Lyondellbasell Icorene 1761 Bwn 8810 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BWN 8810 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BWN 8810 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 408401
    Density 0.917 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 119 °C
    Vicat Softening Point 91 °C
    Tensile Strength At Yield Md 8.96 MPa
    Tensile Strength At Yield Td 8.27 MPa
    Tensile Strength At Break Md 34.5 MPa
    Tensile Strength At Break Td 27.6 MPa
    Elongation At Break Md 500 %
    Elongation At Break Td 700 %
    Tensile Modulus Md 172 MPa
    Tensile Modulus Td 207 MPa
    Dart Drop Impact 220 g
    Elmendorf Tear Strength Md 120 g
    Elmendorf Tear Strength Td 350 g
    Haze 6 %
    Gloss 85 %
    Coefficient Of Friction 0.2
    Seal Initiation Temperature 105 °C

    As an accredited LyondellBasell Icorene 1761 BWN 8810 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 BWN 8810 comes in 25 kg polyethylene-lined bags, palletized and shrink-wrapped for secure transport.
    Container Loading (20′ FCL) Container Loading (20′ FCL): LyondellBasell Icorene 1761 BWN 8810 metallocene LLDPE, palletized 25 kg bags, about 18–20 metric tons net.
    Shipping LyondellBasell Icorene 1761 BWN 8810 is a non-hazardous linear low density polyethylene (metallocene) resin. It is not regulated for transport (no UN number). Typical shipments use 25 kg bags, octabins, bulk trucks, or railcars. Store dry, avoid excessive heat, and secure loads to prevent pellet spills.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and oxidizing agents. Keep containers or bags closed and palletized off the floor to prevent moisture and contamination. Avoid excessive stacking, prolonged UV exposure, and physical damage. Follow first-in, first-out stock rotation. Maintain normal ambient temperatures; no special ventilation is required under typical handling conditions.
    Shelf Life Shelf life: typically 24 months when stored unopened in original packaging, cool, dry, well-ventilated, away from direct sunlight and heat.
    Application of LyondellBasell Icorene 1761 BWN 8810 Polyethylene, Linear Low Density, Metallocene

    LyondellBasell Icorene 1761 BWN 8810 is brought onto high-stalk blown-film lines where the converter certifies the finished article under FDA 21 CFR 177.1520(c) for olefin polymers and under EU Commission Regulation (EC) No 10/2011 with overall migration not exceeding 10 mg/dm² in the selected food simulant. Grade-specific melt flow rate and density are verified against the lot certificate; typical metallocene LLDPE film-grade envelopes are 0.9–1.2 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 and 0.916–0.920 g/cm³ per ISO 1183-1:2019, with processing parameters adjusted proportionally when certificate values fall outside this window. The typical extrusion hardware is a 60 mm or 75 mm grooved-feed single-screw extruder with L/D 30:1 and a barrier screw designed for narrow-molecular-weight distribution metallocene resins. Barrel temperatures from hopper to die range 170–205 °C, the adaptor and die are held at 205–215 °C, and melt temperature measured by infrared pyrometer is maintained within 195–210 °C. Die gap is set to 1.8–2.4 mm, blow-up ratio 2.2:1 to 2.8:1, frost-line height 500–650 mm, and specific output 0.55–0.75 kg/h per mm of die circumference. Slip masterbatch based on erucamide is added at 0.5–1.0 wt%, silica antiblock at 0.5–1.5 wt%, and fluoropolymer process aid at 200–400 ppm if die-lip fouling appears. The resulting films are converted into pillow pouches, vertical form-fill-seal bags for sugar confectionery, and frozen vegetable packages; seal initiation is typically below 95 °C and is verified by ASTM F1921-18 for hot tack and ASTM F88/F88M-21 for seal strength.

    What Stabiliser Carriers Preserve Clarity in Three-Layer Greenhouse Cover Film Based on Metallocene LLDPE?

