Lyondellbasell Icorene 1761 Grn 6654 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 GRN 6654 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 GRN 6654 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 375597
    Density 0.918 g/cm³
    Melt Flow Rate Mfr 1.0 g/10 min (190°C/2.16 kg)
    Melting Temperature 119 °C
    Vicat Softening Temperature 100 °C
    Tensile Strength At Yield 9.00 MPa
    Tensile Strength At Break 24.0 MPa
    Tensile Elongation At Break 500%
    Flexural Modulus 0.240 GPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g

    As an accredited LyondellBasell Icorene 1761 GRN 6654 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 GRN 6654 is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for safe transport.
    Container Loading (20′ FCL) 20′ FCL: LyondellBasell Icorene 1761 GRN 6654 metallocene linear low-density polyethylene in 25 kg bags, palletized, stretch-wrapped, approx. 20 MT.
    Shipping LyondellBasell Icorene 1761 GRN 6654 is a non-hazardous, solid metallocene LLDPE resin supplied as pellets. Standard shipping includes 25 kg polyethylene bags, palletized and stretch-wrapped, or bulk trucks/railcars. Protect from moisture, UV, and contamination; store cool and dry. No special DOT/UN hazard classification required.
    Storage Store LyondellBasell Icorene 1761 GRN 6654 polyethylene resin in original, closed bags or containers in a cool, dry, well-ventilated area. Protect from sunlight, heat, moisture, and contamination. Keep away from ignition sources and oxidizing agents. Minimize dust and static; ground equipment. Avoid prolonged elevated temperatures, ensure intact packaging, stable pallets, first-in-first-out rotation, and follow SDS/local regulations.
    Shelf Life Store in a cool, dry, well-ventilated area; shelf life is 24 months from date of manufacture in original unopened packaging.
    Application of LyondellBasell Icorene 1761 GRN 6654 Polyethylene, Linear Low Density, Metallocene

    Above-ground storage vessels for aqueous process chemicals—including sodium hydroxide at concentrations up to 50% at ambient temperature, ferric chloride at 38–42%, and sodium hypochlorite at 10–15% available chlorine—are rotationally moulded from a nominal 35-mesh powder of Icorene 1761 GRN 6654 where supplier-approved chemical resistance data under EN 13575:2012 indicates a satisfactory rating for the specific chemical, concentration, and service temperature. The dry blend for single-wall tanks is typically 100 phr of the metallocene LLDPE compound, 0.2–0.5 phr hindered phenolic antioxidant, 0.5–1.0 phr high-molecular-weight HALS stabiliser for outdoor UV resistance, and 0.05–0.2 phr zinc stearate as internal mould release. If pulverised powder is stored in an unheated silo at relative humidity above 60% for more than 24 h, pre-drying at 70–80°C for 1–2 h is required before charging the mould; otherwise steam pinholes tend to appear in the parting-line region and around the vent port. The production route is biaxial rotational moulding on a turret-type three-arm machine with a major-to-minor axis speed ratio of 4.0:1, major-axis speed of 4–8 min⁻¹, oven set points between 285°C and 310°C, and a peak internal air temperature target of 210–220°C for wall sections of 6–12 mm. This is the critical processing boundary: when PIAT exceeds 220°C on production equipment, the inner surface has shown oxidative discoloration, microvoid formation, and a measurable reduction in environmental stress-crack resistance under ASTM D1693-15, while PIAT below 195°C leaves unmelted powder and pinhole paths at the parting-line weld. Sieve analysis should show no more than 2% retention on a 35-mesh screen; a higher coarse fraction has caused pinholes at wall thicknesses below 5 mm. The moulding is cooled with forced air for 10–15 min until the mould surface is below 90°C, followed by water spray; excessively rapid water cooling has produced warpage in flat top sections on 2,000 L and larger tanks. Terminal articles produced under this scenario include 1,000–10,000 L cylindrical vertical storage tanks, double-wall containment basins, dosing and day tanks, and rotationally moulded bunded pallets for chemical dispensing.

