| HS Code | 326232 |
| Density | 0.917 g/cm³ |
| Melt Flow Rate | 1.6 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 10.0 MPa |
| Tensile Strength At Break | 24.0 MPa |
| Elongation At Break | 800% |
| Tensile Modulus | 193 MPa |
| Dart Drop Impact | 110 g |
| Elmendorf Tear Strength | 250 g |
| Haze | 4.0% |
| Gloss | 85% |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 1761 GRY 7770 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaging: typically supplied in 25 kg polyethylene-lined bags on pallets; LyondellBasell Icorene 1761 GRY 7770 metallocene linear low-density polyethylene resin. |
| Container Loading (20′ FCL) | 20′ FCL: 20 MT LyondellBasell Icorene 1761 GRY 7770 metallocene LLDPE, packed in 25 kg bags, securely palletized and stowed. |
| Shipping | Shipping description: LyondellBasell Icorene 1761 GRY 7770 Polyethylene, Linear Low Density, Metallocene, solid resin pellets. Typically non-hazardous, not regulated for transport. Pack in moisture-barrier bags or octabins. Store dry at ambient temperature, away from heat, ignition, moisture, and contaminants. Prevent pellet loss; ship by standard freight. |
| Storage | Store in a cool, dry, well-ventilated area away from heat, ignition sources, direct sunlight, and strong oxidizers. Keep original containers closed, palletized, and off the floor to prevent moisture pickup and contamination. Avoid excessive stacking, dust generation, and static discharge. Use appropriate grounding/bonding during handling. Maintain stable ambient temperatures, and follow the supplier’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original unopened packaging in a cool, dry area. |
For rotationally moulded agricultural water storage and liquid fertilizer tanks, Icorene 1761 GRY 7770 is processed as a dry-flowing rotomoulding powder with particle size distribution controlled for even wall thickness in closed moulds. The primary service requirement is not monotonic short-term tensile strength but long-cycle environmental stress-crack resistance under continuous hoop stress, particularly in tanks that remain filled next to livestock yards or irrigation ponds. On production-scale shuttle-type rotomoulding machines, oven set points between 260 °C and 320 °C are applied while internal air temperature is monitored as the controlling variable. A peak internal air temperature below 190 °C in thick-section bosses and spigots produces a poorly coalesced weld line at the mould parting line, leading to crack initiation when tank walls are exposed to sustained stress. Internal air temperatures above 230 °C may accelerate stabilizer consumption during the long oven dwell. Because metallocene LLDPE has a narrower short-chain branching distribution than conventional Ziegler-Natta C4-LLDPE at similar density, stress-crack resistance measured according to ASTM D1693 using 10% Igepal CO-630 at 50 °C is typically higher; resin datasheet values, however, are not article-level warranties. Finished tanks intended for potable water service require certification as complete articles under NSF/ANSI/CAN 61, and the resin alone does not confer that approval. Fertilizer and agrochemical tanks require additional compatibility testing per ISO 175:2020 with the actual field mixture, because high-ionic-strength solutions, surfactants, and trace metal salts can reduce stress-crack resistance relative to clean water. For outdoor field exposure, a UV/HALS masterbatch is dry-blended at 2–4 wt% depending on wall thickness and intended service life; higher loadings can reduce powder dry-flow and cause static bridging in the hopper. The dominant processing bottleneck is uneven cooling: forced-air cooling on the outside of the mould while the inner surface remains molten introduces residual stress near moulded ribs and spigots. Programmed air cooling with staged mould rotation reduces warpage but increases cycle time. The terminal articles are typically 500–20,000 L vertical or horizontal tanks with wall thickness from 4 mm to 12 mm, moulded-in tie-down lugs, and UV-stabilised outer surfaces for open-field exposure.
