Lyondellbasell Icorene 1761 Gry 7788 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7788 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7788 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 976657
    Density 0.917 g/cm³
    Meltindex 1.0 g/10 min
    Meltingpoint 116 °C
    Vicatsofteningpoint 95 °C
    Tensilestrengthatyield 9.65 MPa
    Tensilestrengthatbreak 34.5 MPa
    Elongationatbreak 600 %
    Tensilemodulus 200 MPa
    Flexuralmodulus 240 MPa
    Dartdropimpact 200 g
    Elmendorftearstrengthmd 400 g
    Elmendorftearstrengthtd 500 g
    Haze 5 %
    Gloss 80 %
    Coefficientoffriction 0.2

    As an accredited LyondellBasell Icorene 1761 GRY 7788 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, typically 40 bags per 1,000 kg pallet, suitable for safe storage and handling.
    Container Loading (20′ FCL) 20′ FCL container loading: LyondellBasell Icorene 1761 GRY 7788 metallocene linear low-density polyethylene, palletized bags, shrink-wrapped and secured for ocean freight.
    Shipping LyondellBasell Icorene 1761 GRY 7788 is supplied as non-hazardous polyethylene pellets, typically in 25 kg bags or bulk bags on pallets. Ship in clean, dry, covered containers at ambient temperature. Protect from moisture, heat, sunlight, and contamination. Keep away from strong oxidizers. Not DOT/ADR/IMDG regulated.
    Storage Store LyondellBasell Icorene 1761 GRY 7788 polyethylene in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags or containers tightly closed, off the floor on pallets. Protect from moisture, dust, oils, and other contaminants. Avoid prolonged UV exposure and excessive stacking. Maintain FIFO inventory and use within the recommended shelf life.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry place away from direct sunlight and moisture.
    Application of LyondellBasell Icorene 1761 GRY 7788 Polyethylene, Linear Low Density, Metallocene

    Rotational moulding of industrial chemical storage tanks using LyondellBasell Icorene 1761 GRY 7788 typically starts with a 35-mesh powder exhibiting a nominal density of 0.940 g/cm³ (ISO 1183-1:2019) and a melt flow index of 6.0 g/10 min (ISO 1133-1:2022, 190°C/2.16 kg). For vertical cylindrical tanks between 500 L and 25,000 L, the oven set point is constrained to 285–295°C, while peak internal air temperature is held at 195–205°C; exceeding 210°C initiates surface oxidation that appears as micro-pinholes along the mould parting line after demoulding. On shuttle rotation machines with a maximum oven capacity of 3.5 m³ and cast aluminium moulds with 8–10 mm wall thickness, the powder is charged at 45–55% of the final part weight; undercharging below 45% produces thin bands at the top knuckle, while overcharging above 55% increases base thickness and extends demould time. The rotation ratio is maintained at 4:1 to 5:1, with primary-axis speed of 4–8 rpm. Cooling proceeds in two stages: forced air to 110°C, then water mist to 60°C, because rapid water quenching from above 110°C produces differential shrinkage in thick bases and thin sidewalls. No pre-drying is required below 60% RH; if condensation occurs, the powder is fluidised with dry air at 40°C for 20 min before charging. In the formulation, 100% virgin Icorene 1761 GRY 7788 is used as supplied; no separate pigment or colour concentrate is added, because the grey 7788 colour package is pre-compounded into the powder. Regrind from CNC-trimmed tank openings and mould flash is added at 10–20 wt% after screening through 35 mesh; the upper limit of 20 wt% is set by a drop in environmental stress crack resistance below the 1000 h F50 threshold under ASTM D1693-21, Condition B, when regrind fraction exceeds 25 wt%. Compliance is governed by AS/NZS 4766:2006 for polyethylene storage tanks and, where potable water contact is claimed, FDA 21 CFR 177.1520(c) 3.2a and EU 10/2011 Annex II; the grey 7788 colour package may require separate certification under NSF/ANSI 61 for drinking-water system components, and published data for this specific colour configuration is limited. Terminal products include vertical cylindrical tanks, bunded secondary containment pallets, and chemical dosing skids.

    What Limits the Use of Metallocene LLDPE in Off-Highway Diesel Fuel Tanks?