    Potable Water Tanks and the NSF/ANSI/CAN 61 Extraction Protocol

    Where the moulded vessel is intended for contact with drinking water, the formulation is restricted to additives that are individually listed under FDA 21 CFR §177.1520 for polyolefins and EU Regulation 10/2011, and the finished article must be tested under NSF/ANSI/CAN 61 for extraction of metals, volatile organic compounds, and residual additives. A typical dry blend is 100 phr Icorene 1761 GRN 6654, 0.2–0.4 phr phenolic antioxidant, 0.5–1.0 phr UV stabiliser, and 0.05–0.15 phr calcium stearate acid scavenger; no zinc stearate internal mould release is used because potable water specifications frequently restrict zinc extraction under NSF/ANSI/CAN 61 and local plumbing codes. The process is biaxial rotational moulding, but the PIAT is held tighter at 205–215°C and the oven set point is limited to 290–305°C to reduce oxidative degradation products that contribute to taste and odour. Wall thicknesses range from 5–8 mm; demoulded tanks are post-cured in a segregated clean area before the NSF/ANSI/CAN 61 exposure test, and production lines use a closed-loop cooling water system to prevent external contamination of the inner surface. Terminal product types include 500–5,000 L loft tanks, underground or basement cisterns, emergency water storage tanks, and header tanks for rural gravity-fed distribution.

    Tractor-mounted saddle tanks and trailed sprayer tanks are exposed to repeated immersion in glyphosate formulations, emulsifiable concentrates, and liquid fertiliser mixtures; the applicable compliance base is EN 13575:2012 for chemical storage tanks, with the sprayer installation bearing environmental requirements under ISO 16119-2:2013. The dry formulation uses 100 phr of the base compound, 0.3–0.5 phr HALS, 0.1–0.25 phr phosphite antioxidant, and 1.5–3.0 phr UV absorber masterbatch for tropical outdoor service, because wall sections below 5 mm on saddle tanks are more sensitive to UV embrittlement than thick chemical storage tanks. Moulding is performed with threaded inserts and moulded-in baffle ribs on a shuttle-type rotational moulder; inserts are preheated to 120–150°C before charging to reduce pull-out stress at the thread root. Oven temperature is 285–300°C, PIAT is held at 205–215°C, and cooling is slowed with forced air only to minimise insert pull-out stress and flat-panel warpage. Terminal products are 300–1,500 L tractor-mounted saddle tanks, trailed sprayer tanks, rinse-water tanks, and saddle hoppers for granular fertiliser distribution.

    Material Handling Bins, Fish Tubs, and Logistics Pallets in Cold-Chain Service

    In cold-chain handling, the moulded article is frequently a double-wall body with a nominal inner wall thickness of 4–5 mm and an outer wall of 5–6 mm, surrounding a polyurethane foam core with a density of 40–60 kg/m³. The food-contact surfaces are governed by FDA 21 CFR §177.1520 and EU Regulation 10/2011, while the overall food-contact material must additionally satisfy EC 1935/2004. The formulation is 100 phr Icorene 1761 GRN 6654, 0.1–0.2 phr hindered phenol antioxidant, 0.5–1.0 phr slip/antiblock only if the article is nested, and 5–15 wt% metallocene polyolefin elastomer when the service temperature drops to −30°C for fish tubs and meat lugs. Processing occurs on a biaxial machine with a 4.0:1 arm ratio, oven residence of 20–26 min, and PIAT of 205–215°C; the foam cavity is injected after demoulding and cooling, requiring a vent hole pattern that prevents overpressure during the polyol-isocyanate reaction exotherm. Terminal parts include 200–1,000 L insulated fish tubs, meat lugs, dunnage trays, collapsible pallet boxes, and harvesting totes used in food processing and cold-chain logistics.