For chemical containment basins, secondary spill pallets, and vertical storage tanks handling mild acids, alkalis, and mixed industrial fluids, the relation between metallocene LLDPE molecular architecture and stress-crack resistance is both an advantage and a limitation. Icorene 1761 GRY 7770 can be used for double-wall containment structures where the outer shell functions as a secondary barrier. The outer wall is rotationally moulded with a wall thickness of 5–8 mm, while the inner tank is either moulded separately or integrally with ribs. The pigment package in the GRY 7770 designation changes radiant heat absorption under infrared oven heating, so internal air temperature, rather than oven set point, remains the process control reference. While ASTM D1693 with 10% Igepal CO-630 at 50 °C provides a relative ranking of stress-crack resistance, chemical storage tanks should be tested under ISO 175:2020 with the actual chemical formulation and service temperature. Aromatic solvents, concentrated surfactants, and oxidising solutions interact with polyethylene in ways that the standard wetting agent does not fully replicate. Secondary containment basins in hazardous waste accumulation areas must meet the volume and compatibility requirements of US EPA 40 CFR 264.175, while composite IBCs assembled with steel cages are tested under UN 31A/Y as complete transport packages. Article-level drop, stacking, and hydraulic pressure tests are required even if the resin datasheet reports suitable ESCR and density. The typical failure mode on production lines is not gross wall rupture but slow crack growth from the inside corner of the containment basin where rotational cooling creates a high-crystallinity boundary layer. To reduce this risk, rotomoulders use thicker corner radii, internal air temperature targets close to 200–210 °C, and controlled cooling through the crystalline solidification range. The grey compound is processed without additional filler; if an external UV masterbatch is added for outdoor basins, let-down above 3 wt% can shift internal air temperature readings because pigments change infrared absorption. The terminal articles include 110% secondary containment basins, pump pads, and cylindrical double-wall storage tanks for non-flammable process fluids.
Where below-grade telecommunications vaults and electrical junction boxes are rotationally moulded, the component is expected to survive decades of soil compression, freeze-thaw cycles, and occasional maintenance loading from utility vehicles. Icorene 1761 GRY 7770 is converted into single-piece enclosures with wall sections between 6 mm and 25 mm, depending on the load rating. Because mLLDPE has a flexural modulus below that of a high-density rotomoulding grade, designers compensate with ribs, gussets, and double-wall corner sections rather than increasing wall thickness alone. Flexural modulus is measured according to ASTM D790 or ISO 178 to compare design options; tensile yield is measured according to ASTM D638. The narrow branching distribution of the metallocene resin yields more uniform fracture resistance at low temperatures, which is relevant for enclosures installed in northern climates where soil temperature can remain below 0 °C for long periods. The relevant article-level test for below-grade enclosures is often ANSI/SCTE 77, which specifies load, impact, and environmental tests on the finished enclosure; compliance is not established by resin properties alone. Where a UL 94 V-0 or V-2 rating is specified, this grade is not the appropriate selection unless a flame-retardant layer or post-treatment is validated; standard polyethylene rotomoulding compounds typically achieve only an HB classification. In production, the main difficulty is maintaining wall thickness at the deep draw of the vault body and around cable entry ports. Slow rotation, proper venting, and strict powder-size control reduce porosity in thick bosses. Mould surface temperature and internal air temperature are tracked separately because oxidation of the internal surface occurs when the inner air remains above 230 °C while the outer wall has already begun cooling. External masterbatch addition should not exceed 2–3 wt% to avoid particle segregation in deep draw sections. Terminal products include handholes, pedestal enclosures, splice vaults, and pad-mount transformer bases with moulded-in conduit entries.
In marine aquaculture floats, marker buoys, and foam-filled mooring fenders, the rotomoulded shell functions as a waterproof skin and abrasion-resistant jacket around a closed-cell polyurethane foam core. Icorene 1761 GRY 7770 can be used for the outer shell because the metallocene LLDPE retains impact toughness at water temperatures approaching 0 °C and because its low moisture absorption limits hull weight gain. Shell wall thickness for small marker buoys is typically 4–6 mm, while larger mooring floats require 10–16 mm walls and local reinforcement around metal eye inserts. The process differs from tank moulding because the foam core is often injected after the shell has cooled and the mould has been opened. The shell must retain enough ductility to resist foam expansion pressure during filling. In production, one recurring bottleneck is bridging at the foam-fill port when the shell wall is under-cured; the internal air temperature at that port must reach at least 195–210 °C before cooling begins. Long-term marine formulations often use an increased UV/HALS masterbatch let-down of 3–5 wt% for continuous saltwater and sunlight exposure. The table below lists typical rotomoulder settings for thin-wall buoy shells and thick-wall mooring floats using metallocene LLDPE.
