| HS Code | 826407 |
| Density | 0.917 g/cm³ |
| Melt Index | 1.0 g/10 min (190°C/2.16 kg) |
| Color | Grey |
| Tensile Strength At Yield | 10.0 MPa |
| Tensile Strength At Break | 43.0 MPa |
| Elongation At Break | 600% |
| Tensile Modulus | 200 MPa |
| Dart Drop Impact | 250 g |
| Elmendorf Tear Strength | 200 g |
| Haze | 4% |
| Gloss | 80% |
| Melting Point | 120°C |
| Vicat Softening Point | 100°C |
As an accredited LyondellBasell Icorene 1761 GRY 7203 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg polyethylene-lined bags, 40 bags per pallet (1,000 kg total), for LyondellBasell Icorene 1761 GRY 7203 metallocene LLDPE. |
| Container Loading (20′ FCL) | 20′ FCL container loading: LyondellBasell Icorene 1761 GRY 7203 metallocene LLDPE pellets, palletized, shrink-wrapped, and securely braced for ocean shipment. |
| Shipping | LyondellBasell Icorene 1761 GRY 7203 is a non-hazardous metallocene linear low-density polyethylene resin. It is not regulated for transport by DOT, IMDG, IATA, or ADR. Typical shipping: pellets in 25-kg bags, bulk bags, octabins, or bulk trucks/railcars. Store cool and dry; avoid moisture, contamination, and direct sunlight. |
| Storage | Store Icorene 1761 GRY 7203 polyethylene resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or octabins tightly closed to prevent moisture, dust, and contamination. Avoid strong oxidizers and excessive stacking. Protect from UV exposure and physical damage. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically 24 months when stored unopened in original packaging, in a cool, dry area away from direct sunlight and heat. |
Double-wall secondary containment sumps manufactured from Icorene 1761 GRY 7203 on three-arm carousel machines are typically produced at a charge weight calculated for a nominal wall of 6.0–8.0 mm in the inner shell. The compliance frame for static thermoplastic sumps under EPA 40 CFR 112 secondary containment rules draws on ASTM D1998-15 for upright polyethylene tanks and EN 13575:2012 where European site directives apply; suitable joints are tested by the tank manufacturer to ASTM D638-14 Type IV at a crosshead speed of 50 mm/min. Formulation is held at 100 wt% of the supplied 35-mesh powder; no pigment dispersion is added because GRY 7203 contains the color and UV package, and regrind from the same colored grade is capped at 10 wt% to avoid lowering environmental stress crack resistance. The downstream process uses fabricated aluminum molds preheated to 60–80°C, charged at room temperature, and heated in a forced-convection oven at 280–300°C until internal air temperature reaches 195–205°C. The critical process conflict is the inside corner: if the mold is removed before the internal air has held at 200°C for at least 8–12 minutes, the powder at the corner coalesces but does not fully densify, yielding microporosity that later propagates under hydrostatic cycling. Cooling is staged at 0.5–1.0°C/min through the crystallization plateau of 115–120°C, then accelerated below 60°C; faster cooling in this interval has been observed on shuttle machines to produce warpage beyond 2 mm on 1,200-mm flange spans. Terminal products include sump basins with conical bottoms, pump plinths, acid drip trays, and double-wall interstitial leak-detection basins.
In arid-zone fertigation reservoirs, the grade’s metallocene short-chain branching distribution provides an improvement in environmental stress crack resistance over conventional Ziegler-Natta LLDPE when exposed to dilute ammonium nitrate and urea solutions at 35–45°C. Chemical resistance is screened under ISO 175:2010 using 28-day immersion; UV retention is evaluated by ISO 4892-2:2013 cycles with UVA-340 lamps and wetting, referencing the Florida outdoor exposure correlation in ASTM D1435 only for natural weathering. The formulation is pressed to 100 wt% supplied powder; if flow-line scrap is reground, it is blended at a maximum 15 wt% and only from the same gray lot, because dry blending of clear or uncolored mLLDPE regrind alters the total UV absorber concentration and shifts the weathering failure time at the weld line. Production on shuttle rotational molding equipment uses sheet steel molds with a rotation ratio of 4:1 on the minor axis and 1:1 on the major axis, oven set point 280–310°C, and internal air temperature of 195–200°C. The process window is deliberately narrowed to avoid over-cure: above 210°C internal air, the pre-compounded hindered amine stabilizer package may degrade more rapidly, and surface oxidation appears as yellowing or micro-crazing after 1,000 h of QUV exposure. Molding is terminated by forced-air cooling to 80°C before demolding. Terminal articles include horizontal sprayer tanks from 1,000 L to 20,000 L, nurse tanks for drip irrigation, acid fertigation dosing tanks with secondary containment, and rainfall capture cisterns. Strong oxidizing agents and aromatic solvents above 40°C are not recommended because the chemical resistance classification drops below the required retention threshold.
