Lyondellbasell Icorene 1761 Bue 5914 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 981219
    Density 0.918 g/cm3
    Melt Index 1.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 8.27 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 600%
    Flexural Modulus 207 MPa
    Vicat Softening Point 95.0°C
    Melting Point 118°C
    Haze 8.0%
    Gloss 74%
    Coefficient Of Friction 0.20
    Dart Drop Impact 180 g
    Elmendorf Tear Strength Md 500 g
    Elmendorf Tear Strength Td 600 g

    As an accredited LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 BUE 5914 is typically packaged in 25 kg moisture-resistant bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL: 20 pallets, 55 x 25 kg bags per pallet, total 27.5 MT, securely shrink-wrapped and strapped for transport.
    Shipping Typically, LyondellBasell Icorene 1761 BUE 5914 is shipped as non-hazardous, free-flowing polyethylene pellets in moisture-barrier 25 kg bags or 1,000 kg bulk bags on pallets, or in bulk trucks/railcars. Transport under dry, ambient conditions; avoid heat, moisture, and contamination. No special dangerous goods labeling required. Store cool and dry.
    Storage Store Icorene 1761 BUE 5914 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Use clean pallets and avoid prolonged UV exposure. Handle to minimize dust and static. Maintain ambient temperatures, protect from physical damage, and follow local regulations.
    Shelf Life Store in a cool, dry, well-ventilated area away from direct sunlight; shelf life is two years in unopened original packaging.
    Application of LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene

    High-line-speed cast stretch film and the shear heating constraint

    LyondellBasell Icorene 1761 BUE 5914 is processed on five-layer cast stretch film lines as the primary skin and core component at 75–95 wt%, with the remaining mass balanced by a metallocene plastomer or high-pressure low-density polyethylene to modify cling, puncture resistance, and unwind behaviour. In this application, density 0.918 g/cm³ (ISO 1183-1:2019), melt mass-flow rate 1.0 g/10 min at 190 °C under 2.16 kg (ISO 1133-1:2022), and a DSC melting peak of approximately 119 °C (ISO 11357-3:2018) produce a narrow-molecular-weight-distribution rheology that permits die exit temperatures to be held within 240–260 °C. At draw speeds above 450 m/min, shear heating in the outermost die lip region raises the measured melt temperature by 3–6 °C, and die-lip oxidation can deposit local gel particles after continuous runs exceeding 72 h if lip cleaning is not scheduled. The downstream process uses a five-layer cast film line with slot die width 1,500–2,200 mm, die gap 0.8–1.2 mm, air gap 15–30 mm, chill roll temperature 15–25 °C, and line speed 300–600 m/min, producing machine-direction pre-stretch film at 12–23 µm thickness. Finished pallet wrap is tested for puncture propagation by ASTM D5748-95(2024) and cling by ISO 8295:1995; gauge uniformity is monitored by on-line beta transmission with a tolerance of ±1.5 µm. Compliance documentation for pallet-wrap films not intended for direct food contact references Directive 94/62/EC Annex II heavy-metal aggregate limits of 100 mg/kg for lead, cadmium, mercury, and hexavalent chromium, with REACH Regulation (EC) No 1907/2006 SVHC disclosure at the 0.1 wt% threshold. Terminal product types include 500-mm and 750-mm machine pallet wrap rolls, pre-stretched hand wrap, and high-elongation bundling film. An operational limitation is that increasing the metallocene LLDPE fraction above 95 wt% without a fluoropolymer processing aid can raise adaptor pressure fluctuation to 20–35 bar because the narrow molecular weight distribution lacks the shear-thinning contribution of long-chain branched polyethylenes, and melt temperatures above 265 °C for more than 5 min are to be avoided due to oxidative chain scission.

