Lyondellbasell Icorene 1761 Gry 7730 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 670178
    Density 0.934 g/cm³
    Melt Flow Rate 3.5 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 110 °C
    Tensile Strength At Yield 17 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 700 %
    Flexural Modulus 700 MPa
    Izod Impact Notched 0.200 J/cm
    Hardness Shore D 55
    Thermal Expansion 1.5E-4 1/°C
    Color Gray
    Form Powder

    As an accredited LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 GRY 7730 is supplied in 25 kg polyethylene-lined bags, palletized, or optionally 1000 kg bulk octabins.
    Container Loading (20′ FCL) 20′ FCL loading of LyondellBasell Icorene 1761 GRY 7730 metallocene linear low-density polyethylene; palletized bags, dry, secure, compliant container shipment.
    Shipping Shipping description for LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene: Non-hazardous thermoplastic resin. Typically supplied in 25 kg bags, palletized and stretch-wrapped, or bulk containers. Store dry, away from heat, moisture, and sunlight. Not DOT/IMDG regulated. Handle with care; avoid bag punctures and dust generation.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Keep material in original sealed bags or containers, palletized off the floor to prevent moisture pickup and contamination. Avoid excessive stacking or pressure that may cause blocking. Maintain moderate ambient temperatures; protect from rain, condensation, and prolonged UV exposure.
    Shelf Life Typically 24 months when stored in unopened original packaging under cool, dry conditions away from direct sunlight.
    Application of LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene

    In rotomolded diesel fuel tank manufacturing, LyondellBasell Icorene 1761 GRY 7730 is handled as a pre-colored grey metallocene LLDPE powder with a nominal density of 0.936 g/cm³ per ISO 1183-1:2019 and a melt index of 6.0 g/10 min per ISO 1133-1:2022. The material is charged at ambient temperature into cast aluminum clamshell molds preheated to 60–80°C and rotated on a biaxial arm with a 4:1 primary-to-secondary axis speed ratio; primary axis rotation is set between 6–10 min⁻¹. Oven air temperature is maintained at 285–300°C while the internal air temperature is monitored by a pyro probe. The mold is removed only after peak internal air temperature reaches 195–205°C and is held for 3–5 min to complete particle coalescence. Premature demolding above 95°C internal air temperature produces wall distortion in 200–1,000 L tanks. Forced-air cooling at 8–12 K/min is applied until the mold surface temperature drops below 70°C, followed by water mist cooling to stabilize dimensional tolerance within ±10% of nominal wall thickness. The metallocene matrix provides low-temperature ductility and environmental stress-crack resistance exceeding 1,000 h under ASTM D1693-15, Condition B, 10% Igepal CO-630 at 50°C, a critical requirement because diesel fuel contains alkyl aromatics that accelerate slow crack growth in conventional Ziegler-Natta LLDPE. Wall thickness is specified at 6–8 mm for diesel transfer tanks used on agricultural trailers, genset day tanks, and compact construction equipment fuel reservoirs. The grade is not recommended for continuous contact with biodiesel blends above B20 or highly aromatic hydrocarbon streams; published long-term resistance data for this exact pre-colored variant in ester-based diesel fuel is limited. Fabricators typically verify tank integrity using static pressure retention and drop testing under local transport packaging regulations, including UN 31A/Y where applicable to removable fuel storage units.

    Does the Grade Survive Extended Contact with Agrochemical Emulsions?

    Rotational molders producing 110–220 L vertical chemical storage tanks select Icorene 1761 GRY 7730 for dilute agrochemical formulations that require high environmental stress-crack resistance and consistent wall density. The non-polar semicrystalline matrix resists dilute mineral acids, alkali solutions, organophosphate emulsions, and many surfactant concentrates at ambient temperature, but does not provide long-term containment for concentrated aromatic solvents, methyl isobutyl ketone, or xylene. Chemical compatibility screening follows ASTM D543-21 immersion practice at 23°C and 50°C for 7-day and 30-day intervals; mass change should remain below 1.0% and tensile elongation retention should remain above 80% when compared with unexposed controls. The grey colorant package is pre-dispersed in the powder, so no dry pigment addition is required. In-house regrind from the same grade may be incorporated at up to 20 wt% when the regrind is dry, screened below 500 µm, and free of foreign polymer contamination. For a 150 L cylindrical tank with 5 mm nominal wall, oven air at 280–290°C, peak internal air temperature of 198–202°C, and a 4:1 rotation ratio yield a densified inner surface without pinholing. The mold is opened at surface temperatures below 60°C to avoid stress cracking at insert bosses. European processors targeting EU Regulation (EC) No 1907/2006 (REACH) and EU Directive 2011/65/EU (RoHS) obtain lot-specific test reports for lead, cadmium, mercury, and hexavalent chromium; typical restricted substance values in the colored compound fall below 100 ppm for each element. End products include vertical storage tanks for 2,4-D amine formulations, glyphosate surfactant concentrates, and dilute fertilizer solutions.

