–0.940 g/cm³ and a melt flow rate of 4.5–5.5 g/10 min; the exact values for Icorene 1761 GRY 7907 require the batch release certificate.

    The GRY 7907 suffix indicates a pre-compounded grey colour package, not a dry-blend pigment masterbatch. This package is typically dispersed on a co-rotating twin-screw extruder with a length-to-diameter ratio of 40:1 or greater before pelletising and pulverising to a rotomoulding powder. The advantage is the elimination of colour segregation during storage and the reduction of pigment agglomerates that can act as stress-concentration sites. The limitation is that regrind from the coloured variant cannot be re-entered into natural resin clean streams without colour contamination.

    The designation “metallocene” refers to the catalyst type, not to a specific comonomer. Depending on the production line, the comonomer may be 1-butene, 1-hexene, or 1-octene. High-toughness mLLDPE rotomoulding grades are commonly based on 1-hexene or 1-octene because the longer side branches increase tie-molecule formation. The comonomer identity is not always disclosed in the public designation; when chemical compatibility work depends on comonomer type, the request should be routed through the supplier technical service channel.

    How does the metallocene catalyst architecture influence rotomoulded part toughness?

    Metallocene catalysis produces a more uniform interchain branching distribution than multi-site Ziegler-Natta chemistry. The practical consequence in rotomoulding is that the resin can reach a given level of toughness at a lower density penalty. When a fully coalesced wall is cooled at 5–10 °C/min, the mLLDPE solidifies with a narrower lamellar thickness distribution and fewer large tie-chain-deficient spherulites. The resulting rotomoulded panels retain ductile failure down to approximately −60 °C when tested for brittleness temperature according to ASTM D746-20. Environmental stress crack resistance under ASTM D1693-15 can exceed 1000 h at F50 using 10% Igepal. A Ziegler-Natta LLDPE of the same density commonly falls between 200 h and 600 h under the same condition.

    The narrower molecular weight distribution reduces melt elasticity and zero-shear viscosity. This can improve coalescence at lower peak internal air temperature, but it also lowers melt stand-up strength on deep-draw cavities. On biaxial rotomoulding machines, the metal surface temperature must exceed 220 °C for void elimination; below this threshold, pinhole formation is concentrated at the inside radius of the pour bed. At the upper bound, metal surface temperatures above 290 °C initiate oxidative chain scission, visible as yellowing and a measurable drop in instrumented puncture energy under ISO 6603-2:2016.

    The homogeneous branching also lowers the cold-temperature modulus response. A rotomoulded tank wall made from the mLLDPE class typically yields a flexural modulus of 700–900 MPa under ISO 178:2019, which is lower than HDPE rotomoulding grades at 900–1200 MPa. Where the service requirement is hoop stiffness, this difference must be compensated by part design or wall thickness. Where the requirement is resistance to slow crack growth from internal stress, the mLLDPE grade is generally selected over HDPE despite the stiffness deficit.

    Compared with high-pressure low-density polyethylene, the linear low-density metallocene product gives higher tensile yield and puncture resistance at equivalent wall thickness. Compared with HDPE rotomoulding grades, it sacrifices flexural modulus and creep resistance but improves slow crack growth resistance and low-temperature impact. For potable water tanks, the metallocene grade may also offer lower extractable fractions, although actual regulatory approval remains article-specific and depends on the pigment formulation.

    Processing window constraints on slow-cooled rotomoulded walls

    Rotomoulding with a pre-pigmented mLLDPE powder requires tighter thermal control than a high-shear compounding step. The powder is ground to a target 35-mesh (500 µm) particle size. Excess fines below 100 µm can create electrostatic clumping and uneven wall build-up, while oversize particles above 850 µm require longer coalescence time. On production carousel machines, batch-to-batch shifts in the 35-mesh oversize fraction of ±10% have been observed to change optimum oven dwell by 3–5 min. The effective processing window for parts with wall stock below 3 mm can narrow to ±5 °C at the oven setpoint because the grey pigment accelerates radiative heating.

    Drying is required when ambient humidity exceeds 60% relative humidity. A desiccant hopper set at 70 °C for 1–2 h reduces surface moisture below 200 ppm, avoiding microvoids at the inner wall surface. Direct flame impingement on mould surfaces should be avoided; zone temperatures above 300 °C promote oxidation. A two-stage cooling sequence—forced air at 15–20 °C/min to 100 °C, followed by gentle water mist for 2–3 min—reduces residual stress and part distortion. Demoulding should not occur above 70 °C for flat panels.

    The grey pigment modifies surface temperature response. With the same radiant setpoint, the pre-pigmented powder can reach coalescence temperature earlier than a natural resin. Operators should reduce the initial radiant setpoint by 5–10 °C and confirm the mould surface temperature with contact pyrometry. Insufficient adjustment produces interior gas bubbles at the surface of the pigment-rich layer. Polypropylene contamination from feed lines and mould release residues are incompatible and must be purged with low-melt-flow polyethylene before charging.

