| HS Code | 151929 |
| Density | 0.918 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 9.0 MPa |
| Tensile Strength At Break | 28.0 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 210 MPa |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 9% |
| Gloss | 75% |
| Color | Green |
| Form | Pellets |
| Polymer Type | Metallocene Linear Low Density Polyethylene |
| Catalyst Type | Metallocene |
As an accredited LyondellBasell Icorene 1761 GRN 6248 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | LyondellBasell Icorene 1761 GRN 6248 LLDPE is packaged in 25 kg polyethylene-lined paper bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with 25 kg bags of LyondellBasell Icorene 1761 GRN 6248 metallocene LLDPE, approximately 20 MT net. |
| Shipping | LyondellBasell Icorene 1761 GRN 6248 Polyethylene, Linear Low Density, Metallocene is shipped as non-hazardous resin pellets in sealed 25 kg bags or octabins, palletized and stretch-wrapped. Transport in clean, dry trucks or containers at ambient temperature; protect from moisture, heat, sunlight, and contamination. Not regulated for transport. |
| Storage | Store Icorene 1761 GRN 6248 polyethylene resin indoors, off the floor, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers tightly closed to prevent moisture, dust, and contamination. Protect from UV exposure and excessive stacking. Maintain ambient temperatures and use first-in, first-out inventory. Avoid inhaling dust or fines during handling. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in original packaging, cool, dry, protected from sunlight and moisture. |
In a coextruded blown film sealant web for vertical form-fill-seal and horizontal flow-wrap equipment, Icorene 1761 GRN 6248 is placed in the inner layer of a three-layer structure where the finished pouch must attain a hermetic seal without breaching the polyethylene recyclability stream. The layer is compounded at 60–80 wt% Icorene 1761 GRN 6248 with 20–40 wt% high-pressure low-density polyethylene having a melt index of 0.3–0.7 g/10 min under ISO 1133-1:2022; the LDPE co-feed suppresses sharkskin melt fracture at die shear rates above 500 s⁻¹. An antiblock masterbatch is added at 5,000–12,000 ppm when blocking force exceeds 8 N/cm² under ASTM D3354-15 on high-speed stacking equipment. Food-contact compliance rests on FDA 21 CFR 177.1520(c) 3.1/3.2 and Regulation (EU) No 10/2011 Annex I and II, with overall migration verified below 10 mg/dm² under EN 1186-1 and seal strength measured to ASTM F88/F88M-21. Where the GRN 6248 colorant system is present, the colorant must also hold clearance under 21 CFR 178.3297 or the European positive list in Regulation (EU) No 10/2011.
Production-scale blown film lines with 30:1 L/D single-screw extruders, barrier screws, and die diameters between 250 mm and 400 mm operate with a die gap of 1.8–2.4 mm, a blow-up ratio of 2.0–2.5, and a melt temperature of 190–230°C. A failure mode observed on these lines is bubble chatter when the frost line height exceeds 4–6 times the die diameter, producing seal layer gauge variation above ±4%; the variation shifts seal initiation by 2–4°C and increases leakage at the back-fin seal of a vertical form-fill-seal machine. Internal bubble cooling at an exhaust temperature of 10–18°C and an oscillating haul-off matched to the film path length are used to keep the sealant web flat and within ±6% thickness. Terminal finished goods include mono-material stand-up pouches, frozen-food flow wrap, stickpacks, and ready-to-eat snack sachets.
Cast pallet containment film for transit packaging uses Icorene 1761 GRN 6248 in the outer skin layers where puncture resistance and load retention determine packaged stability. The formulation for a five-layer cast coextrusion line places 70–85 wt% of the resin in the two skin layers, while the core uses 15–30 wt% of a second mLLDPE or high-pressure LDPE; a tackifier concentrate is added at 2–5 wt% in the surface sub-skin to achieve unwind cling values specified under ASTM D5458-95(2020). Industrial transit packaging compliance is anchored to ISO 527-3 for tensile properties, ASTM D5748-95(2012) for puncture resistance, and Regulation (EC) No 1907/2006 REACH for EU market access.
Line speeds of 400–600 m/min are sustained on a 2,200–2,800 mm slot die with a die gap of 0.8–1.2 mm; the melt is quenched on a chill roll held at 16–24°C. Draw resonance becomes the limiting defect above 600 m/min unless the die-to-roll distance is maintained below 30 mm and air knife pressure is increased; edge trim is returned to the extruder at 8–12 wt% of layer throughput. Finished product types include stretch hood films for palletized cement, appliances, and bottled-beverage loads, as well as industrial hand-wrap rollstock.