    For outdoor playground panels, tunnel sections, and slide bed modules, the decisive mechanical criterion is low-temperature ductility after weathering, and the applicable standards are EN 1176-1:2017 for playground equipment safety and ASTM F1487-21 for public playground equipment. The dry blend is 100 phr of the green compound, 1.0–2.5 phr UV stabiliser masterbatch, and 0.2–0.4 phr antioxidant; because the grade already contains the GRN 6654 pigment, no additional colour concentrate is added. Moulding is done on a carousel rotational moulding line at 285–295°C oven set point with PIAT of 205–215°C; wall thickness is held at 5–7 mm to meet impact requirements after accelerated weathering. Post-mould operations include trimming, drilling for fasteners, and assembly with metal frames; the rotomoulded shell is selected over HDPE blow moulding for slides and tunnels because the mould allows uniform corner radii and no weld-line stress concentration. Terminal products are slide beds, crawl tunnels, roof caps, climbing panels, and shaped seating shells for public and school playgrounds.

    When a Pontoon Shell Is Foam-Filled for Buoyancy

    When a pontoon shell is foam-filled for buoyancy, the moulded wall must resist both flexural fatigue at the waterline and slow puncture from dock hardware. Material specifications for rotationally moulded marine floats typically invoke ASTM D3350-21 cell classification for polyethylene, and the part is designated under ISO 17855-1:2016 as a polyethylene material. The formulation is 100 phr Icorene 1761 GRN 6654, 2.0–3.0 phr marine-grade UV/HALS masterbatch, and 0.2–0.4 phr antioxidant; internal mould release is reduced to 0.05–0.1 phr or eliminated because foam adhesion to the inner wall improves structural stiffness under wave load. The shell is moulded on a biaxial machine with a 4.0:1 speed ratio, oven set point 285–300°C, PIAT 205–215°C, and wall thickness of 6–10 mm. After demoulding, the hollow shell is filled with closed-cell polyurethane foam at 40–60 kg/m³; the exothermic foam rise is controlled by venting at the top surface. Terminal products include floating dock pontoons, marina breakwater floats, shellfish aquaculture floats, and buoyancy modules for dredge lines and swim platforms.

    Free Quote

    Competitive LyondellBasell Icorene 1761 GRN 6654 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 GRN 6654 is a precoloured metallocene linear low-density polyethylene (mLLDPE) supplied under the Icorene brand. The full product designation combines the base resin series, Icorene 1761, with the pigment suffix GRN 6654, which identifies a green 6654 colour preparation. The base polymer is an ethylene-α-olefin copolymer produced via single-site metallocene catalysis, not a conventional heterogenous Ziegler-Natta catalyst system. That distinction controls the short-chain branch distribution, crystallisation behaviour, optical clarity, and seal response. The natural base resin is positioned at a nominal density of 0.918 g/cm³ determined by ISO 1183-1 or ASTM D1505, and at a melt flow rate of 1.0 g/10 min determined at 190 °C under a 2.16 kg load according to ISO 1133-1:2022 or ASTM D1238. Because the product is supplied already pigmented, the finished melt flow value may shift within a typical tolerance of ±0.2 g/10 min and the density may shift by up to 0.002 g/cm³, depending on the colour concentrate carrier resin and let-down ratio. The material is specified for blown film and cast film applications in which a green layer is required for identification, light screening, agricultural mulch, or decorative packaging while retaining the low seal initiation and high dart impact of the metallocene base class.

    Target film structures include food packaging laminates, heavy-duty sacks, agricultural stretch film, and industrial liners. In coextruded formats, the green 6654 layer is commonly placed in a skin layer rather than as a direct food-contact sealing layer unless the specific colourant system has been cleared by the converter. The grade can be processed as a neat film layer, but on high-speed blown film lines it is frequently blended with 10–20 % by mass of high-pressure LDPE to increase bubble stability. That addition raises the heat seal initiation temperature and reduces dart impact, so the blend ratio must be fixed before final film specifications are approved.

    Why Does Metallocene Catalysis Alter the Short-Chain Branch Distribution?

    Conventional Ziegler-Natta LLDPE is produced by multiple active site populations, generating a broad distribution of comonomer placement and molecular weight. Icorene 1761 GRN 6654 instead contains a metallocene-catalysed base resin with a narrower molecular weight distribution and a more uniform short-chain branch distribution. The crystallite thickness distribution therefore narrows, which reduces the temperature interval between initial melting and complete melting and lowers the onset of heat sealing. The more uniform comonomer incorporation also reduces the high-crystallinity fractions that scatter light, so haze is lower than an equivalent-density Ziegler-Natta LLDPE film. The same mechanism reduces the low-crystallinity, high-extractable fraction that can migrate under use conditions. Characterisation by temperature rising elution fractionation or differential scanning calorimetry under ISO 11357-3 typically shows a narrower melting distribution for the metallocene grade than for a broad-distribution Ziegler-Natta resin at the same nominal density.