    When fresh-cut produce films are downgauged from 40 µm to 28 µm, haze and seal integrity become simultaneous constraints in vertical form-fill-seal operations. The three-layer blown-film structure incorporates LyondellBasell Icorene 1761 BUE 5914 at 60–80 wt% in the seal and core layers, with the balance consisting of a high-pressure low-density polyethylene selected for bubble stability; this formulation maintains the narrow metallocene molecular weight distribution while compensating the slight strain-hardening deficit of linear chains. Compliance for direct food contact structures is established under Regulation (EU) No 10/2011 Annex II with overall migration below 10 mg/dm² for simulant testing, FDA 21 CFR 177.1520 for olefin polymers, and Commission Regulation (EC) No 2023/2006 good manufacturing practice. The downstream extrusion process uses a three-layer blown-film die of 200–300 mm diameter, die gap 1.8–2.4 mm, blow-up ratio 2.2–2.8, and frost line height 700–1,000 mm, with melt temperature held at 190–225 °C and internal bubble cooling maintaining output between 300–500 kg/h. Optical haze after conversion is measured under ISO 14782:2021, and dart impact is measured under ISO 7765-1:2004 Method A. Terminal film products include fresh produce pillow pouches, frozen vegetable bags, and pre-washed salad packaging. A production-scale instability is observed when the LDPE fraction falls below 20 wt% at blow-up ratios above 3.0: bubble flutter at the frost line introduces gauge bands of ±4 µm, and web breaks at the post-nip collapsing frame increase significantly. If pellet surface moisture is suspected from storage at RH > 70%, hopper drying at 60–70 °C for 2–4 h is required before processing to prevent torpedo void defects in the film.

    In lamination sealant webs for adhesive-laminated pouches, the grade is introduced as the heat-sealing plies at 85–100 wt%, with the remaining 0–15 wt% assigned to a metallocene plastomer or an anti-block masterbatch to control blocking during roll storage after corona treatment. Seal-initiation temperature in this configuration is controlled by the metallocene short-chain branch distribution; published data for this exact additive combination is limited, but commercial laminators typically set crimp-seal jaw temperatures at 95–115 °C when the sealant web thickness is 30–50 µm. Industry compliance documentation follows Regulation (EU) No 10/2011 total migration limits and FDA 21 CFR 177.1520 for food-contact olefins, with REACH declarations required at the 0.1 wt% SVHC threshold for downstream converters. The production sequence employs a three-layer cast-film line with slot die width 1,650–2,000 mm, die gap 0.7–1.0 mm, melt temperature 230–255 °C, and polished chill rolls set to 18–24 °C to achieve a surface roughness below 0.15 µm; after cooling, the web is corona-treated to 40–44 mN/m to support polyurethane or acrylic adhesive wetting. Coefficient of friction is monitored by ISO 8295:1995, and hot-tack force is measured on a J&B or equivalent hot-tack instrument according to ASTM F1921-12(2018). Terminal laminate structures include stand-up pouches, pillow pouches, lidding films for dairy and meat trays, and retort-adapted three-side-seal pouches where the sealant layer is not the sole retort-bearing ply. The operational boundary is set by blocking: if the anti-block concentration is reduced below 1,000 ppm while corona treatment exceeds 46 mN/m, roll blocking in the third unwind can produce telescoping and seal contamination at the laminator.

    When high dart impact resistance above 1,200 g is required, does the die gap need to exceed 2.4 mm?

    Heavy-duty sack and flexible intermediate bulk container liner structures represent a process window where die gap and blow-up ratio interact with the narrow molecular weight distribution of the metallocene LLDPE. In this application, LyondellBasell Icorene 1761 BUE 5914 is formulated at 60–80 wt%, with high-density polyethylene at 15–25 wt% to raise modulus and the balance as high-pressure low-density polyethylene to maintain extrusion homogeneity. Compliance for industrial packaging must satisfy Directive 94/62/EC heavy-metal limits at 100 mg/kg aggregate and, when the liner is used as an inner component of a UN-certified FIBC, the validation path under ISO 21898:2021 requires tensile and elongation testing of the woven outer/film inner composite. The downstream conversion is a three-layer blown-film line with die diameter 350–500 mm, die gap 2.4–3.0 mm, blow-up ratio 2.5–3.5, and melt temperature 200–235 °C; high-output internal bubble cooling sustains line output of 500–700 kg/h while maintaining frost line height at 1,000–1,500 mm. Terminal products include heavy-duty shipping sacks, FIBC liners for hygroscopic powders, and construction-grade liners. The die gap threshold of 2.4 mm is not arbitrary: when the gap is reduced to 2.0 mm at a blow-up ratio of 3.0, producers have reported dart impact values falling by 12–18% under ISO 7765-1:2004 Method A because the higher shear history freezes in machine-direction orientation and reduces transverse extensibility. Conversely, raising the HDPE fraction above 25 wt% improves creep resistance but produces a discontinuity in dart impact because the blend enters a co-continuous crystalline morphology and puncture propagation energy decreases. Melt temperature should not be raised above 245 °C to compensate for low die gap because oxidative gel formation accelerates at the mandrel lips and generates visible inclusions in the film.