| Process parameter | Thin-wall buoy shell (4–6 mm) | Thick-wall mooring float (10–16 mm) |
|---|---|---|
| Typical oven set point | 260–280 °C | 285–305 °C |
| Peak internal air temperature | 195–210 °C | 200–220 °C |
| Cooling sequence | Forced air, staged rotation | Air-mist until mould surface 90–110 °C, then fan cooling |
| Common defect | Bridging at foam-fill port | Core void at metal inserts |
The values are class-typical and should be qualified on each mould geometry. Long-term marine weathering performance of this specific grey formulation is not fully covered by standard ISO 4892-3 UV-condensation cycles; published data for this specific configuration is limited. Article-level salt-spray testing and outdoor Florida or North Sea exposure should be used where physical properties after 5–10 years of service are contractually specified. The terminal products are navigation buoys, aquaculture collars, floating dock fenders, and oil-spill containment floats.
In insulated shippers, pharmaceutical cold-chain boxes, and hygienic material handling containers for food processing, Icorene 1761 GRY 7770 is rotationally moulded into double-wall shells that are subsequently injection-foamed with polyurethane. The resin is relevant because the hollow shell must resist cracking at freezer temperatures and also withstand repeated washdown cycles with mild detergents. Wall thickness is usually between 3 mm and 7 mm; thick sections are avoided because the insulated container relies on the foam core for thermal resistance, not on the polyethylene shell. The base olefin polymer class falls under the olefin polymer provisions of FDA 21 CFR 177.1520(c) when the supplier confirms that the compounded lot and colorant package are food-contact compliant. Finished-article migration testing with the intended food simulant is still required because the foam and any laminated inner surfaces form part of the food-contact system. In production, the main failure mode is shell distortion during foam injection; when the shell is too thin or the foam exotherm exceeds the heat-distortion range of the resin, the inner wall can bulge inward and reduce thermal resistance. Rotomoulders control this by setting foam-fill pressure to match the shell modulus and by maintaining a minimum shell wall thickness of 3 mm at the fill port. External mould release agent application is limited to 0.05–0.15 g/m² on mould surfaces to avoid transfer to the hygienic surface. Hygienic pallets and tote boxes are a second terminal class within this segment; they require smooth, cleanable surfaces without parting-line flash that can entrap contaminants. For those parts, tooling is designed with uniform heat transfer and positive venting, and the mould parting line is kept above the floor contact surface. The terminal products include insulated pharmaceutical shippers, cold-chain fish tubs, sanitary pallet containers, and washdown tote boxes used in meat and dairy plants.
Rotomoulded playground components such as tunnel sections, slide hoods, and climbing features use metallocene LLDPE for its ductile failure mode and low-temperature toughness. The grey-pigmented Icorene 1761 GRY 7770 grade is normally limited to structural or non-high-chroma components because the grey colour does not provide the bright colour coding required by many playground equipment specifications. The processing window for complex multiaxis play structures is narrower than for simple tanks: the part must be fully coalesced at the inner surface without overheating the outer skin that is in contact with the mould surface. Peak internal air temperature in the range of 200–215 °C is commonly targeted for wall thicknesses between 5 mm and 10 mm. Impact resistance after weathering is more important than initial notched impact strength, so UV stabilizer packages are selected to retain a measurable fraction of the original low-temperature impact after exposure under ISO 4892-2 or ASTM G154 cycles. The powder blend for structural grey components uses no additional high-chroma pigment; colour is achieved by post-mould coating or by using a separately coloured outer shell. Adhesion of post-mould coatings is checked according to ASTM D3359. Article-level testing under ASTM F1487 for public playground equipment may require head impact, protrusion, and entanglement testing; those results are structural design criteria, not resin properties. On production lines, warpage at the tunnel seam and sink marks over internal ribs are common when cooling is not uniform. Mould rotation must continue through the crystalline solidification range, and release from the mould should occur only after the outer skin has cooled below the practical heat-distortion range. The terminal components are rotationally moulded play tunnels, slide hoods, climbing panels, and structural spacers for modular playground systems.
