Lyondellbasell Icorene 1761 Bue 5502 Polyethylene Linear Low Density Metallocene

LyondellBasell Icorene 1761 BUE 5502 Polyethylene, Linear Low Density, Metallocene

    • Product Name: LyondellBasell Icorene 1761 BUE 5502 Polyethylene, Linear Low Density, Metallocene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 750978
    Density 0.917 g/cm³
    Meltindex 1.0 g/10 min (190°C/2.16 kg)
    Meltingpoint 116 °C
    Vicatsofteningpoint 96 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 600 %
    Flexuralmodulus 200 MPa
    Hardnessshored 48
    Thermalconductivity 0.33 W/m·K
    Waterabsorption 0.01 %

    As an accredited LyondellBasell Icorene 1761 BUE 5502 Polyethylene, Linear Low Density, Metallocene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing LyondellBasell Icorene 1761 BUE 5502 Polyethylene is packaged in 25 kg polyethylene-lined paper bags, palletized for storage and transport.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags of Icorene 1761 BUE 5502 metallocene LLDPE, stretch-wrapped, securely loaded for dry export.
    Shipping LyondellBasell Icorene 1761 BUE 5502 is shipped as metallocene linear low-density polyethylene pellets, typically in 25 kg bags, bulk bags, or octabins on pallets. Transport in clean, dry trucks or containers, protected from moisture, heat, sunlight, and contamination. Store in a cool, dry, well-ventilated area. Non-hazardous; follow local regulations.
    Storage Store in a cool, dry, well-ventilated warehouse at ambient temperature. Keep bags or containers closed, palletized, and off the floor. Protect from direct sunlight, moisture, heat, flames, and strong oxidizers. Avoid dust generation and contamination. Use first-in, first-out stock rotation. Do not store near incompatible materials or ignition sources. Follow the manufacturer’s SDS and local regulations. Ensure containers remain labeled.
    Shelf Life Typically 24 months when stored in original, unopened packaging in a cool, dry place away from direct sunlight and heat.
    Application of LyondellBasell Icorene 1761 BUE 5502 Polyethylene, Linear Low Density, Metallocene

    Icorene 1761 BUE 5502 is dry-blended with a 2.0–4.0 wt% hindered amine light stabiliser masterbatch and, for UV-opaque service, a 2.5–3.5 wt% carbon black concentrate before being charged to a biaxial rotational moulding machine producing 1,000–10,000 L chemical storage tanks and intermediate bulk containers. Oven air temperature is controlled at 280–320°C, while the internal air temperature at the mould surface is ramped to a peak of 190–210°C; lower peak temperatures below 185°C produce incomplete sintering at the mould parting line and microvoids detectable by a 25 kV spark test, whereas temperatures above 215°C oxidise the metallocene polyethylene matrix and reduce environmental stress crack resistance measured by ASTM D1693 under 100% Igepal CO-630 at 50°C. Arm speed is set at 4–8 rpm on the primary axis and 0.5–2.0 rpm on the secondary axis, with a speed ratio near 4:1 to avoid localised wall thinning at tank corners. Cooling is staged: forced air for 15–25 min, followed by water mist at 2–3 L/min until mould surface temperature falls below 70°C; cooling rates above 12°C/min are avoided to limit post-mould warpage of the top flange.

    For chemical containment service, the moulded vessel is pressurised to 0.35 bar and held for 30 min with a liquid penetrant applied to the outer wall seam, while drop impact resistance is evaluated by ASTM D5628 with a 3.0 kg striker at −20°C on specimens cut from the lower sidewall. The grade is tested for density by ISO 1183-1 and melt mass-flow rate by ISO 1133-1, with melt flow control in the 4.0–6.0 g/10 min range typical of rotational moulding powders. Compliance for dangerous goods service follows UN 31A/Y for rigid intermediate bulk containers and EN 13341 for static thermoplastic tanks, with weld line sections subjected to tensile testing per ASTM D638 at 50 mm/min. End products are secondary containment bunds, dosing tanks for water treatment chemicals, and vertical tanks for surfactants and fertilisers; the material is not qualified for aggressive oxidising acids unless post-mould fluorination is applied.

    What Happens to the Hot Tack Window When the Sealant Layer Is Down-Gauged to 12 µm on Vertical Form-Fill-Seal Lines?