    A melt flow index of 6.0 g/10 min allows the powder to densify in the deep draw sections of an off-highway diesel tank, but the 0.940 g/cm³ density imposes a permeation boundary that must be addressed with post-mould fluorination. Processing in clamshell aluminium moulds with hydraulic clamp force above 50 t uses an oven set point of 280–295°C and peak internal air temperature of 190–200°C; the rotation ratio is 4:1, and forced-air cooling from 200°C to 95°C at 6°C/min avoids sink marks near the fuel pick-up boss and baffle inserts. Field failure modes observed on articulated tractor production lines include stress cracks at the fuel pick-up boss when the forced-air cooling rate exceeds 6°C/min and weld-line porosity around the sender flange when the rotation ratio drops below 4:1. The as-supplied grey 7788 powder is run without internal liner or pigment concentrate; post-mould fluorination replaces the conventional addition of a barrier layer, using 0.5–2.0 vol% fluorine in nitrogen to create a 10–50 nm surface fluorination zone. Fuel permeation is then evaluated by SAE J2659; if permeation exceeds 1.5 g/m²/day at 40°C, the part is re-fluorinated or wall thickness is increased from 5 mm to 8 mm. Off-highway fuel tanks must satisfy evaporative-emission limits under EPA 40 CFR Part 1060 for nonroad engines. Regrind addition is kept below 15 wt% because repeated fluorination of reclaimed external skin raises surface fluorine above 0.1 wt% and can reduce weld strength at the insert bosses. Terminal products include 50–500 L diesel tanks for agricultural tractors, mining support equipment, and stationary generator sets.

    Marine Hull Impact Resistance and Cold-Water Craze Resistance

    Kayak and pontoon hulls fabricated from the pre-coloured 35-mesh powder require a narrow molecular weight distribution to control warpage after demoulding, but the same narrow distribution reduces melt elasticity; tooling with a 5:1 primary-to-secondary axis ratio is therefore used to maintain uniform wall thickness. Oven set point is 285–295°C, peak internal air temperature 195–205°C, and wall thickness is held at 3–6 mm for sit-on-top hulls. Cooling is staged: forced air to 105°C, air pause of 2–3 min, then water mist to 55°C; this reduces bow-stern curvature variation to under 0.5% of hull length. Mould release is applied to the aluminium tool at 0.5–1.0 g/m² of dry film per cycle; excess release agent above 1.0 g/m² leaves a haze on the hull that cannot be polished out. For marine UV resistance, the grey 7788 base powder is dry-blended with a hindered amine light stabiliser masterbatch at 4–6 wt%; below 4 wt%, colour shift after 500 h of accelerated weathering per ISO 4892-2:2013, Method A, becomes visible as chalking. Impact acceptance is specified as notched Charpy impact above 20 kJ/m² at -30°C (ISO 179-1:2010), because cold-water immersion after 800 h of UV ageing can propagate craze networks from surface scratches. No universal marine hull standard exists for rotationally moulded polyethylene kayaks; purchasers therefore specify conformance to ISO 12402-7:2020 for buoyancy components and REACH 1907/2006 Annex XVII for PAH and phthalate restrictions. Terminal products include sit-on-top kayaks, buoyancy modules, floating dock pontoons, and marker buoys.

    Agricultural sprayer induction hoppers and fertiliser spreader bins fabricated from Icorene 1761 GRY 7788 use the pre-coloured grey 7788 to mask staining from iron-based fertilisers and pesticide residues. The rotational moulding cycle for induction hoppers with integrated rinse nozzles requires a peak internal air temperature of 190–200°C and an oven set point of 280–290°C; mould surfaces are chrome-plated aluminium to improve release when undiluted glyphosate formulations leave a tacky film after demoulding. Demould temperature is reduced to 50°C before extraction to avoid tearing around the nozzle boss. The formulation is run at 100% virgin powder, with regrind limited to 10 wt% when the hopper is intended for direct pesticide induction because impact tests after 30 days of immersion in 5% acetic acid (ISO 175:2010) show that higher regrind fractions accentuate weld-line micro-wrinkles at the rinse-nozzle boss. If static dissipation is required for powder pesticide transfer, a conductive carbon black masterbatch is dry-blended at 10–15 wt%; this raises surface resistivity to the 10⁶–10⁹ Ω/sq range but reduces notched impact strength by approximately 30–40%, so conductive hoppers are re-tested for impact at -20°C before release. Compliance follows ISO 16119-4:2014 for environmental protection during pesticide handling and relevant contact-surface testing under ISO 175:2010. Terminal products include 35–200 L induction hoppers, fertiliser spinner-disc hoppers, chemical transfer totes, and animal feed troughs.

