| HS Code | 979034 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Catalysttype | Metallocene |
| Comonomertype | Butene-1 |
| Density | 0.917 g/cm3 |
| Meltindex | 1.0 g/10 min (190°C/2.16 kg) |
| Tensilestrengthatyield | 9.0 MPa |
| Tensilestrengthatbreak | 25.0 MPa |
| Elongationatbreak | 600% |
| Flexuralmodulus | 200 MPa |
| Vicatsofteningpoint | 95°C |
| Meltingpoint | 116°C |
| Haze | 6% |
| Gloss | 80% |
| Dartdropimpact | 150 g |
| Elmendorftearstrengthmd | 200 g |
| Elmendorftearstrengthtd | 400 g |
| Coefficientoffriction | 0.20 |
As an accredited LyondellBasell Icorene 1761 BUE 5503 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Icorene 1761 BUE 5503 is supplied in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg), stretch-wrapped. |
| Container Loading (20′ FCL) | LyondellBasell Icorene 1761 BUE 5503 metallocene LLDPE: palletized 25 kg bags loaded into 20′ FCL; payload depends on carrier and destination. |
| Shipping | LyondellBasell Icorene 1761 BUE 5503 is shipped as non-hazardous LLDPE metallocene pellets, typically in 25 kg bags or 1,000 kg bulk bags on pallets. Transport in clean, dry, covered trucks, railcars, or containers. Store away from heat, moisture, sunlight, and contamination. No special DOT/IMDG/ADR hazard classification required. |
| Storage | Store LyondellBasell Icorene 1761 BUE 5503 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and ignition sources. Keep in original sealed packaging on pallets, off the floor. Protect from moisture, dust, and contamination. Avoid prolonged UV exposure and temperatures above 50°C. Use FIFO rotation; keep away from strong oxidizers. |
| Shelf Life | Shelf life is 24 months from production when stored in original, unopened packaging under dry, cool conditions away from direct sunlight. |
Primary sealing layers in frozen logistics require a combination of low-temperature puncture resistance and consistent heat-seal strength at high fill speeds. In this segment the metallocene linear low-density polyethylene is introduced as a skin or core layer in three-layer blown film coextrusion, where die diameters are typically 200 mm to 500 mm and screw L/D ratios are 25:1 to 30:1. The supplier technical data sheet lists a density of 0.918 g/cm³ under ISO 1183-1:2019 and a melt flow rate of 1.0 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022. Typical blend formulation places LyondellBasell Icorene 1761 BUE 5503 at 20 wt% to 40 wt% of total polymer mass, with a high-pressure LDPE carrier phase at 55 wt% to 75 wt%, erucamide slip concentrate at 400 ppm to 800 ppm, and synthetic silica antiblock at 1,000 ppm to 2,000 ppm. Downstream extrusion parameters include die gaps of 1.6 mm to 2.4 mm, blow-up ratios of 2.2:1 to 3.0:1, melt temperatures of 185°C to 210°C, and frost-line heights of 6 to 9 die diameters. Compliance is anchored to EU 10/2011 Annex I for overall migration and FDA 21 CFR 177.1520 for olefin polymers in food-contact films; specific migration testing follows EN 1186-1:2002 and EN 13130-1:2004. Finished articles produced under this configuration include frozen vegetable pouches, ice cream liners, modified-atmosphere salad films, and flow-pack films for chilled meat and poultry. The narrow comonomer distribution suppresses a premature seal-strength plateau at low film thickness; however, extruder barrel temperatures should remain below 220°C to prevent gel formation from thermal oxidation of low-molecular-weight fractions.