    In three-layer agricultural blown-film lines, the metallocene grade is placed in the outer and inner layers of an A/B/A structure, with a total thickness of 150–200 µm and a layer ratio of 1:2:1 or 1:3:1. The outer layer receives hindered amine light stabiliser masterbatch at 1.0–2.0 wt% and a benzophenone or benzotriazole UV absorber at 0.3–0.8 wt%; the inner layer receives anti-fogging additives at 0.5–1.5 wt% to control condensation on the crop-facing surface. Processing is conducted on a 250 mm three-layer die with die gap 2.2 mm, blow-up ratio 2.4:1 to 2.8:1, and melt temperature 200–215 °C. The narrow molecular weight distribution of the metallocene resin improves optical clarity after bubble collapse, but bubble instabilities occur when frost-line height is displaced by more than ±150 mm from the setpoint because the film lacks long-chain branching. High-acid filler masterbatches containing unneutralised carboxylic acid residues are avoided because they can compete with HALS and reduce stabiliser efficiency. Accelerated weathering qualification follows ISO 4892-2:2013 at 0.35 W/m²·nm at 340 nm with tensile retention measured by ISO 527-3:2018 after 2000 h exposure; published multi-year outdoor data for this specific grade are limited, so converters qualify each masterbatch lot against the standard rather than relying on supplier generic values. Moisture-sensitive polar masterbatches are pre-dried at 70 °C for 4 h when fractional moisture exceeds 0.1 % to prevent surface splay. Terminal articles include greenhouse covering film, low tunnels, and silage clamp covers.

    In three-layer cast stretch lines running above 400 m/min, the metallocene grade is selected for the core layer to provide drawability while polyolefin plastomers or lower-density copolymers form the cling layers. Melt temperature at the cast die is 230–245 °C, die gap is 0.5–0.8 mm, air gap 15–30 mm, and chill roll temperature 18–25 °C; vacuum box and air knife are used to pin the melt curtain and limit neck-in. Polyisobutylene tackifier is metered into the cling layer at 0.5–2.0 wt%, and excessive tackifier beyond 2.5 wt% causes chill roll plate-out and transfer fogging. Edge trim is reground into the core layer at 5–10 wt%, and higher regrind fractions increase gel count as measured by film-surface defect scanning. Pre-stretch ratios for machine wrap are set at 150–250 % on powered pre-stretch units, while hand wrap is stretched 50–100 % at the point of application. Ultimate tensile properties are tested using ASTM D882-18, puncture propagation resistance using ASTM D5748-18, and cling performance using ASTM D5458-18. Terminal products include pallet unitisation film, pre-stretched hand rolls, and dispenser rolls for high-speed automatic wrappers.

    Extrusion Coating Melt Curtain Stability Is Controlled by LDPE Blending and Air-Gap Geometry

    For liquid packaging board coating, Icorene 1761 BWN 8810 is blended with 20–40 wt% high-pressure LDPE to raise melt strength and reduce neck-in; the LDPE fraction is adjusted lot-by-lot using the neck-in value measured on a 1200 mm coating line at 200 m/min. Extrusion coating runs a 90 mm single-screw extruder with L/D 30:1, barrel temperatures from 200 °C at the hopper to 300–320 °C at the die, and a coat weight of 15–25 g/m². The die gap is set to 0.4–0.6 mm, and the air gap is maintained at 180–220 mm; increasing air gap beyond 250 mm destabilises the curtain under plant airflow. Melt pressure at the screen changer is held between 10 MPa and 14 MPa; a rise to 16 MPa at constant screw speed indicates breaker plate blockage and requires screen pack replacement. Paperboard is pre-treated by corona to a surface energy of 42–46 mN/m and may receive a water-based primer before coating. Adhesion is checked with peel tests at 90° and 300 mm/min after lamination.

