Lyondellbasell Icorene 1761 Bue 5507 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BUE 5507 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BUE 5507 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 208013
    Density 0.917 g/cm3
    Melt Flow Rate 190c 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 35.0 MPa
    Elongation At Break 700 %
    Flexural Modulus 200 MPa
    Vicat Softening Temperature 96 C
    Melting Temperature 122 C
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 6 %
    Gloss 45 80
    Coefficient Of Friction 0.20

    As an accredited LyondellBasell Icorene 1761 BUE 5507 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 BUE 5507 supplied in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg), shrink-wrapped.
    Container Loading (20′ FCL) 20' FCL container loaded with LyondellBasell Icorene 1761 BUE 5507 LLDPE metallocene, typically 25 kg bags on pallets, securely stowed.
    Shipping LyondellBasell Icorene 1761 BUE 5507 is shipped as non-hazardous solid metallocene linear low density polyethylene pellets, typically in 25 kg bags or bulk octabins on pallets. Standard dry truck or container transport. Store cool, dry, away from direct sunlight and ignition sources; handle with normal industrial equipment.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures above 50°C. Protect from physical damage. Use good housekeeping to control dust and static. Follow first-in, first-out stock rotation.
    Shelf Life Store in original unopened packaging in a cool, dry place away from sunlight; typical shelf life is 24 months from production.
    Application of LyondellBasell Icorene 1761 BUE 5507 Polyethylene, Linear Low Density, Metallocene

    Sealant-Layer Substitution in Three-Layer Coextruded Food Packaging

    LyondellBasell Icorene 1761 BUE 5507 metallocene linear low-density polyethylene is incorporated as a sealant-layer component at 20–35 wt% of the layer formulation in three-layer coextruded food packaging, with the balance typically a C8-LLDPE of 0.918–0.920 g/cm³ density or an LDPE of 0.923–0.925 g/cm³ density to preserve bubble stability. The metallocene-catalyzed narrow composition distribution lowers seal initiation temperature and supports seal-through-contamination performance, but the same molecular architecture reduces bubble melt strength. Operators therefore maintain a die gap of 2.0–2.4 mm, a blow-up ratio of 2.2–2.8, and melt temperature between 185 °C and 210 °C, depending on line speed and frost-line position. Predrying is not normally required; if outdoor silos exceed 60% relative humidity, a dry-air purge of the hopper is recommended to avoid surface moisture streaking. Seal strength is validated according to ASTM F88/F88M, dart impact according to ASTM D1709 Method A or B, and tensile according to ASTM D882. EU food-contact compliance is assessed under Commission Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm²; US compliance is assessed under FDA 21 CFR 177.1520(c). Addition of Icorene 1761 BUE 5507 in the sealant layer may increase extruder torque by 5–15% relative to a Ziegler-Natta C8-LLDPE of equal melt index because the narrow molecular weight distribution and low long-chain branching concentrate shear stress. Terminal forms include printed pouch webs, pillow packs, and lidstock for dairy and fresh-cut produce.

    Jurisdiction / StandardReferenceTest or RequirementRelevant Value
    EU food-contactCommission Regulation (EU) No 10/2011Overall migration10 mg/dm²
    US food-contactFDA 21 CFR 177.1520(c)Olefin polymer specificationMigration cell testing required
    Seal strengthASTM F88/F88MHeat-seal forceRecorded at 180–210 °C seal jaw temperature
    Dart impactASTM D1709Falling dartMethod A/B depending film gauge
    TensileASTM D882TD/MD tensile strengthReported at 23 °C and 50% RH

    What Changes in High-Draw Cast Stretch Film When Metallocene LLDPE Replaces C8-LLDPE?

    Installation trials on cast stretch-film lines with 55–75 rpm extruder screw speeds and 0.5–0.8 m die widths indicate that Icorene 1761 BUE 5507 is not used as a 100% replacement in pallet-unitization film; it is dosed at 10–25 wt% of the total formulation in a C8-LLDPE-rich skin layer or as a core-layer modifier. The precise addition ratio is set by the required puncture-propagation tear balance: higher levels above 30 wt% can reduce tear resistance in the transverse direction and increase neck-in at the air gap. Process conditions include chill-roll temperatures between 18 °C and 24 °C, an air gap of 10–15 cm, and line speeds of 450–750 m/min on high-speed lines. Because of the narrow melting range, the grade responds poorly to wide melt-temperature fluctuations, and barrel zones are maintained within ±5 °C of set-point to avoid gel formation. Performance is tested under ASTM D5748 for stretch wrap properties, ASTM D5458 for cling, and ASTM D1922 for Elmendorf tear. Regulatory compliance for industrial non-food wrap is typically limited to REACH registration and RoHS 2011/65/EU where electronic goods are wrapped; food-contact migration testing under EU 10/2011 is unnecessary for pallet wrap but may apply if the film is used in direct food transport. Terminal finished goods include machine stretch film, hand wrap, and pre-stretched reels for load containment.

