Lyondellbasell Icorene 1761 Gry 7715 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7715 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7715 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 274207
    Color Grey
    Density 0.918 g/cm³
    Melt Flow Rate 1.0 g/10 min (190°C/2.16 kg)
    Melting Point 115 °C
    Vicat Softening Temperature 95 °C
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 500 %
    Flexural Modulus 200 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 10 %
    Gloss 45 70
    Coefficient Of Friction 0.20
    Hardness Shore D 50
    Thermal Conductivity 0.33 W/m·K
    Specific Heat 1.9 J/g·°C
    Water Absorption <0.01 %
    Processing Temperature 200 °C
    Die Temperature 210 °C
    Blow Up Ratio 2.5:1

    As an accredited LyondellBasell Icorene 1761 GRY 7715 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 GRY 7715 is supplied in 25 kg polyethylene bags, typically 40 bags per pallet (1,000 kg), stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of LyondellBasell Icorene 1761 GRY 7715 metallocene LLDPE, stretch-wrapped and secured for transport.
    Shipping LyondellBasell Icorene 1761 GRY 7715 is typically shipped as free-flowing polyethylene pellets in sealed, moisture-resistant bags, octabins, or bulk railcars/trucks. Generally non-hazardous and not DOT-regulated. Keep dry, cool, and away from direct sunlight; protect packaging from punctures, contamination, and excessive heat or moisture during handling.
    Storage Store LyondellBasell Icorene 1761 GRY 7715 Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed and palletized to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Protect from punctures and crushing. Store at ambient temperature. Use first-in, first-out inventory and follow the manufacturer’s SDS.
    Shelf Life The shelf life for Icorene 1761 GRY 7715 is 24 months when stored in original unopened packaging under cool, dry conditions.
    Application of LyondellBasell Icorene 1761 GRY 7715 Polyethylene, Linear Low Density, Metallocene

    In single-layer rotational molding of large chemical storage shells, the dry-blend charge contains Icorene 1761 GRY 7715 at 95–100 wt%, with 2–4 wt% of a UV-stabilizer masterbatch and 0–30 wt% of in-house regrind only where the end-user specification has validated the regrind source against UN 31H1 dropping and stacking test protocols. The principal compliance framework is ASTM D1998-21 for upright rotationally molded polyethylene storage tanks, FDA 21 CFR 177.1520(c) for potable-water and repeated food-contact layers, and Chapter 6.5 of the UN Recommendations on the Transport of Dangerous Goods for composite IBC inner bottles of design type 31H1 or 1H1. On three-arm carousel machines with 4:1 or 5:1 biaxial rotation, the mold surface is heated to 260–290 °C while the internal air temperature is held at 190–210 °C for 18–35 min depending on a nominal wall thickness of 4–10 mm; single-arm shuttle lines can produce wall-thickness variation of ±10% if the major-axis speed is not kept below 6 rpm during the first half of the heating cycle. Cooling is staged, using forced ambient air until the internal air temperature falls below 120 °C, then water mist at 5–15 °C on large flat sections to reduce warpage. Terminal parts include conical-bottom agricultural sprayer tanks, 1000–25,000 L vertical storage tanks, horizontal transport tanks, and UN-certified composite IBC inner bottles with steel cages.

    When Does Low-Temperature Impact Resistance Govern Marine Buoy Shelling?

    Marine shells are qualification-tested at -40 °C according to ISO 179-1:2010 Type 1 notched specimens or ASTM D256-23 Method A, because a ductile-to-brittle transition is observed when the mold internal air temperature falls below 185 °C at the inner-wall fusion line. The resin is charged at 97–100 wt% as the outer shell matrix, with 0.3–0.8 wt% of a high-molecular-weight hindered amine light stabilizer and 0–2 wt% of a low-yellowness UV absorber; mineral fillers are excluded because they increase notch sensitivity below -20 °C. The downstream process is a two-stage rotational molding and foaming sequence: the shell is molded in a cast aluminum tool at 190–205 °C internal air temperature, demolded after slow cooling at ≤ 8 °C/min, then transferred to a foaming fixture where closed-cell polyurethane froth is injected at 45–60 kg/m³ core density. The foam exotherm must not drive the polyethylene inner wall above 80 °C or the inside weld line will stress-relax and lose burst resistance. Compliance for mooring and dock fender products includes ISO 4892-3:2024 Method A cycle 1 for UV exposure and ISO 179-1:2010 for low-temperature impact; where floatation is a safety feature under EU inland-waterway use, selected components may be assessed against the Recreational Craft Directive 2013/53/EU. Terminal finished parts include cylindrical mooring buoys, foam-filled dock fenders, harbor float shells, and pontoon float bodies.

