Lyondellbasell Icorene 1761 Gry 7782 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7782 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7782 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 829837
    Polymer Type Linear Low Density Polyethylene (LLDPE), Metallocene
    Color Grey (GRY 7782)
    Form Pellets
    Density 0.917 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.7 g/10 min
    Melting Point 122 °C
    Vicat Softening Temperature 95 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 25.5 MPa
    Elongation At Break 600%
    Flexural Modulus 220 MPa
    Shore D Hardness 50
    Thermal Conductivity 0.33 W/m·K
    Water Absorption 0.01%
    Dielectric Constant 2.3
    Volume Resistivity 1E16 ohm·cm
    Processing Method Injection Molding

    As an accredited LyondellBasell Icorene 1761 GRY 7782 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg), stretch-wrapped and palletized for transport.
    Container Loading (20′ FCL) 20′ FCL loaded with LyondellBasell Icorene 1761 GRY 7782 metallocene LLDPE in 25 kg bags, palletized and secured for shipment.
    Shipping LyondellBasell Icorene 1761 GRY 7782 is a non-hazardous metallocene linear low-density polyethylene resin, typically shipped as pellets in 25-kg bags, octabins, or bulk bags on pallets. Transport in dry, clean vehicles/containers at ambient temperature; protect from moisture, contamination, and UV. Not DOT/IMDG/IATA regulated. Keep sealed until use.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed and palletized to prevent moisture pickup and dust accumulation. Maintain clean, dry floors to avoid slipping. Segregate from oxidizing agents and incompatible chemicals. Avoid prolonged high temperatures and UV exposure to preserve resin properties. Follow local regulations and supplier recommendations.
    Shelf Life Shelf life is typically 24 months when stored in original packaging, cool, dry, and away from direct sunlight.
    Application of LyondellBasell Icorene 1761 GRY 7782 Polyethylene, Linear Low Density, Metallocene

    Rotational molding of agricultural chemical storage tanks from Icorene 1761 GRY 7782 begins with control of the powder bed rather than with a generic oven recipe. The metallocene LLDPE base resin, supplied as a pulverized powder with the GRY 7782 gray color code, should be stored at 23 ± 2 °C and 50 ± 10% relative humidity before charging to minimize electrostatic clumping and moisture-driven pinhole formation. A typical particle size distribution for rotomolding powder passes a 35 mesh (500 µm) screen with less than 10 wt% fines smaller than 200 µm; excess fines segregate during rotation and produce thin corners on conical-bottom induction tanks and sprayer tanks. The target peak internal air temperature, measured by a radio-frequency or trailing thermocouple inside the mold cavity, should be held between 170 °C and 190 °C for wall sections of 5–8 mm. Oven air temperature setpoints of 250–300 °C are common on carousel-type machines, but terminal control should be based on internal air temperature rather than dwell time because the gray pigment modifies radiant heat absorption relative to unpigmented metallocene LLDPE. Regrind of the same lot may be dry-blended at up to 20 wt% without losing tensile yield, but only if the regrind is screened to the same particle size distribution and is free of cross-contamination from rotomolding mold release agents. Pesticide contact is evaluated by chemical resistance testing per ASTM D543-21 using the specific formulation at the intended service temperature; potable water-contact parts are subject to finished-part testing under NSF/ANSI 61 and the base polymer may be assessed under FDA 21 CFR 177.1520. Demolding before the mold skin reaches 60 °C increases flat-panel warpage on horizontal sprayer tanks; ejection above 75 °C causes corner deformation and should be avoided. The terminal part range includes horizontal cylindrical sprayer tanks, conical-bottom induction tanks, and stock watering troughs.

    What Limits Chemical Containment Sump Life Under Oxidizing Acid Fume Exposure?