| Standard/Regulation | Designation / Clause | Measured Parameter |
|---|---|---|
| EU 10/2011 | Annex I | Overall migration limit 10 mg/dm² |
| FDA 21 CFR | 177.1520 | Polyethylene food-contact compliance |
| ISO 1133-1:2022 | 190°C/2.16 kg | Melt flow rate |
| ASTM D638-14 | Type IV | Tensile yield stress and elongation |
| ASTM D1709-16a | Methods A/B | Dart drop impact |
| ASTM F88/F88M-15 | — | Heat-seal strength |
When three-layer laminates of polyester and aluminium foil require a low-seal-initiation layer for horizontal form-fill-seal machines, the grade is extruded as a monolayer web at 18 µm to 35 µm and then adhesive-laminated to the barrier substrate. The lamination sealant web uses a coextruded seal layer containing 70 wt% to 90 wt% LyondellBasell Icorene 1761 BUE 5503 and 10 wt% to 30 wt% high-pressure LDPE to reduce melt pressure and improve bubble stability. Slip addition is limited to 300 ppm to 600 ppm erucamide because excessive migration into the adhesive interface can reduce laminate bond strength below 2.5 N/15 mm as measured by ASTM F88/F88M-15. Downstream conversion is performed on tandem blown-film lines with chill-roll take-up, die gaps of 1.8 mm to 2.2 mm, and blow-up ratios of 2.0:1 to 2.5:1. Seal initiation temperature in such structures is typically 85°C to 95°C, enabling dwell times below 0.4 s on HFFS machines. Compliance references are EU 10/2011 for plastic multilayers and FDA 21 CFR 177.1520 for the food-contact olefin layer; printing inks and adhesives must separately meet EU 2023/2006 good manufacturing practice. Finished product types include stand-up pouches for dry foods, pillow pouches for granular products, and sachets for instant beverages. Published mechanical data for this specific grade in aluminium-foil laminates under retort conditions above 121°C are limited, and such use is outside the supplier’s documented processing envelope.
Bulk sack liners and e-commerce mailers are produced on high-output blown film lines where the key failure mode is dart impact under cyclic flexing rather than tensile elongation. The formulation for this segment replaces a portion of the metallocene LLDPE with an LDPE-rich phase: 55 wt% to 65 wt% LyondellBasell Icorene 1761 BUE 5503, 30 wt% to 40 wt% high-pressure LDPE, and 5 wt% to 10 wt% recycled LLDPE of known melt flow rate 0.7 g/10 min to 1.5 g/10 min. A fluoropolymer processing aid is added at 200 ppm to 400 ppm to delay the onset of sharkskin melt fracture on extrusion lines with die gaps of 1.8 mm to 2.2 mm and output rates above 180 kg/h on 300 mm dies. Bubble geometry is run at a blow-up ratio of 2.5:1 to 3.0:1 and a frost-line height of 8 to 10 die diameters, yielding a final film thickness of 80 µm to 120 µm. Compliance for heavy-duty packaging is assessed under ISO 21898:2004 for classification and marking of sacks, ASTM D1709-16a for dart drop impact, and ASTM D1004-13 for trouser tear. Finished product types include FIBC liners, e-commerce mailers, heavy-duty shipping sacks, and liners for bulk agricultural products. Melt temperature should not exceed 220°C; higher temperatures accelerate oxidation in the recycled-LLDPE fraction and may produce gel-related dart impact loss in cyclic flex testing.
At film widths above 3 m, the choice of stabilizer package becomes the limiting variable in multi-season greenhouse covers. Metallocene LLDPE alone has insufficient weathering resistance for such exposure, so LyondellBasell Icorene 1761 BUE 5503 is blended as the base polymer at 70 wt% to 80 wt% with a UV masterbatch at 2.5 wt% to 4.0 wt% containing hindered amine light stabilizers and a nickel quencher, plus 1.0 wt% to 2.0 wt% of a UV-stabilized white pigment masterbatch for thermal reflection. Downstream extrusion is performed on wide blown-film lines with die gaps of 2.0 mm to 2.5 mm and blow-up ratios of 2.5:1 to 3.5:1; film thickness ranges from 120 µm to 200 µm for greenhouse covers and 25 µm to 40 µm for low tunnels. Compliance for structural agricultural films is referenced to EN 13206:2017 for polyethylene horticultural films and ISO 4892-2:2013 for accelerated weathering; mechanical durability is checked by ASTM D638-14 tensile elongation after 5,000 h of accelerated aging. Finished product types include greenhouse side sheets, low tunnels, silage covers, and temporary crop protection films. Compatibility of the selected UV masterbatch with the metallocene polymer matrix must be verified before full-scale production; carrier resins based on traditional LDPE may lower interlayer adhesion in coextruded structures when distributed unevenly across the melt stream.
