| HS Code | 586102 |
| Density | 0.917 g/cm³ |
| Melt Flow Rate | 1.0 g/10 min |
| Tensile Strength At Yield | 1.00 ksi |
| Tensile Strength At Break | 5.00 ksi |
| Elongation At Break | 500% |
| Flexural Modulus | 30.0 ksi |
| Vicat Softening Point | 95.0 °C |
| Melting Point | 116 °C |
| Haze | 10% |
| Gloss | 80% |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength | 300 g |
| Coefficient Of Friction | 0.20 |
| Color | Grey |
As an accredited LyondellBasell Icorene 1761 GRY 7774 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 GRY 7774 is packaged in 25 kg multiwall bags, 40 bags per shrink-wrapped pallet (1,000 kg total). |
| Container Loading (20′ FCL) | 20′ FCL loaded with palletized bags of LyondellBasell Icorene 1761 GRY 7774 metallocene linear low-density polyethylene, secured for ocean transport. |
| Shipping | Non-hazardous metallocene linear low-density polyethylene resin pellets, shipped in moisture-resistant bags, octabins, or bulk trucks/railcars. Not DOT/IMDG/IATA regulated. Keep dry, clean, away from heat, sunlight, and contamination. Store at ambient temperature; follow SDS and local transport rules. Handle with normal industrial hygiene. |
| Storage | Store LyondellBasell Icorene 1761 GRY 7774 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep in original, sealed packaging on pallets to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and UV exposure. Protect bags from puncturing and physical damage. Use first-in, first-out stock rotation and maintain good housekeeping; no smoking. |
| Shelf Life | Typically 24 months when stored unopened in a cool, dry, ventilated area, protected from direct sunlight, heat, and moisture. |
LyondellBasell Icorene 1761 GRY 7774 is processed as a free-flowing powder in closed-chamber biaxial rotational moulding machines. The metallocene-catalysed polyethylene has a narrower short-chain branching distribution than conventionally catalysed linear low density polyethylene, which reduces the temperature interval between particle coalescence and oxidative degradation. During the heating phase, powder particles pass through agglomeration, densification, spread and consolidation. The primary control variable in production is not oven air temperature alone but the internal air temperature measured with a through-bolt Type K thermocouple inserted into the mould cavity. For metallocene LLDPE rotomoulding powders in the density class 0.938 g/cm³ to 0.942 g/cm³ measured to ISO 1183-1:2019, full densification generally begins between 150 °C and 170 °C. Peak internal air temperature is typically held between 195 °C and 210 °C until the inner wall surface loses all residual powder print and a pinhole-free skin forms around inserts and port shut-offs.
Oven air temperature setpoints of 280 °C to 300 °C are common for monolayer vertical storage tanks on carousel machines with direct gas-fired burners and closed-chamber recirculation. At peak internal air temperatures below 185 °C, fine powder around tooling bosses, threads and inserts may not fully melt, leaving through-thickness voids that appear as pinholes after cooling. At peak internal air temperatures above 215 °C, the outer skin in contact with the hot mould wall can oxidize and harden, lowering elongation at break and initiating weld-line cracks under hydrostatic loading. Cycle-to-cycle variation of internal air temperature greater than ±5 K is a known cause of increased scrap in multi-cavity water tank tools because wall thickness and impact ductility are both sensitive to peak internal air temperature. Ovens without even burner output or without internal air temperature logging therefore represent a practical processing bottleneck.
| Control variable | Typical monolayer setpoint | Observed field failure outside window |
|---|---|---|
| Oven air temperature | 280 °C to 300 °C | Below 260 °C: incomplete densification; above 310 °C: surface oxidation and embrittlement |
| Peak internal air temperature | 195 °C to 210 °C | Below 185 °C: pinholes at inserts; above 215 °C: brittle outer skin and weld-line fracture |
| Forced-air cooling rate | 8 K/min to 15 K/min | Water quench: warpage and high residual stress; below 4 K/min: long cycle time and coarse spherulitic structure |
| Demould temperature | 70 °C to 80 °C | Below 65 °C: difficult release; above 85 °C: sag under self-weight on large flat panels |
| Powder moisture content | Below 0.03% by mass to ISO 15512:2019 | Higher moisture in humid shops: surface voids and internal porosity during densification |
Compliance for potable water contact requires positive confirmation of extraction performance under NSF/ANSI 61 or AS/NZS 4020 on the finished rotomoulded article, not merely on the raw resin. If the grade is supplied with food-contact certification, the olefin polymer requirements under FDA 21 CFR 177.1520 may be applicable subject to end-use temperature and food type conditions. For chemical storage tanks, the material is generally resistant to aqueous acids, alkalis and salt solutions but is not recommended for continuous contact with chlorinated solvents, aromatic hydrocarbons or strong oxidizing acids at elevated temperature. The tank manufacturer must prove service compatibility through ISO 16101:2004 or an equivalent chemical resistance assessment. Terminal components produced from this grade include vertical bulk storage tanks, secondary containment sumps, sprayer platform tanks and acid-neutralization vessels with wall thicknesses normally between 5 mm and 12 mm.
