| HS Code | 387578 |
| Density | 0.918 g/cm³ |
| Melt Mass Flow Rate Mfr 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Temperature | 118 °C |
| Vicat Softening Temperature | 95 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 25 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 200 MPa |
| Hardness Shore D | 50 |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 100 g/mil |
| Elmendorf Tear Strength Td | 200 g/mil |
| Haze | 5% |
| Gloss | 80% |
| Coefficient Of Friction | 0.20 |
As an accredited LyondellBasell Icorene 1761 BUE 5533 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Available in 25 kg polyethylene bags or 1,000 kg bulk bags, typically palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with metallocene linear low-density polyethylene, LyondellBasell Icorene 1761 BUE 5533, in 25 kg bags on pallets. |
| Shipping | LyondellBasell Icorene 1761 BUE 5533 is shipped as non-hazardous, solid metallocene linear low-density polyethylene pellets. Standard packaging includes 25 kg PE bags, octabins, or bulk trucks/railcars. Store in a cool, dry area, away from direct sunlight, moisture, and ignition sources. No special hazardous transport classification is required. Handle using normal warehouse practices. |
| Storage | Store LyondellBasell Icorene 1761 BUE 5533 polyethylene in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid excessive stacking or pressure. Store separately from incompatible materials, protect from physical damage, and follow manufacturer recommendations. |
| Shelf Life | Shelf life is typically 24 months from production when stored unopened in original packaging, cool, dry, and protected from sunlight. |
Machine-direction-oriented pallet wrap manufactured on high-speed cast film lines is the principal downstream conversion route for Icorene 1761 BUE 5533 when film gauge below 12 µm and pre-stretch ratios above 200% are specified by end users. In production-scale formula practice, the metallocene linear low density polyethylene is introduced at 70–85 wt% of the total polymer phase, with LDPE extrusion modifier at 10–20 wt%, polyisobutylene tackifier at 0.5–2.0 wt%, and a slip/antiblock masterbatch at 0.5–1.5 wt%. The LDPE component is not a filler but a melt strength modifier that stabilises the edge region of the web and reduces neck-in on chill roll quench systems. Industry compliance for the film is anchored to ISO 527-3 for tensile properties, ASTM D5748 for puncture resistance, ASTM D5458 for cling/peel, and ASTM D1894 for coefficient of friction; under REACH EC 1907/2006, SVHC screening is mandatory, while direct food contact is generally not claimed for industrial pallet wrap, so EU Directive 94/62/EC recycling and marking duties apply instead of food-contact migration limits. The downstream production process typically employs a five-layer cast line with die widths between 1,800 mm and 2,500 mm, a polished chill roll held at 18–32 °C, an air gap of 150–250 mm, and edge pinning by air knife or vacuum box; melt temperature at the die is maintained between 210 °C and 240 °C, while power-driven pre-stretch rollers impose an elongation of 200–300% immediately before wrapping. Failure modes observed on high-speed cast lines include film tear propagation at the unwind after pre-stretch when the slip agent has migrated excessively, and gauge bands caused by inadequate die lip adjustment at speeds above 500 m/min. An operational boundary is that melt residence time above 250 °C can generate gel particles, and edge trim recycle above 20 wt% is not recommended because transverse direction tear resistance measured by ASTM D1922 declines disproportionately at gauge below 12 µm. The terminal finished product is 12–23 µm machine-grade stretch film in 500 mm roll widths and 1,500 m linear lengths for rotary-arm and turntable pallet wrappers used in warehouse logistics.