    For bale wrap and silage covers exposed to UV radiation and repeated wind stress, LyondellBasell Icorene 1761 BUE 5914 is combined with a high-pressure low-density polyethylene at 70–80 wt% mLLDPE fraction in the polymer phase, while a UV-stabilizer masterbatch based on hindered amine light stabilizers and a benzotriazole UV absorber is dosed at 6–12 wt% of the outer layer formulation; the mid-layer retains the mLLDPE without high stabilizer loading to preserve dart impact and tear propagation resistance. Compliance for agricultural film is assessed against EN 13206:2017 for thermoplastic films used in agriculture and horticulture, including tensile and tear resistance after artificial weathering, with REACH SVHC documentation at 0.1 wt%. The extrusion process uses a three-layer blown-film die of 250–400 mm diameter, die gap 2.0–2.6 mm, blow-up ratio 2.5–4.0, and melt temperature 215–245 °C; slower frost line advancement is maintained by moderate internal bubble cooling to avoid quenching the UV-stabilized outer layer too quickly, which can cause additive bloom. Terminal products include silage bale wrap film, silo bags, and greenhouse repair sheeting. A documented incompatibility occurs when highly polar UV absorber masterbatches use certain carrier resins that phase-separate from the metallocene matrix at film thickness below 40 µm, producing visible gel specks and lowering tear resistance by more than 10% under ISO 6383-2:1983; converters therefore qualify each masterbatch lot by pilot extrusion before production runs. The shear-thinning mismatch between mLLDPE and low-grade LDPE in the outer layer can also generate melt fracture at the die lip if the LDPE melt flow index is more than 2.0 g/10 min higher than the mLLDPE base, requiring melt temperature increases of 5–8 °C or a switch to a wider die gap.

    If peel force tolerance is held to ±0.4 N/15 mm, the seal layer formulation changes

    Sterile barrier packaging for medical devices imposes a peel-force reproducibility window that is narrower than typical food-packaging seals. LyondellBasell Icorene 1761 BUE 5914 is employed in the sealant layer at 85–100 wt%, with the balance allocated to a metallocene plastomer or low-friction anti-block masterbatch to adjust seal initiation and handling. Compliance is anchored to ISO 11607-1:2019 for terminally sterilized medical device packaging, EN 868-5:2018 for paper and plastic film constructions, and FDA 21 CFR 177.1520 for the polymer component; extractables testing may be required under ISO 10993-18:2020 when the device contact claim is evaluated. The downstream process is a three-layer cast or blown film line housed in an ISO Class 7 clean room, with melt temperature 210–250 °C, die gap 1.0–1.6 mm, and on-line thickness control with gauge variation held to ±2 µm at 30–60 µm total film thickness. Sealing is performed on medical pouch machines at jaw temperatures 115–130 °C, dwell times 0.5–1.0 s, and pressure 2–4 bar, producing peel strength in the range 1.0–2.5 N/15 mm when measured by EN 868-5:2018 Annex D. Terminal product types include chevron pouches for syringes, tubing sets, surgical drapes, and ethylene oxide sterilized kit packaging. The central processing limit is that thickness variation exceeding ±2 µm in the sealant layer changes heat-transfer dynamics at the seal bar and widens peel force beyond the ±0.4 N/15 mm tolerance; if the mLLDPE fraction is reduced below 85 wt%, the seal initiation window shifts upward by 3–7 °C and may exceed the temperature at which Tyvek fibre tear is acceptable. Sterilization load data should be revalidated after any change in seal-layer addition ratio because ethylene oxide residue dissipation and water vapour transmission through the film are influenced by the metallocene crystalline distribution.