Agricultural sprayer tanks and induction hoppers are rotationally moulded from Icorene 1761 GRY 7774 where low-temperature impact resistance is as important as hydrostatic creep resistance. The sprayer tank itself operates under nominal pump pressures from 0.3 MPa to 0.5 MPa, but surge loads and hydraulic agitation produce cyclic side-wall flexure that can expose small weld-line defects. The metallocene matrix distributes short-chain branches more evenly than heterogeneously branched LLDPE, which increases tensile impact at equal density and enhances ductility at sub-zero temperatures. Low-temperature impact testing under ISO 8256 or ISO 179-1:2023 at -20 °C is therefore used by some rotational moulders as an incoming powder screening method. Finished tanks should additionally be conditioned for 24 h at -20 °C and subjected to a full-volume drop test from 1.2 m onto a concrete slab; ductile yielding without crack propagation is the acceptance criterion because rotational mould parting lines control practical failure behaviour.
Wall thickness in the bottom dome is normally increased by 20% to 40% relative to side walls to reduce creep under hydrostatic load. The tool rotates at a primary-to-secondary speed ratio near 4:1 for cylindrical tanks, with secondary axis motion adjusted to prevent powder accumulation in the dome. Polyethylene welding rod used for baffle, flange and outlet fitting assembly must be produced from the same grade family; mismatched melt index in the welding rod can create visible seams with reduced elongation after hot-plate welding. Under European agricultural chemical handling requirements, the final tank must be assessed under the REACH Regulation, but the article itself does not carry a CLP classification if no hazardous substance is intentionally released above threshold limit values during use. Terminal components include self-supporting sprayer tanks, rinsing tanks, foam marker reservoirs and induction hoppers mounted to agricultural equipment.
Rotomoulded kayak hulls and dock floats made from LyondellBasell Icorene 1761 GRY 7774 expose the polymer to continuous water immersion, ultraviolet radiation and mechanical abrasion from sand and gravel. The grey pigmentation in GRY 7774 is not decorative alone; it functions as a UV barrier by absorbing and scattering incident radiation within the outermost 0.1 mm to 0.2 mm of the shell. Outdoor exposure testing under ISO 4892-2:2013 or ASTM G155-13 is recommended to predict colour retention and surface chalking. A metallocene LLDPE of nominal density 0.940 g/cm³ generally retains more tensile elongation after 1,000 h xenon-arc exposure than higher-density polyethylene because lower crystallinity reduces the formation of brittle surface microcracks. Published data for the specific grey-pigmented GRY 7774 variant in marine duty are limited; therefore end-use qualification on a production-intent hull is required before long-term outdoor warranty commitments are made.
The clamshell mould for kayaks requires a multi-axis machine with internal air temperature probes on both tool halves. Uneven heating between upper and lower shell faces causes differential shrinkage; a maximum inter-shell temperature difference of 8 K at peak cycle is commonly tolerated before warpage becomes visible on the keel line. Cooling is usually performed with forced air rather than water mist to avoid high thermal gradients through the hull wall. Demoulding at 70 °C to 80 °C reduces in-mould recovery stress and dimensional error. Hull thickness for recreational kayaks is designed between 3 mm and 5 mm; below 3 mm, the part is prone to sand abrasion and point-impact puncture. The finished product may require an additional UV-stabilized topcoat or in-mould graphics, but the grey base tint reduces the thickness of any decorative coating required for opacity. Terminal parts include kayak hulls, dock floats, fish boxes, storage locks and deck plate covers.