For masterbatch producers running thin-film carrier resins, the key constraint is dispersion stability at high pigment loadings. When LyondellBasell Icorene 1761 BUE 5503 is used as a carrier, the formulation consists of 60 wt% to 70 wt% carrier resin and 30 wt% to 40 wt% pigment or functional additive loading; a low-molecular-weight wax internal lubricant is added at 2 wt% to 4 wt% of total batch. Compounding is run on co-rotating twin-screw extruders with L/D ratios of 40:1 to 44:1, screw speeds of 600 to 900 rpm, specific energy input of 0.18 kWh/kg to 0.25 kWh/kg, and strand or water-ring pelletizing. The downstream pellet product is then let down into blown or cast film at 2 wt% to 5 wt% in the final polymer stream. Compliance for masterbatches intended for food-contact film follows FDA 21 CFR 178.3290 for colorants for polymers and EU 10/2011; nonfood packaging applications fall under RoHS 2011/65/EU Annex II. Finished product types include white and colored masterbatches for thin-gauge films and slip/antiblock additive masterbatches for high-output packaging lines. Processing temperatures should not exceed 220°C at the compounder discharge; higher melt temperatures accelerate carrier degradation and produce gel counts above 50 particles/m² in subsequent film.
Competitive LyondellBasell Icorene 1761 BUE 5503 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
LyondellBasell Icorene 1761 BUE 5503 is a pelletized metallocene-catalysed linear low-density polyethylene supplied as a black ultraviolet-stabilized compound. The product designation combines the base-grade number 1761 with the suffix BUE 5503, which identifies a black UV-stabilized additive and colour configuration rather than a change in the metallocene catalyst architecture. The base resin is specified by melt mass-flow rate and density. Published data for the unmodified Icorene 1761 grade commonly list a nominal melt mass-flow rate of 6.0 g/10 min at 190 °C and 2.16 kg in accordance with ISO 1133-1:2022, and a nominal density of 0.917 g/cm³ in accordance with ISO 1183-1:2019. The BUE 5503 pigment and stabilizer may shift measured density and ash content slightly; therefore, the lot-specific certificate of analysis rather than a single nominal value should govern incoming inspection.
In terms of classification, the resin falls under ISO 1872-1 as an ethylene/α-olefin thermoplastic. The density of 0.917 g/cm³ is lower than that of the 0.935–0.940 g/cm³ rotational-moulding mLLDPE grades, reducing flexural modulus but increasing low-temperature ductility. In cast film and thin-wall injection moulding, the 6.0 g/10 min melt mass-flow rate permits moderate shear viscosity; however, metallocene resins of this viscosity exhibit less shear thinning than a Ziegler-Natta LLDPE of identical MFR. This difference can be observed as higher screw torque and melt pressure at equivalent throughput despite the same melt index.
Incoming resin inspection for the BUE 5503 variant should include melt mass-flow rate, density, moisture, carbon black content, and oxidative induction time. The base resin specification relies on ISO 1133-1:2022 for MFR and ISO 1183-1:2019 for density. Because the product is black and UV-stabilized, ISO 6964 is commonly applied for carbon black content or dispersion, and ISO 11357-6 is used for oxidative induction time. The moisture content of metallocene LLDPE pellets is usually low after commercial degassing; however, condensation during silo storage can increase surface moisture above 0.05 wt%, which may generate surface defects in cast film at high screw speeds. Pre-drying at 60–80 °C for 2–4 h in a desiccant dryer is recommended only when visible moisture or high ambient humidity above 60% RH is reported; unnecessary drying consumes antioxidant and can shift the melt flow rate.
The black pigment in BUE 5503 introduces inorganic solids that are not present in natural Icorene 1761. These solids increase density by roughly 0.001–0.003 g/cm³ depending on carbon black loading. The UV stabilizer package retards chain scission initiated by ultraviolet radiation, but it does not prevent thermal-oxidative degradation during processing. The grade should be regarded as a compounded product: the molecular architecture of the base resin is metallocene, but the final melt rheology is influenced by pigment dispersion quality, additive melting, and lot-to-lot masterbatch variation.
For cast-film and extrusion-coating lines, the 6.0 g/10 min melt mass-flow rate allows melt temperatures from about 210 °C to 240 °C at the die, with barrel profiles beginning near 170 °C and rising through 200–220 °C in the compression and metering zones. A single-screw extruder with a 24:1–30:1 L/D ratio and a barrier screw is generally sufficient; a Maddock mixer or static mixer improves thermal homogeneity and pigment distribution. In cast film, the die gap is typically set between 0.4 mm and 0.8 mm, and the chill-roll temperature is controlled between 15 °C and 30 °C to balance optical quality and web tracking. Because metallocene LLDPE has a narrow molecular weight distribution, the melt can exhibit surface melt fracture at high shear stress; reducing die land temperature or increasing die gap can move the shear stress below the critical value. In thin-wall injection moulding, the same architecture lowers injection-pressure dependence on part thickness but may require higher melt cushion and lower decompression than Ziegler-Natta LLDPE to prevent drool.