Blown-film conversion of Icorene 1761 BUE 5533 into gusseted heavy-duty shipping sacks and industrial box liners requires a three-layer die configuration because the metallocene resin alone does not provide the bubble stability needed at high blow-up ratios. The formulation addition ratio in the core layer is 55–70 wt% mLLDPE, with 20–35 wt% LDPE as melt strength modifier, 5–15 wt% HDPE or a colour masterbatch for stiffness, and 0.5–1.0 wt% fluoropolymer processing aid; above 60 wt% mLLDPE, bubble diameter oscillation typically increases unless an internal bubble cooling system and a segmented air ring are installed. Compliance testing for the finished sack follows ISO 527-3 for tensile, ASTM D1709 for falling dart impact, ISO 7965-2 for vertical drop, and ASTM D1922 for tear propagation; dangerous goods sacks are further qualified under the UN drop protocol referenced in ADR/IMDG for solids, and EU packaging waste obligations are set by Directive 94/62/EC. On a production extruder with a 250–350 mm die, 1.6–2.0 mm die gap, and 2.0:1–2.5:1 blow-up ratio, the frost line is fixed at 3–5 die diameters above the die to control blocking and dart impact retention; melt temperatures are held at 195–215 °C, and backpressure must remain within the extruder manufacturer’s thrust-bearing limit, commonly below 35 MPa, to avoid excessive screw wear. A known production failure mode is melt fracture at the die lip when the processing aid level is below 0.3 wt% or when the die gap is reduced below 1.2 mm without increasing the melt temperature. The terminal product is 80–120 µm gusseted shipping sacks and liners for 25 kg to 50 kg packaging of polymer pellets, fertilizers, and mineral fillers.
In triplex laminated structures for dry food and medical device packaging, the sealant web is produced from Icorene 1761 BUE 5533 because the narrow molecular weight distribution lowers the seal initiation temperature while preserving hot-tack strength during vertical form-fill-seal operations. The sealant layer formulation consists of 70–85 wt% of the metallocene LLDPE, 10–20 wt% LDPE or plastomer, 1,000–3,000 ppm silica antiblock, and 500–1,200 ppm erucamide slip; the slip agent is deliberately kept below 1,500 ppm because migration above that level reduces laminate bond strength after solventless adhesive is applied. When direct food contact is claimed, the converter must document compliance under FDA 21 CFR 177.1520 for olefin polymers and under EU Regulation (EU) No 10/2011 with migration testing per EN 1186-1; seal performance is measured according to ASTM F88/F88M for seal strength, ASTM F1921 for hot tack, and ISO 14782 for haze. The downstream conversion of the sealant web is performed on a five-layer coextrusion blown film line with a 250 mm die, 1.2 mm die gap, and 2.0:1 blow-up ratio; melt temperature is controlled at 190–210 °C, and the resulting 20–30 µm web is subsequently laminated to biaxially oriented PET or BOPP on a solventless laminator running at 80–120 m/min with nip roll temperature of 60–75 °C. A production limitation observed on packaging lines is that hot-tack performance under ASTM F1921 becomes dependent on cooling air temperature when the sealing bar dwell time falls below 0.3 s; published data for this specific sealant configuration is limited, so pilot-line validation is required rather than extrapolation from resin datasheet values. The terminal products are stand-up pouches, flow-wrap packs, and lidding films for dry foods, pharmaceutical powders, and non-aseptic medical device pouches.
Breathable diaper backsheet production requires a filled compound in which Icorene 1761 BUE 5533 acts as the carrier resin at calcium carbonate loadings of 45–60 wt%, because the metallocene resin’s narrow molecular weight distribution permits web survival during machine-direction orientation. The total formulation contains 30–45 wt% metallocene LLDPE, 45–60 wt% ground calcium carbonate, 1–3 wt% titanium dioxide, and 0.5–1.5 wt% polymer processing aid; an additional 5–10 wt% LDPE may be introduced to lower extruder pressure and reduce motor load at filler loadings above 55 wt%. Biocompatibility for skin contact is assessed under ISO 10993-10 for irritation and sensitization, while general product safety compliance is maintained through REACH EC 1907/2006 and the General Product Safety Directive 2001/95/EC; water vapour transport is measured by ASTM E96/E96M and air permeance by ASTM D737. The production sequence uses a cast film line with a flat die gap of 0.8–1.0 mm, extrusion temperature of 200–230 °C, and an embossed casting roll maintained at 25–40 °C; the film is then heated to 70–90 °C and stretched in machine direction at a draw ratio of 1.5:1–3.5:1 between a series of independent heater rolls. The critical operational boundary is that tensile break in the oriented web occurs when draw ratio exceeds 3.5:1 at film thickness below 15 µm, producing film breaks and requiring a reduction in calcium carbonate particle size below 5 µm median diameter. The specific moisture vapour transmission rate for this formulation requires validation on pilot-scale MDO equipment because laboratory cast sheet data do not reliably predict pore structure development. Terminal finished goods are 15–30 g/m² breathable backsheets supplied in slit reels for diaper, adult incontinence, and sanitary napkin production lines.