    Rheological measurements under ISO 11443 show that this metallocene base resin tends to have lower shear viscosity at high shear rates than an equivalent melt-flow Ziegler-Natta LLDPE but also lower melt strength. The single-site molecular structure reduces long-chain branching, so draw ratio and frost line height must be managed differently from LDPE-rich formulations. For a 25 µm blown film produced on a single-flighted extruder with a 30:1 L/D barrier screw and a 150 mm die, the melt temperature is usually maintained at 190 °C to 230 °C. A screen pack of 80/120 mesh or finer is recommended when the green pigment dispersion must be filtered, but excessive back pressure above 350 bar may cause gel formation at the screen pack.

    A Film Extrusion Route with Reverse-Temperature Barrel Profiling

    The barrel profile for this precoloured mLLDPE should be set with a flat to reverse temperature configuration: feed zone 170–180 °C, compression zone 190–210 °C, metering zone 210–220 °C, and adapter/die 220–230 °C. Running the die hotter than the metering zone improves surface wet-out and reduces die-lip buildup from the pigment concentrate. On a 45 mm extruder at a screw speed of 80 rpm, a stable bubble may require a blow-up ratio of 2.0:1 to 3.0:1 and a frost line position of 3 to 5 die diameters above the air ring. When high-pressure LDPE is added to improve melt strength, the addition should be limited to 10–20 % by mass; higher levels raise seal initiation temperature and reduce dart impact. Screw wear and colour changeover should be monitored because the green 6654 pigment can retain in the screw root and flanks. A purging compound based on a high-viscosity polyolefin is preferred before switching to a natural resin.

    PropertyTest standardMetallocene LLDPEZiegler-Natta LLDPEHigh-pressure LDPE
    Short-chain branch distributionISO 11357-3 DSC melt distributionNarrow, uniformBroad, heterogeneousLong-chain branched, broad
    Dart impactASTM D1709A at 25 µmHigher at equal densityReferenceGenerally lower at equal thickness
    Heat seal initiationASTM F1921Lower by 8–12 °C relative to Ziegler-Natta grade at 0.918 g/cm³ReferenceHigher
    Optical hazeASTM D1003Lower than Ziegler-Natta LLDPEHigherModerate
    Capillary viscosity profileISO 11443Lower high-shear viscosityModerateHigher low-shear viscosity and melt strength

    When the Icorene 1761 base resin is coloured with the GRN 6654 concentrate, the melt viscosity may drop slightly if the concentrate carrier is a high-flow LDPE or LLDPE, or may remain neutral if the carrier is an mLLDPE of the same class. The resulting film properties therefore cannot be transferred directly from natural-grade datasheets; a colour-matched engineering trial on the target line is necessary. Additives such as slip and antiblock should be introduced only in pre-dispersed masterbatch form because direct blending of powder additives into the coloured film resin can create screen-pack pressure fluctuations and visible gel formation. If the green film is used for agricultural or horticultural service, UV stabilisation should be specified separately; the pigment alone does not provide sufficient long-term light stabilisation under ISO 4892-2.

    When Additives and Colour Concentrates Are Introduced into the Melt Stream

    Processing with a green 6654 precoloured mLLDPE requires attention to pigment dispersion and filtration. In blown film production, the use of a melt pump between the extruder and die reduces pressure pulsation and improves layer thickness uniformity in multilayer structures. Typical melt filtration consists of a breaker plate and a screen pack of 60/100/120 mesh; the final mesh is selected to retain undispersed pigment agglomerates larger than 100 µm. Back pressure should be monitored with a pressure transducer. If the pressure exceeds 300–350 bar at normal throughput, the screen pack should be changed to prevent pigment build-up and polymer decomposition. The pigment carrier and any lubricant system must be compatible with low-density polyolefin processing. Polyethylene wax carriers are acceptable; incompatible ester or amide additives can increase screw slip and reduce output stability in the feed zone. No pre-drying is normally required for the neat polyethylene, but if sacks have been stored in ambient relative humidity above 60 % or visible surface condensation is present, drying at 60 °C for 4 h in a dehumidified-air hopper dryer prevents moisture-related surface defects in film.