Silage bale wrap is produced as a three-layer cast film in which Icorene 1761 GRN 6248 constitutes 92–97 wt% of the total extrudate, with a UV masterbatch added at 3–8 wt% in the outer layers and a cling additive concentrate at 2–4 wt% in the surface layers to permit multi-wrap retention on a round bale. The compliance framework for this segment is EN 14932:2018 for bale wrapping films, ISO 527-3 for tensile properties, ASTM D5748-95(2012) for puncture resistance, and ISO 4892-2:2013 for accelerated weathering; outdoor field performance is commonly specified as retained elongation beyond 50% after 1,000 h of xenon-arc exposure, although published data for this exact green concentrate in silage wrap is limited and must be confirmed by separate weathering trials.
Downstream production on a 3-layer cast line with 30:1 L/D extruders uses a melt temperature of 220–250°C, a die gap of 0.9–1.4 mm, and a primary chill roll temperature of 16–22°C. The operational boundary imposed by tackifier concentrates is oxidative degradation above 250°C, which generates smoke, plate-out on die lips, and gel spots; startup purges with LDPE and residence time below 45 s are therefore used. Terminal product types include 750 mm and 500 mm round bale wrap rolls, silage tubes, and pre-stretched agricultural film.
In extrusion coating of paperboard and aluminium foil for aseptic beverage cartons, Icorene 1761 GRN 6248 is introduced as a 30–50 wt% modifier to high-pressure LDPE in the internal sealant coating, reducing seal initiation temperature while preserving adhesion within the polyolefin layer. The coating weight is maintained at 15–25 g/m² on lines where a 90–120 mm single-screw extruder with 30:1 L/D and barrier screw delivers melt at 280–320°C to a slot die with a 0.7–1.0 mm gap. Food-contact compliance is regulated by FDA 21 CFR 177.1520(c) 3.1/3.2 and Regulation (EU) No 10/2011, with seal strength measured on the finished laminate to ASTM F88/F88M-21 and overall migration verified below 10 mg/dm² under EN 1186-1.
Production experience indicates that edge-neck-in increases sharply when the die-to-nip distance exceeds 150 mm or when melt temperature falls below 285°C; a short draw length and an edge encapsulation feed are used to keep coating width variation below ±2 mm. Draw resonance is suppressed by retaining at least 10 wt% high-pressure LDPE in the coating blend. Terminal finished goods include aseptic brick packs, stickpack laminates, and sterile liquid pouch stock.
The dart impact resistance and seal integrity of a monolayer blown film in this application are obtained with Icorene 1761 GRN 6248 at 90–100 wt% of the product, with 0–10 wt% high-density polyethylene added to increase tensile modulus when liner insertion on automated equipment demands stiffer film handling. Antiblock is added at 3,000–6,000 ppm; slip additive levels are kept below 800 ppm because higher slip concentrations reduce the coefficient of friction required for stable rolled film tension during bag conversion. Compliance for FIBC liners is tied to ISO 21898:2004 for non-dangerous goods, ASTM D1709-16A for dart impact, and ASTM F88/F88M-21 for seal strength; if the liner is used in dangerous goods packaging, the outer FIBC must meet the applicable test provisions of 49 CFR Part 178.
Manufacturing on a high-stalk blown film line equipped with a 300 mm die, 2.0–2.8 mm die gap, and 30:1 L/D extruder uses a blow-up ratio of 2.5–3.5 and a melt temperature of 185–220°C. The processing window is bounded by bubble instability: a stalk height beyond 8 die diameters creates oscillation under ambient air currents, while a collapse below 4 die diameters produces wide dart-impact distribution and increases bottom-seal failures under a 1.2 m drop test. Internal bubble cooling with exhaust at 12–16°C and an oscillating haul-off with ±5° angular deviation normalize gauge. Finished goods include FIBC inner liners, polyethylene shipping-sack liners, and moisture-barrier rollstock for construction powders.