Because marine flotation modules are subjected to hydrostatic flexure and low-temperature impact, the specification priority shifts from tensile yield to dart impact retention after seawater immersion. The applicable mechanical qualification includes ASTM D256-23 Izod impact at -20°C on notched specimens cut from molded plaques and ASTM D1693-15 environmental stress crack resistance under Condition C with a 10% Igepal CO-630 solution at 50°C; marine acceptance is typically documented through ISO 178:2019 flexural modulus measurements taken on specimens machined parallel and perpendicular to the mold parting line. Formulation practice keeps the supplied GRY 7203 powder at 100 wt%, with no addition of calcium carbonate or talc because inorganic fillers reduce low-temperature impact and increase water absorption at the surface. The rotational molding sequence begins with a charge of 35-mesh powder into a cast aluminum mold at 25–35°C; the mold rotates biaxially while the oven air temperature is held at 285–305°C until internal air reaches 200–205°C. To minimize residual stresses in hull shells, cooling is conducted in still air inside the oven at 0.3–0.6°C/min down to 80°C, then outside with forced air; this is slower than standard tank cooling and is critical for maintaining the low-temperature impact of the outer skin. Terminal products include mooring buoy shells, pontoon floats for floating walkways, fender sleeves, and cable route marker buoys. The operational boundary is that continuous flexure of a fully filled pontoon at temperatures below -25°C may exceed the cumulative fatigue capability of unfilled polyolefin skins, and published data for this specific configuration is limited.
Outdoor telecommunication plinths and cable joint housings demand dimensional stability across a -30°C to +60°C surface temperature range while carrying equipment loads. The governing standards are IEC 62208:2023 for empty enclosures used in low-voltage distribution, ISO 4892-2:2013 for weathering of the gray outer skin, and ASTM D648-18 deflection temperature under flexural load at 0.455 MPa. Formulation is maintained at 100 wt% of the supplied powder; because brass or stainless thread-forming inserts are installed post-molding, no internal release agent is used, and regrind content above 8 wt% is avoided in the insert bosses because microvoids from unmelted regrind particles degrade pull-out strength. Molding on carousel equipment uses steel molds with aluminum inserts in the boss areas; the oven set point is 275–295°C and the internal air temperature is kept at 195–202°C. The dimensional risk is asymmetric shrinkage: the wall thickness varies from 5 mm in the base to 10 mm at the flange, so the part is held in the closed mold at 60–70°C for 20–30 minutes after cooling to stabilize the plinth base before insert installation. Terminal articles include concrete-base plinths, fiber splice pit liners, antenna cowls, and meter box bases. The product is not appropriate where regulatory specifications demand UL 94 V-0 flame retardancy because unfilled polyethylene grades burn readily.