When the same rotomoulding powder is used for playground slide hoods, tunnel shells and swing seat panels, the critical engineering concerns shift toward impact ductility after outdoor weathering and pigment migration limits under child-contact safety regulations. The grey compound must be assessed for heavy-metal release under EN 71-3:2019+A1:2021 if the assembled structure falls under toy safety legislation. It is the pigment concentrate in the final compound, not the base resin alone, that must satisfy migration limits; a certificate of analysis for natural polymer is not sufficient for a finished playground component. The producer should also confirm compliance with EU 10/2011 overall migration and specific migration limits where mouth contact is a foreseeable but unintended use. Since the grade is supplied pre-compounded in grey, quality control should retain a reference sample from each production lot to track colour drift under site-specific UV exposure.
Playground parts are frequently installed as twin-wall or ribbed panels to increase section modulus without increasing wall thickness. Rotationally moulded ribs can act as unintentional shrink concentrators if the mould radius is too sharp. A rib root radius of at least 1.5 times the nominal wall thickness is used to prevent sink marks and stress concentration during cooling. The low shear surface finish of mLLDPE allows textured in-mould skins to reproduce fine graining, but textured surfaces also create micro-notches that can lower impact performance. Under ASTM D1693 condition C, metallocene rotomoulding grades of this density class commonly show no crack propagation beyond 1,000 h; however, this laboratory test in nonylphenoxy poly(ethyleneoxy) ethanol at 50 °C does not fully reproduce cyclic playground loading. Production-scale qualification should therefore include an instrumented drop weight test on a complete part at 0 °C to confirm part integration before series release. Terminal products include slide hoods, roof caps, climbing tunnel segments, swing frames and access panels.
| Standard or method | Application condition | Terminal relevance |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer food contact | Food contact bins only if lot-specific certification is available |
| EU 10/2011 | Overall migration and specific migration limits | Child-contact playground panels and food-like mouth contact |
| EN 71-3:2019+A1:2021 | Migration of heavy elements | Toy-like playground components |
| NSF/ANSI 61 | Drinking water system components | Potable water tanks only if certified on finished article |
| REACH Regulation (EC) No 1907/2006 | SVHC content below 0.1% w/w per article | All industrial goods shipped into the EU |
| RoHS Directive 2011/65/EU | Cadmium, lead, mercury, chromium VI, PBB and PBDE limits | Grey pigmented consumer articles and electronic enclosure accessories |
| ISO 4892-2:2013 | Xenon arc weathering | Outdoor tanks, marine hulls and playground structures |
Double-wall rotational moulding of insulated tanks and portable sanitation units introduces a two-layer structure: an outer skin of Icorene 1761 GRY 7774 and a foamed polyethylene core or inner layer. The dry blending route involves mixing the mLLDPE powder with a foamable polyethylene powder in a low-shear tumble blender before charging the mould. Addition levels depend on target foam density and wall thickness; foam concentrate loadings commonly start at 3 wt% and rarely exceed 8 wt% because higher loadings create gas pockets that collapse at the skin interface during the early heating phase. Blending time must be sufficient to achieve a coefficient of variation below 5% in the concentration of blowing agent across the shot; extended high-shear mixing should be avoided to prevent fines segregation and premature gas evolution.
Temperature offsets are required because the decomposition exotherm of the blowing agent adds heat inside the mould cavity while the outer wall is still densifying. In comparison with monolayer processing, production-scale ovens have successfully used oven air temperatures 10 K to 15 K lower for the first heating ramp. Peak internal air temperature is normally held at 190 °C to 200 °C, and the cooling rate is reduced to allow gas expansion to be frozen into a closed-cell structure. Rapid water-mist cooling of a foamed mLLDPE outer wall can cause surface dimpling and skin delamination because the solid skin contracts faster than the still-soft foam core. Demoulding below 60 °C is advised for foamed tanks with wall thickness above 20 mm. Equipment with precise temperature ramp control is therefore a hard requirement; simple timer-controlled ovens without programmable ramps show higher delamination rates in this double-wall process. Terminal parts include insulated chemical storage tanks, temperature-sensitive process water tanks, portable sanitation units and cold-chain transport boxes.