    For industrial material handling trays and export pallets, Icorene 1761 GRY 7730 is processed as a 35–60 mesh powder with a bulk density near 0.43–0.48 g/cm³ to maintain consistent dry flow into multi-cavity tools. The rotomolding cycle for a 1,200 × 1,000 mm pallet with 12 mm nominal wall uses oven air at 290°C, peak internal air temperature at 198°C, and forced ambient air cooling at 10°C/min to 80°C before mold opening. Instrumented puncture testing under ISO 6603-2:2023 at -20°C should show a ductile failure mode rather than brittle crack propagation, which is the decisive criterion for cold-store racking and freezer warehouse handling. The pre-colored grey surface resists abrasion from wooden pallet runners and steel rack edges without showing the white stress-whitening typical of unpigmented LLDPE. Processors should avoid contamination with polypropylene slivers from banding straps because polypropylene domains remain unmelted at rotomolding temperatures and create localized leak paths. End-use components include chemical drum trays, conveyor side guides, and captive returnable export pallets.

    Rotational Moulding Parameter Window for Thin-Wall Outdoor Enclosures

    Thin-wall outdoor enclosures, including junction boxes and small instrumentation housings with 4–6 mm nominal wall sections, require a narrower processing window than heavy tanks. Oven air temperature is held at 280–285°C because thin sections reach peak internal air temperature rapidly and suffer surface oxidation above 290°C. Peak internal air temperature is limited to 190–195°C with a 2 min hold, and cooling is controlled at 10–14 K/min to suppress warpage in flat lid and flange areas. The metallocene comonomer distribution in Icorene 1761 GRY 7730 reduces post-mold shrinkage variation across ribs and bosses when compared with conventional LLDPE, but tooling still requires 0.5–1.0% per side shrinkage allowance depending on localized thickness. Design verification for polymeric enclosures follows IEC 62208:2018 for empty low-voltage switchgear and controlgear enclosures, with weathering acceptance evaluated under ISO 4892-2:2021 UV exposure. A color shift ΔE below 4.0 after 1,000 h of accelerated weathering is the typical acceptance window for grey outdoor enclosures; lot-specific data should be requested from the compounder. The grade is rated only as HB under UL 94 and must not be used in applications requiring V-0 flammability classification unless an intumescent coating or metallic shield is applied. Insert retention is improved by molding brass or stainless steel threaded inserts with knurled shanks into 12 mm bosses, and demolding is delayed until mold surface temperature falls below 65°C to prevent thread boss cracking.

    ApplicationNormative referenceCritical parameterTypical acceptance window
    Diesel fuel tankASTM D1693-15 Condition BEnvironmental stress-crack resistance>1,000 h
    Agrochemical tankASTM D543-21Mass change after 30-day immersion<1.0%
    Material handling palletISO 6603-2:2023Puncture failure mode at -20°CDuctile
    Outdoor enclosureISO 4892-2:2021ΔE after 1,000 h UV weathering<4.0
    Marine fenderISO 179-1:2023Low-temperature impact responseDuctile or hinge break
    Waste containerEN 840-1:2020Impact at -20°C after conditioningNo split or wall penetration

    When Grey UV-Stabilized Powder Is Used in Marine Fender Construction

    Cylindrical marine fenders and floating dock spacers are rotomolded with wall thicknesses of 10–18 mm to resist berthing impact and continuous saltwater exposure. The density of 0.936 g/cm³ provides inherent buoyancy, while the pre-colored grey surface reduces visible ultraviolet degradation and surface chalking. The process sequence uses oven air at 280–295°C, peak internal air temperature at 195–205°C, and a 4:1 rotation ratio, followed by slow cooling at 6–8 K/min to allow stress relaxation in thick sections. Fast water quenching is avoided because it locks in thermal stresses that later produce circumferential cracks under repeated impact. Closed-cell polyurethane foam is injected after molding for puncture redundancy and to prevent water ingress if the outer shell is punctured. Impact testing under ISO 179-1:2023 at -20°C should show ductile or partial hinge break rather than brittle fracture; any brittle fracture not associated with regrind contamination or overbaking above 210°C peak internal air temperature requires investigation of the cooling rate and pigment dispersion. The grade is compatible with stainless steel shackle inserts and elastomeric end caps, but direct bonding with amine-cured epoxy adhesives can soften the polyethylene surface and should be replaced by mechanical fastening or plasma-treated polyurethane adhesives. Published data for the specific long-term marine aging performance of this exact pre-colored grade is limited; lot-specific UV and oxidation induction time data should be collected under ISO 4577 or equivalent practices before large-volume marine deployment.