For granular bulk handling hoppers and abrasive discharge liners, the key processing issue is not chemical exposure but the resistance of the inner wall to erosive wear during repeated gravity flow of angular particles. Wear-screening data on rotomolded mLLDPE liners are generated by the rotating drum method in ISO 4649:2017 for comparison only, with tensile yield stress measured under ISO 527-2:2012 at 23°C and 50 mm/min. The powder charge is 100 wt% supplied GRY 7203; fine quartz or ceramic anti-slip additives are not used because dry blending modifies the melt coalescence rate and creates surface roughness without improving bulk abrasion resistance. Where discharge lips are reinforced, the molder may add 8–10 wt% of same-grade regrind from punched or trimmed sections, but only after sieving through a 500 μm screen to remove irregular particles that would otherwise persist as visible pinholes at the inner wall. The production process uses rock-and-roll machines with steel molds, an oven set point of 285–305°C, and a peak internal air temperature of 200–208°C. A critical process boundary is the transition from the thin wall to the thick discharge lip: if the mold does not dwell at peak internal air temperature for 10–15 minutes, the thick section retains unmelted powder grains that later cause premature wear at the liner joint. Terminal articles include dockable hoppers, discharge chute liners, flexible intermediate bulk container handling trays, and abrasive media collection bins.
Industrial scrap trays and sump liners are produced from the grade when leachate pH falls in the range of 4–9 and operating temperature does not exceed 45°C. The compliance approach uses ASTM D543-21 for chemical resistance of plastics after immersion in representative leachate, ASTM D746-20 brittleness temperature for low-temperature handling in unheated warehouses, and ASTM D638-14 tensile property retention after 1,000 h weathering. Formulation is set at 100 wt% of the premixed gray powder; black conductive masterbatch or metallic additives are not added because they increase melt viscosity and disrupt the powder consolidation at the mold surface. Processing on shuttle machines uses cast aluminum molds with a draft angle of 3–5°, oven temperature 280–300°C, and internal air temperature 195–203°C. The process is run to a higher internal air endpoint than thin-walled tanks because tray bases can exceed 15 mm in reinforced ribs; a dwell of 15–20 minutes at peak internal air temperature is used to sinter the rib core, and the mold is cooled at 0.8–1.2°C/min to avoid sink marks. Terminal products include battery washdown trays, pallet sumps, leachate collection basins, and drum containment trays. The polymer is unsuitable for continuous immersion in concentrated acids, ketones, or chlorinated solvents; chemical suitability must be confirmed on the specific process stream under ISO 175:2010 before service.
Competitive LyondellBasell Icorene 1761 GRY 7203 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 GRY 7203 is a metallocene-catalyzed linear low-density polyethylene (mLLDPE) rotational molding powder supplied with a grey 7203 pigment package. The 1761 designation corresponds to a base resin having a nominal density of 0.935 g/cm³ and a melt flow rate of 6.5 g/10 min when measured at 190°C under 2.16 kg load in accordance with ISO 1133-1:2022. The grade is intended for rotational molding of hollow parts requiring a balance of stiffness, low-temperature impact resistance, environmental stress-cracking resistance, and dimensional stability. Compared with conventional Ziegler-Natta LLDPE rotomolding powder, the metallocene architecture yields a narrower molecular weight distribution and more uniform comonomer placement, which reduces part warpage and improves mechanical property consistency at equivalent density. Because the 7203 grey designation incorporates a pigment package, density and melt rheology may shift slightly from the unpigmented base resin; lot-specific certificates of analysis govern exact processing parameters.
Typical uses include agricultural liquid containment, outdoor equipment housings, material handling bins, recreational parts, and general industrial hollow moldings. The product is differentiated from black UV-stabilized rotomolding grades and from high-density polyethylene rotomolding powders by its combination of density, metallocene-derived toughness, and grey coloration. Where the grey pigment package is used for outdoor service, weathering performance must be verified separately because the 7203 grey does not provide the same UV screening as a filled black compound.
The primary difference is the catalyst system and the resulting molecular architecture. Metallocene catalysis produces a narrow molecular weight distribution and, more importantly for polyolefin copolymers, a statistically more uniform distribution of short-chain branches across the molar-mass range. In conventional Ziegler-Natta LLDPE, comonomer tends to incorporate preferentially into the lower-molecular-weight fraction, while higher-molecular-weight chains remain relatively linear. This heterogeneity creates density and crystallinity gradients that can appear as warpage and localized brittle regions in rotomolded parts. The homogeneous branching of Icorene 1761 GRY 7203 increases tie-chain density and reduces the concentration of low-melting extractable waxes.