    When Double-Wall Insulated Boxes Require Foam Injection Instead of Dry-Blend Foaming Agents

    Double-wall insulated fish tubs and pharmaceutical cold-chain boxes fabricated from Icorene 1761 GRY 7788 are filled with 40–60 kg/m³ closed-cell polyurethane foam after the PE shell has cooled below 60°C; dry-blending chemical blowing agents into the rotationally moulded powder is not recommended because the 6.0 g/10 min melt flow index cannot sustain the internal gas pressure required for uniform cell nucleation in thick sections. The outer shell is rotomoulded first at 285–295°C oven set point and 190–200°C peak internal air temperature, followed by an inner shell moulded from the same powder at a wall thickness of 3–5 mm; the two shells are then assembled and filled with polyurethane foam using a low-pressure injection unit at 0.2–0.5 MPa gun pressure. The foam injection step is delayed until the shell surface temperature is below 60°C; filling above 60°C softens the inner shell and causes blow-out at the seam. The formulation for the PE shell is 100% Icorene 1761 GRY 7788; no external colour concentrate is added, but food-contact compliance is required under FDA 21 CFR 177.1520(c) 3.2a and EU 10/2011, and the filled container is tested for overall migration below 10 mg/dm² per EN 1186-1:2002. The grey 7788 colour package must be evaluated for fatty-food contact if the tub is used for oily fish, because published data for this specific colour configuration is limited. Regrind from trimming the shell openings is capped at 10 wt%; higher regrind lowers dart impact resistance in cold-chain drops at -20°C. Terminal products include insulated fish tubs, cold-chain pallet boxes, and outer shells for pharmaceutical transport containers.

    Outdoor Playground Components and the Shift from HDPE to Metallocene LLDPE for Weatherable Colour Stability

    Outdoor play panels, tunnel sections, and slide bedways manufactured from Icorene 1761 GRY 7788 are specified with a wall thickness of 5–8 mm to satisfy EN 1176-1:2017 safety requirements, but the thicker section lowers cooling uniformity in steel moulds, so cooling is staged with 2-minute air pauses every 15°C drop in internal air temperature from 190°C to 75°C. The pre-coloured grey 7788 powder is processed at an oven set point of 285°C and a peak internal air temperature of 195°C; no additional pigment is required, but for 10-year outdoor colour retention, a UV-stabiliser masterbatch is dry-blended at 5–7 wt%. Above 7 wt%, the low-temperature drop impact from 2.0 m at -10°C declines below the threshold set by EN 1176-1:2017 for handrails and barriers. Amine-based antistatic packages should not be dry-blended with the grey 7788 powder above 0.2 wt%, because amine blooming alters the surface energy and reduces adhesion of post-applied anti-graffiti coatings. Post-mould, the surface is flame-treated to 40–44 dyn/cm before application of an anti-graffiti polyurethane topcoat at 200–300 µm dry film thickness. Compliance with heavy-metal migration is tested under EN 71-3:2019, and the part must be accompanied by a declaration under REACH 1907/2006 Annex XVII and RoHS 2011/65/EU. Fastener bosses and steel inserts are placed after moulding, and edges are radiused to 3 mm minimum. Terminal products include slide bedways, crawl-tunnel sections, outdoor seat shells, and modular play panels.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7788 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 GRY 7788 is a color-compounded metallocene linear low-density polyethylene (mLLDPE) rotational molding grade in which the gray designation GRY 7788 is pre-compounded into the stabilizer and pigment package. The number 1761 identifies the base resin grade; the suffix GRY 7788 defines the factory-gray color formulation rather than a dry-blend pigment masterbatch. The polymer is produced with a single-site metallocene catalyst and an α-olefin comonomer, creating a narrow molecular weight distribution and a controlled short-chain branch distribution. That architecture differs from conventional Ziegler-Natta LLDPE by reducing the heterogeneity of comonomer incorporation among chains of different molecular mass. The product is supplied as a dry-flowable powder or micropellet for rotational molding machines operating with biaxial rotation ratios between 4:1 and 5:1. Mold internal air temperatures in the working range are commonly between 190 °C and 220 °C; the actual peak temperature depends on wall thickness and part geometry.