Competitive LyondellBasell Icorene 1761 GRY 7770 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Specified for rotationally molded parts that must carry a uniform grey surface finish without post-molding painting, LyondellBasell ICORENE 1761 GRY 7770 is a linear low-density polyethylene produced by metallocene single-site catalysis. The material is supplied as a precoloured compound; the base resin designation 1761 identifies the polyethylene grade within the ICORENE series, while GRY 7770 identifies the grey pigment package incorporated into the polymer matrix.
The grade is intended primarily for low-shear melt processing, particularly rotational molding, in which the powder or micropellet charge is heated under biaxial rotation until interparticle coalescence forms a void-free wall. Component categories associated with this material include agricultural sprayer tanks, water storage vessels, industrial hoppers, material handling trays, and machinery covers. These applications demand a balance of low-temperature ductility, dimensional stability, environmental stress-cracking resistance, and resistance to detergent or chemical exposure. The grey colour is practical for outdoor equipment, but the pigment system does not itself indicate ultraviolet stabilization unless the grade-specific datasheet explicitly lists a UV package.
Grade-specific values for melt flow rate, density, additive type, and pigment loading are controlled in the supplier’s certificate of analysis. Melt flow rate is determined at 190°C under 2.16 kg in accordance with ISO 1133-1:2022. Density is measured on compression-molded plaques using ISO 1183-1:2019 or ASTM D792-20. Tensile properties are obtained at 50 mm/min with ISO 527-2:2012 type 1B specimens. Environmental stress-cracking resistance is benchmarked by ASTM D1693-15, Method B, in 10% Igepal CO-630 at 50°C, though the specific test condition should be taken from the batch certificate because commercial specifications can vary. Instrumented puncture energy is characterized by ISO 6603-2:2023, and post-molding shrinkage is assessed by ISO 294-4:2018 after 48 h at 23°C.
Published numeric data for this specific grey-coloured configuration is limited outside the batch certificate of analysis. Tooling decisions should therefore be verified with a pilot-scale molding trial on the intended production oven, using the actual mold geometry and cooling protocol.
In conventional Ziegler-Natta LLDPE, active sites are structurally heterogeneous, producing a broad interchain short-chain branching distribution. Low-molecular-weight chains may be highly branched, while high-molecular-weight chains may be nearly linear. This leads to a low-melting tail, broad crystallite thickness distribution, and variable tie-molecule density between lamellae. Metallocene catalysis, by contrast, uses a constrained-geometry single-site catalyst that inserts the α-olefin comonomer more uniformly across the molecular weight distribution. ICORENE 1761 GRY 7770, as a metallocene product, therefore develops a narrower composition distribution and a more uniform crystalline structure than a conventional Ziegler-Natta LLDPE of similar density and melt flow rate.
| Characteristic | Test basis | Metallocene LLDPE class | Ziegler-Natta LLDPE class |
|---|---|---|---|
| Short-chain branching distribution | ASTM D6474-20 cross-fractionation | Uniform comonomer placement; reduced low-melting and high-melting fractions | Broad distribution; measurable composition heterogeneity |
| Molecular weight distribution | ISO 16014-1:2019 GPC | Narrow; lower polydispersity | Broad; higher polydispersity |
| Shear viscosity at high apparent shear rates | ISO 11443:2021 capillary rheometry | Less shear thinning; higher viscosity may require larger gates in injection molding | Greater shear thinning; easier fill at narrow gates |
| Environmental stress-cracking resistance | ASTM D1693-15 | Higher at equivalent density and melt flow rate | Lower to variable |
| Instrumented puncture energy | ISO 6603-2:2023 | Higher energy absorption at low temperature | Lower energy absorption |
| Rotomolding process tolerance | Production-scale peak internal air temperature mapping | Narrower peak internal air temperature window; overcure embrittlement may be masked by melt uniformity | Broader visual tolerance but lower ultimate toughness |
The above comparison is class-level and does not constitute a grade-specific performance claim for ICORENE 1761 GRY 7770. Confirmation against the batch certificate and a pilot trial is required because the grey pigment package may slightly alter crystallisation, shrinkage, and stabilizer behaviour relative to natural metallocene LLDPE.