    Secondary containment sumps and pump bases molded from Icorene 1761 GRY 7782 are evaluated first for environmental stress crack resistance, because the exposure pattern is intermittent chemical contact combined with sustained structural loading. ESCR should be measured on compression-molded plaques per ASTM D1693-15, Condition B, at 50 °C in 100% Igepal CO-630. Service life predictions from that value are valid only when the rotomolded wall has been sintered to full densification with no undercooked core; an undercooked core at the parting line retains microvoids that act as crack initiators. The application is incompatible with silicone-based external mold release agents: silicone transfer reduces post-mold weld-line strength and can compromise the leak detection channel introduced in double-wall sump bodies. Molds with PTFE-modified release surfaces or internally lubricated polymer grades are preferred. Chemical resistance for acid fume exposure should be confirmed by ASTM D543-21 immersion tests using the actual oxidizing solution at the upper service temperature; intermittent exposure to pH 2 through 12 is generally within the capability envelope, while continuous immersion in strong oxidizing acids above 40 °C should be rejected unless long-term testing shows less than 15% change in tensile elongation at break. The gray pigmentation may increase surface temperature during oven residence; cavity air probes should be used to terminate the cook when the inner wall reaches 185 °C, because thermal oxidation accelerates above 200 °C internal air and produces gas bubbles at the parting line. On carousel-type rotational molding machines, a double-wall sump with nominal wall thickness of 12 mm may require longer oven residence than unpigmented mLLDPE; published data for this specific gray-compounded configuration is limited, so each mold should be profiled with a minimum of three internally mounted thermocouples. Regrind from post-industrial scrap may be added at up to 15 wt% for non-load-bearing sump bases only, provided the scrap is clean and has not been exposed to cleaning solvents. EU importers must maintain technical documentation under REACH Regulation (EC) No 1907/2006 and verify that the supplied gray pigment package does not introduce substances of very high concern above the communicable threshold. Terminal parts include double-wall pump chambers with leak detection channels, acid neutralization basin liners, and secondary containment trays for chemical drums.

    ApplicationTest standardParameterRelevance to Icorene 1761 GRY 7782
    All rotomolded partsASTM D1238-20Melt flow rate at 190 °C/2.16 kgConfirms lot-to-lot flow consistency before charging
    All rotomolded partsASTM D1505-18 or ISO 1183-1:2019DensityVerifies metallocene LLDPE grade band and charge weight calculation
    Agricultural tanks, playground panelsASTM D638-14Tensile yield, elongation at breakBaseline mechanical property after rotomolding
    Chemical containment, automotive DEF reservoirsASTM D1693-15ESCR Condition B, 50 °CPrimary lifetime predictor for intermittent chemical exposure
    Marine buoys, utility vaultsISO 6603-2:2023Instrumented puncture impact at -20 °CLow-speed impact behavior in service
    Outdoor applicationsISO 4892-3:2016UV exposure with condensation cyclesWeathering and color retention of gray pigmented surfaces
    Chemical containment, agricultural tanksASTM D543-21Chemical resistance immersionSpecific fluid compatibility at service temperature
    Potable water-contact tanksNSF/ANSI 61, FDA 21 CFR 177.1520Extractables and olefin polymer complianceRegulatory basis for water-contact service
    Playground equipmentEN 1176-1:2017, ASTM F1487-23Structural integrity and impact performanceFinished-part certification for public use
    Underground utility enclosuresANSI/SCTE 77-2017Rating for below-grade enclosuresLoad rating and ingress protection

    In marine buoy assemblies, the combination of UV exposure, saltwater flexure, and low-temperature dock impact places a premium on the metallocene short-chain branching distribution of Icorene 1761 GRY 7782. The base powder should be dry-blended only with marine-grade UV stabilization packages; benzophenone-based UV absorbers at 0.1–0.3 phr and a hindered amine light stabilizer system at 0.05–0.15 phr are typical for a 10-year weathering target under ISO 4892-3:2016 fluorescent UV testing with 8 h UV at 60 °C and 4 h condensation at 50 °C. The foam-core buoy is produced by a double-shot procedure: the first charge forms a solid outer skin of 6 mm, and the second charge introduces a foamed polyethylene core. For the foam layer, azodicarbonamide at 0.3–0.8 wt% is used; its decomposition onset near 205 °C requires the peak internal air temperature during the second shot to be held above 190 °C so that the core density falls below 0.85 g/cm³. If the internal air drops below 190 °C, foaming is incomplete and the filled part remains above 0.85 g/cm³, losing buoyancy. Skin/core adhesion is tested on cut strips with a 90° peel jig at 50 mm/min; cohesive foam failure is required, and interfacial separation at less than 5 N/mm indicates insufficient sintered surface temperature during the transition from first to second shot. Moisture uptake in the blowing agent is a more common production failure than resin degradation; azodicarbonamide should be pre-dried at 80 °C for 4 h in a desiccant dryer when ambient relative humidity exceeds 60%. The terminal parts include channel markers, dock edge fenders, and floating net pen collars. Published data for this specific gray-compounded configuration in double-shot marine foam structures is limited; plant validation should include buoyancy retention after 1000 h salt spray exposure per ASTM B117-19 and low-temperature impact after -20 °C conditioning.