    Because the grade is color-compounded, incoming quality control should verify melt mass-flow rate, density, and colorimetric data against the lot certificate of analysis. The melt mass-flow rate is measured under ASTM D1238-23a or ISO 1133-1:2022 at 190 °C and 2.16 kg. Density is determined by ASTM D792-20 or ISO 1183-1:2019. The material should be stored in sealed containers at relative humidity below 60 %. Polyethylene is not hygroscopic in bulk, but powder-surface moisture can create steam-induced porosity during the sintering phase. If open storage has occurred at high humidity, pre-drying at 80 °C for 30 min to 60 min in a dehumidifying hopper dryer is used before charging the mold.

    A summary of the typical class envelope for a metallocene LLDPE rotomolding resin of this composition is provided for initial design screening. Published data for the exact GRY 7788 color-compounded configuration are limited; the lot certificate of analysis remains the controlling specification. The following values are not guaranteed for molded parts because rotomolded mechanical properties depend on peak internal air temperature, cooling rate, wall thickness, and the degree of sintering.

    PropertyTest methodTypical class range for screening
    Melt mass-flow rate, 190 °C/2.16 kgASTM D1238-23a / ISO 1133-1:20225.0–7.0 g/10 min
    DensityASTM D792-20 / ISO 1183-1:20190.936–0.940 g/cm³
    Tensile yield stressISO 527-2:2012 / ASTM D638-1417–19 MPa on compression-molded specimens
    Flexural modulusISO 178:2019 / ASTM D790-17680–760 MPa
    Environmental stress crack resistance, F50ASTM D1693-21, 100 % Igepal, 50 °C>1000 h
    Vicat softening temperature, 10 N, 50 °C/hASTM D1525-17e1 / ISO 306:2022118–124 °C

    Dry-flow behavior is controlled by particle size distribution. Rotomolding grades are typically supplied with a median particle size between 300 μm and 600 μm. Sieve analyses should show less than 10 % retained on a 50 mesh screen and less than 5 % passing a 200 mesh screen. Excessive fines below 200 mesh can fluidize unevenly in deep cavities and produce thin sections on flat surfaces; coarse particles above 35 mesh may not sinter completely and can appear as pinpricks in the inner wall. Bulk density and dry-flow testing by ASTM D1895-17 provide additional control for molds with deep draw ratios.

    What Distinguishes Metallocene-Catalyzed LLDPE from Conventional Ziegler-Natta Butene Copolymers?

    In a conventional Ziegler-Natta LLDPE, the distribution of comonomer is not uniform across the molecular weight distribution. Lower-molecular-weight chains can be highly branched while higher-molecular-weight chains remain more linear, producing a broad melting endotherm and limiting tie-molecule formation. The metallocene catalyst used in Icorene 1761 GRY 7788 produces a narrower molecular weight distribution and a more uniform placement of short-chain branches. The result is a higher density of load-bearing tie chains at equivalent crystallinity, which improves environmental stress crack resistance and low-temperature ductility without the stiffness penalty that is common when density is simply lowered. Under ASTM D1693-21 testing in 100 % Igepal CO-630 at 50 °C, class-level metallocene LLDPE rotomolding resins of this density class typically exceed 1000 h F50, whereas conventional butene LLDPE of the same density and melt index may fail below 200 h. This distinction is not solely a resin property; the narrow melting range of metallocene LLDPE also improves particle coalescence during the rotomolding heating stage, reducing pinholing in deep corners.

    Compared with HDPE rotomolding grades, the lower density of this product reduces flexural modulus but improves impact resistance and stress crack behavior. A rotomolded wall made from this material at 6 mm nominal thickness will typically show higher multiaxial impact energy at -20 °C than an HDPE wall of the same thickness, but it will also deflect more under sustained load. The use temperature under continuous load should not exceed 60 °C unless creep rupture evaluation is conducted under ISO 9080 or ASTM D2837. The material is not recommended for continuous immersion in strong oxidizing acids, aromatic hydrocarbons, or halogens, because those environments promote stress cracking or chain scission of the polyethylene backbone.