The property consequences are measurable with standard methods. Environmental stress-cracking resistance, evaluated under ASTM D1693-21 condition B with 100% Igepal, is typically above 1000 h for the base resin, which is substantially higher than many Ziegler-Natta LLDPE grades of equivalent density. Low-temperature impact by the ARM method is improved because homogeneous short-chain branching delays brittle fracture at -40°C. Shrinkage is more isotropic, so parts removed from symmetrical molds show less out-of-plane distortion than comparable Ziegler-Natta powders. This dimensional stability is significant in deep-draw rotational molding tools and in parts with varying wall thickness.
Compared with high-density polyethylene rotomolding powders having densities near 0.945–0.955 g/cm³, the 0.935 g/cm³ density of Icorene 1761 GRY 7203 sacrifices tensile modulus but provides higher ductility and a broader service temperature window before crack initiation. Compared with low-density polyethylene homopolymers, the linear molecular structure provides higher tensile strength and improved creep resistance. The 7203 grey variant is not equivalent to black rotomolding compounds; its weathering resistance and UV screening depend on the pigment type and loading in the final part.
Published data for the specific 7203 grey configuration is limited for some organoleptic and outdoor aging endpoints. The base-resin data should not be assumed to transfer unchanged to thin-walled parts below 3 mm wall thickness, where cooling rates and surface-area effects can alter crystallinity and impact response.
Rotomolded tanks for agricultural liquid storage and water handling use the grade because environmental stress-cracking resistance is critical at weld lines, insert regions, and fittings. The base resin ESCR exceeding 1000 h under ASTM D1693 condition B provides a useful ranking value, but system-level performance depends on wall thickness, residual stress, service temperature, and the specific chemical environment. For potable water applications in North America, NSF/ANSI/CAN 61 listing is a device-level approval; a resin with FDA 21 CFR 177.1520 olefin polymer status contributes only one part of the compliance dossier. The grey 7203 pigment must also meet the applicable colorant requirements in the jurisdiction of use.
Outdoor recreational parts and equipment housings use the grade because the metallocene structure reduces part-to-part warpage after cooling and improves surface finish after demolding. Published data for the 7203 grey configuration under long-term UV weathering is limited; processors should commission accelerated aging per ISO 4892-2 or ASTM D2565 when the part is exposed beyond incidental outdoor service. The weathering life depends more on the stabilizer and pigment package than on the base mLLDPE resin.
On single-arm carousel machines or shuttle-type rotational molders, the grade is typically processed with oven setpoints between 280°C and 300°C and a peak internal air temperature target of 190–205°C. Rotational molding powders with a density of 0.935 g/cm³ must fully densify before oxidative degradation becomes measurable; underheating leaves inner-surface pinholing, while overheating above 210°C can cause yellowing and a loss of low-temperature impact. The grey pigment may alter radiant heat absorption slightly. Processors should map peak internal air temperature with an internal thermocouple or infrared non-contact sensor positioned at the mold’s slow-moving center, rather than relying solely on oven dwell time.
Particle size distribution and dry flow are controlling variables. Rotomolding grades are ground to sub-500 µm particles, commonly assessed by ASTM D1921 or equivalent sieve analysis. Fine particles improve surface definition but can increase electrostatic adhesion and reduce powder flow; coarse particles reduce wall-thickness uniformity. Because metallocene resins have a narrow molecular weight distribution, their melt viscosity is less shear-thinning than broad-MWD Ziegner-Natta LLDPE. Densification therefore occurs by sintering and coalescence rather than by low-viscosity wetting. This requires consistent biaxial rotation speed, typically in the 4:1 to 8:1 rotation-ratio range, to maintain melt distribution across the mold surface.
Cooling rate determines shrinkage, crystallinity, and warpage. Forced-air cooling after demolding at or below 80°C is often used to reduce cycle time, but high cooling rates can increase residual stress. For grey 7203 parts with variable wall sections, slow ambient cooling and controlled mold-release use are recommended to avoid sink marks and ejection stress. The powder should be stored dry; if condensation occurs after outdoor storage at relative humidity above 60%, moisture should be checked by ISO 15512 Method A and the powder dried before charging. No specific moisture threshold is given in the standard datasheet for this grey variant, so processor validation is required.