    ESCR Retention in Molded Automotive Diesel Exhaust Fluid Reservoirs After Post-Mold Annealing

    Selective catalytic reduction fluid reservoirs require dimensional stability, urea solution compatibility, and low-temperature impact performance from -40 °C to 80 °C. Icorene 1761 GRY 7782 is processed into twin-shell tanks by rotational molding with molded-in threaded inserts. Insert temperature should be preheated to 120 °C before powder charging to avoid localized cooling defects around bosses. The urea solution specification is defined by ISO 22241-1:2019 as a 32.5 wt% aqueous urea solution; compatibility of the reservoir material should be evaluated by immersion of 3 mm rotomolded plaques in the candidate fluid at 60 °C for 1000 h, followed by tensile property retention per ASTM D638-14 and ESCR per ASTM D1693-15. Burst pressure and vibration testing follow vehicle manufacturer specifications; published international standards do not define a single pass criterion for this specific configuration, so the molder must validate to the end-user test plan. Regrind use should not exceed 15 wt% in DEF reservoirs, and the regrind must be free of engine oil, coolant, or mold release residues because these contaminants act as stress crack promoters. Post-mold annealing at 80 °C for 2 h may be required to stabilize insert threads and reduce residual stresses; annealing above 100 °C can soften unsupported flat surfaces and is not recommended. Terminal parts include DEF reservoirs for heavy trucks, off-road agricultural tractors, and stationary generator sets. RoHS obligations under Directive 2011/65/EU as amended by (EU) 2015/863 are not typically triggered for the polymer body itself, but electrical level senders and wiring integration must be assessed separately.

    Outdoor play structures and site furniture fabricated from Icorene 1761 GRY 7782 rely on the gray pigmentation to provide visual density while retaining the impact performance required by EN 1176-1:2017 and ASTM F1487-23. The powder should be dry-blended with a hindered amine light stabilizer concentrate at 2 wt% when the molder is certifying parts for a 10-year high-UV service interval; laboratory UV exposures should follow ISO 4892-3:2016 with color change measured by CIE L*a*b* difference and tensile property retention per ASTM D638-14. Wall thickness for rotomolded play panels should be maintained between 4 mm and 8 mm, with internal reinforcing ribs designed at 2× nominal wall to resist bending moments. The mold charging weight is calculated from the part surface area at approximately 2.5 kg/m² for a 5 mm nominal wall when powder bulk density is 0.45 g/cm³; incorrect charge weight produces either thin corners or gas entrapment at rib roots. Impact resistance is tested per ASTM F1487-23 and EN 1176-1:2017; flammability may be evaluated under ASTM E84-23a if site furniture is specified for indoor use. Sliding contact surfaces should not be flame-polished because the surface oxidation layer reduces mar resistance and can create microcracks under repeated bending. Post-mold adhesive bonding of pads or handles should be pre-tested for compatibility with the pigment package; high-solvent adhesives may plasticize the surface and reduce ESCR, especially near flat-panel edges. Terminal parts include play tunnel panels, spring rider seats, and site furniture bench shells.

