Lyondellbasell Icorene 1761 Gry 7702 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRY 7702 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRY 7702 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 653590
    Density 0.918 g/cm3
    Melt Index 1.0 g/10 min
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 25.0 MPa
    Elongation At Break 600%
    Flexural Modulus 200 MPa
    Vicat Softening Temperature 95°C
    Melting Temperature 119°C
    Haze 5%
    Gloss 80%
    Coefficient Of Friction 0.20
    Dart Drop Impact 200 g

    As an accredited LyondellBasell Icorene 1761 GRY 7702 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 GRY 7702 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure industrial shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with LyondellBasell Icorene 1761 GRY 7702 metallocene linear low-density polyethylene in 25 kg bags on pallets.
    Shipping LyondellBasell Icorene 1761 GRY 7702 is shipped as non-hazardous metallocene LLDPE pellets in 25 kg bags, 1000 kg bulk bags, or bulk trucks/railcars. Store dry, cool, ventilated, away from sunlight, heat, and ignition sources. Avoid moisture, contamination, and prolonged UV exposure. Follow local transport regulations.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain ambient temperatures, use first-in/first-out stock rotation, and follow local regulations and supplier guidance. Do not store near foodstuffs or incompatible materials.
    Shelf Life Shelf life is approximately 24 months from manufacture when stored unopened in original packaging under cool, dry conditions.
    Application of LyondellBasell Icorene 1761 GRY 7702 Polyethylene, Linear Low Density, Metallocene
    Rotational moulding of secondary containment bunds for agricultural crop-protection mixing stations uses the grey 7702 powder without a post-mould paint layer. The pigment is dispersed through the polymer matrix in the supplied powder, eliminating the coating thickness variation that would otherwise interrupt the stress-crack resistance of the metallocene LLDPE. The LyondellBasell Icorene 1761 grade is specified for this service on the basis of a density in the 0.936 g/cm³ class under ISO 1183-1:2019 and a melt index near 6.0 g/10 min under ISO 1133-1:2022 at 190 °C with 2.16 kg load. Bund walls are normally moulded to 6–10 mm thickness in shuttle-type rotational moulding equipment with an arm ratio of 4:1. The oven set point is 280 °C and the internal air temperature is held at 190–200 °C for 18–22 min to densify the inner wall without generating low-molecular-mass oxidation products. The terminal component is a one-piece containment floor with integral vertical walls and a moulded-in sump, eliminating the weld seams that become leak paths in fabricated steel bunds. Environmental stress-crack resistance is assessed on pressed plaques under ASTM D1693 condition B, 100% Igepal CO-630, where metallocene-catalysed LLDPE of this density class typically exceeds 1000 h before failure. The narrow comonomer distribution suppresses the low-molecular-weight tail that swells and initiates craze growth in surfactant-laden pesticide rinse waters. Published data for this specific grey formulation in concentrated nonylphenol ethoxylate solutions above 10 wt% is limited, so immersion testing in the actual stored fluid is performed before a bund is released for service. The UV-stabilised grey compound is preferred over natural resin because crack-initiation sites are not hidden by surface whitening from an external coating.

    What limits peak internal air temperature when the powder is sintered into double-walled insulated fish tubs?

    Double-wall insulated tubs for iced catch handling are produced as a single rotomoulded outer shell with an inner liner and a polyurethane foam core inserted before the outer wall is fully densified. The limiting process variable is the residual heat retained by the inner polyethylene layer at the point the foam charge is located. If the internal air temperature exceeds 200 °C, the blowing agent in the foam can generate sufficient pressure to deform the inner wall and alter the intended 30–50 mm insulation thickness. Production-scale carousel machines therefore control the inner-wall sintering hold at 185–195 °C and air-cool the mould to 110–120 °C before the foam bung is placed. An infrared mould-cavity pyrometer is used because the external mould surface lags the internal air by 15–20 °C during cooling. Low-temperature Charpy notched impact testing under ISO 179-1/1eA at -20 °C is used to qualify the inner wall after contact with seawater ice. The grey outer skin contains the compounded weathering package of the 7702 designation; accelerated xenon-arc ageing under ISO 4892-2:2013 with a daylight filter is used to compare retained tensile elongation against unaged reference plaques. The terminal tub bodies are used for catch holding and transport after the fish are wrapped or bagged, because the specific regulatory status of this grade for direct food contact must be confirmed from the supplier documentation before unlined use. The same tub design is not recommended for continuous immersion in hot wash water above 80 °C, because the insulation core can retain heat and soften the inner wall during cleaning cycles.