    Comparative property intervals across rotational moulding polyethylene classes
    PropertyTest methodmLLDPE rotomoulding classZiegler-Natta LLDPE rotomoulding classHDPE rotomoulding class
    DensityISO 1183-1:20190.936–0.940 g/cm³0.930–0.940 g/cm³0.940–0.955 g/cm³
    Melt flow rateISO 1133-1:2022, 190 °C/2.16 kg4.5–5.5 g/10 min4.0–5.0 g/10 min5.0–8.0 g/10 min
    Tensile yield stressISO 527-2:201218–22 MPa16–20 MPa22–28 MPa
    Flexural modulusISO 178:2019700–900 MPa500–700 MPa900–1200 MPa
    ESCR F50ASTM D1693-15>1000 h200–600 h50–200 h
    Brittleness temperatureASTM D746-20<−60 °C−40 to −50 °C−40 °C
    Instrumented puncture energyISO 6603-2:2016180–220 J120–160 J100–140 J

    Intervals represent class-typical published ranges from mLLDPE, Ziegler-Natta LLDPE, and HDPE rotomoulding datasheets, not batch certificates for the specific Icorene 1761 GRY 7907 configuration. The batch certificate remains the controlling document for release limits.

    For direct food-contact use, the natural polyolefin base of this product class is typically assessed under FDA 21 CFR 177.1520 as an olefin polymer. The finished grey article must also meet EU 10/2011 overall migration requirements, with verification executed on the final wall thickness and pigmentation level. Under EU 10/2011, the overall migration limit is 10 mg/dm²; specific migration of the pigment carrier and any slip additives must be verified under Annex IV. Dry-colour or regrind made from mixed-colour scrap is outside a single-grade food-contact declaration.

    Compliance matrix for food-contact and restricted-substance verification
    FrameworkTest or clausePractical scope
    FDA 21 CFR177.1520Olefin polymer base for food-contact articles; n-hexane extractable fraction depends on food type and use temperature.
    EU 10/2011Annex IVOverall migration limit 10 mg/dm²; specific migration limits for pigment carriers and additives.
    REACH SVHCArticle 33Communication required if a substance of very high concern exceeds 0.1% w/w in the article.
    RoHS 2011/65/EUIEC 62321XRF screening for Cd, Pb, Hg, CrVI, PBB, and PBDE in electrical and electronic housing applications.

    Outdoor service in grey parts requires weathering validation beyond base resin plaque data. The grey pigment provides limited UV screening and does not replace hindered amine or benzotriazole stabilisers. Accelerated weathering should follow ISO 4892-2:2013 or ASTM D2565-16, with colour difference ΔE and retained tensile elongation recorded at intervals up to 2000 h. Failure criteria are application-dependent, but retained elongation below 50% of the unexposed value is commonly treated as embrittlement in storage tanks and marine fenders.

    A complete engineering specification for this product should include density by ISO 1183-1:2019, melt flow rate by ISO 1133-1:2022 procedure A, tensile yield stress and elongation at break by ISO 527-2:2012, flexural modulus by ISO 178:2019, and environmental stress crack resistance by ASTM D1693-15. For low-temperature service, brittleness temperature by ASTM D746-20 and instrumented puncture by ISO 6603-2:2016 are added. A complete certificate of analysis for the grey variant should also report the ash content of the pigment package and the particle size distribution at 35-mesh and 80-mesh sieves. Colour ΔE against a reference plaque should be controlled under ASTM D2244-23.

    When replacing a Ziegler-Natta LLDPE rotomoulding charge with Icorene 1761 GRY 7907

    Substitution in an existing mould requires modification of the heating profile rather than a direct drop-in. Because the metallocene grade coalesces at lower internal air temperature, the oven temperature setpoint should initially be reduced by 10–15 °C relative to the Ziegler-Natta powder. On a biaxial machine, the rotation ratio may be moved from 4:1 to 5:1 for symmetrical hollow parts, with major-axis speed between 6 rpm and 8 rpm and minor-axis speed between 1.5 rpm and 2 rpm. The servo-driven carousel should be programmed to hold the lower setpoint for the first 2–3 min of the oven cycle, then ramp to full mould contact temperature of 260–280 °C on the metal surface.

    Differences in shrinkage and warpage must be characterised using production-scale moulds. The lower modulus of the mLLDPE class can reduce demoulding force on straight-sided parts, but the more uniform crystallisation may increase linear mould shrinkage by a few tenths of a percent relative to HDPE. Dimensional verification should follow ISO 294-4:2018 for shrinkage, while tensile and weld-line verification follow ISO 527-2:2012 and ASTM D638-14. On production lines, weld-line strength is measured from a multi-piece mould insert; reduction below 80% of the parent wall strength indicates either contaminant carryover or insufficient coalescence.

    Regrind from this prefilled grey variant may be reintroduced up to 15–20 wt% in the same part, provided it is dried and free of polypropylene. Above 20 wt%, pigment degradation products and crosslinked gels from previous thermal histories increase surface pitting and lower environmental stress crack resistance. Amine-based antifog or antistatic additives should be avoided in direct contact with the melt because they can alter crystallisation kinetics and cause localised grey discolouration. For service in high-humidity chemical storage, compatibility testing with the contact fluid should follow ASTM D543-20 or the relevant chemical resistance protocol for the stored liquid. Published data for this specific prefilled grey configuration is limited; field validation on production-scale multi-arm shuttle moulders remains necessary before cycle parameters are locked.

    Top