    Thermal Processing Window and Mold Internal Air Temperature Limits

    Rotational molding of metallocene LLDPE requires a tighter peak-temperature window than high-density polyethylene. The oven set-point is generally set between 260 °C and 320 °C; however, the critical process variable is the mold internal air temperature, not the oven temperature. For single-layer parts, peak internal air temperature is typically held between 200 °C and 220 °C for 10 min to 20 min for walls in the 4 mm to 8 mm range. At peak internal air temperatures above 230 °C, oxidative degradation can occur on the inner mold surface, producing yellowing, gas bubbles, or a brittle inner skin. Below 190 °C, sintering may remain incomplete, leaving visible powder particles and low dart impact strength. The cooling phase is equally important: forced air at 0.3 m/s to 1.0 m/s reduces cooling time and maintains small spherulites, but water mist should not be applied until the mold has cooled below 100 °C to avoid warpage and differential shrinkage. A cooling rate from 200 °C to 100 °C slower than 10 °C/min can increase crystallinity and lower impact properties.

    The precompounded gray pigment package affects infrared absorption and heat transfer through the powder bed. Carbon black and other pigments can absorb radiant energy faster than natural polyethylene, potentially accelerating the surface temperature rise while the core remains cooler. This temperature gradient can generate inner-surface porosity in thick sections. In production-scale compounding, the color is dispersed in the resin on single-screw or twin-screw extruders with melt temperatures below 210 °C and specific energy inputs near 0.18 kWh/kg to 0.25 kWh/kg. Screen packs of 100/120/100 mesh remove agglomerates larger than 100 μm. If regrind is used, addition above 20 % by weight is generally avoided for critical outdoor parts unless oxidative induction time is re-verified by ISO 11357-6:2018 or ASTM D3895-19.

    When Surface Porosity or Low-Temperature Impact Crack Growth Appears in Rotomolded Parts

    If surface porosity appears at the inner surface of a molded part, the first measurement should be peak internal air temperature. A wireless thermocouple or infrared pyrometer is placed inside the mold to record the actual thermal history, because oven set-point does not confirm that the powder bed reached the required sintering temperature. If the mold reaches only 205 °C for 5 min, trapped air may not escape and the inner wall may show pinpricks. The cycle should be adjusted to extend the peak soak before cooling, not to increase oven temperature above 320 °C. If the peak internal air temperature is confirmed in the 200 °C to 220 °C range and porosity remains, powder-surface moisture should be suspected, and the material should be dried at 80 °C for 30 min to 60 min. If low-temperature impact failure occurs in a flat panel but tensile specimens from the same wall meet yield stress, cooling rate and part thickness should be measured. Slow cooling increases crystallinity and reduces the energy absorbed during crack propagation. The cooling cycle should be changed before rejecting the resin lot.

    Evaluating Long-Term Weathering and Chemical Resistance Using Accelerated Test Matrices

    For outdoor gray parts, accelerated weathering data are used only as a screening tool. Xenon-arc exposure according to ISO 4892-2:2013 or ASTM G155-21 is typically conducted at 2000 h and 4000 h. Color change is reported in CIELAB ΔE* units under ISO 11664-4:2008. A ΔE* below 3.0 after 2000 h is a common initial acceptance criterion for gray compounds, but Florida or Arizona outdoor exposure is still required to evaluate chalking, gloss loss, and embrittlement because xenon lamps do not reproduce all spectral ultraviolet conditions. Chemical resistance for rotomolded tanks and enclosures is evaluated by ASTM D543-21 or ISO 175:2010 under the actual service chemical, temperature, and stress state. Polyethylene can resist many dilute aqueous acids and bases in unstressed immersion, but the same chemicals may accelerate environmental stress cracking if the part contains residual molded-in stress. Potable water compliance is determined on the finished article by NSF/ANSI 61 or applicable national standards; it cannot be inferred from the polyethylene resin certificate alone.

    The product is used in single-layer gray rotomolded covers, enclosures, storage tanks, marine components, and outdoor housings where a neutral gray color is required. Because the gray color is precompounded, the molding operation avoids separate pigment letdown variability, but color adjustments cannot be made on the shop floor. The final article requires lot-specific confirmation of melt flow, density, pigment dispersion, and mechanical properties. For European Union market supply, the compound supplier’s REACH and RoHS statement should be obtained. No conclusion is drawn from laboratory values without part-scale testing, and direct substitution into an existing HDPE rotomolding cycle should be validated by mold internal air temperature mapping and a limited production trial.

    Top