    Free Quote

    Competitive LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 BUE 5914 Polyethylene, Linear Low Density, Metallocene is a rotational-moulding-grade mLLDPE supplied as a dry powder. The base resin is produced by single-site catalysis, which controls short-chain branching placement and molecular weight distribution more narrowly than conventional Ziegler-Natta systems. The BUE 5914 suffix identifies a colour or stabiliser package; pigment carriers and stabiliser loadings can alter melt-flow behaviour, so process settings should be taken from the lot certificate and not from unpigmented base-resin data. The material is typically specified for rotationally moulded tanks, enclosures, liners, and industrial bodies requiring low-temperature impact resistance, thin-wall rigidity, and surface finish.

    Because published data for the exact BUE 5914 formulation is limited, the following representative ranges are drawn from metallocene LLDPE rotational-moulding powders with similar density and melt-flow profiles and should be replaced by lot certificates for production validation. In preliminary process design, the powder is typically specified with a density of 0.924–0.936 g/cm³ per ISO 1183-1:2019, a melt flow rate of 0.45–0.80 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022, and a bulk density of 0.35–0.42 g/cm³ per ISO 60. Powder dry-flow for rotational moulding grades is commonly 25–35 s/100 g per ASTM D1895, and the particle size distribution shows a D50 of 300–600 µm per ASTM D1921.

    What Distinguishes Single-Site mLLDPE from Ziegler-Natta LLDPE in Rotomoulding Powder Grades?

    Single-site catalysis in mLLDPE yields a narrow comonomer distribution and a lower catalyst-residue profile, but also a sharper melting peak. This affects processing differently from conventional Ziegler-Natta LLDPE. In rotomoulding, a narrower melting endotherm reduces the temperature interval between incomplete bubble removal and oxidative degradation. On a shuttle machine with a 2.5 m arm, a peak internal air temperature of 200–220°C is normally sufficient for metallocene grades, while Ziegler-Natta LLDPE may require 220–240°C for comparable surface quality. Excessive internal air temperatures above 230°C for more than 5 min can cause yellowing and inner-surface porosity in mLLDPE because the polymer has low melt viscosity after complete melting and limited tolerance to prolonged air exposure. The observed field failure mode is pinhole clusters near vents and weld lines when oven residence time is increased to compensate for thin-wall underfill.

    PropertyTest standardMetallocene LLDPE envelopeZiegler-Natta LLDPELDPEHDPE
    DensityISO 1183-1:20190.924–0.936 g/cm³0.918–0.940 g/cm³0.917–0.935 g/cm³0.940–0.970 g/cm³
    Melt flow rate at 190°C/2.16 kgISO 1133-1:20220.45–0.80 g/10 min0.30–0.80 g/10 min0.20–0.80 g/10 min0.30–0.80 g/10 min
    Tensile yield stressISO 527-2:201212–18 MPa11–17 MPa8–12 MPa22–28 MPa
    Tensile modulusISO 527-2:2012250–450 MPa280–450 MPa150–250 MPa800–1200 MPa
    Vicat softening temperatureISO 306:2022104–118°C104–118°C85–95°C120–126°C

    On a production-scale shuttle rotational-moulding machine with a 2.5 m arm and a single-chamber oven, a 15 kg charge of Icorene 1761 BUE 5914 is heated at an oven temperature of 280–300°C for sections of 4–6 mm wall thickness. Heating time is typically 12–18 min for steel tooling; sections of 8–12 mm require 20–28 min. The powder bed passes through tackifying, densification, and melt-out stages. Instrumented trials on similar mLLDPE powders have shown that part density and impact strength plateau near a peak internal air temperature of 205°C, with no measurable gain in tensile modulus per ISO 527-2:2012 beyond this point.

    Cooling after demoulding is a critical control point. Forced air at 0.5–1.5 m/s followed by a water mist is applied to bring the part surface from 180°C to 80°C over 8–15 min. Cooling rates above 25°C/min through the crystallization plateau can increase warpage in flat panels with thickness below 3 mm. Slow cooling below 5°C/min extends cycle time and may coarsen crystalline aggregates, reducing low-temperature impact. This sensitivity is more pronounced in metallocene LLDPE than in Ziegler-Natta LLDPE because the narrower crystallite size distribution produces a sharper solidification front.