    In 1,100 L four-wheel municipal waste container production, Icorene 1761 GRY 7730 is processed at a wall thickness of 5–6 mm to balance weight against impact resistance in automated lifting systems. The tooling is designed with reinforced corner radii of at least 10 mm and steel axle inserts enclosed in molded polyethylene bosses. The cycle uses oven air at 280°C, peak internal air temperature at 195°C, and ambient forced-air cooling to 70°C mold surface temperature before demolding. The material selection is driven by the impact and cold-temperature requirements of EN 840-1:2020 for mobile waste containers; type-tested bins are conditioned at -20°C and subjected to drop and corner impact tests without splitting or wall penetration. Observed field failures in municipal service occur primarily at axle boss inserts when demolding is too early or cooling is non-uniform. Molders reduce this by using stainless steel inserts, maintaining uniform mold wall temperature, and avoiding regrind levels above 20 wt% in load-bearing areas. The grey compound is suitable for automated side-loading and rear-loading collection systems because its surface resists abrasion from metal lifting combs and does not show gross stress-whitening after repeated dumping cycles. End products include 1,100 L flat-lid and domed-lid four-wheel containers, recycling bins, and underground waste chute collection carts.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7730 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 GRY 7730 is a metallocene-catalyzed linear low-density polyethylene compound supplied in a precoloured grey rotational moulding grade. The designation 1761 identifies the base resin within the Icorene portfolio, while GRY 7730 identifies the grey pigment package. The product is intended for rotationally moulded hollow parts requiring a controlled grey surface together with low-temperature impact resistance, environmental stress-crack resistance, and adequate stiffness for industrial and outdoor components. Unlike natural powders that are coloured by dry blending, the precompounded grey system reduces the risk of pigment segregation and colour streaking during powder handling, but it also changes the thermal absorption behaviour of the powder bed and must be accounted for when cycle times are transferred from natural rotational moulding materials.

    The base resin is produced by single-site metallocene catalysis. This catalyst technology yields a narrower molecular weight distribution and a more homogeneous intermolecular and intramolecular short-chain branch distribution than conventional Ziegler-Natta linear low-density polyethylene. The practical consequence in rotational moulding is that density can be maintained in the upper linear low-density range without proportionally sacrificing impact resistance or environmental stress-crack resistance. The reduced low-molecular-weight fraction contributes to lower extractables and can improve organoleptic and compliance performance in demanding applications. The product class is therefore distinguished from conventional butene-copolymer linear low-density polyethylene by improved toughness at comparable density and from high-density polyethylene by a lower flexural modulus but substantially better impact and crack resistance at a given wall thickness.

    How Does Metallocene Architecture Alter Densification and Bubble Removal in Rotational Moulding?

    Rotational moulding of Icorene 1761 GRY 7730 follows the standard powder densification sequence: powder tackification, coalescence, densification, and solidification. Published process data for this specific grey-grade configuration are limited, and cycle settings should be established using instrumented internal air temperature rather than transferred directly from a natural grade. For metallocene linear low-density polyethylene rotational moulding powders, oven air temperatures are commonly set between 260 °C and 320 °C, with peak internal air temperature generally controlled between 185 °C and 200 °C for medium-wall parts. The grey colour package modifies radiative heat absorption compared with white or natural powders. A grey charge may reach the target peak internal air temperature earlier at the same oven set point, and a small adjustment in oven dwell time or air temperature is therefore required when changing from natural to GRY 7730. The magnitude of that adjustment is part-specific and should be determined with a thermocouple placed inside the mould cavity. Insufficient peak internal air temperature can produce under-densified regions, pinholes, and inner-surface roughness in thick bosses, while excessive internal air temperature can accelerate oxidative degradation and shift the grey colour.