    For automotive interior and heating, ventilation, and air-conditioning ducting, the dry-blend is formulated at 85–95 wt% Icorene 1761 GRY 7715 with 5–15 wt% of an ethylene-octene plastomer to reduce scratch whitening on textured surfaces, plus 0.5–1.0 wt% of a phenolic-phosphite antioxidant package to control volatile generation during long oven cycles. The sector is governed by FMVSS 302 and ISO 3795:1989 interior burn-rate limits of 100 mm/min, VDA 278:2011 for VOC and FOG screening, and ISO 6452:2021 for fogging characteristics of trim materials; OEM specifications frequently tighten fogging mass to ≤ 5 mg per 10 cm². The conversion route is rotational molding in electroformed nickel or cast aluminum tools with 0.5–1.2 mm grain depth, at an internal air temperature of 185–200 °C. The lower bound is limited by knit-line pinholing in deep female corners, while the upper bound is limited by volatile evolution from antioxidant decomposition above 200 °C; demolding at 70–80 °C reduces post-mold dimensional drift. Published data for this specific grade in rotomolded HVAC ducting is limited; the stated processing window is derived from general metallocene LLDPE rotor molding practice rather than a grade-specific material datasheet. Terminal products include HVAC distribution housings, instrument panel storage trays, seat-back panels, and rotary-molded interior door lower sections for off-road and agricultural vehicles.

    Outdoor Telecommunication and Electrical Enclosure Resin Requirements

    Outdoor equipment enclosures rotomolded from metallocene LLDPE are specified for UL 94 HB or ASTM D635-22 horizontal burn behavior, IEC 60529 ingress protection ratings up to IP65, and NEMA 250 Type 4 or 4X enclosures when the application includes incidental water spray. The dry-blend formulation retains Icorene 1761 GRY 7715 at 90–98 wt% with 2–5 wt% of a carbon black or gray UV masterbatch and 0.5–2 wt% of an acid scavenger; no halogenated flame retardant is added because polyethylene does not attain V-0 without additive loadings sufficiently high to reduce impact and weld-line strength. Production on carousel or shuttle rotomolding machines uses a wall thickness of 4–8 mm, oven set point 260–280 °C, internal air temperature 190–205 °C, and a rotation ratio of 4:1. Metal inserts are preheated to 150–180 °C before placement to prevent premature solidification at the insert-polymer interface. Terminal products include street-side telecommunications splice cabinets, irrigation controller housings, power distribution boxes, and outdoor instrumentation enclosures.

    Downstream segmentCompliance referenceTest method or designationNumerical threshold or processing criterion
    Chemical storage and transportASTM D1998-21, UN 31H1, FDA 21 CFR 177.1520(c)UN Chapter 6.5 drop test, ASTM hydrostatic test190–210 °C internal air temperature
    Marine buoyancyISO 179-1:2010, ISO 4892-3:2024, 2013/53/EUnotched impact at -40 °C185–205 °C fusion-line window
    Automotive interiorFMVSS 302, ISO 3795:1989, VDA 278:2011, ISO 6452:2021fogging mass per 10 cm²≤ 5 mg per 10 cm²
    Electrical enclosuresUL 94 HB, IEC 60529, NEMA 250ingress protectionIP65
    Food contact bins and pallet boxesFDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011, NSF/ANSI/CAN 51overall migration≤ 10 mg/dm²
    Water treatment vesselsNSF/ANSI/CAN 61, AS/NZS 4020:2018, ISO 9080:2012cooling ramp 120–60 °C≤ 10 °C/min

    Direct food-contact conversion of bins and pallet boxes uses the resin at 100 wt% virgin material, or ≤ 10 wt% of in-plant regrind only when the converter maintains lot-level traceability to the same food-contact grade under 21 CFR 177.1520(c)(2.1). Compliance is documented against FDA 21 CFR 177.1520(c) for olefin polymers, EU Regulation (EU) No 10/2011 Annex I and IV with overall migration below 10 mg/dm² in food simulants, and NSF/ANSI/CAN 51 for food equipment materials when specified. The process is dry-flow rotational molding without solvent-based mold release; only food-grade silicone or fluoropolymer mold release at 0.5–1.0 g/m² is used. Peak internal air temperature is held at 190–210 °C, and cycle time is capped to minimize oxidative degradation at the inner surface. Batch-to-batch pigment dispersion in pre-compounded gray material must be checked by melt-mixing; if colorant agglomerates exceed 35 µm, pinhole formation increases in flat-bottom bin corners. Terminal products include ingredient storage bins, pallet boxes, side-wall trays, and bulk handling containers for dry powders and granules.