    Variable-thickness play structure panels and the drop-impact retention limit

    Playground shell components such as tunnel sections, slide hoods, and climb-through panels are rotomoulded with nominal walls from 4 mm to 12 mm across a single part. The thin-wall regions require early sintering to retain shape, while the thick bosses around through-bolts must not remain un-melted at demoulding. The mould is run at 280–285 °C in an off-axis carousel machine with a 4:1 primary-to-secondary rotation ratio, and the peak internal air is held at 195 °C for not less than 15 min in sections of 8 mm or greater. Impact damage is evaluated against EN 1176-1:2017 for playground equipment, where the acceptance criterion is the absence of sharp fragments, exposed fasteners, or brittle crack propagation after impact. The metallocene structure retains ductile puncture rather than brittle fracture, which is relevant for outdoor installations in cold climates. The grey 7702 formulation avoids a post-mould coating that could mask stress-whitening at high-strain areas. The terminal parts are assembled with through-bolts and rubber washers; bolt holes are drilled rather than moulded-in, so the polymer’s orientated surface layer is not disrupted during demoulding. Weathering is evaluated under ISO 4892-3 exposure cycles, and colour variation is measured with ISO 7724-2 to determine whether the grey surface remains acceptable after extended service. The freeze-thaw cycle does not introduce plasticizer migration because no external plasticiser is used in this grade.For foam-filled marine buoyancy bodies the solid density of the moulded shell remains below the density of seawater, so even a punctured compartment retains a calculable reserve buoyancy. The outer shell is produced at 8–12 mm wall thickness in a rock-and-roll machine equipped with a 4:1 arm ratio, because the asymmetric fender geometry requires more powder residence time on the lower quadrant. The 0.936 g/cm³ density class under ISO 1183-1:2019 provides the solid-volume reserve, and water absorption after 24 h immersion under ASTM D570 is expected to remain below 0.01%, which prevents progressive weight gain during seawater service. The main process risk is the use of mineral-based external release agents, which can migrate from the mould surface and reduce adhesion of the closed-cell polyurethane foam fill. Instead, the mould is cleaned with a dry fluoropolymer release system and baked at 300 °C for 1 h after every 20 cycles to remove oxidized residues. The grey 7702 weathering package is specified for quayside UV exposure; accelerated xenon-arc testing under ISO 4892-2:2013 is used to track surface chalking. Foam-filled parts are terminal buoyancy modules and floating fender cores. They are not specified for permanent hydrocarbon immersion, and they are not load-bearing hull penetrations.

    Dimensional stability limits in modular cold-store material handling trays cycle between −30 °C and ambient washdown

    The moulded tray is a rectangular pallet box with fork pockets. The base is nominally 8 mm thick and the sidewall is 6 mm. After demoulding, parts are cooled slowly in still air at ≤5 °C/min between 140 °C and 40 °C to reduce post-mould curl. Rapid forced-air or water-mist cooling increases warpage because the outside of the thick base crystallizes before the inner layer. The linear backbone of the metallocene LLDPE gives lower free shrinkage than LDPE homopolymer, but residual stress remains constrained around the fork pockets. Trays are evaluated under ISO 8611-1:2011 for pallet racking performance, and low-temperature flexural behaviour is measured under ISO 178:2019 at −30 °C. The material is accepted for cold-store service when the stress-strain curve remains non-brittle. The grey 7702 compound is not blended with mineral fillers for this application because filler increases component density and reduces low-temperature impact. Terminal use is returnable dunnage in automated freezer warehouses, with washdown temperatures not exceeding 80 °C. The temperature limit prevents thermal relaxation of the moulded-in base and maintains stacking interlock within the ±2 mm design tolerance. The moulding must be supported on a flat surface during cooling because unsupported edges distort beyond the tolerance interval.