For agricultural silage bale wrapping, Icorene 1761 BUE 5533 is selected as the primary cling film component because the finished film must withstand tearing and puncture from plant stems while maintaining anaerobic fermentation conditions over several months outdoors. The formulation addition ratio is 75–90 wt% mLLDPE, 5–15 wt% LDPE, 2–6 wt% white or black masterbatch containing titanium dioxide and hindered amine light stabilizers at 0.3–0.8 wt% active additive, and 0.5–2.0 wt% polyisobutylene tackifier; the upper mLLDPE limit is constrained by cling noise and unwind stability in cold weather below 5 °C. Product performance is certified under EN 14932, which sets requirements for elongation at break, puncture resistance, cling, and UV durability, with additional screening under ISO 527-3 and ASTM D5748. The downstream production process is a three-layer cast stretch film line with die width between 1,500 mm and 2,000 mm, chilled rolls at 20–30 °C, and an embossing pattern selected to provide air release during bale wrapping; the film is wound onto 500 mm reels and applied on bale wrappers at 55–70% pre-stretch, yielding a final stretched thickness of 20–30 µm. A field failure mode observed in agricultural wrap converting is split propagation at the bale edge when the UV stabilizer package is depleted before the storage period ends, so the HALS additive must be compounded at the higher end of the stated range for films intended for overwinter storage. The terminal article is 500 mm × 1,500 m and 750 mm × 1,500 m bale wrap rolls in black or white used for round bales of fermented forage.
Multi-pack collation shrink film for beverage cans and bottled water bundles is another downstream route where tear strength measured by ASTM D1922 and low-temperature sealability support thin-gauge shrink webs. In this application, Icorene 1761 BUE 5533 is blended at 50–70 wt% with 20–40 wt% LDPE and 5–10 wt% plastomer or EVA; slip and antiblock masterbatch is added at 0.5–1.5 wt% to prevent blocking of printed film on the shrink packaging machine. Industry compliance includes ISO 14616 for shrink stress and contraction stress, ASTM D2732 for unrestrained linear thermal shrinkage, ISO 527-3 for tensile, and ASTM D1922 for tear; print adhesion is qualified under ASTM F2252 or equivalent internal ink adhesion protocols. The conversion process is based on a high-stalk blown film line with a die diameter of 200–300 mm, die gap of 1.0–1.4 mm, blow-up ratio of 2.5:1–3.0:1, and frost line height sufficient to freeze in transverse direction orientation; the resulting 50–70 µm film is printed and slit, then passed through a shrink tunnel at 140–160 °C on packaging lines running at 60–120 packs/min. The operational boundary is that an mLLDPE fraction above 70 wt% can reduce final transverse shrinkage below the level required to stabilise the bundle; the exact balance must be tuned with a blown film extrusion trial because the shrink force measured by ISO 14616 is nonlinear with blend ratio. Terminal finished products are printed collation shrink films used to bundle aluminium beverage cans, bottled water multipacks, and club-store consumer units.
Competitive LyondellBasell Icorene 1761 BUE 5533 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 BUE 5533 is a metallocene-catalyzed linear low density polyethylene (mLLDPE) supplied as a pelletized extrusion grade. The grade carries a nominal density of 0.917 g/cm³ and a nominal melt flow rate of 6.1 g/10 min at 190 °C/2.16 kg when determined according to ASTM D1238 / ISO 1133-1. Density is controlled under ASTM D1505 / ISO 1183-1. The alphanumeric designation BUE 5533 identifies the additive package; because slip, antiblock, and stabilization levels are part of this suffix, substitution of a different suffix should require revalidation of film coefficient of friction, blocking, and organoleptics. The product is intended primarily for cast-film, monolayer, and coextruded film structures where low seal initiation, low haze, and high dart impact at reduced thickness are required.