As a carrier resin for white and additive masterbatch production, Icorene 1761 GRN 6248 is incorporated at 20–40 wt% of the finished pellet, with a titanium dioxide or carbon black active loading of 60–70 wt% and a processing aid package at 0.5–1.5 wt%. The metallocene backbone provides pigment wetting at lower torque than a Ziegler-Natta LLDPE of equivalent melt index; however, filler loading above 70 wt% raises torque above 90% of gearbox capacity on a 44:1 L/D twin-screw extruder and shortens screw life. Compliance requirements depend on the end-use matrix: if the masterbatch is intended for food-contact film, the carrier must comply with FDA 21 CFR 177.1520(c) 3.1/3.2 and Regulation (EU) No 10/2011; dispersion is monitored by pressure rise across 80–120 mesh screen packs, and gel counts are kept below 10 gels per 5 m² under ASTM D3351-10.
The compounding sequence consists of pre-blending in a high-speed mixer at 800–1,200 rpm for 3–5 min, followed by twin-screw extrusion at melt temperatures of 190–230°C and screw speeds of 400–700 rpm, with side feeding of pigment after the main polymer melting zone to avoid viscous heating. A water-ring pelletizer produces finished pellets with bulk density 0.50–0.55 g/cm³; screw and barrel wear become the limiting operational boundary when mineral filler loading exceeds 70 wt% and specific mechanical energy rises above 0.25 kWh/kg. Published data for this exact pigment-bearing grade in mineral-filled masterbatch is limited; the 0.25 kWh/kg threshold is therefore a screening limit to be verified on the target line. Terminal product types include white masterbatch pellets, additive concentrates, and color concentrates for polyolefin film and molding.
Competitive LyondellBasell Icorene 1761 GRN 6248 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 GRN 6248 is a metallocene-catalysed linear low-density polyethylene grade supplied with a green colour formulation. The designation “GRN” is interpreted as a green colorant package; “6248” identifies the colour formulation or lot-control code rather than a separate polymer architecture. The base resin belongs to the Icorene metallocene LLDPE platform, in which single-site catalysts produce a narrower molecular weight distribution and more homogeneous short-chain branch placement than conventional Ziegler-Natta LLDPE. The product is relevant to converters producing pre-coloured moulded or extruded articles where green tinting is required without separate masterbatch addition. Typical conversion routes for metallocene LLDPE include injection moulding, cast film, and profile extrusion; the presence of the colour package makes the grade more specific to opaque or tinted parts, though translucency is possible at thin wall sections. Because published datasheet values for this specific green-formulated grade are limited, the certificate of analysis should be treated as the controlling specification. Density should be verified by ISO 1183-1:2019 at 23 °C, melt mass-flow rate by ISO 1133-1:2022 at 190 °C and 2.16 kg, and tensile properties by ISO 527-2:2012 or ASTM D638-14 after moulding. The green colourant is not inert: pigment dispersion, nucleating effects, and thermal stability require incoming and moulded-part verification. The information below addresses structural differences, processing constraints, specification controls, and regulatory boundaries rather than repeating nominal property values that may not apply to the supplied lot.
Metallocene LLDPE differs from conventional Ziegler-Natta LLDPE primarily in molecular weight distribution and comonomer placement. Published gel-permeation chromatography data for commercial metallocene LLDPE grades generally report Mw/Mn between 2 and 3, while conventional Ziegler-Natta grades commonly fall between 3 and 5 depending on reactor configuration. The absence of a high-molecular-weight tail reduces elastic memory and die swell; the uniform comonomer distribution suppresses the formation of highly branched, low-melting fractions. These fractions in Ziegler-Natta LLDPE can migrate and contribute to organoleptic or extraction issues in food-contact applications. For Icorene 1761 GRN 6248, the base resin is therefore expected to show a sharper melting endotherm under ISO 11357-3:2018, typically in the 105 °C to 125 °C range for mLLDPE of the common 0.915 g/cm3 to 0.925 g/cm3 density band. The exact density of this grade should be read from the certificate of analysis; published data for this specific green-formulated grade is limited.
Tensile response follows density and crystallinity rather than catalyst type alone. Under ISO 527-2:2012, Type 1A specimen, at 50 mm/min, representative metallocene LLDPE materials in the density band above show yield stress between 8 MPa and 14 MPa and strain at break above 500 % at 23 °C. However, the pre-compounded green colour may reduce elongation-to-break compared to an uncoloured base resin because pigment aggregates act as micro-stress concentrators. The durability of the material should therefore be evaluated on the as-supplied colour formulation, not on the natural base resin. Notched Izod impact per ASTM D256-10(2018) or ISO 180:2019 and dart drop impact per ASTM D1709-16a for film may not transfer to thick-walled injection-moulded parts; the processor should use part-level tests that replicate gate orientation and weld-line position.