    When 10–20 wt% post-industrial regrind is introduced into the mould charge without reformulation of the UV package

    Plants running returnable agricultural containers sometimes add clean in-house regrind from rejected parts. The regrind is coarse-ground through a 10 mm screen and then pulverized to a top size of 500 µm before dry blending. At 10–20 wt% regrind, mould charge flow remains acceptable in a bulk-powder hopper with a 50 mm vibratory feed port. Above 25 wt%, the melt flow rate shifts because the regrind contains oxidized surfaces and a slightly increased crystalline fraction from the previous cooling history. The processing window narrows by approximately 5–8 °C, and this must be verified by measuring melt flow rate under ISO 1133-1:2022 and oxidative induction time under ISO 11357-6:2018 at 200 °C. A drop in oxidative induction time below 20 min indicates excessive shear history in the original moulding cycle. The terminal use for regrind-containing mould charge is non-critical agricultural covers and dunnage; it is not specified for chemical containment unless impact and environmental stress-crack resistance are re-qualified under ASTM D1693 and the relevant end-use standard. No additional acid scavenger is required at the 10–20 wt% level if the regrind is dry and stored below 0.05% moisture. Higher moisture requires pre-drying in a desiccant hopper at 70 °C for 3 h before pulverizing, because steam bubbles at the inner wall cause surface pinholes during the densification stage.
    Free Quote

    Competitive LyondellBasell Icorene 1761 GRY 7702 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 GRY 7702 is a metallocene-catalysed linear low density polyethylene supplied as a pre-coloured gray rotational moulding powder. The designation combines the base resin grade 1761 with the colour package code GRY 7702; the base polymer is an ethylene copolymer produced using a metallocene catalyst system. This places the material in the mLLDPE rotomoulding class, distinct from conventional Ziegler–Natta LLDPE and from HDPE rotational moulding grades. Published data for this specific pre-coloured configuration are limited; the Icorene 1761 base resin class is reported with a density of approximately 0.938 g/cm³ when measured to ISO 1183-1 and a melt mass-flow rate of approximately 5.0 g/10 min at 190 °C under 2.16 kg when measured to ISO 1133-1. These values refer to the base resin class and do not replace the certificate of analysis for the pigmented GRY 7702 variant. The product is intended for rotational moulding of thick-walled hollow parts in which low-temperature toughness, chemical resistance, and outdoor durability are performance requirements.

    The supplied form is a powder rather than pellets. In rotational moulding, the powder must sinter, densify, and consolidate at low pressure inside a heated mould, so particle-size distribution, bulk density, and dry-flow behaviour control wall thickness uniformity more directly than melt flow alone. Incoming powder should be checked by sieve analysis according to ASTM D1921 and bulk density according to ASTM D1895. Fine particles below 75 µm can improve surface appearance but may increase dust and reduce bulk density, while oversize particles above 500 µm may require extended oven residence time to fully melt in thick sections. A consistent powder bed is critical for bubble removal because the low-shear rotational moulding process cannot rely on high-shear dispersion to break up porosity.

    What Distinguishes the Metallocene Architecture of Icorene 1761 GRY 7702 from Conventional LLDPE and HDPE Rotomoulding Grades?

    The principal difference originates in the metallocene catalyst system. Metallocene catalysis produces a narrower molecular weight distribution and a more uniform intermolecular comonomer sequence than conventional Ziegler–Natta LLDPE. This structural regularity translates into measurable differences in mechanical behaviour: at comparable density, mLLDPE grades typically show better low-temperature impact resistance and environmental stress-cracking resistance when measured by ISO 6603-2 and ASTM D1693. The same architecture, however, reduces shear thinning relative to broad-distribution LLDPE. In rotational moulding, where shear rates are low, the loss of shear thinning is usually subordinate to sintering and thermal stability; in high-shear extrusion, the same characteristic may generate higher torque or melt pressure.