    Cast film processors running vertical form-fill-seal lines typically blend 70–80 wt% Icorene 1761 BUE 5502 with 20–30 wt% low-density polyethylene from a high-pressure tubular reactor to suppress neck-in and draw resonance at 12 µm gauge. The blend is extruded through a 30:1 L/D barrier screw at melt temperatures of 240–260°C and a die gap of 0.5–0.7 mm, with the chill roll held at 15–18°C and air knife flow adjusted to eliminate oil haze. The metallocene catalyst narrows the short-chain branching distribution, so the seal initiation temperature shifts downward by approximately 15–20°C relative to conventional Ziegler-Natta butene LLDPE. Hot tack force is measured by ASTM F1921 using a 25.4 mm wide specimen, a 0.5 N/mm² seal bar pressure, and a 0.5 s dwell; acceptable hot tack for the down-gauged sealant layer is typically 3.0–5.0 N/25 mm across the 95–115°C window. Seal strength after cooling is determined by ASTM F88 with a 300 mm/min jaw separation on a 25 mm strip.

    For food contact, the blend meets FDA 21 CFR 177.1520(c) for olefin polymers in conditions of use B through H, and EU Regulation (EU) No 10/2011 Annex I requires total migration below 10 mg/dm² under the intended time-temperature conditions. The grade is also assessed for coefficient of friction by ASTM D1894, with slip masterbatch added at 0.5–1.5 wt% only when the film is converted on high-speed pouching machines. End articles are frozen vegetable pouches, fresh pasta flow wrap, and premade stand-up pouches for dry snacks; the formulation is not recommended for hot-fill above 85°C because the seal peels under sustained thermal load.

    When 30–35 g/m² extrusion coating is required onto aluminium foil for liquid packaging, melt draw limits for the metallocene grade are managed by using a 45 mm single-screw extruder with a 28:1 L/D ratio, a 0.4 mm die gap, and an air gap of 120–180 mm. Neck-in is controlled by blending 15–20 wt% high-pressure LDPE and by maintaining melt temperature at 285–305°C; draw-down speed is increased stepwise until the coating weight reaches the target while the edge bead is trimmed below 8 mm per side. The coated substrate is corona treated to 42–46 dyn/cm and laminated to paperboard within 24 h. Adhesion to foil is tested by a 180° peel method at 100 mm/min, with failure required in the polyethylene matrix rather than at the foil interface. The metallocene resin provides a low heat seal initiation temperature of about 95°C, allowing sealing of gable-top cartons at lower jaw temperatures. Compliance for aseptic cartons falls under FDA 21 CFR 177.1520 and EU No 10/2011, with aluminium foil barrier governed by the converter’s laminate specification. End products are aseptic drink cartons, laminated sachets, and barrier paperboard trays.

    High-Stalk Blown Film Bubble Stability with 20–30% LDPE Blending

    In high-stalk blown film extrusion for heavy-duty shipping sacks, the resin is combined with 20–30 wt% high-pressure LDPE and 3–5 wt% of a 25% silica anti-block masterbatch in the core or skin layer. Extrusion uses a 100 mm single-screw with a dual-lip air ring, die diameter 250 mm, die gap 2.0 mm, and blow-up ratio set at 2.5:1, with frost line height maintained at 700–900 mm. The narrow molecular weight distribution of the metallocene grade reduces high-shear viscosity, permitting melt temperatures 15–20°C lower than conventional butene LLDPE and lowering the specific energy input to 0.22–0.28 kWh/kg. Bubble stability is monitored by capacitance thickness scanning across 256 points; gauge variation across the web is maintained below ±6%. Dart impact is measured by ASTM D1709 Method A using a 38 mm diameter dart, with values above 800 g for 50 µm film expected in the blend, while Elmendorf tear resistance by ASTM D1922 is recorded in machine direction and transverse direction. End products are collation shrink sacks, heavy-duty mailer films, and frozen poultry bags; the resin is not suitable for high-clarity shrink film due to haze from LDPE blending.