Table 1 lists representative properties for the Icorene 1761 base resin and expected shifts for the 7203 grey powder. These values are engineering references, not lot guarantees, and must be confirmed against the certificate of analysis.
| Property | Test method | Base resin typical value | GRY 7203 expected shift or range |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.935 g/cm³ | 0.936–0.938 g/cm³ |
| Melt flow rate | ISO 1133-1:2022, 190°C/2.16 kg | 6.5 g/10 min | 6.0–7.0 g/10 min |
| Tensile yield stress | ISO 527-2:2012, type 1B, 50 mm/min | 18 MPa | 17–20 MPa |
| Tensile modulus | ISO 527-2:2012 | 620 MPa | 600–650 MPa |
| Flexural modulus | ISO 178:2019, 2 mm/min | 550 MPa | 530–580 MPa |
| Tensile elongation at break | ISO 527-2:2012 | >600% | >500% |
| Vicat softening temperature | ISO 306:2022 A50 | 122°C | 120–124°C |
| Environmental stress-cracking resistance | ASTM D1693-21, condition B, 100% Igepal | >1000 h | >800 h |
| ARM low-temperature impact at -40°C | ARM Low-Temperature Impact Method | base resin >30 J | grey-specific data limited; verify |
The main difference from conventional Ziegner-Natta LLDPE rotomolding powder is not necessarily density or melt flow but the property balance. The metallocene grade retains ESCR and low-temperature ductility while reducing warpage during cooling. Published data for the 7203 grey configuration’s low-temperature impact as a compounded powder is limited; the base-resin value should not be assumed for thin-walled parts below 3 mm.
Warpage in rotomolded mLLDPE parts is driven by non-uniform cooling and temperature gradients across the mold during sintering. The grey 7203 pigment package can produce differential heating in thin and thick sections because thin sections reach peak internal air temperature earlier and may be quenched before thicker walls consolidate. Tooling with uniform wall thickness and consistent mold-surface emissivity is therefore required. Processors use thermocouple arrays and infrared pyrometry to map temperature distribution, and published technical bulletins recommend that the coldest point of the mold reach at least the lower peak internal air temperature threshold before oven exit.
Demolding forces must be controlled because mLLDPE parts below 60°C exhibit lower rigidity than HDPE rotomolding grades. Ejection against undercuts can distort the part. Mold release use is acceptable with zinc stearate or silicone-based releases, but compatibility with food-contact requirements must be revalidated if the part is used in food-contact service. Reprocessed regrind from the same grade may be introduced at low percentages; addition of HDPE regrind alters density, ESCR, and impact balance and should be evaluated against ASTM D1693 and ISO 179-1:2023 Charpy impact before production use.
Chemical exposure at service temperatures above 40°C can reduce environmental stress-cracking resistance. Grease, strong acids, oxidizing agents, and polar organic solvents should be tested according to ASTM D543 or ISO 4433-1:2019 using the actual part thickness and residual stress level. Reliance on room-temperature ESCR data alone is insufficient when the part contains molded-in inserts or sharp geometry that concentrates service stress.
| Designation | Requirement or status | Notes |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer may comply subject to conditions A–H | Grey 7203 pigment must meet applicable colorant requirements |
| EU Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² | Material-specific verification required for food contact |
| REACH (EC) No 1907/2006 | Polymer is exempt from registration; monomers and pigments are subject | SDS required for the compounded powder |
| RoHS Directive 2011/65/EU | Pb, Hg, Cd, Cr(VI), PBB, PBDE thresholds | Verify pigment lot for heavy metals |
| NSF/ANSI/CAN 61 | System-level potable water contact approval | Base resin alone does not confer certification |
| ASTM D543 or ISO 4433-1:2019 | Chemical immersion resistance | Required for chemical storage applications |
The grey 7203 color variant does not inherently carry food-contact or outdoor-weathering certification; each commercial part must be validated at the system level. This grade differs from black rotomolding powders in that the grey pigment package provides limited UV screening unless additional stabilizer is incorporated. In rotational molding, the operational boundary is defined less by the resin alone than by tooling temperature uniformity, cooling control, and pigment-induced lot-to-lot shifts.