    Compared with HDPE rotomoulding powders, the Icorene 1761 class carries a lower density and generally lower flexural modulus. A part moulded from this material will normally exhibit greater ductility and environmental stress-crack resistance than an equivalent HDPE part, but it may require ribbing, thicker walls, or a revised structural design to achieve the same load-bearing stiffness. Compared with conventional Ziegler–Natta LLDPE, the metallocene structure can reduce the number of high-molecular-weight tails, altering bubble dissolution during densification. This is why the grade is processed with a narrower peak internal air temperature band than some Ziegler–Natta powders. The trade-off is not a defect but a process characteristic: the mLLDPE grade demands closer thermal control in exchange for higher toughness.

    Specification methods for this product are organized around the material class and the rotomoulding process. The following table summarizes the standard designations relevant to incoming powder inspection and moulded-part qualification. The values for the base resin are batch-dependent and must be read from the supplier’s product data sheet and certificate of analysis; the pre-coloured gray powder may shift some values because the pigment and stabilizer package adds mass and modifies crystallisation behaviour.

    Property categoryStandard or test methodRelevance to Icorene 1761 GRY 7702
    DensityISO 1183-1Determines final part mass and toughness/stiffness balance; pre-coloured gray may show a slight shift compared with natural base powder.
    Melt mass-flow rateISO 1133-1 at 190 °C and 2.16 kgConfirms molecular weight class and batch-to-batch consistency; rotomoulding powders in this family are typically in the medium-flow range.
    Tensile propertiesISO 527-2Provides yield stress and elongation data for design comparisons; specimens are usually compression-moulded from the powder.
    Environmental stress-cracking resistanceASTM D1693Indicates long-term resistance to stress cracking in tanks and packaging exposed to surfactants, acids, or agricultural chemicals.
    Puncture and falling-dart impactISO 6603-2 or ASTM D5628Measures ductile failure resistance at low temperature; important for outdoor and transport applications.
    Powder particle-size distributionASTM D1921Controls powder bed sintering rate and surface finish; excessive fines or oversize particles can increase scrap.
    Powder bulk densityASTM D1895Affects mould filling and part wall thickness consistency.

    Because published data for the pigmented configuration are limited, the above standards should be used to generate internal process capability data on the production moulding line. A qualified processor will establish lower and upper control limits for melt mass-flow rate and particle size after three consecutive batches rather than relying solely on the supplier’s nominal value. This is particularly important for gray powder because recycled regrind from trimmed parts can contain a different pigment concentration than virgin powder if grinding is not controlled.

    When the Gray Pigment Package Alters Heating Rate in a Rotomoulding Oven

    A pre-coloured gray powder absorbs radiant heat differently from natural or white powders. The pigment package in GRY 7702 may include inorganic pigments such as titanium dioxide and carbon-bearing gray pigments; these inorganic particles modify the infrared absorption of the powder bed. In a gas-fired carousel or shuttle rotational moulding machine, the practical result is that oven residence time and oven setpoint temperature cannot be transferred blindly from a natural powder. Heating rate must be determined from the internal air temperature curve obtained with a data logger placed inside the mould. The process target for the moulded mLLDPE class is typically a peak internal air temperature between 180 °C and 200 °C, but the exact value depends on wall thickness, oven temperature, mould material, and pigment heat absorption. A lower peak internal air temperature may leave porosity at the inner wall because the powder has not completed densification; a higher peak may accelerate thermo-oxidative degradation and reduce environmental stress-cracking resistance.

    The pigmented grade also influences cooling and demoulding. Gray parts can retain heat longer than natural parts in some mould configurations, particularly when the mould is fabricated from cast aluminium or stainless steel sheet. If demoulding occurs before the internal temperature falls below the crystallization range, the part can exhibit warpage, shrinkage variation, or stress whitening at sharp corners. Mould release timing should therefore be based on the cooling curve and part temperature, not on a fixed cooling fan interval. In practice, processors running a 3.0 m shuttle machine with forced-air cooling have reported the need to revalidate demoulding time when switching from natural to pre-coloured gray because the thermal emissivity of the outer surface changes. Published data for this specific configuration are limited, but the operational observation is consistent with radiative heat transfer principles.