    Storage and handling of Icorene 1761 BUE 5914 should follow standard rotational-moulding powder practice. Storage below 40°C in sealed packaging avoids compaction and oxidative ageing. Pre-drying is not required at relative humidity below 60%; however, condensation onto cold powder can increase surface moisture and cause bubble defects when the powder is charged directly into a hot mould. If the powder is exposed to cyclic temperature swings, controlled hopper drying at 60–80°C for 1–2 h is applied before processing to restore dry-flow.

    When the End-Use Requires Food-Contact Compliance and Low Extractables

    Food-contact status for Icorene 1761 BUE 5914 is not an inherent property of the polymer backbone; the final article must be evaluated with the exact stabiliser and pigment package. For compliance with U.S. FDA 21 CFR 177.1520, the olefin polymer must meet the extractives limitations and end-use conditions set out in that section. The BUE 5914 package may require additional extraction testing because pigments and processing aids can affect the overall extractables profile. In the European Union, rotomoulded parts are assessed under Regulation (EU) No 10/2011 and its amendments. Overall migration into food simulants is limited to 10 mg/dm² for general food-contact plastics, tested according to the EN 1186 series. Specific migration limits apply to authorised monomers and additives. Article conformity requires migration testing on the final pigmented part, not on unpigmented base powder.

    For industrial and electrical enclosures, the material is commonly checked against REACH and, where applicable, RoHS 2011/65/EU. The supplier declaration should confirm that candidate-list substances of very high concern are below 0.1% w/w in the finished article. The presence of a coloured package in BUE 5914 may require wet-chemical screening for cadmium, lead, hexavalent chromium, mercury, and brominated flame retardants, because colour concentrates can contain regulated metal-based pigments.

    RegulationScopeTest method or conditionRequired result
    FDA 21 CFR 177.1520Olefin polymers for food contactEnd-use extraction per FDA specificationsSupplier compliance; final article testing
    EU Regulation 10/2011Plastic food-contact materialsEN 1186 overall migration≤ 10 mg/dm²
    REACHSubstances in articlesSVHC candidate-list declaration< 0.1% w/w
    RoHS 2011/65/EUElectrical/electronic equipmentXRF or wet-chemical screeningPb, Hg, Cd, Cr(VI), PBB, PBDE limits

    Brittle Impact Transition and Low-Temperature Toughness in Thin-Walled Parts

    Metallocene LLDPE retains impact resistance at low temperatures because the homogeneous short-chain branching distribution limits high-density regions that can initiate brittle fracture. For rotational-moulded parts, instrumented impact testing is carried out at -20°C to -40°C using ISO 6603-2 or ASTM D3763. Comparative studies with the same part thickness and cooling history generally show higher energy-to-peak force for mLLDPE than for Ziegler-Natta LLDPE of the same density. The brittle-to-ductile transition temperature is often lower by 5–15°C, but the actual BUE 5914 lot should be tested on the target part because impact performance is sensitive to peak internal air temperature, cooling rate, and part thickness.

    Compared with LDPE, the mLLDPE class of Icorene 1761 BUE 5914 offers higher tensile yield stress and better environmental stress-cracking resistance, but lower melt strength, which can be a limitation in large open-mould surfaces and complex vertical walls. Compared with HDPE, the lower density reduces stiffness and elevated-temperature creep resistance but improves flexibility and low-temperature impact. Compared with Ziegler-Natta LLDPE, the metallocene architecture provides higher gloss and lower haze at the same thickness, measured per ISO 2813 and ISO 14782; however, the narrower molecular weight distribution can produce lower orientation-induced hardening in fast-cooled sections. For rotational moulding, those differences translate into improved outer-surface appearance and more uniform wall thickness at equivalent powder flow, provided the peak internal air temperature is held within the narrow mLLDPE window.

    Mechanical property validation for production parts should follow ISO 291 conditioning at 23°C/50% RH and ISO 527-2:2012 tensile testing at a test speed of 50 mm/min. Because rotomoulded parts are anisotropic, test specimens should be extracted from both inner and outer surfaces and, for large tanks, from the top and bottom regions. Density determinations per ISO 1183-1:2019 on cut sections can detect incomplete densification or voiding; a density drop of more than 0.002 g/cm³ from the certified powder value indicates undercure or trapped air.