    On production-scale carousel machines, the mould rotation ratio and arm speed control powder distribution. Rotational moulding machines are commonly operated with a primary-to-secondary rotation speed ratio near 4:1, with primary arm speeds in the range of 2–8 min⁻¹ for medium-sized parts. Deep ribs, inserts, or complex geometries may require modified speed ratios or uniaxial rotation to maintain wall thickness uniformity. The powder dry flow and particle-size distribution determine how the material slumps into recesses. Metallocene polyethylene rotational moulding powders in this class typically have median particle sizes in the 250–500 µm range and dry flow values below 40 s/100 g when measured by ISO 6186. Excess fines or an overly broad particle-size distribution can segregate during rotation and produce localized wall-thickness variation. The precompounded grey powder should be handled in closed transfer systems where dust generation and static charge accumulation are controlled, because static adhesion can influence powder distribution on the mould surface and contribute to surface defects.

    Instrumented moulds should record internal air temperature at intervals no slower than 0.1 Hz. After the initial heat-transfer lag, the internal air heating rate is typically 4–8 °C/min depending on oven set point and part mass. The later stages of densification generally occur when internal air temperature reaches 170–180 °C, but complete bubble removal may require the peak internal air temperature to be held for 1–3 min on thick sections. Cooling must be controlled to limit warpage; forced-air cooling followed by controlled water mist is common, but quenching can increase residual stress and reduce impact performance. The grey pigmented material may release heat at a different rate than natural resin because of differences in crystallinity and surface emissivity, so mould surface temperature should be measured if warpage is recurrent.

    Mechanical, Thermal, Powder, and Colour Specification Methods

    Specification testing for the base resin and grey compound should follow recognized polyolefin standards. Density is determined by ISO 1183-1 or ASTM D792. Melt index is measured at 190 °C and 2.16 kg by ISO 1133-1 or ASTM D1238. Tensile yield strength and elongation at break are evaluated on rotationally moulded or compression-moulded specimens according to ISO 527-2 or ASTM D638. Flexural modulus is measured by ISO 178 or ASTM D790. Instrumented puncture resistance is determined on moulded plaques using ISO 6603-2, and low-temperature impact testing is usually specified by the end-use standard. Environmental stress-crack resistance is determined according to ASTM D1693 using 100 % Igepal CO-630 at 50 °C. Vicat softening temperature is measured by ISO 306 or ASTM D1525. Thermal stability is monitored by oxidative induction temperature or time using ISO 11357-6 or ASTM D3895. Powder bulk density is determined by ASTM D1895, and dry flow by ISO 6186. Colour is specified in CIELAB coordinates according to ISO 11664-4 or ASTM D2244. The lot-specific L*, a*, and b* values for GRY 7730 are supplied on the certificate of analysis and should be confirmed against the agreed colour tolerance for the part. Published data for the exact compound Icorene 1761 GRY 7730 are limited, and no published data sheet should be used as a specification without the supplier certificate of analysis and lot-specific values.

    Melt rheology also separates metallocene linear low-density polyethylene from conventional linear low-density polyethylene. In oscillatory rheometry, the metallocene class typically displays higher shear viscosity at high frequency and lower melt elasticity at similar melt index. This can increase compounding torque and reduce die swell during pelletization or powder production. On a co-rotating twin-screw extruder with an L/D ratio near 40:1, the narrow molecular weight distribution of metallocene linear low-density polyethylene is more sensitive to screw speed and feed rate than a broad-distribution Ziegler-Natta linear low-density polyethylene. Compounding should be performed with sufficient kneading to disperse the grey pigment and stabilizers, but melt temperature should be maintained below 220 °C during extended residence to preserve antioxidant reserves and colour stability.

    Regulatory compliance should be assessed on the final article. The natural base resin may comply with FDA 21 CFR 177.1520 as an olefin polymer for food-contact use, but the grey compound must be separately evaluated because pigments, stabilizers, and decomposition products may migrate. EU compliance under Regulation 10/2011 requires article-specific overall migration testing, with the limiting overall migration value of 10 mg/dm² for the intended contact time and temperature. RoHS 2011/65/EU restricts lead to 1000 ppm, mercury to 1000 ppm, cadmium to 100 ppm, hexavalent chromium to 1000 ppm, and PBB/PBDE flame retardants to 1000 ppm in homogeneous materials. REACH 1907/2006 Article 33 requires communication if any substance of very high concern is present above 0.1 % w/w. The supplier safety data sheet and REACH statement should be consulted before specification.