Thermal behaviour also influences secondary operations. The sharp melting peak of metallocene LLDPE can provide faster melting in extrusion and lower screw torque than a broad-MWD grade of equivalent density, but the same narrow distribution may increase injection pressure at high shear. Differential scanning calorimetry per ISO 11357-3:2018 can be used to confirm whether the green pigment has increased the crystallization temperature. A shift of 2 °C to 5 °C compared with the natural base resin is not unusual for nucleating pigments and is significant in multi-cavity tools because earlier solidification increases gate freeze time and changes hold-pressure requirements.
Compared with high-pressure LDPE, metallocene LLDPE has different failure mechanics. LDPE contains branched architectures that give high melt elongation and strain-hardening in tensile deformation; mLLDPE derives its toughness from linear chains with homogeneous short-chain branches. The consequence is that low-density polyethylene films may outperform mLLDPE in applications requiring high melt strength or extended bubble stability, while metallocene LLDPE generally provides higher tensile and puncture resistance at equivalent density. Film converters evaluate puncture resistance by ASTM D5748-18 or ASTM F1306-21, and tear strength by ISO 6383-2:1983. For injection moulding, high-pressure LDPE is rarely used for load-bearing parts, so the comparison with conventional Ziegler-Natta LLDPE and HDPE is more relevant. Against HDPE, Icorene 1761 GRN 6248 is expected to have lower crystallinity and lower flexural modulus, but higher environmental stress-crack resistance and lower notched impact transition temperature. Flexural modulus is measured by ISO 178:2019 at 2 mm/min. Environmental stress-crack resistance is assessed by ASTM D1693-15 with a surface-active agent such as nonylphenoxy poly(ethyleneoxy)ethanol under constant strain. Processors replacing HDPE with this grade should verify that the part retains sufficient stiffness under load and that the tool cooling layout can handle longer cycle time from slower crystallization.
On reciprocating-screw injection moulding machines with screw length-to-diameter ratios of 18:1 to 22:1, metallocene LLDPE compounds are typically processed with barrel set-point temperatures from 180 °C to 230 °C and mould temperatures from 10 °C to 40 °C. The lower end of the mould-temperature window is acceptable for thick-walled articles where cooling dominates cycle time, but mould temperatures below 10 °C can create condensation and surface defects in plants operating above 50 % relative humidity. A back pressure of 0.5 MPa to 1.5 MPa assists pigment dispersion in the melt; excessive back pressure raises melt temperature and can consume the stabiliser package before the resin reaches the cavity. The screw should have a shallow compression section and a non-return valve clearance specified for low-viscosity polyolefin; a worn valve can produce shot-weight variation above 1 %, which is visible as dimensional scatter in multi-cavity closures. At injection shear rates near 104 s−1, the narrow molecular weight distribution of metallocene LLDPE may generate higher melt viscosity than a broad-MWD Ziegler-Natta grade of equal melt index, increasing peak injection pressure and clamp force. A 1200 kN toggle-clamp machine may require a safety margin of at least 10 % above the hydraulic pressure calculated for conventional LLDPE when the tool has long hot-runner channels. These observations are consistent with published processing comparisons; the processor should verify them on the actual lot because colourant and additive packages can shift viscosity.
Start-up and shutdown procedures are part of the processing boundary. Purging with a high-density polyethylene of similar melt flow rate is standard before introducing the metallocene grade to avoid gel creation at temperature transitions. Melt residence time should be kept below the thermal-oxidative stability limit of the colour concentrate; for pigmented polyolefins, this is often specified as no more than 5 min to 10 min at barrel temperature when the screw is idle, but grade-specific limits from the supplier control. The use of hot-runner valve gates should be confirmed by short-shot studies and gate-seal time checks per ISO 294-1:2017. Moisture is generally not a storage issue for unopened polyolefin boxes, but material exposed to relative humidity above 60 % may be predried at 60 °C to 80 °C for 1 h to 2 h to reduce surface splay. The drying step is a handling recommendation; it is not a substitute for correct venting or melt-temperature control.