On a capillary rheometer, a metallocene LLDPE with a 6.0 g/10 min MFR and density 0.917 g/cm³ typically shows an apparent shear viscosity at 230 °C and 100 s⁻¹ in the range of 150–250 Pa·s; the corresponding Ziegler-Natta LLDPE may be 20–30% lower in shear viscosity at the same MFR because of broader molecular weight distribution. This viscosity difference is reversed at low shear rates, where the mLLDPE may show lower viscosity. Such rheological data support equipment sizing. On a 30:1 L/D grooved-feed extruder, the higher pressure sensitivity of metallocene LLDPE may require barrel temperatures in the feed zone to be held below 160 °C to avoid excessive melt film formation. In injection moulding, the injection velocity should be profiled because the narrow MWD reduces melt elasticity and can permit jetting in thick sections; a moderate-to-high injection speed of 100–200 mm/s at the screw is commonly used for thin-wall packaging, while holding pressure is typically maintained at 300–600 bar for 0.5–2.0 s per millimetre of part thickness.
The performance distinction is not simply density or MFR. The metallocene catalyst used for Icorene 1761 produces an ethylene/α-olefin copolymer with a narrow molar mass distribution and a more uniform sequence-length distribution. The practical consequence is that the low-molecular-weight fraction is smaller than in Ziegler-Natta LLDPE; this reduces low-temperature extractables, improves organoleptic properties in food packaging, and lowers the probability of plate-out during cast-film production. At equivalent density and MFR, a metallocene LLDPE generally exhibits higher dart impact and puncture resistance than a Ziegler-Natta LLDPE because tie-chain concentration is more efficiently generated when comonomer units are distributed uniformly across the molecular weight range. These comparisons are measurable by ASTM D1709 or ISO 7765-1 for dart drop and by ISO 527-3 for tensile properties.
However, the narrow molecular weight distribution also reduces shear thinning. The melt viscosity of a 6.0 g/10 min mLLDPE remains closer to its low-shear value at high extrusion rates than a Ziegler-Natta LLDPE of the same MFR. This property requires more drive torque and may raise melt temperature by viscous dissipation in long adiabatic extrusion. The absence of long-chain branching, which is present in high-pressure LDPE, further lowers melt strength and extensional viscosity. In cast film, the practical effect is a lower tendency to form unstable necks but a higher tendency to draw resonance above a critical draw ratio. In blown film, neat mLLDPE may collapse under high-stalk bubble configurations; processors commonly blend 10–30 wt% high-pressure LDPE to stabilize the bubble without eliminating the toughness contribution of the metallocene component.
| Property | Icorene 1761 BUE 5503 mLLDPE | Ziegler-Natta LLDPE | High-pressure LDPE |
|---|---|---|---|
| Molecular weight distribution | narrow; typical Mw/Mn 2.0–3.0 in metallocene LLDPE | broad; Mw/Mn often 3.5–8.0 | broad with long-chain branch distribution |
| Comonomer sequence distribution | homogeneous; branch-rich and branch-poor chain fractions reduced | heterogeneous; low-Mw fraction can be highly branched | short-chain branching mainly from radical transfer |
| Melt strength at matched MFR | lower; limited neck-in resistance in extrusion coating | moderate; better bubble stability than mLLDPE | high; used to stabilize blown-film bubbles |
| Typical processing risk | draw resonance, melt fracture, drool after decompression | gel formation, torque variation, higher backpressure | melt fracture at high shear, higher heat sensitivity |
| Density and MFR design range | base grade: 0.917 g/cm³; 6.0 g/10 min | commonly 0.916–0.940 g/cm³; MI 0.5–25 g/10 min | commonly 0.918–0.930 g/cm³; MI 0.2–70 g/10 min |
Thermal analysis of metallocene LLDPE with 0.917 g/cm³ density under ISO 11357-3 generally yields a peak melting temperature in the range 120–126 °C and a crystallization peak near 104–110 °C at 10 °C/min cooling. The specific heat capacity at melt temperature affects barrel heating; values around 2.2–2.5 J/(g·K) are common for LLDPE of this density class. Published data for this specific configuration is limited; therefore, thermal properties are best measured on the compounded pellets rather than predicted from base resin data. The same limitation applies to mechanical design values such as tensile modulus, yield stress, and environmental stress-cracking resistance, which should be generated under the intended processing conditions and test standards.