    If Sulfate-Containing Process Water Is Stored, Post-Molding Internal Stress Must Be Controlled

    In water treatment and filtration tank production, the rotomolded shell must resist environmental stress cracking in sulfate- and chloride-containing service fluids, so the molding protocol uses a slower cooling ramp of ≤ 10 °C/min between 120 °C and 60 °C to reduce frozen-in residual stress. Icorene 1761 GRY 7715 is charged at 95–100 wt%, with 0.5–2 wt% of a water-contact-stabilized UV package and 0–5 wt% of a high-density polyethylene stiffening component only in tall vertical vessels where creep resistance must be increased. The applicable compliance set includes NSF/ANSI/CAN 61 for drinking water system components, AS/NZS 4020:2018 for products in contact with drinking water, and ISO 9080:2012 for long-term hydrostatic strength of thermoplastic piping materials where applicable to vessel wall sections. Processing is performed on independent-arm carousel machines at 190–205 °C internal air temperature; the mold surface is not allowed to exceed 285 °C because surface oxidation produces gloss variation and a measurable loss of inner-surface chemical resistance. Published stress-cracking data for this specific rotomolding formulation in sulfate-containing waters is limited; the cooling-rate guidance is based on general polyethylene stress-cracking behavior rather than a grade-specific ESC test. Terminal products include filter housings, brine tanks, softening vessels, dosing tanks, and pressure surge tanks.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7715 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The LyondellBasell Icorene 1761 GRY 7715 is a pigmented metallocene-catalysed linear low-density polyethylene powder supplied for rotational moulding and particle-sintering operations. The base-resin designation Icorene 1761 identifies an ethylene-alpha-olefin copolymer produced with a single-site metallocene catalyst; the suffix GRY 7715 identifies a grey colour package that may be introduced as a compounded colour concentrate or as a controlled dry blend. Incoming-material qualification for this powder normally includes melt flow rate at 190 °C/2.16 kg under ISO 1133-1 or ASTM D1238, moulded density under ISO 1183-1 or ASTM D1505, tensile yield stress and elongation at break under ISO 527-2 or ASTM D638, flexural modulus under ISO 178 or ASTM D790, Shore hardness under ISO 868 or ASTM D2240, environmental stress-crack resistance under ASTM D1693, and low-temperature impact by the ARM method or ISO 6603-2. The grey pigment shifts infrared energy absorption, crystallisation behaviour, and antioxidant consumption relative to the natural base resin, so lot-specific technical data must be used for acceptance rather than generic polyethylene class data. The numerical suffix does not encode viscosity or density, and the colour code must be retained in purchasing specifications to avoid substitution with natural or differently stabilised material.

    What separates the metallocene base resin from Ziegler-Natta LLDPE at equivalent density?

    The dominant structural difference is the uniformity of alpha-olefin comonomer placement. Ziegler-Natta LLDPE is produced at multiple active-site chemistries, producing chains with broad and non-uniform short-chain branching; the high-molecular-weight fraction is typically less branched and crystallises earlier during slow cooling, yielding a heterogeneous lamellar texture. Metallocene catalysis gives a narrower molecular weight distribution and more uniform comonomer distribution, so the rotomoulded wall develops a more homogeneous crystalline superstructure. Differential scanning calorimetry under ISO 11357-3 therefore records a sharper melting endotherm and a narrower crystallisation exotherm for the metallocene grade than for a conventional LLDPE of the same density. This microstructural difference reduces moulded-in stress and warpage in thick sections cooled on the mould surface. Low-temperature drop testing using the ARM method or ISO 6603-2 generally shows a ductile-to-brittle transition several degrees lower for the metallocene grade, with published comparative studies often reporting differences of 5–10 °C. Environmental stress-crack resistance under ASTM D1693 also improves because the more regular tie-molecule population resists slow crack growth through the intercrystalline regions. The processing consequence is a steeper viscosity decline above the melting point, requiring closer peak internal air temperature control than broad-MWD Ziegler-Natta LLDPE.