    Regulation / StandardClause or MethodLimit / Condition
    U.S. FDA21 CFR 177.1520(c)Olefin polymer use in contact with food, conditions of use A–H
    EU Framework Regulation(EC) No 1935/2004Overall migration limit not to exceed 10 mg/dm²
    EU Plastics Regulation(EU) No 10/2011, Annex I and IIIOML < 10 mg/dm²; simulant selection based on food type
    GMPRegulation (EC) No 2023/2006Traceability, process control, and documentation of printing inks and adhesives

    Terminal articles are gable-top carton inner sealants and aseptic brick packaging where the polyolefin layer is in direct contact with liquid dairy products or juices.

    When Heat Seal Initiation Below 95 °C Is Required in Snack Food Laminations

    In adhesive-laminated snack packaging, the metallocene LLDPE is positioned as the sealant web against a BOPP or PET print web, with adhesive lamination rather than extrusion lamination to preserve high-surface-energy print quality. Heat seal initiation for the sealant layer is measured by ASTM F88/F88M-21 after sealing at 105–140 °C, dwell time 0.3 s, and jaw pressure 0.5 MPa; acceptable seal strength for dry snack packs is typically 12–18 N/25 mm at 130 °C. Hot-tack performance is measured by ASTM F1921-18 across a sealing temperature range of 80–140 °C; the practical hot-tack window narrows below 85 °C when filler or antiblock levels exceed 1.5 wt%. Slip and antiblock packages are limited to 0.3–0.8 wt% to maintain coefficient of friction between 0.15 and 0.25 when tested by ASTM D1894-14; higher loadings degrade seal strength. Terminal products include metallised snack pouches, chocolate bar wrappers, and frozen seafood bags.

    Heavy-Duty Sack Downgauging and Puncture Resistance Metrics

    Industrial sack lines running 40–80 µm film use the metallocene grade in a blend with 10–25 wt% C4-LLDPE or 5–15 wt% high-density polyethylene to raise modulus and reduce stretch during filling. Extrusion conditions include a 70 mm single-screw line with L/D 30:1, die gap 2.0–2.5 mm, blow-up ratio 2.0:1 to 2.5:1, and melt temperature 190–210 °C. Drop impact is tested by ISO 7765-1:1988 with a dart mass sufficient to produce failure in 50 % of specimens; Elmendorf tear is measured by ISO 6383-2:1983 in machine and transverse directions. Downgauging from 80 µm to 60 µm retains acceptable dart impact only when the HDPE content is kept at or below 15 wt%; above this threshold, the tear propagation resistance in the transverse direction falls below the level required for mineral fertiliser bags. Surface treatment is held at 38–42 mN/m for flexographic printing, and masterbatch addition of carbon black at 2–3 wt% is required for UV protection in outdoor storage. Terminal applications are petrochemical resin sacks, mineral fertiliser bags, and construction powder liners.

    Free Quote

    Competitive LyondellBasell Icorene 1761 BWN 8810 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 BWN 8810 is a metallocene-catalysed linear low-density polyethylene supplied for blown film extrusion. The grade is specified with a nominal density of 0.918 g/cm³ determined in accordance with ISO 1183-1:2019 or ASTM D1505 and a nominal melt flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load using ISO 1133-1:2022 or ASTM D1238. The metallocene active centre produces a substantially uniform short-chain branching distribution and a narrower molecular weight distribution than conventional Ziegler-Natta LLDPE. The reduction in high-density homo-ethylene fractions and low-molecular-mass oligomeric species alters the sealing, optical and mechanical response of the grade in monolayer and coextruded film structures.

    The product is typically supplied as a natural pellet with a thermal stabilizer package; the presence or absence of slip and antiblock additives should be verified against the current lot certificate and technical datasheet because film surface coefficient of friction is governed by additive loading. Published data for the specific comonomer identity is limited; film grades of this density and melt-flow class are commonly produced with C6 or C8 comonomer to raise Elmendorf tear and dart impact relative to butene-based LLDPE. That molecular distinction has direct implications for downgauging and seal performance.