The BUE 5503 formulation includes a black pigment package that reduces ultraviolet transmission through the polymer. Carbon black functions as a UV absorber and free-radical scavenger, but its effectiveness depends on particle size, dispersion, and loading. For outdoor articles, accelerated weathering by ISO 4892-2 is the standard laboratory indicator; however, product-specific data for this configuration is limited. A black UV-stabilized metallocene LLDPE typically retains mechanical integrity longer than natural mLLDPE under the same irradiance, but the degree of stabilization is not uniform because carbon black dispersion quality can vary between compounding lots and converters.
Thermal stabilization remains an independent boundary. Processing at melt temperatures above 250 °C or allowing melt residence times beyond 10–15 min can consume primary antioxidants and reduce the oxidative induction time measured by ISO 11357-6. The black pigment can mask early discoloration caused by degradation, so processors should not use visual inspection as the sole acceptance criterion. Melt-pressure and torque stability are more informative. In applications with continuous outdoor exposure, the combination of UV radiation, moisture, and mechanical load can produce stress cracking; the lower crystallinity of 0.917 g/cm³ mLLDPE usually improves resistance to slow crack growth relative to higher-density polyethylene, but environmental stress cracking resistance should be verified by ASTM D1693 or ISO 22088-2 for the specific detergent, oil, or chemical service.
Die-lip deposit is influenced by low-molecular-weight species, additives, and pigment concentrates. The metallocene catalyst produces fewer low-Mw oligomers than Ziegler-Natta, but the black UV-stabilized masterbatch can introduce waxes or processing aids that migrate to the die lip. If die-lip build-up occurs on cast-film dies, lower die exit temperatures or use of a fluoropolymer processing aid at 200–400 ppm can reduce deposit adhesion without changing the resin specification. Any additive adjustment should be evaluated for interaction with the UV package by measuring oxidative induction time and accelerated weathering before production approval.
If a converter is considering substituting this grade for a Ziegler-Natta LLDPE in an existing tool, the parting-line and venting design may need adjustment because the metallocene resin has a lower elastic recovery at low shear. Shrinkage values measured by ISO 294-4 can differ from the Ziegler-Natta reference by a few tenths of a percentage point depending on wall thickness and pigment loading. In black UV-stabilized grades, the inorganic pigment can act as a nucleating agent in some cooling regimes, reducing spherulite size and altering post-mould shrinkage. Published data for this specific configuration is limited; therefore, prototype runs with in-mould pressure transducers and post-de-mould dimensional checks over 24–48 h are required to establish tool-specific shrinkage compensation.
Polyethylene products of this class are often intended for food-contact service. In the United States, the relevant federal citation is 21 CFR §177.1520, which covers olefin polymers. The regulation permits the use of polyethylene in contact with food when the polymer meets specified density and extraction limitations. For this product, the manufacturer should provide a food-contact statement that confirms the base resin and the additive package comply with the applicable paragraph, including the maximum extractable fraction for the intended food type and temperature condition. In the European Union, Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food applies. Verification requires overall migration testing with a limit of 10 mg/dm² or 60 mg/kg depending on the article geometry and food simulant, and compliance of the additive package with the Union list of authorized substances. Specific migration limits for additives in the black UV-stabilized package must be confirmed through the supplier’s statement of compliance; the generic resin designation alone is not sufficient.
| Framework | Relevant provision | Typical verification threshold or requirement |
|---|---|---|
| FDA 21 CFR | §177.1520 | olefin polymer density and extraction limits; food-type conditions |
| EU Plastics Regulation | (EU) No 10/2011 | overall migration 10 mg/dm² or 60 mg/kg; authorized additives |
| REACH | Annex XVII entries | SVHC and PAH restrictions; no product-specific migration data without supplier statement |
| RoHS 2011/65/EU | Heavy metal limits | lead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg, chromium VI 1000 mg/kg |
When downgauging film or reducing part wall thickness with this metallocene LLDPE, the crystallinity and modulus of the base resin must be considered against the mechanical loads of the final article. For a density of 0.917 g/cm³, the tensile modulus is lower than a 0.925–0.930 g/cm³ Ziegler-Natta LLDPE, and the black pigment does not compensate for the modulus reduction. The lower density, however, translates into improved low-temperature impact and higher elongation at break; this trade-off should be quantified by ISO 527-3 tensile tests on specimens cut in the machine and transverse directions, rather than relying on the MFR and density specification alone.