    In a forced-air carousel or shuttle rotomoulder, the oven environment is commonly set between 260 °C and 330 °C, but the control parameter is the peak internal air temperature. For metallocene LLDPE powders, the PIAT window is generally 200–230 °C; values below 190 °C leave sinter necks between powder particles incompletely coalesced and produce microvoiding at the inner wall, while values above 240 °C accelerate thermo-oxidative chain scission. The melt flow rate of an overtemperature moulded sample can rise by more than 10% relative to the virgin powder, indicating antioxidant consumption and molecular weight reduction. Because sinter flow occurs at low shear, the zero-shear viscosity is more relevant than high-shear melt viscosity; the narrow-MWD metallocene resin has a lower zero-shear viscosity than a broad-MWD Ziegler-Natta resin at equivalent MFR, allowing bubble removal and densification at lower temperature. Dynamic oscillatory shear measurements at 190 °C on a parallel-plate rheometer commonly show lower complex viscosity at 0.1 rad/s than a Ziegler-Natta LLDPE of matching MFR, consistent with narrower molecular weight distribution. The GRY 7715 grey pigment absorbs radiant heat, and the outer resin surface may run 20–50 °C hotter than the internal air thermocouple reads. Process optimisation should map oven dwell against PIAT for the actual mould and charge weight rather than transferring natural-powder cycles directly. After the peak temperature is reached, forced-air cooling to 90–110 °C before water-mist cooling reduces differential shrinkage in dark grey parts; abrupt water quenching can create warpage because the pigmented surface has higher emissivity and releases heat faster.

    When a grey pigment package alters infrared absorption, stabilizer performance, and part colour retention

    Grey rotomoulding formulations may contain carbon black, titanium dioxide, iron oxide, or mixed-metal oxide pigments; the precise composition of GRY 7715 is controlled by the supplier’s colour specification. Carbon black is an effective ultraviolet screen but also increases radiant heat absorption during rotomoulding, raises surface temperature, and can alter the apparent activity of hindered phenolic antioxidants. For exterior components, accelerated weathering should be performed under ISO 4892-2 xenon-arc exposure or ASTM D2565. Colour change, gloss retention, and retained tensile elongation are typically monitored after 1000–3000 h of exposure as screening benchmarks, but these durations are not universal acceptance limits. Pigment dispersion is also a direct quality indicator: poorly dispersed carbon black creates grey streaks, lowers coating-level UV screening, and produces local crystallisation nuclei that can embrittle thin sections. For outdoor grey parts, the supplier’s stabilizer package should be confirmed because a grey colour alone does not guarantee long-term weathering performance. In chemical service, pigment particles can nucleate crystallisation and slightly reduce diffusion coefficients for small molecules, but the improvement is not a replacement for barrier-layer design or permeation testing under ASTM D3985.

    Numerical acceptance limits should be taken from the current LyondellBasell datasheet for the Icorene 1761 GRY 7715 grade, because the coloured variant may be released with pigment-adjusted tolerances. For the unfilled base resin, published supplier data commonly place nominal density near 0.938 g/cm³ and melt flow rate near 4.5 g/10 min at 190 °C/2.16 kg. The grey pigment can raise moulded density by approximately 0.001–0.003 g/cm³ and may produce a measurable shift in melt flow rate. Typical mechanical values for unfilled metallocene LLDPE of this density class fall between 15 MPa and 20 MPa for tensile yield stress, exceed 600% elongation at break, and fall in the 600–800 MPa range for flexural modulus. These ranges are class-typical and must not be used as certified lot-release limits. The following table summarises the principal test methods and their function during rotomoulded-part acceptance.

    Property Test method Function in acceptance
    Melt flow rate ISO 1133-1, ASTM D1238 Detects pigment- and reclaim-induced viscosity shift at 190 °C/2.16 kg
    Moulded density ISO 1183-1, ASTM D1505 Confirms stiffness and shrinkage class of the fused wall
    Tensile yield and elongation ISO 527-2, ASTM D638 Verifies powder fusion, void content, and molecular degradation
    Flexural modulus ISO 178, ASTM D790 Measures load-bearing stiffness for tank and panel service
    Environmental stress-crack resistance ASTM D1693 Predicts slow crack growth under chemical and stress service
    Low-temperature impact ARM, ISO 6603-2 Screens for ductile-to-brittle transition in cold environments

    Powder particle-size distribution is equally important to fusion. Rotomoulding powders of the Icorene family are generally dry-sieved with a median particle diameter between 200 µm and 500 µm and a controlled fines fraction below 100 µm. Excessive fines reduce dry-flow and promote static adhesion, while coarse particles require longer sintering and leave a granular inner surface. Dry-flow testing is performed by a funnel method or by measuring bulk density under ASTM D1895; a bulk density below the supplier range indicates particle-size segregation, moisture, or high pigment concentrate addition. If storage has occurred at relative humidity above 60% and dry-flow time exceeds a site-defined limit, the powder may be pre-dried at 30–40 °C for 12–24 h under dry air before charging.