    Melt Rheology and Single-Screw Extrusion Boundaries at the Die Lip

    At shear rates typical of annular film dies, metallocene LLDPE exhibits reduced shear-thinning compared with branched high-pressure LDPE. The power-law index is higher, so a change in screw speed produces a stronger change in apparent viscosity and die pressure. On a production extruder with a 24:1–30:1 L/D single-screw barrier screw, the grade is more likely to show elevated die pressure and motor load than a fractional-melt LDPE of similar nominal melt index. The die gap is therefore maintained at 1.5–2.5 mm, and die temperature is normally held between 190 °C and 210 °C. Process temperatures above 240 °C should be avoided to limit oxidative degradation of the stabilizer package and generation of gel specks.

    Bubble stability is a known bottleneck with this molecular architecture. The lower melt strength of mLLDPE relative to LDPE requires a smaller die gap, higher cooling-air velocity, and a frost line height between 2 and 5 die diameters. Batch-to-batch variation in melt flow rate is generally narrow because of the single-site catalyst; however, hopper residence time, air-ring imbalance, and screw wear can generate process drift when recycled edge trim exceeds 20 wt% without proper regrind classification.

    Representative blown film extrusion starting conditions for this melt-flow class
    ParameterWindowEquipment reference
    Barrel set temperature170–210 °CSingle-screw extruder, L/D 24:1–30:1
    Die set temperature190–210 °CSpiral mandrel blown film die
    Die gap1.5–2.5 mmAdjustable-lip blown film die
    Blow-up ratio2.0–3.0Bubble geometry and air-ring adjustment
    Frost line height2–5 die diametersAir-ring and internal bubble cooling control
    Maximum melt temperature240 °CMelt thermocouple before die body

    The tabulated values are starting points rather than formulation specifications. They must be adjusted to die diameter, cooling-air configuration, ambient humidity, and target film gauge. Failure to maintain a stable frost line height commonly produces gauge bands and edge curl on high-speed converting lines.

    When Coextruded Sealing Layers Demand a Low Seal Initiation Temperature

    Where coextruded sealing layers require a low seal initiation temperature, Icorene 1761 BWN 8810 can be used as the sealant layer in three-layer or five-layer structures at thicknesses from 5 µm to 15 µm. The uniform comonomer distribution reduces the temperature interval between onset of melting and complete seal formation; hot-tack behaviour is therefore maintained at short dwell times. Seal strength is determined by ASTM F88/F88M and hot tack by ASTM F1921. Typical vertical form-fill-seal equipment operating at seal-bar dwell times below 0.8 s requires a resin with a low seal initiation envelope; the metallocene resin achieves this by minimising the high-melting homo-ethylene fraction present in Ziegler-Natta LLDPE.

    In coextruded structures, the sealant layer contributes disproportionately to seal integrity and organoleptic performance. Metallocene catalysis reduces the low-molecular-mass fraction that can migrate from the sealant layer into food simulants. Converters should nevertheless verify overall migration on the final article because the tie layer, printing ink, and outer polyethylene layer also contribute extractable species.

    Directly following the sealing layer in a cast or blown coextruded line, optical properties are governed by crystal size and surface roughness. The homogeneous molecular architecture produces smaller crystallite dimensions than an equivalent-density Ziegler-Natta butene-LLDPE, which reduces light scattering and improves clarity. Actual haze, gloss and dart drop impact values are line-specific and must be extracted from the current manufacturer technical datasheet because published data for this specific configuration is limited. In coextruded films, the sealant-layer contribution to total haze is not additive; interfacial roughness and tie-layer optical properties also control the final film appearance.

    Physical Property Set and Test Method Alignment

    The following matrix aligns the grade to standardised test protocols used for lot release and film qualification. The methods do not by themselves define acceptance limits; the grade specification and current certificate of analysis control lot release.