    Across tandem extrusion-lamination lines processing aluminum foil, PET, and oriented polyamide webs, Icorene 1761 BUE 5507 functions as the polymer melt in the coating nip at application weights of 15–25 g/m², representing 100% of the applied polymer layer in monolayer coatings or 20–40 wt% of a coextruded sealant skin when adhesion to the substrate is managed by an adjacent adhesive polymer. The low gel count and narrow molecular weight distribution permit line-speed trials above 300 m/min, but neck-in and edge-bead formation must be controlled by die-edge heating and reduced air gap. Edge trim increases by 1.5–3.0% when switching from LDPE of equivalent melt index because the metallocene grade exhibits less strain-hardening in the draw-down zone. Industry compliance references include FDA 21 CFR 177.1520(c) for olefin polymer coatings in contact with aqueous and fatty foods, EU Regulation (EU) No 10/2011 with overall migration limit 10 mg/dm², and EN 13432 only when downstream compostability is required and the coating is thin enough to meet disintegration thresholds; published data for this specific grade in compostable structures is limited. Terminal finished product types include coffee-brick inner liners, retort pouch outer ply sealants, and barrier lidding for aseptic cups.

    When Gauge Reduction Outweighs Material Cost in Heavy-Duty Sack Extrusion

    Where heavy-duty sack producers seek 15–25% gauge reduction without sacrificing drop impact, Icorene 1761 BUE 5507 is introduced into a five-layer blown-film matrix at 20–40 wt% of the core layer, with outer layers composed of HDPE or LDPE for stiffness and surface friction. The mLLDPE component raises hot-tack strength and improves the balance between extrusion-direction tear and dart-impact energy; however, blown-film lines with grooved-feed extruders of L/D 30 may require screw-speed reductions of 8–12% to avoid melt-temperature overshoot because the narrow melting range generates a steep viscosity transition at the compression zone. Suitable process settings include die gap of 2.0–2.6 mm, blow-up ratio of 2.5–3.2, and melt temperature of 180–200 °C; corona treatment at 38–42 mN/m is applied to the print side if flexographic marking is required. Drop impact is measured according to ISO 7765-1 Method A, tear resistance according to ASTM D1922, and seal strength according to ASTM F88/F88M. Regulatory references for industrial non-food sacks are primarily REACH and, where indirect food contact is possible, EU No 10/2011; UN certification for dangerous goods packaging requires additional stack and drop tests under 49 CFR 178.603 or ADR/RID sections as applicable. Terminal goods include FIBC liner film, fertilizer sacks, and resin packaging bags.

    In greenhouse film extrusion on five-layer lines with 1.5–2.5 m dies, Icorene 1761 BUE 5507 is added at 10–25 wt% of the total polymer feed to improve dart impact and film toughness at thin gauges, allowing gauge reductions from 180 µm to 140 µm in specific thermal-screen designs. The addition level must remain below 30 wt% in outer layers because higher loadings reduce UV stabilizer retention and can create haze variability when the film passes over oscillating haul-off equipment. Processing includes melt temperatures of 190–215 °C, blow-up ratio of 2.0–2.5, and die gaps of 2.2–2.8 mm; wide-die lines exhibit edge instability when the mLLDPE fraction exceeds 25 wt%, requiring edge encapsulation with LDPE to maintain bubble symmetry. Durability is validated under ISO 527-3 for tensile, ASTM D1003 for haze, ISO 7765-1 for impact, and UV stability according to EN 13206 or ASTM G154 with exposure conditions specified by the film producer. Food-contact certification is not applicable for agricultural covers, but REACH and local fertilizer-contact standards govern chemical resistance; European agricultural film waste is assessed under EN 17033 for biodegradable mulch only where applicable. Terminal finished product types include thermal greenhouse covers, silage wrap liners, and low-tunnel perforated films.

    Free Quote

    Competitive LyondellBasell Icorene 1761 BUE 5507 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    LyondellBasell Icorene 1761 BUE 5507 is a metallocene-catalysed linear low-density polyethylene supplied as a pelletized extrusion grade. The product identifier embeds the resin family, an order of magnitude of the melt flow rate, and the stabilizer or processing aid package. The suffix BUE indicates a butene-based extrudate for film conversion. Unlike conventional Ziegler-Natta C4-LLDPE, the single-site metallocene catalyst architecture produces a narrow molecular weight distribution and a more uniform short-chain branching distribution. This reduces the fraction of highly branched low-molecular-weight material, lowers seal initiation temperature, and improves optical clarity when converted into thin film. The grade is positioned for flexible packaging structures in which sealant performance and abuse resistance are specified. It is not a general-purpose injection molding grade, and the published properties are oriented toward blown film and coextrusion rather than rotational molding or pipe extrusion.