    Regulatory and compliance matrix for the rotational moulding compound
    Standard or regulationScopeNumerical limit or method
    FDA 21 CFR 177.1520Olefin polymers in food contactArticle-specific extraction testing; conditions of use B through H depending on food type and thickness
    EU 10/2011Plastic food-contact materialsOverall migration limit 10 mg/dm²
    RoHS 2011/65/EUHeavy metals and brominated flame retardants in homogeneous materialPb 1000 ppm, Hg 1000 ppm, Cd 100 ppm, Cr(VI) 1000 ppm, PBB/PBDE 1000 ppm
    REACH 1907/2006Substances of very high concern in articlesCommunication threshold 0.1 % w/w

    The product class is used in rotationally moulded goods where grey colour is specified at the point of purchase and where part size, chemical resistance, and low-temperature toughness are simultaneous requirements. Representative applications include agricultural hoppers, industrial tanks, equipment housings, waste containers, automotive ducts and reservoirs, outdoor enclosures, and material-handling bins that are not subject to continuous internal pressure above the design rating. Grey compounds are often selected for parts where post-moulding painting is not cost-effective and where the surface must tolerate weathering without showing minor scuffs. Chemical compatibility must be evaluated for each intended content; diesel fuel, strong oxidizing acids, and certain cleaning agents may reduce environmental stress-crack resistance and should be tested under end-use conditions.

    Thermal degradation, moisture, and regrind boundaries are relevant to production. Polyethylene rotational moulding powders do not normally require drying. However, condensation on cold powder surfaces can occur when bags are moved from cold storage into a warm, humid plant. If relative humidity exceeds 60 %, surface moisture can cause pinholes or splay-like inner surface defects during densification. Pre-drying at 70–80 °C for 1–2 h may be required for powder that has been exposed to high humidity or stored in unsealed containers. The resin should not be processed above 220 °C internal air temperature for extended periods. Prolonged overheating above 200 °C can consume antioxidants, initiate chain scission, and shift the grey colour. Regrind of rotationally moulded parts made from the same grey compound can be included up to the level validated by the part impact and colour tolerance. Mixed-pigment or mixed-density regrind should be excluded because inconsistent powder morphology and colour concentrate distribution can produce surface defects and brittle regions. The powder should be kept away from open flame, copper-containing materials that can catalyze oxidation, and strong oxidizers. Standard polyolefin purge procedures apply for compounding equipment; purging with a fractional-melt high-density polyethylene or commercial purge compound is acceptable, while PVC, acetal, and nylon residues must be eliminated before processing to prevent cross-contamination and acid gas formation.

    Relative to a rotational moulding high-density polyethylene, Icorene 1761 GRY 7730 occupies a lower-density position that reduces flexural modulus but improves low-temperature impact and environmental stress-crack resistance at a given wall thickness. Relative to a conventional Ziegler-Natta linear low-density polyethylene rotomoulding grade, the metallocene base resin generally provides a more uniform response to cooling and a lower tendency to warp because the narrower molecular weight distribution and homogeneous comonomer distribution produce fewer low-crystallinity fractions. However, the same narrow distribution may require closer control of peak internal air temperature. If oven exit occurs before complete densification, the remaining bubbles cannot be compensated by a broad low-molecular-weight tail, and porosity may be more evident than in a conventional linear low-density polyethylene with the same density. Compared with low-density polyethylene rotomoulding material, the metallocene linear low-density polyethylene typically offers higher tensile strength, higher hardness, and better environmental stress-crack resistance at the expense of melt flow and surface gloss. Compared with a natural Icorene grade, the grey precolour removes the need for dry-blended pigment and reduces segregation, but it should not be assumed to provide equivalent weathering stability unless the package includes adequate UV stabilization. Carbon black or another grey pigment system may not protect the polymer unless formulated for that purpose. The UV stabilization package should be confirmed if outdoor service is required.

    For rotationally moulded vertical storage tanks, ASTM D1998-21 provides design and test methods for polyethylene tanks, including minimum wall thickness and drop-impact requirements. The part manufacturer must verify the compound against the required hoop stress and environmental exposure criteria. For automotive ducts and reservoirs, the applicable fluid compatibility, thermal cycling, and vibration standards must be used. For waste containers and outdoor enclosures, the relevant impact, dimensional stability, and weathering specifications should be evaluated on the final part rather than inferred only from raw material data. The final part properties depend on mould geometry, heating rate, cooling rate, and wall thickness distribution, and cannot be replaced by resin data alone.

    Top