    When Underground Utility Vaults Require Low-Temperature Ductility Below -30 °C

    Underground enclosures for electrical splice boxes and telecommunications vaults are single-piece rotomolded structures that must resist soil pressure, occasional vehicle load transfer, and brittle fracture at sub-freezing earth temperatures. The metallocene LLDPE powder is formed into boxes with wall sections from 6 mm to 12 mm; tooling is designed with 3° draft angles and corner radii not less than 6 mm to reduce notch sensitivity. Low-temperature notched impact resistance on specimens cut from molded parts is evaluated according to ASTM D256-23 at -30 °C; the grade retains ductile behavior when the specimen thickness is below 10 mm. Above that thickness, cooling rate gradients reduce spherulitic uniformity, and published data for this specific gray-compounded configuration is limited; instrumented full-thickness impact testing should be conducted on the box wall rather than on thin laboratory plaques. Soil chemical exposure is generally limited to pH 4 through 9; aggressive industrial soil conditions require chemical resistance screening per ASTM D543-21 before installation. A mineral-filled masterbatch may be dry-blended at 5 wt% to increase cover modulus for load-bearing applications; addition above 8 wt% reduces ESCR below acceptable values and should be rejected for vaults that may sit in wet soil. The enclosure rating follows ANSI/SCTE 77-2017 for below-grade enclosures, and ingress protection is verified separately. Terminal parts include transformer vaults, telecommunications splice boxes, and water meter pits. The gray pigmentation has the added function of reducing visible surface temperature differences in above-ground portions, but the primary engineering criterion remains low-temperature ductility at the bottom wall where frost loading is highest.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7782 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 GRY 7782 is a grey-pigmented linear low-density polyethylene produced with metallocene single-site catalyst technology. The numeric designation 1761 identifies the ethylene/α-olefin copolymer base grade, while the suffix GRY 7782 is consistent with a controlled grey colour formulation incorporated during melt compounding. The pigmented compound contains dispersed inorganic and organic colorants that function as additional heterogeneous nucleation phases and alter heat absorption relative to the natural base resin. Grade-specific specification values must therefore be obtained from the LyondellBasell certificate of analysis and safety data sheet; generic metallocene LLDPE family data are not a substitute for lot-level release limits. Published data for this specific grey configuration is limited, and side-by-side qualification on production equipment is required before substitution.

    Metallocene single-site catalysis produces a linear low-density polyethylene with a narrow molecular weight distribution and a more uniform short-chain branch distribution than conventional multi-site Ziegler-Natta LLDPE. Polydispersity indices in the range 2.0–3.0, measured by gel permeation chromatography according to ISO 16014-4, are typical for metallocene LLDPE, whereas Ziegler-Natta LLDPE grades commonly fall between 3.5 and 5.0. The reduced population of low-molecular-weight, highly branched chains lowers extractable content and improves low-temperature toughness. Environmental stress crack resistance measured by ASTM D1693 Condition B often exceeds 500 h for well-processed metallocene LLDPE parts. The molecular regularity also produces more consistent shrinkage and densification in thick walls, but it reduces melt strength and shear thinning compared with a Ziegler-Natta LLDPE of equivalent melt index.

    When Metallocene Catalysis Narrows the Molecular Weight Distribution

    A narrowed molecular weight distribution changes the shear-thinning response of the melt. Capillary rheometry according to ISO 11443 at 190 °C and apparent shear rates from 100 s−1 to 1000 s−1 is recommended before process scale-up because the metallocene grade may exhibit higher viscosity at high shear rates than a conventional LLDPE of identical melt mass-flow rate. The lower melt strength also narrows the processing window in operations that require high melt extensibility, such as high blow-up-ratio blown film or thick-sheet sag. These limitations are inherent to the metallocene LLDPE architecture and are not specific defects of the GRY 7782 colour package.

    In solid-state behaviour, the homogeneous comonomer distribution improves the balance between stiffness and impact toughness. Tensile properties evaluated according to ISO 527-2 and flexural modulus evaluated according to ISO 178 can be maintained without sacrificing low-temperature impact resistance measured by ISO 179-1/1eA. The low brittle point, often below −60 °C by ASTM D746, supports use in outdoor containers exposed to sub-zero conditions. The grey pigment masks optical clarity, but the underlying mechanical benefits of metallocene catalysis remain measurable as reduced notch sensitivity and improved resistance to slow crack growth under stress-cracking agents.

    On a Carousel-type rotational moulding machine with arm radii above 2.5 m, oven temperatures in the range 280–320 °C are typically required to achieve peak internal air temperatures of 190–210 °C in wall sections of 4–6 mm. Failure to reach this internal air temperature produces incomplete particle coalescence and can reduce Charpy impact strength by more than 30%. Exceeding 230 °C internal air temperature can initiate oxidative embrittlement and colour shift in the grey compound. Field observations on dual-axis machines indicate that batch-to-batch powder bulk-density variation of ±3% can alter wall thickness distribution unless charge weight is adjusted for each container.