    The base resin is characterized by a density of approximately 0.918 g/cm³ and a melt flow rate of approximately 1.0 g/10 min when tested at 190 °C under 2.16 kg. These two values are normally batch-release parameters under ISO 1133-1:2022 and ISO 1183-1:2019. The melting peak is typical of a butene-based linear low-density polyethylene, in the range of 120 °C to 123 °C. The molecular weight distribution is narrow, with polydispersity values below 3.0 reported for metallocene polyethylenes when measured by high-temperature size exclusion chromatography according to ISO 16014-4:2019. The comonomer is 1-butene, which means the seal initiation benefit is accompanied by lower low-temperature toughness than hexene- or octene-based metallocene grades of equivalent density. The additive package typically includes a hindered phenolic antioxidant and an acid scavenger; the exact slip and antiblock loadings are grade-specific and may be modified by the converter.

    What Are the Typical Physical, Mechanical, and Thermal Benchmarks for Icorene 1761 BUE 5507?

    The table below consolidates representative values from LyondellBasell technical documentation and standardized test methods. These values are not intended as release specifications; batch certificates generated under ISO 9001 quality systems control the actual lot-to-lot range. The test methods selected reflect film-conversion practice: mechanical values use ISO 527-3:2018 on 25 µm blown film unless otherwise stated.

    Representative property envelope for Icorene 1761 BUE 5507
    PropertyRepresentative valueTest method
    Melt flow rate1.0 g/10 min at 190 °C / 2.16 kgISO 1133-1:2022
    Density0.918 g/cm³ISO 1183-1:2019
    Melting temperature121 °CISO 11357-3:2018
    Vicat softening point104 °CISO 306:2013
    Tensile modulus260 MPaISO 527-3:2018
    Tensile stress at yield11 MPaISO 527-3:2018
    Tensile stress at break42 MPaISO 527-3:2018
    Elongation at break650 %ISO 527-3:2018
    Dart drop impact900 gASTM D1709A
    Haze5 %ASTM D1003
    Gloss at 60° geometry85ASTM D2457

    On film lines, Icorene 1761 BUE 5507 is usually processed as a monolayer or as the sealant skin of a coextruded structure. The recommended melt-temperature band is 190 °C to 230 °C. At temperatures below 190 °C, the melt may not homogenize completely on short-barrel extruders and can produce visible gel streaks. Above 230 °C, optical haze increases and thermally oxidized volatile species may deposit on the die lip. The die gap should be kept between 1.8 mm and 2.5 mm; narrower gaps can induce sharkskin melt fracture because the resin has low melt elasticity. Blow-up ratios from 2.0:1 to 3.0:1 provide a useful tear balance in 25 µm to 60 µm films. Frost-line height is commonly set at 4 to 6 die diameters. Lower frost-line settings increase machine-direction orientation and reduce transverse-direction tear resistance. Bubbles with high stalk heights above 8 die diameters may become unstable when air turbulence or ambient air temperature exceeds 30 °C. Published data for this exact grade on a specific die diameter are limited; therefore, start-up trials should record melt pressure, film gauge, haze, dart impact, and seal strength against the grade\u2019s certificate of analysis.

    Production-scale experience with metallocene butene LLDPE indicates that edge folds and blocking in slit reels are common when winder tension is set too high or when the slip package is insufficient. Because the 5507 formulation includes antiblock but may have a low slip level, high-speed slitting may require a slip masterbatch to reduce the coefficient of friction to the target range. If the film shows blocking at the winder, the first interventions are reducing winding tension by 10% to 15%, lowering reel stacking temperature below 35 °C, and increasing the gap between nip rolls. Melt fracture at the die lip is corrected by increasing the die gap to 2.5 mm, adding a fluoropolymer processing aid at 200 ppm to 500 ppm, or raising the die temperature by 5 °C to 10 °C. These interventions are not unique to this product but are relevant because its narrow molecular weight distribution reduces melt elasticity compared with broad-distribution Ziegler-Natta grades.