    Rotational Moulding of Insulated Fish Boxes and Pharmaceutical Shipping Containers

    Foam-filled insulated boxes for fish transport and temperature-sensitive pharmaceutical distribution are rotationally moulded as double-walled shells with a 45–55 kg/m³ polyurethane foam injected into the cavity after demoulding. The polyethylene shell is processed from a dry blend of 100 parts of Icorene 1761 BUE 5502 powder and 0.5–1.0 parts of a food-grade colour masterbatch; the mould is heated in a shuttle oven with a peak internal air temperature of 195–205°C, and the primary axis speed is reduced to 3–5 rpm while the secondary axis runs at 0.5–1.0 rpm to maintain uniform wall thickness in the 4.0–6.0 mm range. Low-temperature impact performance is checked by ASTM D5628 on flat panels at −30°C using a 3.0 kg striker; brittle failure is rejected, and the foam-filled structure is subjected to a 1.5 m drop test at −20°C with a full payload. The material meets FDA 21 CFR 177.1520 for repeated food contact, and for pharmaceutical use the outer shell is cleaned with 70% isopropyl alcohol before foam injection. End products are seafood tote boxes, vaccine shippers, and laboratory sample transport containers.

    If Thin-Wall Injection Moulding Requires a 40:1 Flow Path at 1.5 mm Nominal Wall Thickness

    Thin-wall storage totes and housewares with flow length-to-wall ratios above 40:1 are moulded from the grade on hydraulic injection moulding machines with clamp forces of 2,500–5,000 kN. The mould temperature is held at 20–30°C, the barrel profile is set from 180°C at the feed throat to 230°C at the nozzle, and the injection velocity is set to 100–150 mm/s to avoid short shots in the base corners; holding pressure is maintained at 40–60 MPa for 2–3 s per millimetre of wall thickness. Because the metallocene resin has a narrow molecular weight distribution, warpage after ejection is lower than that of conventional LLDPE, but the packing phase is more sensitive to gate freeze time; the gate diameter is kept above 1.2 mm to extend hold time. Melt mass-flow rate is checked by ISO 1133-1 at 190°C/2.16 kg within the production control range, and notched Izod impact is measured by ISO 180/A at 23°C and −20°C. Published data for this exact thin-wall configuration with BUE 5502 is limited; qualification is performed by injection plant trials using short-shot analysis and mould filling simulation. End products are stackable storage totes, drawer housings, and waste bins. The material meets FDA 21 CFR 177.1520 for food contact containers and RoHS Directive 2011/65/EU for electrical housings.

    Free Quote

    Competitive LyondellBasell Icorene 1761 BUE 5502 Polyethylene, Linear Low Density, Metallocene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    As a metallocene-catalyzed linear low density polyethylene, LyondellBasell Icorene 1761 BUE 5502 is a formulated blown film grade in which the base resin and the additive package are specified jointly. The “1761” designation identifies the base polymer, while the “BUE 5502” suffix identifies a pelletized formulation with processing and surface additives intended for blown film conversion; the exact slip and antiblock loadings should be verified from the current technical data sheet. The resin is classified as a polyolefin with a predominantly linear backbone and controlled short-chain branching. Unlike high-pressure low density polyethylene, it contains no significant long-chain branching. The metallocene catalyst provides a narrower molecular weight distribution and a more uniform comonomer placement than conventional Ziegler-Natta linear low density polyethylene.

    Representative property ranges for the 0.918 g/cm³ / 1.0 g/10 min class are shown in Table 1. These ranges are not batch-release limits and should be checked against the current certificate of analysis and the LyondellBasell technical data sheet.

    Table 1. Representative physical property ranges for the metallocene LLDPE class.

    PropertyTest methodRepresentative range
    DensityISO 1183-1 method A0.917–0.919 g/cm³
    Melt mass-flow rateISO 1133-1 at 190 °C/2.16 kg0.9–1.1 g/10 min
    Melting peak temperatureISO 11357-3121–125 °C
    Vicat softening pointISO 306 A50100–106 °C
    Tensile modulus, blown filmISO 527-3170–210 MPa
    Dart impact F50, 40 µm filmASTM D1709 method A800–1500 g
    HazeASTM D10033–8 %

    How Do Melt Flow and Density Parameters Govern Film Extrusion?