    Food-contact status for the natural grade may be based on FDA 21 CFR 177.1520 for olefin polymers and on Regulation (EU) No 10/2011 with overall migration testing under Annex V. For the green 6654 version, the final film converter must verify that the pigment formulation and all additives meet the same end-use requirements, because the colour concentrate is a separate component. The grade is not automatically suitable for direct contact with fatty foods unless migration testing under simulant D2 or D1 is completed for the specific film thickness and temperature. For non-food industrial applications, the standard compliance matrix can include REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU for restricted heavy metals in electrical and electronic plastics. The green colourant should be checked for compliance with packaging waste and supplier-specific heavy-metal limits.

    Regulatory domainReferencePosition for Icorene 1761 GRN 6654
    US food contact21 CFR 177.1520Base olefin polymer; coloured variant requires end-test verification
    EU food contactRegulation (EU) No 10/2011, Annex VOverall migration ≤ 10 mg/dm² for the applicable food simulant
    REACH SVHCEC 1907/2006, Annex XVIISupplier confirmation required for final article
    RoHS heavy metals2011/65/EUCd ≤ 100 ppm, Pb ≤ 1000 ppm in homogeneous plastic

    Film Mechanical Testing and Heat Seal Response

    Film properties should be measured on 25 µm or 50 µm unsupported film. Tensile strength and elongation are determined by ISO 527-3 or ASTM D882 at a test speed of 500 mm/min. Elmendorf tear strength is measured by ISO 6383-2 or ASTM D1922. Dart impact is measured by ASTM D1709A using a 38.1 mm diameter dart and a drop height of 660 mm. Seal initiation can be determined by heat sealing at 10 °C intervals from 80 °C to 120 °C and measuring seal strength according to ASTM F88/F88M. Published data for this specific green 6654 film configuration is limited, so a verification run on the converter’s film line is the only reliable basis for comparing seal initiation and hot-tack against a natural mLLDPE or a Ziegler-Natta LLDPE. The lower melting peak of mLLDPE generally reduces seal initiation by several degrees, but the pigment, cool-line placement, and corona treatment can shift the response.

    This grade should not be processed above 240 °C melt temperature for extended residence times because oxidative decomposition can form crosslinked gel particles in the die lip and reduce film clarity. Purging after PVC, PVDC, or halogenated polymers requires complete barrel and die cleaning; halogen residuals can degrade polyolefins and may attack metal surfaces. The low melt strength of the neat metallocene resin means that deep-throat hopper flooding and high-shear screw elements should be avoided. When the product is used in multilayer structures, the green layer should be positioned away from high-temperature sealant layers unless the sealant resin demonstrates equivalent seal strength after colour addition. In outdoor service, a UV-stabilised and weathering-tested formulation is required; the green 6654 pigment alone is not a substitute for a hindered amine light stabiliser package.

    What Lot-to-Lot Variations Should Be Controlled in a Coloured mLLDPE Supply?

    Incoming QC for the coloured grade should require melt flow rate by ASTM D1238 or ISO 1133-1, density by ISO 1183-1, and colour coordinates by spectrophotometry against a master standard. The specification should include a melt flow tolerance of ±0.2 g/10 min around the target and a density tolerance of ±0.002 g/cm³. Film evaluation from each lot should include dart impact at 25 µm, tensile yield and break according to ISO 527-3, and visual gel count on 1 m² of film. Colour measurements under ISO 11664-4 CIE L*a*b* conditions may reveal batch-to-batch variation in the green 6654 concentrate; a ΔE of more than 1.5 is often visible in side-by-side packaging applications. Because published data for this specific prepigmented configuration is limited, lot qualification on the production line is required.

    Top