    Start-up lines equipped with gravimetric blender and internal bubble cooling should record feed throat temperature and cooling air dew point. The feed throat should remain below 50 °C to avoid bridging and feed starvation; if the resin pellets become soft, throughput variation appears as gauge bands in the film. Internal bubble cooling systems are operated with chilled air at 10 °C to 20 °C and a balance between intake and exhaust to avoid bubble collapse. On a three-layer line with die diameter 250 mm, a die gap increase from 2.0 mm to 2.5 mm typically reduces melt fracture but also changes the draw ratio. The resulting film may show slightly higher haze and lower machine-direction tear, so the die gap should not be changed without checking the film balance.

    When Metallocene Homogeneity Displaces Ziegler-Natta Catalysis in LLDPE Film Lines

    The clearest differentiation from a Ziegler-Natta C4-LLDPE of the same melt index and density appears in heat-seal and optics. A conventional Ziegler-Natta resin contains a broad distribution of short-chain branches, with some highly branched low-molecular-weight chains and some lightly branched high-molecular-weight chains. This heterogeneity widens the melting range and raises the temperature at which a seal reaches a specified strength. The metallocene architecture of Icorene 1761 BUE 5507 generates a narrower chemical composition distribution, so crystalline domains melt over a sharper interval and the seal initiation temperature may be 10 °C to 15 °C lower. The difference allows a reduction in jaw set point on a vertical form-fill-seal machine, which decreases thermal load on heat-sensitive overwraps and improves sealing speed. The trade-off is extrusion rheology. Metallocene grades typically show lower die swell and lower melt strength than branched LDPE and some broad-molecular-weight LLDPE grades. In bubble formation, this can translate into a smaller stable operating window for high-stalk processes. Converters who run high BUR above 3.5:1 may observe bubble flutter unless additional cooling control or a blend with LDPE is introduced.

    Compared with hexene- or octene-based metallocene LLDPE, the butene comonomer in this resin produces a lower level of tie-molecule reinforcement. This means dart drop impact and puncture resistance at freezer temperatures are generally lower, while the melting point and density are slightly higher. The benefit of the butene formulation is often economic and processing stability, because the resin can run at a slightly lower melt temperature and may show a lower seal initiation threshold than a broad C4 Ziegler-Natta grade. For film structures requiring deep-freeze impact resistance, converters may blend Icorene 1761 BUE 5507 with an octene-based mLLDPE or place it in the sealant layer while a tougher core layer carries mechanical abuse. Published data for the specific blend ratios on this grade are limited; laboratory trials using dart impact testing under ASTM D1709A should define the required addition level.

    Sealing performance is evaluated by progressive heat-seal strength curves generated according to ASTM F2029-16 or equivalent ISO 527-3-adapted methods. In a coextruded film with a 20 µm sealant layer, seal initiation is typically assessed at 105 °C under 0.75 N/mm² and 0.5 s dwell; however, published data for this specific configuration are limited and must be confirmed by the packaging line. Hot-tack testing under ASTM F1921-12 provides the force a seal can bear while still partially molten; this value matters in high-speed vertical form-fill-seal operations where product load acts immediately after sealing. For butene-based mLLDPE sealant webs, hot-tack strength tends to peak between 115 °C and 125 °C and declines above the melting point. Seal strength under ASTM F88/F88M-21 depends strongly on sealant layer thickness, seal pressure, dwell time, and the stiffness of the lamination. A thinner sealant layer transfers heat more quickly and may seal at lower jaw temperature but produces less total sealant mass for caulking and peel strength. Processors should not infer final seal performance from resin density alone; the full film structure and seal bar profile control the result.

    Rheological Signatures and Shear Response in Single-Screw Extruders

    Rheological measurements of metallocene LLDPE reveal a broader shear-thinning region than low-pressure LDPE and a lower plateau modulus at low frequency than broad-distribution Ziegler-Natta resins. The zero-shear viscosity of a 1.0 g/10 min metallocene butene grade is generally lower than that of a 1.0 g/10 min Ziegler-Natta C6 or C8 grade, but the high-shear viscosity is often similar. In single-screw extrusion, this translates into predictable feed section melting and a tendency for head pressure to rise as screw speed increases. Extruders with 24:1 to 30:1 L/D and barrier screws are suitable; grooved-feed extruders increase output but may require reductions in barrel temperature because they introduce additional shear heat. A Maddock or spiral mixer after the metering section helps homogenize the melt and reduces temperature variations. Die pressure on a 45 mm extruder running 25 µm film at 0.5 kg/h per cm of die circumference may reach 25 MPa to 35 MPa; the exact value depends on melt temperature, die gap, and screen pack condition. Published data for this specific grade are limited; therefore, pressure should be trended against output to detect screen blockage or gel build-up.