    Pigment particles can also act as crystallization nuclei. The crystallization temperature of the pigmented grade may be slightly higher than that of the natural base powder, which can shorten the cooling portion of the cycle but increase shrinkage non-uniformity in thick sections. Differential scanning calorimetry according to ISO 11357-3 can quantify the shift in crystallization onset. For parts with wall thickness above 10 mm, a slower heat ramp or lower oven setpoint may be required to prevent the outer surface from reaching full densification long before the inner layer consolidates. If the outer skin remains above 200 °C while the core is still porous, surface oxidation and inner-wall porosity can occur in the same part.

    Another process conflict arises with regrind. Rotational moulding generates scrap from cut-outs and rejected parts; gray regrind must be blended in consistent proportions with virgin powder or the pigment concentration and stabilization level will vary, causing colour drift and possible changes in heat absorption. A common industrial practice is to limit regrind addition to 10–20 % depending on part specification and to dry the blend when storage humidity exceeds 60 % RH. Polyethylene itself has low moisture absorption, but condensation on cold powder introduces surface water that can form pinholes in thick sections. If the powder has been stored in an unheated silo and then brought into a warm moulding hall, a hopper dryer or dry-air purge at 60 °C is used before charging the mould.

    Application scenarios for Icorene 1761 GRY 7702 are centred on rotational moulding of thick-walled, hollow parts that require a balance of low-temperature toughness, chemical resistance, and outdoor durability. Typical examples include agricultural spray-tank liners, secondary containment basins, industrial floats, equipment housings, and covers exposed to weathering. In these applications, the expected performance is not established by the polymer class alone; the finished part must be tested under the relevant standard—for example, ASTM D1998 for polyethylene storage tanks or end-use loading tests specified by the equipment manufacturer. The grade is not intended for injection moulding, blown film, or high-pressure pipe extrusion, because the supplied powder morphology and heat stabilizer package are formulated for low-shear rotomoulding.

    Tooling design affects material performance more than the polymer specification sheet. In rotomoulding, the powder must reach all mould extremities; deep pockets, ribs, and kiss-offs require venting and a powder flow path that avoids static bridging. Moulds with narrow internal channels may need external heat shields or deflectors to prevent over-cured outer surfaces while the inner core reaches the target peak internal air temperature. The mLLDPE grade’s narrower processing window means that ovens with poor temperature uniformity—more than ±10 °C across the heating chamber—can create inconsistent part properties. Processors should map oven temperature uniformity and adjust burner settings before qualifying the gray powder for production.

    Regulatory Coverage, Powder Handling, and Known Incompatibilities

    Food-contact and potable water approvals cannot be assumed for the pre-coloured grade. The base polyethylene may be covered by FDA 21 CFR 177.1520 and, where relevant, EU Regulation (EU) No 10/2011; however, the gray pigment and stabilizer package requires a separate conformity statement from the supplier. Users requiring REACH or RoHS declarations must specify the complete designation Icorene 1761 GRY 7702 because colour concentrates can contain substances that are absent from the natural base resin. The grade is not formulated for use in medical implants or pharmaceutical packaging unless explicitly validated for that application.

    Known incompatibilities include high-shear processing and arbitrary blending. The powder is not optimized for compounding on a twin-screw extruder; it can be used in compounding only with a documented heat stabilizer package and at controlled throughput. Melt temperatures above 240 °C should be avoided unless the stabilizer system is designed for such conditions, because prolonged high-temperature exposure may generate oxidation products that reduce ESCR. Avoid combining the powder with amine-based additives or masterbatches not approved by the polymer supplier; some hindered amine light stabilizer formulations can interact with the existing stabilizer package and shift colour or reduce long-term heat stability. When external mould-release agents are used, they should be applied sparingly and removed from the powder path; silicone-based release agents can contaminate the powder bed and create localized coalescence defects.

    Moisture exposure at relative humidity above 60 % is not a polymer degradation pathway, but it can create condensation-induced pinholes. The powder should be stored in a dry silo or super-sack at 5–30 °C, away from direct sunlight and welding fumes. Welding fumes containing zinc oxide or ammonia can contaminate the powder surface and alter surface tension. If the powder is conveyed by compressed air, the air supply should be oil-free and dried to a dew point below −20 °C to avoid introducing contaminants. Pressure-bearing parts and pressure vessels require additional design validation, including burst testing according to the applicable national or industry pressure-vessel standard, and are outside the scope of the material supplier’s standard data sheet.

    Top