    The melt mass-flow rate at 190 °C/2.16 kg is the primary molecular-weight indicator for extrusion response. A value of approximately 1.0 g/10 min reflects a high molecular weight relative to many cast film LLDPE grades; this supports high tensile strength and dart impact in blown film but also increases extruder torque and head pressure. The density of approximately 0.918 g/cm³ places the product in the conventional LLDPE range, providing sufficient crystallinity for film handling and stiffness while retaining good low-temperature toughness and sealability. Lower density reduces the crystalline fraction and generally improves dart impact and environmental stress crack resistance, whereas higher density raises modulus and softens heat-seal response.

    Because the metallocene catalyst produces a narrow molecular weight distribution, the shear viscosity at film extrusion shear rates is higher than that of a broad-MWD Ziegler-Natta LLDPE of the same melt index. The flow rate ratio I21.6/I2 is commonly reported in the 15–20 range for such narrow-MWD mLLDPE, compared with 25–35 for many Ziegler-Natta LLDPE resins. This low shear thinning has practical consequences: screw speed, backpressure, and motor load can limit throughput before the melt temperature exceeds the set point. In contrast, high-pressure LDPE exhibits a broader long-chain branched architecture and more shear thinning, but it lacks the uniform short-chain branching needed for the highest impact and clarity.

    Thermal analysis under ISO 11357-3 typically places the melting peak between 121 °C and 125 °C. Vicat softening under ISO 306 A50 is commonly in the 100–106 °C range. Heat-seal response measured under ASTM F88 must be characterized for the specific film gauge and packaging line; typical seal initiation for this density class can be in the 95–105 °C range, depending on dwell time, pressure, and the coextruded skin layer. The seal plateau is usually broader than that of a conventional Ziegler-Natta LLDPE because the more uniform comonomer distribution reduces high-melting fractions that delay seal formation.

    Blown Film Die Performance and Bubble Stability Limits

    On a 90 mm grooved-feed extruder with 30:1 L/D feeding a 250 mm spiral mandrel die with a 1.4 mm die gap, barrel temperatures are often set between 170 °C and 200 °C, with the adaptor and die between 195 °C and 215 °C. The melt temperature is maintained below 220 °C to reduce additive degradation and crosslinked gel formation. Because the resin has limited shear thinning, head pressure can reach levels that challenge extrusion safety limits if the die gap is reduced below 1.2 mm. Operators should treat motor load and die pressure as the controlling variables; set-point temperature alone does not capture the shear heating generated at the screw tip.

    Sharkskin and cyclic melt fracture are defects associated with the narrow-MWD architecture and the absence of long-chain branching. Lip shear rates above 400–800 s⁻¹ may produce sharkskin in unmodified mLLDPE film grades; the onset is accelerated by die gaps below 1.2 mm, low melt temperatures below 190 °C, and high draw rates. A fluoropolymer processing aid at 200–1000 ppm is frequently used to condition the die metal surface and suppress surface melt fracture. The additive should be introduced at low concentration and conditioned for sufficient time to coat the die surface; purging and documentation are required where food-contact status is critical.

    Bubble stability is governed by blow-up ratio, frost line height, and cooling air velocity. Typical operating conditions are a blow-up ratio of 2.0–3.0 and a frost line height of 2–4 die diameters. The lower melt strength relative to high-pressure LDPE can cause bubble whip or fluttering when cooling air is excessive or when the die lip is contaminated. Blending with 10–30 wt% high-pressure LDPE increases bubble stability but reduces clarity and increases seal initiation temperature. Regrind levels above 15 wt% can increase gel counts and specks, particularly if the regrind is heat-aged or contains high-shear history from edge trim.

    Polyethylene does not require desiccant drying for bulk moisture absorption. However, condensation on cold pellet surfaces can occur when packaging is opened in a humid plant above 60% RH. Allowing pellets to reach ambient temperature before conveying and keeping hopper temperatures slightly above the dew point reduces surface-water bubble defects at the die exit. Hydrolysis is not the operative mechanism, but surface water is rapidly converted to steam in the melt stream and appears as elongated bubbles or surface dimples in thin film.