Machine guards and conveyor covers fabricated from Icorene 1761 GRY 7774 exploit the grade’s high elongation and low-temperature flexibility, not flexural modulus. Industrial guards are usually rotationally moulded as large, shallow shells with cut-outs, hinge bosses and snap-fit retention features. Since polyethylene has a low flexural modulus relative to engineering thermoplastics, the part design must use ribbing and curved profiles to achieve sufficient stiffness. A nominal wall thickness of 4 mm to 6 mm is common for guarding; unsupported flat spans exceeding 800 mm often require reinforcing ribs or metal stiffeners. The grey compound provides a neutral panel colour that hides dust and coolant staining, but anti-static performance is not inherent. If the guard is installed in an explosive dust atmosphere, the part must be modified with conductive additives or coated with a certified static-dissipative layer because standard mLLDPE has surface resistivity typically above 1014 Ω under IEC 62631-3-2.
Machining and assembly of rotomoulded guards require the fabricator to account for post-mould shrinkage. A linear mould shrinkage allowance of 2.0% to 2.5% is applied for this product class; the exact value is influenced by mould temperature, cooling rate and part geometry. Holes are drilled or milled after moulding rather than formed by through-thread shut-offs. Threaded brass inserts are installed with ultrasonic or thermal insertion equipment. The heat-affected zone around an ultrasonically installed insert can exhibit stress whitening if the insert vibration amplitude is too high; this is an operational boundary rather than a resin defect. Terminal parts include chain guards, belt covers, hopper lids, spill trays and material transfer chutes.
Competitive LyondellBasell Icorene 1761 GRY 7774 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Within the LyondellBasell rotational moulding portfolio, the grade designation Icorene 1761 GRY 7774 identifies a metallocene-catalysed linear low-density polyethylene supplied as a pigmented powder. The base resin Icorene 1761 is polymerised using a metallocene catalyst system; the suffix GRY 7774 denotes a grey colour package. The material is classified as a linear low-density polyethylene because its density of 0.917 g/cm³ under ISO 1183-1 is below the conventional HDPE threshold of 0.940 g/cm³. Melt flow rate is 6.0 g/10 min at 190 °C with a 2.16 kg load when measured according to ISO 1133-1 or ASTM D1238. The powder is intended for rotational moulding of hollow parts, where uniform wall thickness, low-temperature impact resistance, and environmental stress crack resistance are required.
The metallocene catalyst system produces a narrow molecular weight distribution and a narrow short-chain branching distribution. This architecture is significant for rotational moulding because the resin melts over a narrower temperature interval and solidifies with a sharper freezing front than conventional Ziegler-Natta LLDPE. The consequence in processing is a reduction in the time needed to remove residual gas bubbles after the powder has densified, provided the peak internal air temperature is reached. Representative mechanical data from the public datasheet include tensile modulus of 500 MPa under ISO 527-2, tensile stress at yield of 11 MPa, tensile strain at break of 800%, Shore D hardness of 54 under ISO 868, Vicat softening temperature of 100–105 °C under ISO 306 A/50, and environmental stress crack resistance above 1000 h under ASTM D1693 conditions. These values are typical, not lot-specific specification limits.
Control of the rotational moulding cycle begins with the oven air temperature and the internal air temperature of the part. For a 0.917 g/cm³ metallocene LLDPE powder, the oven air temperature is typically set in the range 260–320 °C, and the peak internal air temperature is generally maintained between 180 °C and 200 °C. If the peak internal air temperature is too low, residual particles remain at the inner surface and pinholes form. If it is too high, oxidative degradation accelerates, and yellowing or loss of impact strength may occur. The biaxial rotation ratio is commonly adjusted between 4:1 and 8:1, although actual machine settings are selected based on part wall-thickness distribution measured by ultrasonic gauging.
Particle size distribution is a further control variable. Rotational moulding powders are typically screened to below 500 µm with a median particle size in the 150–250 µm range. Coarse fractions increase the risk of uneven wall thickness; fines increase dust and can produce local overdensity. Bulk density for this class of metallocene LLDPE powder is often reported between 0.45 g/cm³ and 0.50 g/cm³. Storage above 60% relative humidity can increase moisture uptake. Pre-drying at 70–80 °C for 2–4 h is required before charging if free moisture is suspected, because moisture evolves as steam during the oven cycle and contributes to internal bubble formation.
Cooling rate influences warpage and crystallinity. The mould is cooled by forced air or a water mist after demoulding begins. A rapid cooling rate reduces cycle time but can increase residual stress and warpage, particularly in parts with abrupt wall-thickness transitions. Demoulding is generally performed when the part surface temperature has fallen below 60–70 °C to limit post-mould deformation. Aluminium moulds with wall thicknesses of 6–10 mm are common because aluminium provides the high heat-transfer rate needed to fuse the powder and then remove heat during cooling. Steel moulds can be used, but their lower thermal conductivity lengthens the heating and cooling stages.