The colour package designated by GRN 6248 is a formulation variable, not a simple tinting agent. Green shades in polyethylene compounds are commercially produced with organic pigments, inorganic chromium-based pigments, or blended systems; the specific chemistry affects thermal stability, dispersion, food-contact status, and recycling behaviour. Pigment particles that remain agglomerated act as stress concentrators and can reduce tensile elongation at break by more than 10 % in an otherwise ductile base resin. Dispersion should be assessed on moulded plaques using ISO 18553:2002 or by quantitative image analysis on cryo-microtomed sections. Thermal analysis per ISO 11357-3:2018 should be performed on the as-supplied compound and the fabricated part; a crystallisation temperature shift of 2 °C to 5 °C relative to the uncoloured base resin indicates nucleating effects that may require changes to mould temperature or hold pressure. ISO 294-4:2018 should be used to quantify shrinkage in flow and transverse directions, because asymmetric cooling of a nucleated narrow-MWD grade can produce warped parts even when the mould has balanced filling. Additive-blooming tests, such as storage at 60 °C for 168 h and visual or FTIR assessment, can detect surface migration of processing aids or pigment dispersants; the relevance of such tests depends on the final application.
For food-contact or potable-water applications, the green colour system must not be assumed compliant because the base polyolefin meets FDA 21 CFR 177.1520. In the United States, colourants for food-contact polymers are regulated as colour additives under 21 CFR 178.3297 or specific listings; in the European Union, Regulation (EU) No 10/2011 requires overall migration of the finished article not to exceed 10 mg/dm2 for plastic materials or 60 mg/kg depending on volume-to-surface ratio, with specific migration limits for authorised substances. The processor should request a composition disclosure for the 6248 formulation and verify residual metals when inorganic pigments are present. Ash content according to ISO 3451-1:2019 can provide a quick incoming check for heavy pigment loading; a value outside the supplier’s specified range may indicate compounding error or contamination with another polymer.
Incoming material should be released against a documented specification covering the following methods and parameters.
| Material property | Method | Condition | Specification function |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg | Viscosity/molecular weight consistency |
| Density | ISO 1183-1:2019 | 23 °C | Crystallinity and stiffness baseline |
| Tensile yield stress and elongation | ISO 527-2:2012 | 50 mm/min, Type 1A | Mechanical deformation resistance |
| Flexural modulus | ISO 178:2019 | 2 mm/min | Bending stiffness |
| Notched Izod impact | ISO 180:2019 | 23 °C and −30 °C | Low-velocity toughness |
| DSC melting and crystallization | ISO 11357-3:2018 | 10 K/min | Thermal integrity and pigment nucleation |
| Ash content | ISO 3451-1:2019 | 600 °C | Pigment/filler loading |
The certificate of analysis is controlling for lot release, but standard test plaques may not capture weld-line, gate-seal, or cooling-rate effects. Incoming density and melt flow rate are the primary comparators; a density shift of 0.002 g/cm3 may be sufficient to alter flexural modulus and cycle time. Melt flow rate outside the supplier’s range by more than 10 % can indicate contamination or degradation and should trigger a purge and re-evaluation. Ash content outside the specified range should trigger an investigation of colourant dispersion and potential screw wear from pigment agglomerates. Because the green formulation may consist of multiple pigment and additive lots, colour control by spectrophotometry should be performed on conditioned mouldings; colour variation can be caused by thermal history rather than pigment concentration alone.
Processing history, regrind level, and mould release chemistry change the extractable fraction and mechanical performance of the final part. Regrind addition at 20 % by weight is commonly tolerated in technical polyolefin moulding when the regrind is dry and uncontaminated, but colour shift and impact retention must be verified because the green concentrate may degrade during repeated heat histories. The processor should define a regrind control plan using ISO 1133-1:2022 and ISO 294-3:2017 tensile or impact verification. If the article is intended for medical use, ISO 10993-1:2018 biological evaluation may be required, and the resin supplier’s biocompatibility statement must cover the specific 6248 colour package. For electrical and electronic applications, the compound must meet the substance restrictions of EU RoHS Directive 2011/65/EU, including Annex II lead, cadmium, mercury, and hexavalent chromium thresholds of 0.1 % and 0.01 % by weight in homogeneous material. These regulatory constraints are article-dependent and cannot be inferred from the base polymer alone.
Material substitution from a conventional Ziegler-Natta LLDPE to Icorene 1761 GRN 6248 should be treated as a formulation change rather than a drop-in replacement. The validation protocol should include capillary rheometry per ISO 11443:2021 at three shear rates spanning the injection moulding range, part-level short-shot analysis, and dimensional stability per ISO 294-4:2018 after conditioning per ISO 291:2008. Without such data, process adjustments based on melt index alone can miss the effect of narrow molecular weight distribution on high-shear viscosity, gate freeze, and weld-line performance.