    When the 1761 BUE 5502 formulation is evaluated as a replacement for a conventional Ziegler-Natta butene LLDPE in a coextruded barrier film, the most immediate differences appear in dart impact, optical quality, and seal initiation rather than in density or melt index. The metallocene catalyst produces a narrower comonomer distribution and fewer comonomer-poor, high-density segments. The film therefore shows lower haze, higher gloss, and a lower seal initiation temperature at equivalent density. Dart impact at equal gauge is generally improved because the uniform short-chain branching reduces localized stress concentration. Environmental stress crack resistance under ASTM D1693 condition B can also be significantly higher than that of a conventional butene LLDPE of similar density, although the extent depends on comonomer type, orientation, and test coupon preparation.

    The processing trade-off is higher extruder backpressure and lower bubble stability. Compared with a broad-MWD Ziegler-Natta LLDPE, the resin exhibits higher viscosity at typical die shear rates and less shear thinning; therefore the same extruder may require a higher barrel temperature profile or a larger die gap to maintain output. Compared with high-pressure LDPE, the resin has lower melt strength and less strain hardening, which reduces the self-supporting character of the bubble. The converter should not interpret the 1.0 g/10 min MFR as directly equivalent to an LDPE of the same MFR in terms of bubble behavior; the molecular architecture is different.

    Within the Icorene family, the BUE 5502 additive package distinguishes the grade from an unformulated base resin. If the grade is substituted with a non-formulated mLLDPE of the same density and MFR, blocking behavior and coefficient of friction may change substantially. The antiblock and slip components function as surface-active fillers and migratory additives; their distribution depends on film cooling rate, film gauge, and post-extrusion storage temperature. Published data for this specific additive package across every gauge and coextrusion configuration is limited; converters must verify blocking, coefficient of friction, optical haze, and seal performance on the actual production line.

    When the Formulated Pellet Is Subjected to Food-Contact and RoHS Compliance Requirements

    For food-contact packaging, the base olefin polymer can be assessed under 21 CFR 177.1520 in the US, but the final fabricated article must meet the applicable end-use extraction limits and any additive restrictions associated with the BUE 5502 formulation. In the European Union, plastic food-contact materials are evaluated under Regulation (EU) No 10/2011, with overall migration limits of 10 mg/dm² or 60 mg/kg depending on the food-contact surface area and packaging ratio. The presence of slip and antiblock additives may require specific migration testing if the layer is in direct food contact. The converter is responsible for generating the compliance documentation for the finished package, not merely relying on resin certification.

    Table 2 summarizes the compliance framework often cited for this product class.

    Regulation/StandardScopeVerification boundary
    21 CFR 177.1520US olefin polymer food-contactBase resin plus final article extraction
    EU 10/2011European plastic food-contact materialsOverall migration 10 mg/dm² or 60 mg/kg
    REACH (EC) 1907/2006Registration and SVHC communicationSubstance and article obligations
    RoHS 2011/65/EURestricted hazardous substancesHomogeneous material thresholds
    ISO 9001Quality management at the manufacturing siteLot traceability and release testing

    Additive interactions impose operational boundaries. The slip and antiblock package is designed for blown film to reduce blocking and control friction. Corona treatment to 38–42 mN/m is typical for print and lamination, but treated surfaces decay with time; the window between treatment and converting should be validated. Storage of formulated resin above 40 °C or in direct sunlight may increase additive migration to the pellet surface and shift slip performance. Long-term outdoor exposure is outside the intended use of this grade unless an additional UV stabilization package is supplied; the BUE 5502 designation should not be assumed to contain a hindered amine light stabilizer or carbon black dispersion.

    In coextruded frozen-food and high-speed form-fill-seal packaging, the grade is typically evaluated for the skin layer where low seal initiation and high clarity are required. A conventional Ziegler-Natta LLDPE or LDPE core can maintain bubble stability and stiffness, while the mLLDPE skin lowers seal-bar set points and improves optical appearance. Seal-bar temperature reductions of 5–15 °C relative to a Ziegler-Natta LLDPE skin are often used as an initial trial target, but the final setting must be established from seal-strength curves under ASTM F88 with the actual film gauge and dwell time. Heavy-duty sack lines can use the resin as a toughness modifier in the film core, provided the lower melt strength is managed through die gap selection, blow-up ratio, and LDPE blending. For gauges below 20 µm or above 100 µm, the published data may be limited; qualification trials should include dart impact, tear propagation, seal strength, blocking, and coefficient of friction at production throughput.