| Property | Test method | Typical control envelope |
|---|---|---|
| Melt flow rate | ASTM D1238 / ISO 1133-1 | 6.1 g/10 min at 190 °C/2.16 kg |
| Density | ASTM D1505 / ISO 1183-1 | 0.917 g/cm³ |
| Moisture at packaging | Karl Fischer | ≤ 0.02 wt% |
| Tensile at break MD/TD | ASTM D882 | 40–50 MPa / 30–40 MPa |
| Elongation at break MD/TD | ASTM D882 | 600–750% / 650–800% |
| Dart drop F50 | ASTM D1709 Method A | 300–500 g at 25 µm |
| Elmendorf tear MD/TD | ASTM D1922 | 50–70 g / 70–90 g |
| Haze | ASTM D1003 | 1.5–3.0% |
| Gloss 45° | ASTM D2457 | 70–85 GU |
| Seal initiation | ASTM F2029 | 85–95 °C |
Values in the table are typical control envelopes for mLLDPE of this density and melt flow class; the supplier’s certificate of analysis governs lot-specific release.
Because the metallocene active site produces a narrow molecular weight distribution and more uniform short-chain branching than a conventional Ziegler-Natta catalyst system, the film contains fewer highly crystalline clusters that scatter light and fewer amorphous fractions that create weak boundary layers. In force, a 25 µm cast film typically shows haze below 3.0% per ASTM D1003 and a 45° gloss above 70 GU per ASTM D2457, although values depend on chill-roll finish and die selection. Dart drop impact per ASTM D1709 Method A frequently falls in the 300–500 g band, and Elmendorf tear per ASTM D1922 may show transverse-direction values higher than machine-direction values by 10–30%. These failure properties do not transfer directly to asymmetric coextruded structures; a sealant layer side of 8–15 µm may exhibit different tear propagation unless the overall film is evaluated.
The lower extractables of mLLDPE are exploited in food-contact film where organoleptic performance is sensitive to hexane-extractable content. Extraction values should be measured according to FDA 21 CFR 177.1520 test protocols or EU Regulation (EU) No 10/2011 migration testing; the base resin does not exempt the fabricated film from article-level compliance. Compared with a high-pressure LDPE of equivalent density, the grade lacks long-chain branching and therefore exhibits lower melt strength, more Newtonian shear behavior, and a narrower bubble-stability window on conventional blown-film equipment. This limitation is a direct consequence of the molecular architecture and is not a defect; it requires processing adjustments such as internal bubble cooling, lower stalk heights, and adequate blow-up ratio. Published data for the specific polydispersity index and long-chain branching level of this grade is limited; however, the processing behavior is consistent with an mLLDPE of this density and melt flow class.
| Attribute | Icorene 1761 BUE 5533 mLLDPE | Conventional C4 Ziegler-Natta LLDPE | High-pressure LDPE |
|---|---|---|---|
| Density | 0.917 g/cm³ | 0.917–0.920 g/cm³ | 0.917–0.924 g/cm³ |
| Melt flow rate | 6.1 g/10 min | 1.0–2.0 g/10 min | 0.3–8.0 g/10 min |
| Molecular architecture | Narrow MWD, uniform comonomer | Broad MWD, heterogeneous comonomer | Long-chain branched |
| Seal initiation | Low, typically 85–95 °C | Higher than mLLDPE | Low but lower hot-tack strength |
| Bubble stability | Moderate-low without internal bubble cooling | Better than mLLDPE | High bubble stability |
| Extractables | Low, food-contact film use | Higher than mLLDPE | Higher than mLLDPE for certain additive systems |
Processors running cast-film lines may begin with die gaps of 0.4–0.8 mm, melt temperatures between 190 °C and 230 °C, and chill-roll temperatures from 18 °C to 25 °C. On a 90 mm single-screw extruder with a 30:1 L/D barrier screw and screen pack of 60/80/100 mesh, the 6.1 g/10 min melt flow rate reduces head pressure compared with a 1.0 g/10 min metallocene grade, which can be used to increase throughput or to lower melt temperature. The reduction in pressure should not be confused with improved thermal stability; residence time and free-volume in the feed section remain primary controls for gels and unmelts. If pellet surface moisture exceeds 0.02 wt%, predrying at 70–80 °C for 2–4 h is recommended before deep-draw cast-film lines, especially at relative humidity above 60%.