    Compared with high-pressure low-density polyethylene, the metallocene LLDPE architecture carries fewer long-chain branches but more uniform short-chain branching, and this changes the rotomoulding property balance. LDPE produces softer parts with lower flexural modulus, lower tensile yield stress, and greater creep compliance at equivalent wall thickness; its broad long-chain branching provides high melt strength but does not equal the ESCR and low-temperature impact of a metallocene LLDPE. In differential scanning calorimetry under ISO 11357-3, the metallocene grade typically shows a single main melting peak between 120 °C and 126 °C for a density near 0.938 g/cm³; an LDPE of similar density may display a broader peak with a lower-temperature shoulder because of its more branched architecture. The Icorene 1761 base resin therefore yields higher stiffness and better stress-crack resistance than an LDPE grade of the same density, allowing a thinner wall to be considered only after structural calculations using a recognised method such as ASTM D1998 for stationary polyethylene tanks. However, the metallocene grade must not be processed through high-shear compounding without a moderate-shear twin-screw configuration; excessive viscous heating can reduce molecular weight and shift rotomoulding PIAT. If the cooling-run crystallisation peak shows a high-temperature shoulder, the grade may contain a heterogeneous fraction from added rerun or off-spec pigment concentrate, and its ESCR and warpage behaviour should be reassessed.

    Regulatory compliance and stability constraints in contact end-uses

    Food-contact and potable-water applications require the converter to confirm the regulatory status of the exact GRY 7715 colour package. A natural mLLDPE may be listed under FDA 21 CFR 177.1520 or covered by EU 10/2011, but the grey colourant and any processing aids must be separately authorised, often under 21 CFR 178.3297 for colourants in polymers or the relevant EU 10/2011 annex entries. Overall migration testing and specific migration testing for pigment metals should be conducted on the finished rotomoulded part if contact is intended; the overall migration limit under EU 10/2011 is 10 mg/dm² for general plastic food-contact materials. For agricultural chemical or fuel containment, chemical resistance testing under ISO 175 or ASTM D543 must include the target fluid at the maximum service temperature, because non-polar hydrocarbons plasticize the amorphous phase and reduce stress-crack resistance. The powder should be stored away from direct sunlight and kept at ambient temperatures below 50 °C; exposed surfaces can photo-oxidise and form oxidised species that later appear as fisheyes or pinholes. Amine-based external antistatic agents should not be combined with the grey pigment package unless the supplier has verified the interaction, because basic amines can alter stabilizer and pigment chemistry and reduce long-term thermal stability.

    In rotomoulding shops, Icorene 1761 GRY 7715 is suited to grey industrial parts for which dimensional stability, low-temperature toughness, and pigment durability determine service life. Typical part classes include agricultural fluid tanks, water storage containers, off-highway fender blanks, machine covers, and outdoor enclosures. The powder can be processed on carousel, shuttle, and open-flame rock-and-roll machines. Large flat panels and parts with deep pockets require vibration during the first heating phase to prevent powder bridging. On shuttle machines with automatic powder loading, powder bulk density and dry-flow consistency directly influence shot weight reproducibility; if bridging occurs in the loading hopper, mechanical vibration or a small addition of silica anti-block up to 0.05–0.15 wt% may be used after confirming that impact properties remain within specification. The best impact-stiffness balance is usually obtained when the mould reaches the lower bound of the PIAT window and is cooled gradually to 80–100 °C before demoulding. After demoulding, the part should be checked for inner-wall porosity, colour streaks, and minimum wall thickness using ultrasonic or ball-probe methods. The grey grade is not automatically interchangeable with natural LLDPE in food-contact or high-transmission applications, and it is not a general-purpose LDPE replacement where melt strength dominates the process; but when a neutral grey, metallocene-toughened rotomoulded part is specified, the Icorene 1761 GRY 7715 defines the relevant material envelope.

    Top