    Because grey pigmentation absorbs radiant energy faster than natural resin, the first-pass oven residence time must be re-established when changing from natural to GRY 7782 feedstock. The pigment particles also act as nucleation agents and can increase crystallization rate, reduce warpage, and shift shrinkage behaviour. Differential scanning calorimetry according to ISO 11357-3 should be used to compare crystallization exotherms between natural and pigmented material. Surface defects associated with moisture must be controlled because condensed moisture on pellet surfaces above 0.05 wt%, measured by ISO 15512 Method B, can generate voids or surface pitting in rotomoulded skins.

    What Distinguishes the Icorene 1761 GRY 7782 Compound from Conventional LLDPE and LDPE?

    Compared with a Ziegler-Natta LLDPE of equal density and melt flow rate, the metallocene grade offers higher environmental stress crack resistance, lower low-temperature brittleness, and a more uniform wall section with less warpage. Impact strength measured by ISO 179-1/1eA can be retained at lower wall thicknesses. The trade-off is a narrower processing window in shear-dominated operations and lower melt strength. Against LDPE, the linear structure lacks the long-chain branching that provides high strain hardening and melt extensibility. The Icorene grade is therefore not a direct replacement for LDPE in foaming, high-stretch film, or applications where bubble stability at high blow-up ratios is the controlling variable.

    Against natural or white compounds of the same base resin, the GRY 7782 formulation has different heat absorption and may require a lower oven setpoint or shorter cycle to avoid overheating. The grey pigment also influences visual defect detection; pinholes and gas bubbles are less visible on grey surfaces than on light-coloured parts, so non-destructive inspection should include a pressure decay test or internal surface examination. Against high-density polyethylene, the lower density and crystallinity of the metallocene LLDPE improve impact toughness and ESCR but reduce flexural modulus and continuous load-bearing capacity at elevated temperature.

    Thermal and Mechanical Property Envelope Under ASTM/ISO Protocols

    When lot-specific release data are unavailable, the following table presents the general metallocene LLDPE family envelope for preliminary feasibility calculations only. It does not replace the certificate of analysis for Icorene 1761 GRY 7782, and the pigmented compound may fall outside one or more listed ranges.

    PropertyTest methodTypical mLLDPE family envelope
    Melt mass-flow rateISO 1133-10.5–6.0 g/10 min at 190 °C/2.16 kg
    DensityISO 1183-10.912–0.940 g/cm³
    Tensile yield stressISO 527-210–25 MPa
    Nominal tensile strain at breakISO 527-2400–800%
    Flexural modulusISO 178200–700 MPa
    Vicat softening temperatureISO 306/A5090–120 °C
    Brittleness temperatureASTM D746< −60 °C
    Environmental stress crack resistanceASTM D1693 Condition B> 500 h

    In outdoor storage tanks, agricultural chemical containers, material handling bins, and industrial cladding where grey colour is specified for UV screening and low visibility of surface soiling, the combination of low-temperature impact resistance and ESCR is the principal selection criterion. The final part must be qualified by production trials because the pigmented grade can differ from natural resin in warpage direction, shrinkage rate, and tensile creep. Creep modulus should be evaluated according to ISO 899-2 when the component is loaded vertically or subjected to continuous hydrostatic pressure. Long-term heat ageing should be assessed by ISO 188 before the compound is used in applications exceeding 60 °C continuous service.

    Regulatory status must be confirmed against the extended safety data sheet. REACH Regulation (EC) No 1907/2006 applies to European Union supply, and article 33 communication is required when a substance of very high concern exceeds 0.1 wt%. The grey compound is an industrial colour grade; food-contact status under EU Regulation 10/2011 or FDA 21 CFR 177.1520 must be explicitly verified for the specific pigment package because coloured formulations may require additional migration testing. RoHS Directive 2011/65/EU Annex II restrictions apply only if the moulded article enters electrical and electronic equipment; the base polyolefin is not exempt by product designation alone. The selection of Icorene 1761 GRY 7782 should therefore be documented through a material qualification record that includes the certificate of analysis, processing trial settings, and part-level mechanical test data.