For blown-film operations, the lack of long-chain branching narrows the stable processing envelope. Bubble stability is maintained by using blow-up ratios between 2.0:1 and 2.8:1, short stalk heights, and internal bubble cooling where available. Without internal bubble cooling, frost-line height variations above ±20 cm can generate gauge bands and tear anisotropy. The film should be corona treated to a wetting tension of at least 38 mN/m per ASTM D2578 if it will be laminated or printed; this grade is not a tie resin and will not bond to polyester, polyamide, or aluminum without a adhesive tie layer.
Extrusion coating and laminating trials should use a draw distance of 150–250 mm from die to nip and an air gap sufficient to promote oxidation without excessive neck-in. Because metallocene LLDPE has faster crystallization and lower melt strength than LDPE, neck-in may be higher; converting lines that previously ran LDPE may require a narrower die or edge-pinning air knives.
Film structures that use this grade as a sealant layer in coextruded food packaging generally place the mLLDPE layer at 8–15 µm in a total film of 40–80 µm. The grade can also be used in monolayer produce bags, industrial liners, and lamination films. Compliance with FDA 21 CFR 177.1520 supports use in food-contact olefin polymers, but finished-article testing under EU Regulation (EU) No 10/2011 remains necessary for European Union markets. Oxygen transmission rate should be measured by ASTM D3985 or ISO 15105-2; water vapor transmission rate should be measured by ASTM F1249 or ISO 15106-3. The product is not designed for injection molding, rotomolding, or thick-wall profiles; its melt flow rate and narrow molecular weight distribution are optimized for film applications.
A reduction in film thickness from 25 µm to 15 µm does not produce linear changes in impact and tear. Dart drop impact can fall more rapidly than the thickness ratio would predict because impact energy absorption depends on local yielding and crack propagation through a thinner ligament. Lot acceptance should include ASTM D882 tensile at break, ASTM D1922 Elmendorf tear, ASTM D1709 dart drop, and ASTM F2029 seal initiation. Thickness-normalized tensile values may hide surface defects; therefore, gel and contaminant assessment per ASTM D7310 and optical inspection under polarized light are advisable for high-speed converting.
The highest risk in cast film is anisotropic orientation. If machine-direction orientation dominates, transverse-direction Elmendorf tear may decline disproportionately and cause directional splitting in bag-making. An internal control ratio of machine-direction to transverse-direction tear between 0.8 and 1.4 after conditioning at 23 °C and 50% RH for 48 h per ASTM D618 is one practical response; the exact ratio depends on die gap, line speed, and chill-roll temperature. Seal strength should also be revalidated at the lower sealant thickness because ASTM F88/F88M seal strength depends on the sealed area and cannot be maintained merely by raising sealing temperature without risking film distortion.
Compliance with food-contact regulations is not conferred by base-resin classification alone. Film converters must perform migration testing per EU Regulation (EU) No 10/2011, which sets an overall migration limit of 10 mg/dm² for plastic materials and articles. Simulant selection under Annex III may include 10% ethanol as simulant A, 3% acetic acid as simulant B, 20% ethanol as simulant C, 50% ethanol as simulant D1, vegetable oil as simulant D2, or Tenax as simulant E, depending on the food type and contact conditions. Under FDA 21 CFR 177.1520, the polymer may be used in contact with food, but the finished article must still meet end-use limitations and any additive-specific clearances. The BUE 5533 additive package must be reviewed against regional positive lists because slip or antiblock dosage can affect specific migration limits.
The grade should not be stored or processed near high levels of organic peroxides, free-radical initiators, or strong oxidizing agents. Avoid blending with unclassified post-consumer recyclate containing calcium oxide desiccants or high filler loadings, because these can shift the density and melt flow rate outside the control window and may neutralize part of the stabilizer package. If silo storage exceeds 6 months, verify melt flow rate, density, and moisture before processing. Film that will be sealed against high-density polyethylene or polypropylene substrates should be checked for seal compatibility at the lower end of the sealing temperature range, because the sealant layer’s low melting point does not guarantee adhesion to surfaces with higher crystallinity.