The principal processing risk is not melt flow but interparticle coalescence. In a production-scale rotomolding oven, heat transfer through the mold wall controls the sintering rate. If the peak internal air temperature remains below the target lower bound, the powder particles may soften but not fully densify; microvoids remain in the core of the wall. These voids reduce tensile elongation at break, measured by ISO 527-2:2012, and reduce low-temperature impact energy per ISO 6603-2:2023. Conversely, when the peak internal air temperature exceeds the upper bound, the polymer may enter an oxidative degradation regime. The grey pigment can obscure early yellowing, making visual inspection unreliable.
Operational control therefore depends on continuous internal air temperature measurement with thermocouples inserted through the vent. A profiling trial should map the relationship between oven set temperature, oven residence time, wall thickness, and peak internal air temperature. For a representative 6 mm wall, a ±5°C departure around target peak internal air temperature is often sufficient to change instrumented impact performance; the exact value depends on mold geometry, oven airflow, charge weight, and demolding agent. Published data for this specific configuration is limited, so the operating window must be established on the intended production oven rather than assumed from natural resin data.
Cooling rate after the oven also affects crystallinity and warpage. Quenching can increase toughness but may increase shrinkage variation across the part. Slow air cooling can reduce warpage but may lower environmental stress-cracking resistance in thick sections. The precoloured surface can develop uneven gloss if water fogging is applied too early during cooling. Dimensional verification should be conducted after conditioning to ISO 291:2008 class 2 atmosphere, and shrinkage should be confirmed with ISO 294-4:2018 or by direct comparison with a reference mold.
At very low shear, such as the initial powder sintering stage in rotational molding, metallocene LLDPE particles coalesce by surface wetting and diffusion. At higher shear, such as injection molding or screw extrusion, the narrow molecular weight distribution reduces shear-thinning relative to broad Ziegler-Natta grades. Capillary rheometry under ISO 11443:2021 across apparent shear rates from 10 s⁻¹ to 10⁴ s⁻¹ provides the viscosity curve needed for mold-filling simulation. Tooling for injection molding should consider larger gates, shorter flow paths, or higher melt temperature if used, because the reduced shear-thinning behaviour can increase pressure drop in thin-wall sections.
Compared with LDPE, the metallocene LLDPE class has higher tensile strength, puncture resistance, and environmental stress-cracking resistance, but lower melt strength and less neck-in stability in extrusion. It is not a drop-in replacement for LDPE in processes requiring high melt tension, such as large-parison extrusion blow molding. Compared with HDPE, the material has lower flexural modulus and lower heat deflection temperature, but better environmental stress-cracking resistance and low-temperature toughness. These differences determine part selection: ICORENE 1761 GRY 7770 is specified where crack resistance and low-temperature ductility are more important than top-load stiffness or high-temperature creep resistance.
Regrind of precolored rotomolding powder should be blended with virgin material at a level validated by the processor. Because metallocene LLDPE retains impact resistance with limited additive loss, rework levels up to 20 wt% are common in noncritical interior layers, but the pigment binder may degrade after repeated heat cycles. The melt flow rate and density of each blended lot should be checked prior to production using ISO 1133-1:2022 and ISO 1183-1:2019. Contamination with polypropylene, HDPE, or PVC must be avoided; metallic contamination from grinders or hoppers should be removed by magnetic separators.
Regulatory status for food contact, potable water, or toys must be obtained from the supplier’s grade-specific declaration. Compliance with REACH and RoHS is not implied by the base resin classification; colour additives and processing stabilizers may affect the regulatory profile. No statement is made regarding suitability for medical devices or implantable components. The processor is responsible for verifying that the finished article meets the applicable national and end-use requirements.