    Resin and film qualification methods
    PropertyTest methodCondition or note
    Melt flow rateISO 1133-1:2022 / ASTM D1238190 °C, 2.16 kg
    DensityISO 1183-1:2019 / ASTM D150523 °C
    Tensile stress and strain of filmISO 527-3 / ASTM D882Specific gauge, 500 mm/min
    Dart drop impactISO 7765-1 / ASTM D1709Method A, 25 µm typical gauge
    Elmendorf tearISO 6383-2 / ASTM D1922Propagation resistance, film
    Haze and luminous transmittanceISO 14782 / ASTM D1003Film optical properties
    GlossISO 2813 / ASTM D245760° geometry
    Heat-seal strengthASTM F88/F88MSealed specimen
    Hot tackASTM F1921Seal initiation under peel before cooling
    Vicat softening temperatureISO 306 / ASTM D1525A50 or B50 loading
    Melting peak temperatureISO 11357-3:2018 / ASTM D3418Second heat, 10 °C/min

    Film property values are not single-point specifications. Dart drop impact, Elmendorf tear, and optical haze change with film gauge, blow-up ratio, frost line height, and additive masterbatch loading. A meaningful comparison between Icorene 1761 BWN 8810 and another film resin therefore requires fixed film gauge, fixed die gap, and identical bubble geometry.

    What Are the Operational Boundaries for Thin-Gauge Frozen Food Packaging?

    Low-temperature packaging requires puncture and tear resistance at service conditions. Standard dart impact and tear tests are conditioned at 23 °C and 50% relative humidity; subambient measurements can be conducted in a conditioned chamber as comparative tests, but the standard condition is 23 °C unless otherwise agreed. The ductile-to-brittle transition of metallocene LLDPE is lower than that of Ziegler-Natta butene-LLDPE of equivalent density because the homogeneous branching distribution prevents the long linear ethylene sequences that initiate brittle fracture at low deformation rates. For applications below -40 °C, validation on the actual film structure is mandatory.

    The grade contains no intentionally added UV stabilizers. Outdoor storage or frozen transport in sun-exposed containers requires an additional light-stabilizer masterbatch. In food-contact applications, the resin may be used within the framework of FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 as amended; the overall migration limit for plastic food-contact materials under Article 12 is 10 mg/dm². Converters remain responsible for compliance on the finished article because migration behaviour depends on the full structure, sealing conditions, and food simulant.

    Differentiating This Grade from Ziegler-Natta LLDPE and Lower-Density Metallocene Film Resins

    Compared with a Ziegler-Natta LLDPE of similar density and melt index, the metallocene grade has a narrower molecular weight distribution and a more uniform short-chain branching distribution. The conventional Ziegler-Natta resin typically contains a low-molecular-mass species that acts as an internal processing aid, lowering die pressure and improving bubble stability but also increasing extractables, reducing optical clarity, and delaying hot-tack formation. The metallocene resin shifts the property balance toward lower haze, lower seal initiation temperature, and lower extractables at the expense of more demanding bubble stability and higher specific extrusion energy.

    Compared with high-pressure LDPE, the metallocene resin has lower melt strength and less strain hardening. Extrusion bubble stability is therefore more sensitive to air-ring fluctuations, ambient drafts, and inconsistent frost line height. The compensating advantage is superior impact and tear resistance at equivalent film gauge, which permits downgauging in heavy-duty bags and produce packaging. Compared with lower-density metallocene film resins, a density of 0.918 g/cm³ provides a balance between modulus, dart drop impact, and blocking resistance. Lower density mLLDPE grades can raise impact strength but may reduce film stiffness and increase blocking unless an antiblock masterbatch is used.

    Blending with LDPE at 10–20 wt% is commonly used to improve bubble stability and melt strength. Addition levels above this can raise haze and reduce dart impact. In such blends, the minor LDPE phase increases extensional viscosity but also introduces long-chain branching that changes the shear viscosity curve. The converter should evaluate dart drop impact per ASTM D1709 and haze per ASTM D1003 at the target final gauge because the blend response is not linear with LDPE loading.