Compared with a conventional Ziegler-Natta LLDPE of equivalent density and melt flow rate, Icorene 1761 GRY 7774 exhibits a narrower melting endotherm and a more uniform intermolecular comonomer distribution. The metallocene architecture reduces the concentration of highly branched or low-molecular-weight fractions that can act as failure initiation sites. Under ASTM D1693 environmental stress crack resistance testing, the grade exceeds 1000 h; conventional Ziegler-Natta LLDPE rotational moulding grades may fall below this value depending on comonomer type and molecular weight. Low-temperature notched impact performance is similarly improved. HDPE rotational moulding powders with densities above 0.940 g/cm³ provide higher tensile modulus and heat deflection temperature but lower stress crack resistance and low-temperature impact. The density of 0.917 g/cm³ therefore positions the product in applications where toughness and environmental stress crack resistance dominate over stiffness.
Compared with high-pressure LDPE rotational moulding grades, Icorene 1761 GRY 7774 contains less long-chain branching, which reduces melt sag and allows thinner wall sections to be held during the high-temperature phase. The melting point is higher than typical LDPE, which improves upper service temperature but requires higher internal air temperatures for complete densification. Compared with EVA-modified or plastomer-modified rotational moulding grades, the metallocene LLDPE may exhibit lower low-temperature impact than an EVA-modified blend but offers better chemical resistance and lower surface tack. The exact balance must be confirmed against the intended fluid, temperature, and stress state because comparative data are grade-dependent.
Applications for the grey grade include agricultural and industrial storage tanks, vehicle fluid containers, equipment housings, and outdoor enclosures manufactured by biaxial rotational moulding. The grey colour package provides a uniform appearance and can reduce the need for post-mould painting. However, the pigment package lowers the surface gloss and may reduce the elongation at break by a few percentage points relative to the unpigmented base resin. The exact shift should be obtained from lot certificates because pigment concentration and batch-to-batch variation are not captured in generic datasheet values.
In exterior service, the weatherability of a grey rotationally moulded part is controlled by the stabiliser package and the pigment concentration. Grey pigments based on carbon black or inorganic colourants may reduce ultraviolet penetration and protect the underlying polymer. The base LLDPE is still susceptible to chain scission unless sufficient ultraviolet stabiliser is present. Long-term property retention should be evaluated using ISO 4892-2 or ASTM D2565 accelerated weathering and validated by field data. Published data for this exact commercial colour code is limited, so the manufacturer or compounder should confirm ultraviolet stabiliser content before exterior specification, because the generic grade designation does not inherently guarantee a specific weathering performance.
Chemical-contact service conditions require separate validation. The metallocene LLDPE base resin typically resists aqueous acids, alkalis, and polar solvents at ambient temperature, but strong oxidisers, chlorinated solvents, and low-molecular-weight hydrocarbons may cause swelling or stress cracking. No single ESCR value can cover all chemical environments; testing under ASTM D1693 with 100% Igepal is a comparative indicator only. For chemical tank applications, the part should be tested under the intended fluid, temperature, and stress. The use of external gaseous or liquid media at temperatures above 40–50 °C can accelerate stress crack initiation even when short-term tensile properties remain unchanged.
Regulatory assessment of Icorene 1761 GRY 7774 requires review of the base resin and the pigment package. The base polyolefin may be evaluated under food-contact provisions such as FDA 21 CFR 177.1520, but the grey pigment package may require separate suitability documentation. The product is supplied for industrial use; no blanket food-contact, medical, or potable-water approval should be assumed. REACH Regulation EC No 1907/2006 and CLP Classification, Labelling and Packaging EC No 1272/2008 obligations apply to the supplier and downstream users. For electrical and electronic applications, RoHS Directive 2011/65/EU compliance should be confirmed with the supplier, because the exact grey pigment chemistry determines the heavy-metal profile.
Operational boundaries include dry storage below 60% relative humidity, sieving after prolonged storage, and avoidance of blending with additives that generate acidic species at rotomoulding oven temperatures. The grade should not be dry-blended with heavily acidic flame retardants or with reclaimed powders of unknown melt flow rate without rheological verification, because small changes in melt flow rate and particle size distribution alter the wall-thickness profile in complex tooling. Each incoming lot should be verified for density, melt flow rate, bulk density, and particle size distribution before production release.