    When surface melt fracture appears as regular sharkskin at the die lip, fluoropolymer processing aid is often added at 200 ppm to 500 ppm by weight. Conditioning the die with a precompounded PPA masterbatch before start-up can reduce the time required to clear melt fracture. Excess PPA above 1000 ppm may cause slip anomalies in the final film and can interact with corona treatment, lowering surface energy. Therefore, converters should validate corona treatability under ASTM D2578-17 after any formulation change.

    High-Speed Converting Tightens the Optical and Mechanical Defect Envelope

    In blown film conversion, the optical defect envelope is governed by melt temperature, die lip cleanliness, and frost-line stability. Haze on 25 µm monolayer film is typically below 6% according to ASTM D1003, and gloss at 60° is typically above 80 according to ASTM D2457. These values are reached only when the melt temperature remains below 235 °C and the die lip is cleaned on a regular schedule. Oxidized deposits on the die lip can produce die lines that increase haze and reduce gloss. The coefficient of friction of film made with the 5507 additive package is formulation-dependent; standard antiblock concentrations may yield values between 0.15 and 0.35 under ISO 8295:1995. High-speed horizontal form-fill-seal machines often require a coefficient of friction below 0.25 to avoid web drag and tracking errors. Slip additive in the resin or added as masterbatch reduces friction but may migrate to the seal surface and reduce hot-tack performance. Blocking force measured under ASTM D3354-15 should be monitored on slit reels, particularly when film gauge is below 30 µm and when storage temperature exceeds 35 °C.

    For food-contact applications, the base olefin polymer is typically covered in the United States by FDA 21 CFR 177.1520, which includes specifications for extractable fraction and density. Finished articles may also be evaluated under 21 CFR 176.170(c) for components of paper and paperboard. In the European Union, compliance with EU Regulation 10/2011 requires an overall migration limit of 10 mg/dm² and, for any intentionally used additives, a check against the positive list and specific migration limits. The metallocene catalyst residues in commercial grades are normally low, but the manufacturer\u2019s declaration of compliance should be obtained for each lot. For non-food technical applications, a declaration under REACH Regulation (EC) No 1907/2006 Article 33 is often requested. RoHS assessments are generally limited to heavy-metal absence in polyolefin compounds, and the grade is not expected to contain cadmium, lead, mercury, or hexavalent chromium above the RoHS Directive 2011/65/EU maximum concentration values. These regulatory statements are applicable to the base resin; downstream additives, masterbatches, inks, and adhesives must be assessed separately.

    Storage and handling limits are straightforward. Pellets should be kept below 40 °C and below 60% relative humidity to avoid surface moisture and oxidative embrittlement. Pre-drying is not normally required unless condensation is visible; if drying is needed, 2 h at 65 °C in desiccant air is sufficient. The product should not be exposed to ultraviolet radiation for prolonged periods because polyethylene undergoes photooxidative chain scission; this mechanism is not unique to metallocene grades. If stored in silos, the silo should be purged with dry air and emptied on a first-in-first-out basis. Extended storage beyond two years may shift additive performance, but published data for this specific grade under long-term warehouse conditions are limited.

    Lot-to-lot consistency for metallocene grades is monitored by the producer through melt flow rate, density, and film classification tests. Certificates of analysis usually report values for ISO 1133-1:2022 and ISO 1183-1:2019, while optical and mechanical film properties are typical values rather than release criteria. A converter should request the batch-specific certificate and compare the melt flow rate against the upstream blending and extrusion control system. When a new lot is introduced, a transition purge is advised until the melt pressure and film gauge stabilize; because the molecular weight distribution is narrow, the extruder may respond more quickly to changes in screw speed than to barrel temperature changes. Statistical process control on the film line should monitor film gauge profile, haze, dart impact, and seal initiation to detect lot-to-lot variation before packaging performance is affected.

    Primary documented application fields include monolayer and coextruded blown film for food packaging, lamination film, sealant webs, and agricultural film. In a three-layer structure with a thickness split of 1:2:1, this resin may occupy the outer sealant skins while a HDPE or LDPE core supplies stiffness and throughput. The film can be drawn to gauges as low as 20 µm without losing dart impact when process conditions are optimized; the optimum frost-line height and die gap depend on the die diameter and the target tear balance. In lamination film, the grade is often used as the sealant layer in duplex or triplex structures with PET or BOPP print webs, where low seal initiation temperature supports high-speed conversion and the metallocene purity reduces off-taste and odor. Typical converting operations include form-fill-seal, pouch making, and lidstock; each requires validation of seal strength, hot-tack, and coefficient of friction on the intended pack style because the resin datasheet alone does not guarantee final package performance.

    Top